• Title/Summary/Keyword: sCR1

Search Result 1,395, Processing Time 0.025 seconds

Spherical Indentation Testing to Evaluate Mechanical Properties In 1Cr-1Mo-0.25V Steel (Spherical Indentation Testing에 의한 1Cr-1Mo-0.25V 강의 기계적 물성 평가)

  • Lee, J.M.;Nam, Y.H.;Nham, S.H.;Lee, S.S.;Lee, O.S.
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.266-271
    • /
    • 2001
  • Spherical indentation technique was developed to evaluate the flow properties of metallic materials in carbon steel, stainless steel and alloys, etc. Through the spherical indentation test, differently degraded 1Cr-1Mo-0.25V steel's mechanical properties were observed and compared with conventional standard test data. The flow properties of 1Cr-1Mo-0.25V steels were estimated by analyzing the indentation load-depth curve. To characterize the flow property, we used material yield slope and constraint factor index rather than strain-hardening exponent because the variation of strain-hardening exponent was very little and the data showed irregularly. And the constraint factor's effect was small when the material yield slope was taken into account.

  • PDF

Reduction Efficiency of Cr(VI) in Aqueous Solution by Different Sources of Zero-Valent Irons (수용액 중 영가 철(Zero-Valent Iron)의 특성에 따른 Cr(VI)의 환원 효율 비교)

  • Yang, Jae-E.;Kim, Jong-Sung;Ok, Yong-Sik;Yoo, Kyung-Yoal
    • Korean Journal of Environmental Agriculture
    • /
    • v.24 no.3
    • /
    • pp.203-209
    • /
    • 2005
  • Objective of this research was to assess the effectiveness of the different sources of the zero-valent irons (ZVIs) on the reduction of the toxic Cr(VI) to the nonhazardous Cr(III) in an aqueous solution. The physical and chemical properties of the six ZVIs were determined. Particle size and specific surface area of the ZVIs were in the ranges of $85.55{\sim}196.46{\mu}m\;and\;0.055{\sim}0.091m^2/g$, respectively. Most of the ZVIs contained Fe greater than 98% except for J (93%) and PU (88%). Reduction efficiencies of the ZVI for Cr(VI) reduction were varied with kinds of ZVIs. The J and PU ZVIs reduced 100% and 98% of Cr(VI) in the aqueous solution, respectively, within 3 hrs of reaction. However, PA, F, Sand J1 reduced 74, 65, 29 and 11% of Cr(VI), respectively, after 48 hrs. The pH of the reacting solution was rapidly increased from 3 to $4.34{\sim}9.04$ within 3 hrs. The oxidation-reduction potential (Eh) of the reacting solution was dropped from 600 to 319 mV within 3 hrs following addition of ZVIs to the Cr(VI) contaminated water. The capability of ZVIs for Cr(VI) reduction was the orders of PU > J > PA > F > S > J1, which coincided with the capacities to increase the pH and decrease the redox potentials. Results suggested that the reduction of Cr(VI) to Cr(III) was derived from the oxidation of the ZVI in the aqueous solution.

CONTACT THREE CR-SUBMANIFOLDS OF A (4m + 3)-DIMENSIONAL UNIT SPHERE

  • Kim, Hyang-Sook;Kim, Young-Mi;Kwon, Jung-Hwan;Pak, Jin-Suk
    • Journal of the Korean Mathematical Society
    • /
    • v.44 no.2
    • /
    • pp.373-391
    • /
    • 2007
  • We study an (n+3)($n\;{\geq}\;7-dimensional$ real submanifold of a (4m+3)-unit sphere $S^{4m+3}$ with Sasakian 3-structure induced from the canonical quaternionic $K\"{a}hler$ structure of quaternionic (m+1)-number space $Q^{m+1}$, and especially determine contact three CR-submanifolds with (p-1) contact three CR-dimension under the equality conditions given in (4.1), where p = 4m - n denotes the codimension of the submanifold. Also we provide necessary conditions concerning sectional curvature in order that a compact contact three CR-submanifold of (p-1) contact three CR-dimension in $S^{4m+3}$ is the model space $S^{4n_1+3}(r_1){\times}S^{4n_2+3}(r_2)$ for some portion $(n_1,\;n_2)$ of (n-3)/4 and some $r_1,\;r_2$ with $r^{2}_{1}+r^{2}_{2}=1$.

A Study of Quality Control Environment of Mammography (유방촬영의 화질관리 환경에 대한 고찰)

  • Hwang, In-Sun;Kim, Young-Keun;Joo, Hyung-Yoon
    • Korean Journal of Digital Imaging in Medicine
    • /
    • v.12 no.2
    • /
    • pp.133-138
    • /
    • 2010
  • The purpose of this study was to survey and test quality control of mammography system. The conclusion of this study is as follows ; First, The rate of pass for phantom image test shows that Film-Screen mammography system(F/S) and computed mammography system(CR) is 80%, Indirect digital mammography system(DR) is 100%. Second, The test of exposure dose shows that F/S is 921 mR. CR is 1,140 mR, DR is 474 mR. The grade of this testament is CR > F/S > DR. Third, The test of average glandular dose shows that F/S is 1,336 mGy, CR is 1,635 mGy, DR is 1,26 mGy. The grade of this testament is CR > F/S > DR. Fourth, The testament of resolution shows as follows F/S is 11~13 Lp/mm, CR is 4~5 Lp/mm, and DR is 5~7 Lp/mm(F/S > DR > CR) Fifth, The survey of projection, cassette, development and reading shows that user are indifference.

  • PDF

High Temperature Corrosion of Cr(III) Coatings in N2/0.1%H2S Gas

  • Lee, Dong Bok;Yuke, Shi
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.3
    • /
    • pp.111-116
    • /
    • 2019
  • Chromium was coated on a steel substrate by the Cr(III) electroplating method, and corroded at $500-900^{\circ}C$ for 5 h in $N_2/0.1%H_2S-mixed$ gas to study the high-temperature corrosion behavior of the Cr(III) coating in the highly corrosive $H_2S-environment$. The coating consisted of (C, O)-supersaturated, nodular chromium grains with microcracks. Corrosion was dominated by oxidation owing to thermodynamic stability of oxides compared to sulfides and nitrides. Corrosion initially led to formation of the thin $Cr_2O_3$ layer, below which (S, O)-dissolved, thin, porous region developed. As corrosion progressed, a $Fe_2Cr_2O_4$ layer formed below the $Cr_2O_3$ layer. The coating displayed relatively good corrosion resistance due to formation of the $Cr_2O_3$ scale and progressive sealing of microcracks.

Sargassum confusum for Biosorption of Pb and Cr (알송이 모자반, Sargassum confusum을 이용한 Pb 및 Cr의 생물학적 흡착 및 탈착)

  • SUH Kuen-Hack;ANN Kab-Hwan;CHO Moon-Chul;CHO Jin-Koo;JIN Hyung-Joo;HONG Yong-Ki
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.34 no.1
    • /
    • pp.1-6
    • /
    • 2001
  • Biosorption of Pb and Cr by Sargassum confusum was evaluatet at in the various conditions. The uptake capacities for Pb and Cr were 197.5 mg Pb/g biomass and 133.1 mg Cr/g biomass, respectively. The adsorption parameters for Pb and Cr were determined according to the Langmuir and Freundlich model. Biosorption of Pb and Cr was increased with the increase of pH value. Pb and Cr adsorbed by S. confusum could be recovered by desorption process with 0.1 M HCl, 0.1 M $HNO_3$ and 0.1 M EDTA. The ratio of Pb desorption was above $93\%$, whereas the ratio of Cr desorption was below $30\%$.

  • PDF

MULTIPLIER IDEALS ON CR MANIFOLDS

  • Ryu, Jeong Seog
    • Journal of the Chungcheong Mathematical Society
    • /
    • v.16 no.1
    • /
    • pp.103-112
    • /
    • 2003
  • We consider multiplier ideals on CR manifolds, which is associated to Kiremidjian's work on CR embedding problem. Similar to the Kohn's result, we found that the multipliers form a nontrivial radical ideal.

  • PDF

Corrosion of Fe-(8.5~36.9) wt% Cr Alloys at 600~800℃ in (N2, H2S, H2O)-Mixed Gases (Fe-(8.5~36.9) wt% Cr합금의 600~800℃, (N2,H2S,수증기)-혼합 가스분위기에서의 부식)

  • Kim, Min Jung;Lee, Dong Bok
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.3
    • /
    • pp.218-223
    • /
    • 2012
  • Fe-(8.5, 18.5, 28.3, 36.9) wt% Cr alloys were corroded between 600 and $800^{\circ}C$ for up to 70 h in a 1 atm gas mixture that consisted of 0.0242 atm of $H_2S$, 0.031 atm of water vapor, and 0.9448 atm of nitrogen gas. Their corrosion resistance increased with an increment in the Cr content. The Fe-8.5%Cr alloy corroded fast, forming thick, fragile, nonadherent scales that consisted primarily of an outer FeS layer and an inner (Fe, Cr, O, S)-mixed layer. The outer FeS layer grew into the air by the outward diffusion of $Fe^{2+}$ ions, whereas the inner mixed layer grew by the inward diffusion of oxygen and sulfur ions. At the interface of the outer and inner scales, voids developed and cracking occurred. The Fe-(18.5, 28.3, 36.9)% Cr alloys displayed much better corrosion resistance than the Fe-8.5Cr alloy, because thin $Cr_2O_3$ or $Cr_2S_3$ scales formed.

The Study of Hyperfine Fields for Co0.9Zn0.1Cr1.9857Fe0.02O4 (Co0.9Zn0.1Cr1.9857Fe0.02O4 물질의 초미세자기장 연구)

  • Choi, Kang-Ryong;Kim, Sam-Jin;Kim, Chul-Sung
    • Journal of the Korean Magnetics Society
    • /
    • v.18 no.1
    • /
    • pp.39-42
    • /
    • 2008
  • [ $AB_2X_4$ ](A, B=Transition Metal, X=O, S, Se) are cubic spinel normal ferrimagnets, in which M ions occupy the tetrahedral sites and Cr ions occupy the octahedral sites. Recently, they have been investigated for behaviour of B site ions and A-B interaction. Polycrystalline $[Co_{0.9}Zn_{0.1}]_A[Cr_{1.98}{^{57}Fe_{0.02}}]_BO_4$ compound was prepared by wet-chemical process. The ferrimagnetic transition was observed around 90K. $M\"{o}ssbauer$ absorption spectra at 4.2K show that the well-developed two sextets are superposed with small difference in hyperfine fields($H_{hf}$). The hyperfine fields of $CoCr_{1.98}{^{57}Fe_{0.02}}O_4$ and $Co_{0.9}Zn_{0.1}Cr_{1.98}{^{57}Fe_{0.02}}O_4$ were determined to be 488, 478 kOe and 486, 468 kOe, respectively. We notice that the one of the magnetic hyperfine field values changes with Zn ion substitution. These results suggest the incommensurate states and spin-reorientation temperature($T_S=18K$) changes with Zn ions substitution below spin-reorientation temperature($T_S=28K$) of $CoCr_{1.98}{^{57}Fe_{0.02}}O_4$

ON CONTACT THREE CR SUBMANIFOLDS OF A (4m + 3)-DIMENSIONAL UNIT SPHERE

  • Kwon, Jung-Hwan;Pak, Jin--Suk
    • Communications of the Korean Mathematical Society
    • /
    • v.13 no.3
    • /
    • pp.561-577
    • /
    • 1998
  • We study (n+3)-dimensional contact three CR submanifolds of a Riemannian manifold with Sasakian three structure and investigate some characterizations of $S^{4r+3}$(a) $\times$ $S^{4s+3}$(b) ($a^2$$b^2$=1, 4(r + s) = n - 3) as a contact three CR sub manifold of a (4m+3)-dimensional unit sphere.

  • PDF