• Title/Summary/Keyword: Titanate powder

Search Result 99, Processing Time 0.03 seconds

The Properties of Vibration Absorption according to the Diameter of Fiberous $BaTiO_3$ Powder (섬유상 $BaTiO_3$의 분말 직경에 따른 흡진 특성)

  • Seo, Yong-Gyo
    • Korean Journal of Materials Research
    • /
    • v.4 no.1
    • /
    • pp.3-8
    • /
    • 1994
  • Recently, sound and mechanical vibration are becoming important problems in our life. In the present study, the measurement of vibration absorption characteristics of barium titanate ceramics and the investigation of its relationship to microstructures were carried out. The barium titanate ceramics is expected to be better vibration absorption material owing to its chemical and physical stability than other conventional vibration absorbers like glasswool board. Barium titanate ceramics were prepared by sintering fiberous $BaTiO_{3}$ crystallites in order to enhance the vibration absorption characteristics. The fiberous $BaTiO_{3}$ ceramics were prepared through the ionic exchange after the preparation of fiberous $K_2Ti_4O_9$ with 0.2$\mu\textrm{m}$, 1.2$\mu\textrm{m}$, 2.0$\mu\textrm{m}$, diameter length by KDC method. The fiberous crystallites were oriented in a plane perpendicular to the press direction and sintered. The investigation of the grain diameters of the sintered ceramics, equivalent factor, electromechanical coupling factor($k_1$), and the generated voltage(V) shows that the grain's diameter decreases with the increase of the diameter of the used fiberous crystallites. The vibration absorption increases the crystallites' diameter. That means that the vibration absorption increases with the internal friction of grain boundary. Which was identified by the investigation of the equivallent circuit.

  • PDF

Hydrothermal Synthesis and Characterization of BaTiO3 Fine Powders (BaTiO3 미세 분말의 수열합성 및 특성분석)

  • Park, Jung-Hoon;Park, Sangdo
    • Korean Chemical Engineering Research
    • /
    • v.45 no.5
    • /
    • pp.448-454
    • /
    • 2007
  • Hydrothermal synthesis was conducted with starting material as Barium hydroxide and hydrous titania ($TiO_2{\cdot}xH_2O$) to obtain barium titanate fine Powder. The conversion, crystal structure and properties of as-prepared powder were investigated according to reaction temperature, time and concentration. The effect of variables on conversion was in order of time < temperature < concentration and the maximum conversion reached to 99.5% in the case of hydrothermal synthesis at $180^{\circ}C$ for 2 h with 2.0 M reactant concentration. At low concentration such as 0.25 M, formation of unreacted $BaCO_3$ and $TiO_2$ was not inevitable at even high reaction temperature and these components converted into $BaTi_2O_5$ at high temperature and remained as impurity. As concentration of reactant increased, the size of as-synthesized $BaTiO_3$ powder deceased and Ba/Ti molar ratio approached into 1, showing Ba/Ti ratio of $1{\pm}0.005$ for reaction at $180^{\circ}C$ for 2 h with 2.0 M concentration.

The Synthesis of Eu3+ Doped with TiO2 Nano-Powder and Application as a Pesticide Sensor

  • Yao, Fei;Sun, Yang;Tan, Chunlei;Wei, Song;Zhang, Xiaojuan;Hu, Xiaoyun;Fan, Jun
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.6
    • /
    • pp.932-935
    • /
    • 2011
  • Using tetrabutyl titanate as precursor, $Eu^{3+}$ doped $TiO_2$ nano-powder was prepared by sol-gel method, the nature of luminescence of nano-powder was studied. The interaction of chlorpyrifos with $Eu^{3+}$ doped $TiO_2$ was studied by absorption and fluorescence spectroscopy. The results indicated the fluorescence intensity of $Eu^{3+}$ doped $TiO_2$ was quenched by chlorpyrifos and the quenching rate constant ($k_q$) was $1.24{\times}10^{11}\;L/mol{\cdot}s$ according to the Stern-Volmer equation. The dynamics of photoinduced electron transfer from chlorpyrifos to conduction band of $TiO_2$ nanoparticle was observed and the mechanism of electron transfer had been confirmed by the calculation of free energy change (${\Delta}G_{et}$) by applying Rehm-Weller equation as well as energy level diagram. A new rapid method for detection of chlorpyrifos was established according to the fluorescence intensity of $Eu^{3+}$ doped $TiO_2$ was proportional to chlorpyrifos concentration. The range of detection was $5.0{\times}10^{-10}-2.5{\times}10^{-7}mol/L$ and the election limit ($3{\sigma}$) was $3.2{\times}10^{-11}$ mol/L.

Electrical properties of piezoelectric PZT thick film by aerosol deposition method (에어로졸 증착법에 의한 압전 PZT 후막의 전기적 특성)

  • Kim, Ki-Hoon;Bang, Kook-Soo;Park, Dong-Soo;Park, Chan
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.25 no.6
    • /
    • pp.239-244
    • /
    • 2015
  • Lead zirconate titanate (PZT) thick films with thickness of $10{\sim}20{\mu}m$ were fabricated on silicon substrate by aerosol deposition method. As-deposited films on silicon were annealed at the temperatures of $700^{\circ}C$. The electrical properties of films deposited by PZT powders were characterized using impedance analyzer and Sawyer-Tower circuit. The PZT powder was prepared by both conventional solid reaction process and sol-gel process. The remanent polarization, coercive field, and dielectric constant of the $10{\mu}m$ thick film with solid reaction process were $20{\mu}C/cm^2$, 30 kV/cm and 1320, respectively. On the other hand, the PZT films by sol-gel process showed a poor dielectric constant of 635. The reason was probably due to the presence of pores produced from organic residue during annealing.

Titanate Nanotube Formation and Nanostructure Development from the Reaction of TiO2 Nanopowder and Alkalihydroxide (TiO2 나노분말과 수산화알칼리와의 반응으로부터 티탄산 나노튜브의 형성과 나노구조의 전개)

  • Jin, Eun-Ju;Riu, Doh-Hyung;Huh, Seung-Hun;Kim, Chang-Yeoul;Hwang, Hae-Jin
    • Journal of Powder Materials
    • /
    • v.15 no.2
    • /
    • pp.125-135
    • /
    • 2008
  • [ $TiO_2$ ] nanotubes for photocatalytic application have been synthesized by hydrothermal method. $TiO_2$ nanotubes are formed by washing process after reaction in alkalic solution. Nanotubes with different morphology have been fabricated by changing NaOH concentration, temperature and time. $TiO_2$ nanoparticles were treated inside NaOH aqueous solution in a Teflon vessel at $110^{\circ}C$ for 20 h, after which they were washed with HCl aqueous solution and deionized water. Nanotube with the most perfect morphology was formed from 0.1 N HCl washing treatment. $TiO_2$ nanotube was also obtained when the precursor was washed with other washing solutions such as $NH_4OH$, NaCl, $K_2SO_4$, and $Na_2SO_3$. Therefore, it was suggested that $Na^+$ ion combined inside the precursor compound slowly comes out from the structure, leaving nanosheet morphology of $TiO_2$ compounds, which in turn become the nanotube in the presence of hydroxyl ion. To stabilize the sheet morphology, the different type of washing treatment solution might be considered such as amine class compounds.

Glycothermal synthesis and characterization of $BaTiO_3$ glycolate (Glycothermal법에 의해 제조된 $BaTiO_3$ glycolate의 특성)

  • Kil, Hyun-Sig;Amar, Badrakh;Lim, Dae-Young
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.286-287
    • /
    • 2006
  • Barium titanate ($BaTiO_3$) glycolate particles were synthesized at temperature as low as $100^{\circ}C$ through glycothermal reaction by using $Ba(OH)_2{\cdot}8H_2O$ and amorphous titanium hydrous gel as precursors and ethylene glycol as solvent. The particle size and morphology of $BaTiO_3$ glycolate powders can be controlled by varying the reaction conditions such as the reaction temperature and Ba:Ti molar ratio of starting precursors. After glycothermal treatment at $220^{\circ}C$ for 24 h in 1.25:1(Ba:Ti), the average particle size of the $BaTiO_3$ glycolate powder was about 200-400 nm and low agglomeration. $BaTiO_3$ powders were formed by heat-treating the glycolate powder in air at $500-1000^{\circ}C$. As a result, the size of $BaTiO_3$ crystallites changed from around 50-300 nm. It is also demonstrated that the size and shape of $BaTiO_3$ particles investigated as a function of calcination temperature. The $BaTiO_3$ particles obtained from optimum synthesis condition were pressed, sintered and measured for the dielectric property. The $BaTiO_3$ ceramics sintered at $1250^{\circ}C$ for 2 h had 98 % of theoretical density. The ceramics have an average grain size of about $1\;{\mu}m$ and displays the high dielectric constant (~3100) and low dielectric loss (<0.1) at room temperature.

  • PDF

The Photocatalytic Activity of $TiO_2$ Powder Prepared by Sol-Gel Method (Sol-Gel법으로 제조한 $TiO_2$의 광촉매 활성도)

  • Kim, Dong-Hyeong;Lee, Tae-Gyu;Kim, Gwang-Bok;Lee, Seung-Won
    • Korean Journal of Materials Research
    • /
    • v.6 no.3
    • /
    • pp.282-290
    • /
    • 1996
  • 광화학 반응의 초기 유발을 위한 광촉매로 TiO2가 가장 널리 알려져 있으며, 기존의 상품보다 광촉매 활성도가 높은 촉매를 얻기 위해 Sol-Gel법을 이용하였다. TiO2 광촉매 제조를 위하여 전구체로서 Tetra-eth해-ortho-titanate(TEOT)를 이용하여 xerogeol 분말을 얻었으며, 광화학 반응의 효율을 측정하기 위해 분해대상 물질을 Dichloroacetic acid(DCA)로 선정하였다. 순수 titania 졸을 얻기 위한 최적조건은 알콕사이드 1몰당 물 40몰, 산 0.05몰이었고 pH의 범위는 3.3-3.6이었으며 Hexylene Glycol(HG)의 첨가량은 1몰임을 알 수 있었다. BET-N2방법을 이용하여 표면적을 측정한 결과 물/알콕 사이드의 몰비가 40-80범위에서 비표면적이 급격히 증가되어 DCA 의 광분해율도 증가하였으며, 몰 40몰을 첨가 후 졸-겔법으로 제조한 분말을 40$0^{\circ}C$에서 1시간 열처리한 anatase phase의 TiO2가 최고의 광분해 효율인 약 21%를 보였다. 이는 상업용으로 가장 효율이 높은 Dagussa P-25의 DCA 분해 효율보다 2배 정도 높은 것으로 나타났다.

  • PDF

Synthesis or photocatalytic Ni-doped nanocomposite $TiO_2$ by mechanical alloying and heat treatment (기계적 합금화법과 열처리를 통한 Ni이 도핑 된 광촉매 $TiO_2$ 나노 복합상 제조)

  • Park, Ha-Sung;Kim, Dong-Hyun;Jho, Jae-Han;Kim, Sun-Jae;Lee, Kyung-Sub
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2005.11a
    • /
    • pp.667-672
    • /
    • 2005
  • In order to effectively utilize visible light in the photocatalytic reaction, nanaocomposite of Ni doped $TiO_2$ and $NiTiO_3$ powders were synthesized by mechanical alloying and heat treatment. About 5.4 wt% of $NiTiO_3$ with particle size less than 15nm was uniformly formed in the Ni-doped rutile $TiO_2$ matrix. The UV/VIS-DRS and PL investigation showed that the nanocompasite $TiO_2$ powders had a longer absorpt ion wavelength (600$\sim$650nm, 2.0$\sim$1.9eV) than that of Ni-doped $TiO_2$ or rutile $TiO_2$ powder. The carbon decomposition of 4-CP by the nanocompasite $TiO_2$ powders were higher than other $TiO_2$ (P-25).

  • PDF

$SrTiO_3$ Single Crystal Growth by Verneuil Method (Verneuil법에 의한 $SrTiO_3$ 단결정 성장)

  • Choi, I.S.;Cho, H.;Choi, J.K.;Orr, K.K.
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.9
    • /
    • pp.689-694
    • /
    • 1992
  • Strontium Titanate single crystal is grown by Verneuil method. Feed materials were prepared by coprecipitation method which started with Sr(NO3)2 and TiCl4. SrTiO3 can not be grown from feed materials having the stoichiometric components due to volatilization of SrO, when the powder added more 3 wt% SrO used, the crystal can be grown. Growth conditions that the pressure of oxygen and hydrogen gas was 5 psi, the flow rate of oxygen and hydrogen was 7.3 and 30ι/min respectively, the growth rate was 20 mm/hr were optimum. The grown single crystal has the diameter of 10~15 mm and its length is 30~40 mm. The grown crystal was deep brown color and somewhat transparent. The color of grown crystal was lightened after annealing.

  • PDF

Preparation and Electrical Properties of Lead Zirconate Titanate Thick Films Fabricated by Screen-Printing Method (스크린 프린팅으로 제작된 $Pb(Zr,\;Ti)O_3$ 후막의 제작과 전기적 특성)

  • Park, Sang-Man;Lee, Sung-Gap
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.55 no.9
    • /
    • pp.429-433
    • /
    • 2006
  • PZT(80/0) powder was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The coating and drying procedure was repeated 4 times. And then the PZT(20/80) precusor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5mol/L and the number of coating was varied from 0 to 6. The porosity decreased and the grain size increased with increasing the number of coatings. The thickness of the PZT-6(6: number of coatings) films was about $60{\mu}m$. The relative dielectric constant increased and the dielectric loss decreased with increasing the number of PZT(20/80) sol coatings. The relative dielectric constant and dielectric loss of the PZT-6 thick film were 275 and 3.5%, respectively. The remanent polarization, coercive field and breakdown strength of the PZT-6 film were $19.8{\mu}C/cm^2$, 13.7kV/cm and 130kV/cm, respectively.