• Title/Summary/Keyword: Off-axis sputtering

Search Result 19, Processing Time 0.017 seconds

Crystallized Indium Tin Oxide Thin Films at a Low Temperature on Polymer Substrate by Off-axis RF Magnetron Sputtering

  • Choe, Hyeong-Jin;Jeong, Hyeon-Jun;Yun, Sun-Gil
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.10a
    • /
    • pp.22.1-22.1
    • /
    • 2011
  • In this study, off-axis RF magnetron sputtering was used for the crystallized ITO thin films at a low temperature of about $120^{\circ}C$ instead of the conventional RF sputtering because the off-axis sputtering can avoid the damage for the plasma as well as fabrication of thin films with a high quality. The structural, optical and electrical properties of the obtained films depending on deposition parameters, such as sputtering power, gas flow and working pressure, have been investigated. The ITO thin films grown on PET substrate at $120^{\circ}C$ were crystallized with a (222) preferred orientation. 100-nm thick ITO films showed a resistivity of about $4.2{\times}10^{-4}{\Omega}-cm$ and a transmittance of about 81% at a wavelength of 550nm. The transmittance of the ITO thin films by an insertion of $SiO_2$ thin films on ITO films was improved.

  • PDF

Characterization of the Crystallized ITO Thin Films Grown at a Low Temperature by Off-axis RF Magnetron Sputtering (Off-axis RF 마그네트론 스퍼터링법을 이용하여 저온에서 결정화된 ITO 박막의 특성)

  • Choi, Hyung-Jin;Jung, Hyun-June;Hur, Sung-Gi;Yoon, Soon-Gil
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.2
    • /
    • pp.126-130
    • /
    • 2011
  • In this study, off-axis magnetron sputtering was used for the crystallized ITO thin films at a low temperature of about $120^{\circ}C$ instead of the conventional RF sputtering because the off-axis sputtering can avoid the damage for the plasma as well as fabrication of thin films with a high quality. The ITO thin films grown on PET substrate at $120^{\circ}C$ were crystallized with a (222) preferred orientation. 58-nm thick ITO films showed a resistivity of about $2{\times}10-4{\Omega}{\cdot}cm$ and a transmittance of about 75% at a wavelength of 550 nm. The transmittance of the ITO thin films by an insertion of SiO2 thin films on ITO films was improved.

Characterization of the Crystallized ITO Thin Films Grown at Different Temperatures by Off-axis RF Magnetron Sputtering (유연성 기판 위에 증착된 ITO 박막의 공정 온도에 따른 전기적·광학적 특성 평가)

  • Choi, Hyung-Jin;Yoon, Soon-Gil
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.26 no.5
    • /
    • pp.397-400
    • /
    • 2013
  • Off-axis magnetron sputtering was used for the crystallized ITO thin films deposition at various temperatures from 25 to $120^{\circ}C$. The ITO thin films were crystallized at $50^{\circ}C$ for Si (001) substrates and at $75^{\circ}C$ for PET substrate. The ITO thin films grown onto PET substrate at $120^{\circ}C$ were crystallized with a (222) preferred orientation. The 160-nm thick ITO films showed a resistivity of about $7{\times}10^{-4}{\Omega}{\cdot}cm$ and a transmittance of about 84% at a wavelength of 550 nm. Off-axis sputtering can be applied for low temperature crystallization of the ITO films.

Characterization of ZTO Thin Films Transistor Deposited by On-axis Sputtering and Facing Target Sputtering(FTS) (On-axis 스퍼터링과 FTS 공정으로 증착한 ZTO 박막트랜지스터의 특성)

  • Lee, Se-Hee;Yoon, Soon-Gil
    • Korean Journal of Materials Research
    • /
    • v.26 no.12
    • /
    • pp.676-680
    • /
    • 2016
  • We have investigated the properties of thin film transistors(TFT) fabricated using zinc tin oxide(ZTO) thin films deposited via on-axis sputtering and FTS methods. ZTO thin films deposited by FTS showed lower root-mean-square(RMS) roughness and more uniformity than those deposited via on-axis sputtering. We observed enhanced electrical properties of ZTO TFT deposited via FTS. The ZTO films were deposited at room temperature via on-axis sputtering and FTS. The as-deposited ZTO films were annealed at $400^{\circ}C$. The TFT using the ZTO films deposited via FTS process exhibited a high mobility of $12.91cm^2/V.s$, a low swing of 0.80 V/decade, $V_{th}$ of 5.78 V, and a high $I_{on/off}$ ratio of $2.52{\times}10^6$.

Growth of Heteroepitaxial ZnO Thin Film by Off-axis RF Magnetron Sputtering (Off-axis 고주파 마그네트론 스퍼터링법을 이용한 이종에피텍셜 ZnO 박막 성장)

  • 박재완;박종완;이전국
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.3
    • /
    • pp.262-267
    • /
    • 2003
  • The heteroepitaxial ZnO thin film on sapphire (0001) substrate was prepared by an off-axis Radio Frequency(RF) magnetron sputtering. The crystallinity of ZnO thin film was affected by deposition pressure, RF power, and substrate temperature. High quality heteroepitaxial ZnO thin film was obtained when the kinetic energy of sputtered particles is well harmonized with the surface mobility. In the result of Photoluminescence(PL) of heteroepitaxial ZnO thin film, Ultraviolet(UV) emissions at 3.36 and 3.28 eV were observed at low(17 K) and Room Temperature(RT). respectively. As the ZnO thin film was annealed in O$_2$ambient, the crystallinity was improved while UV emission was drastically decreased.

Study on the Formation of Superconducting Phases of $Bi_2Sr_2Ca_2Cu_3O_x$ Thin Films Prepared by Off-axis Sputtering (Off-axis Sputtering 방법으로 제조한 $Bi_2Sr_2Ca_2Cu_3O_x$ 박막의 초전도상 생성에 관한 연구)

  • 심창훈;양우석;제정호
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.7
    • /
    • pp.715-722
    • /
    • 1994
  • Off-axis supttering using shielder was used to efficiently prevent negative oxygen ions from resputtering deposited films. In this method, the substrate was located vertically to the target and shielded by the semicircled steel plate. By using this method, the resputtering could be reduced, and 2223 high-Tc phase could be formed at the lower substrate temperature and in the broader temperature region. As increasing the substrate temperature, 2212, 2223, 2212 superconducting phases were formed by turns. 2223 phase was formed above 2$\times$10-2 torr, and 2212 phase was formed above 4$\times$10-2 torr.

  • PDF

Fabrication of High-Tc Superconducting $YBa_2Cu_3O_{7-x}$ Thin Films by Off-Axis RF Magnetron Sputtering (Off-Axis RF 마그네트론 스퍼터링에 의한 $YBa_2Cu_3O_{7-x}$ 고온 초전도 박막의 제조)

  • 성건용;서정대;강광용;장순호
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.3
    • /
    • pp.243-251
    • /
    • 1991
  • High-Tc YBa2Cu3O7-x superconducting thin films have been prepared by single-target off-axis RF magnetron sputtering. Optimal ratio of Y : Ba : Cu of the single-target was determined as 1 : 1.65 : 3.35 in order to obtain the stoichiometric films. Tc, crystalline phase, and microstructures of the surface and cross-section of the ex-situ YBa2Cu3O7-x thin films on MgO(100) had a Tc, zero of 80K, and the films on LaAlO3/Si had a Tc, on-set of 90 K and a Tc, zero of 70 K.

  • PDF

Preparation of $Ba_{0.5}Sr_{0.5}TiO_3$ Thin Films by Off-Axis RF Magnetron Sputtering (Off-Axis RF Magnetron Sputtering 방법에 의한 $Ba_{0.5}Sr_{0.5}TiO_3$ 박막의 제조)

  • Shin, Jin;Hahn, Taek-Sang;Kim, Young-Hwan;Lee, Jae-Jun;Park, Soon-Ja;Oh, Myung-Hwan;Choi, Sang-Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1429-1436
    • /
    • 1994
  • We have prepared Ba0.5Sr0.5TiO3 thin films on Si substrate without buffer layer. Deposition was carried out by off-axis rf magnetron sputtering method using Ba0.5Sr0.5TiO3 stoichiometric target. The substrate temperature was changed from 40$0^{\circ}C$ to $700^{\circ}C$ during deposition. As the substrate temperature increased, relative intensity of (110) peak increased up to $600^{\circ}C$, however preferred orientation changed from (110) to (h00) beyond $650^{\circ}C$ of substrate temperature. Deposited films showed microstructures with fine grains whose diameters are less than 100 nm, and columnar structure was observed in the cross-sectional SEM micrograph. AES depth profile showed no significant diffusion at the interfacial reaction area. The effective dielectric constant of films showed maximum value at $600^{\circ}C$, and the leakage current increased with increasing substrate temperature, which may be ascribed to the crystallization of amorphous phases at grain boundary.

  • PDF