다이아몬드 Grit(흑연)/ Cu-13Sn-12Ti 필러합금 진공 브레이징 접합체의 젖음성 및 계면반응 (The wetting and interfacial reaction of vacuum brazed junction between diamond grit(graphite) and Cu-13Sn-12Ti filler alloy)

  • 함종오;;이지환
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.66-66
    • /
    • 2009
  • Various alloy system, such as Cu-Sn-Ti, Cu-Ag-Ti, and Ni-B-Cr-based alloy are used for the brazing of diamond grits. However, the problem of the adhesion strength between the diamond grits and the brazed alloy is presented. The adhesion strength between the diamond grits and the melting filler alloy is predicted by the contact angle, thereby, instead of diamond grit, the study on the wettability between the graphite and the brazing alloy has been indirectly executed. In this study, Cu-13Sn-12Ti filler alloy was manufactured, and the contact angles, the shear strengths and the interfacial area between the graphites(diamond grits) and braze matrix were investigated. The contact angle was decreased on increasing holding time and temperature. The results of shear strength of the graphite joints brazed filler alloys were observed that the joints applied Cu-13Sn-12Ti alloy at brazing temperature 940 $^{\circ}C$ was very sound condition indicating the shear tensile value of 23.8 MPa because of existing the widest carbide(TiC) reaction layers. The micrograph of wettability of the diamond grit brazed filler alloys were observed that the brazement applied Cu-13Sn-12Ti alloy at brazing temperature $990^{\circ}C$ was very sound condition because of existing a few TiC grains in the vicinity of the TiC layers.

  • PDF

다이아몬드 grit(흑연) / Cu-13Sn-12Ti 삽입금속 진공 브레이징 접합체의 젖음성 및 계면반응 (The Wetting and Interfacial Reaction of Vacuum Brazed Joint between Diamond Grit(graphite) and Cu-13Sn-12Ti Filler Alloy)

  • 함종오;이지환
    • Journal of Welding and Joining
    • /
    • 제28권3호
    • /
    • pp.49-58
    • /
    • 2010
  • Various alloy system, such as Cu-Sn-Ti, Cu-Ag-Ti, and Ni-B-Cr-based alloy are used for the brazing of diamond grits. However, the problem of the adhesion strength between the diamond grits and the brazed alloy is presented. The adhesion strength between the diamond grits and the melting filler alloy is predicted by the contact angle, thereby, instead of diamond grit, the study on the wettability between the graphite and the brazing alloy has been indirectly executed. In this study, Cu-13Sn-12Ti filler alloy was manufactured, and the contact angles, the shear strengths and the interfacial area between the graphites (diamond grits) and braze matrix were investigated. The contact angle was decreased on increasing holding time and temperature. The results of shear strength of the graphite joints brazed filler alloys were observed that the joints applied Cu-13Sn-12Ti alloy at brazing temperature $940^{\circ}C$ was very sound condition indicating the shear tensile value of 23.8 MPa because of existing the widest carbide(TiC) reaction layers. The micrograph of wettability of the diamond grit brazed filler alloys were observed that the brazement applied Cu-13Sn-12Ti alloy at brazing temperature $990^{\circ}C$ was very sound condition because of existing a few TiC grains in the vicinity of the TiC layers.

플라즈마 표면처리에 의한 Silk/PLA 바이오복합재료의 계면접착 (Interfacial Adhesion of Silk/PLA Biocomposites by Plasma Surface Treatment)

  • 추보영;권미연;이승구;조동환;박원호;한성옥
    • 접착 및 계면
    • /
    • 제5권4호
    • /
    • pp.9-16
    • /
    • 2004
  • 견섬유와 폴리라틱산(PLA) 사이의 계면접착 특성을 향상시키기 위하여 천연섬유 표면을 아르곤과 에틸렌 플라즈마로 각각 처리하였다. 플라즈마 표면처리 후, 견섬유의 표면 모폴로지와 접착이 크게 변화하였다. 다음의 여러 플라즈마 처리조건이 본 연구에 사용되었다: 10, 25, 50 그리고 150 W의 전력, 1, 3, 5, 7 그리고 10분의 처리시간 및 10과 50 sccm의 가스흐름속도, 플라즈마 처리된 Silk/PLA 바이오복합재료의 계면전단강도는 단섬유 micro-droplet debonding 시험방법으로 측정하였다. 결과는 Silk/PLA 바이오복합재료의 계면접착을 향상시키기 위한 최적의 플라즈마 처리 조건을 제공하여 주었다.

  • PDF

SBR Latex를 이용한 흙 포장의 재료특성 연구 (Study on the Effect of SBR Latex on the Properties of Soil Pavement)

  • 이상염;황성도;양성린
    • 한국도로학회논문집
    • /
    • 제16권5호
    • /
    • pp.73-82
    • /
    • 2014
  • PURPOSES : The purpose of this study is to determine the optimum addition rate of SBR latex through the evaluation of durability and strength of SBR latex applied soil pavement. Formerly used materials such as fly ash and cement in soil pavement had resulted in decreased durability due to micro crack by heat of hydration and shrinkage crack in winter. However, that agglutinated polymers help adhesion to aggregate increased comes up with preventing the crack opening when the number of capillary tubes of SBR latex get decreased in the hydration process of cement. Therefore, in this study, it is suggested that the evaluation of the field applicability of soil pavement be conducted through the performance lab test in terms of strength increment, adhesion improvement, and crack resistance based on SBR latex addition rate. METHODS : In order to evaluate the field applicability of soil pavement, SBR latex was added 0 to 3% by 1% increment, with fixed cement contents of 3% and 5%. The resistance of shear failure and crack of soil pavement were evaluated by performing the uniaxial compressive strength test and indirect tensile strength test at -20 and $20^{\circ}C$, respectively. RESULTSCONCLUSIONS : It was found out that from both tests, resistance of shear failure and crack were improved with increment of curing time, and especially more than 2% of SBR latex addition rate and 5% cement content gave better results.

초고성능 섬유보강 콘크리트로 보강된 콘크리트의 계면 전단강도 결정을 위한 경사전단 실험 (Slant Shear Test for Determining the Interfacial Shear Strength of Concrete Strengthened with Ultra-High Performance Fiber Reinforced Concrete)

  • 임우영;홍성걸
    • 콘크리트학회논문집
    • /
    • 제28권6호
    • /
    • pp.637-646
    • /
    • 2016
  • 이 연구에서는 강섬유 보강 초고성능 콘크리트(Ultra-high performance fiber reinforced concrete, 이하 UHPFRC)로 보강된 콘크리트 계면에서의 전단강도 평가를 위한 경사전단실험을 수행하였다. 실험변수는 면처리 유무와 콘크리트 강도, 그리고 UHPFRC의 강섬유 혼입률이다. 콘크리트의 계면은 숏블라스팅으로 면처리되었다. 실험결과, 숏블라스팅으로 면처리된 실험체의 계면 전단강도는 매끄러운 표면을 가진 실험체의 부착강도에 비해 매우 크게 나타났으며, 거친면을 만들기 위한 숏블라스팅 방법은 매우 효과적인 방법인 것으로 나타났다. 숏블라스팅으로 표면처리를 할 경우, 전단마찰 철근이 없더라도 콘크리트 계면에서 저항하는 전단강도는 현행 기준에서 제시하고 전단강도 상한값을 초과하는 것으로 나타났다. 기존의 콘크리트와 UHPFRC 사이의 전단마찰 설계는 전단마찰 철근의 유무와 상관없이 현행 콘크리트 구조기준을 사용해도 무방할 것으로 판단된다. 다만, 면처리를 하지 않은 경우에는 적절한 전단 보강재가 추가 설치하여야 할 것이다.

Shear bond strength of resin cement to an acid etched and a laser irradiated ceramic surface

  • Kursoglu, Pinar;Karagoz Motro, Pelin Fatma;Yurdaguven, Haktan
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권2호
    • /
    • pp.98-103
    • /
    • 2013
  • PURPOSE. To evaluate the effects of hydrofluoric acid etching and Er,Cr:YSGG laser irradiation on the shear bond strength of resin cement to lithium disilicate ceramic. MATERIALS AND METHODS. Fifty-five ceramic blocks ($5mm{\times}5mm{\times}2mm$) were fabricated and embedded in acrylic resin. Their surfaces were finished with 1000-grit silicon carbide paper. The blocks were assigned to five groups: 1) 9.5% hydrofluoric-acid etching for 60 s; 2-4), 1.5-, 2.5-, and 6-W Er,Cr:YSGG laser applications for 60 seconds, respectively; and 5) no treatment (control). One specimen from each group was examined using scanning electron microscopy. Ceramic primer (Rely X ceramic primer) and adhesive (Adper Single Bond) were applied to the ceramic surfaces, followed by resin cement to bond the composite cylinders, and light curing. Bonded specimens were stored in distilled water at $37^{\circ}C$ for 24 hours. Shear bond strengths were determined by a universal testing machine at 1 mm/min crosshead speed. Data were analyzed using Kruskal-Wallis and Mann-Whitney U-tests (${\alpha}$=0.05). RESULTS. Adhesion was significantly stronger in Group 2 ($3.88{\pm}1.94$ MPa) and Group 3 ($3.65{\pm}1.87$ MPa) than in Control group ($1.95{\pm}1.06$ MPa), in which bonding values were lowest (P<.01). No significant difference was observed between Group 4 ($3.59{\pm}1.19$ MPa) and Control group. Shear bond strength was highest in Group 1 ($8.42{\pm}1.86$ MPa; P<.01). CONCLUSION. Er,Cr:YSGG laser irradiation at 1.5 and 2.5 W increased shear bond strengths between ceramic and resin cement compared with untreated ceramic surfaces. Irradiation at 6 W may not be an efficient ceramic surface treatment technique.

열 충격에 따른 탄소 직물 복합재료의 역학적 특성 평가 (Evaluation of Mechanical Properties of Carbon Fabrics Composite with Thermal Shock)

  • 김재홍;이중호;정경호;강태진
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2005년도 추계학술발표대회 논문집
    • /
    • pp.79-82
    • /
    • 2005
  • In this study, mechanical properties of carbon fabrics composite under the thermal shock cycling were evaluated. Due to the interactions between fiber and polymer matrix, it is reasonable to conclude that both thermal cycles of thermal shock result in improvement of interlaminar shear strength(ILSS) for the longer conditioning time duration. The rise in ILSS may be attributed to the improved adhesion by cryogenic compressive stress and also by the post-curing strengthening effect. However, the flexural and tensile strength were decreased with increasing conditioning time of thermal cycle.

  • PDF

Temporary Bonding and Debonding 공정용 UV 경화형 접착 소재의 코팅 두께에 따른 물성 및 경화거동 (Properties and Curing Behaviors of UV Curable Adhesives with Different Coating Thickness in Temporary Bonding and Debonding Process)

  • 이승우;이태형;박지원;박초희;김현중
    • 한국정밀공학회지
    • /
    • 제31권10호
    • /
    • pp.873-879
    • /
    • 2014
  • UV curable adhesives with different acrylic functionalities were synthesized for temporary bonding and debonding process in 3D multi-chip packaging process. The aim is to study various factors which have an influence on UV curing. The properties and curing behaviors were investigated by gel fraction, peel strength, probe tack, and shear adhesion failure temperature. The results show that the properties and curing behaviors are dependent on not only acrylic functionalities of binders but also UV doses and coating thickness.

양극산화 처리에 따른 탄소섬유 표면의 페놀릭 하이드록실 관능기 비율의 증가가 에폭시기지 복합재료의 기계적 계면결합 특성에 미치는 영향 (Effects of Increase in Ratio of Phenolic Hydroxyl Function on Carbon Fiber Surfaces by Anodic Oxidation on Mechanical Interfacial Bonding of Carbon Fibers-reinforced Epoxy Matrix Composites)

  • 김동규;김관우;한웅;송범근;오상엽;방윤혁;김병주
    • 공업화학
    • /
    • 제27권5호
    • /
    • pp.472-477
    • /
    • 2016
  • 본 연구에서는 전류밀도 변화에 따른 탄소섬유의 양극산화 처리가 탄소섬유 표면과 탄소섬유 강화 복합재료의 기계적 계면결합력에 미치는 영향을 고찰하였다. 양극산화 처리된 탄소섬유 표면 특성은 원자간력 현미경(Atomic force microscope, AFM)과 전계방사형 주사전자현미경(Field emission-scanning electron microscope, FE-SEM), 적외선 분광법(Fourier transform infrared spectroscopy, FT-IR) 및 X선 광전자 분광법(X-ray Photoelectron Spectroscopy, XPS)으로 분석하였으며, Short beam 전단시험을 통해 표면처리에 따른 탄소섬유 강화 복합재료의 계면 전단강도를 측정하였다. 실험 결과 전류밀도가 증가함에 따라 탄소섬유 표면의 거칠기와 산소관능기의 함량의 증가와, 탄소섬유 강화 복합재료의 층간전단강도(Interlaminar shear strength, ILSS)의 향상 및 페놀릭 하이드록실 그룹과의 비례관계를 확인하였다. CF-2.0 시편의 층간전단강도는 87.9 MPa로 CF-AS 시편에 비해 약 4% 증가하였는데, 이러한 결과는 양극산화 처리가 산소관능기와 탄소섬유 표면 거칠기의 증가를 유도하여 탄소섬유와 수지의 계면 결합력이 증가된 것으로 판단된다. 그중 층간전단강도와 비례관계인 페놀릭 하이드록실 그룹은 탄소섬유 강화 복합재료의 계면결합력을 향상시키는 중요한 요소라 판단된다.

낙동강 실트질 모래의 불포화 전단강도특성 (Unsaturated shear strength characteristics of Nak-dong River silty-sand)

  • 차봉근;김영수;박성식;신지섭
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2010년도 추계 학술발표회 2차
    • /
    • pp.53-60
    • /
    • 2010
  • The natural soils are classified in saturated soils and unsaturated soils according to level of ground water but the research for only saturated soils has been conducted by this time. However, there are many proble.ms which are not solved by using the concept and principle of saturated soils on the natural soils. In fact, it is known that unsaturated soils represent the behavior characteristic unlike completely saturated soils because of the adhesion under the influence of negative pore water pressure, the high angle of friction and the low water permeability by the air entry. So it needs to conduct the various researches on insufficient unsaturated soils. In this paper, unsaturated triaxial compressive tests are conducted in order to do research on shear strength characteristic on sands and silty sands of Nakdong river. As a result of the tests, the cohesion is increased in non-linear type according to the change of the matric suction, but the angle of internal friction is not changed much.