Studies on Preparation of $Ti_3SiC_2$ Particulate Reinforced Cu Matrix Composite by Warm Compaction and its Tribological Behavior

  • Ngai, Tungwai L.;Xiao, Zhiyu;Wu, Yuanbiao;Li, Yuanyuan
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.853-854
    • /
    • 2006
  • Warm compaction powder metallurgy was used to produce a $Ti_3SiC_2$ particulate reinforced Cu matrix composite. Fabrication parameters and warm compaction behaviors of Cu powder were studied. Based on the optimized fabrication parameters a Cu-based electrical contact material was prepared. Results showed that in expend of some electrical conductivity, addition of $Ti_3SiC_2$ particulate increased the hardness, wear resistivity and anti-friction ability of the sintered Cu-base material.

  • PDF

연속다공질 SiC-Si3N4 복합체의 미세구조 및 기계적 특성 (Microstructure Control and Mechanical Properties of Continuously Porous SiC-Si3N4 Composites)

  • ;;이희정;장희동;이병택
    • 한국재료학회지
    • /
    • 제16권3호
    • /
    • pp.188-192
    • /
    • 2006
  • The microstructures and mechanical properties of continuously porous $SiC-Si_3N_4$composites fabricated by multi-pass extrusion were investigated at different Si levels added. Si-powder with different weight percentages (0%, 5%, 10%, 15%, 20%) was added to the SiC powder to make the raw mixture powders, with $6wt%Y_2O_3-2wt%Al_2O_3$ as sintering additives, carbon ($10-15{\mu}m$) as a pore-forming agent, ethylene vinyl acetate as a binder and stearic acid ($CH_3(CH_2)_{16}COOH$) as a lubricant. In the continuously porous $SiC-Si_3N_4$ composites, $Si_3N_4$ whiskers like the hairs of nostrils were frequently observed on the wall of the pores. In this study, the morphology of the $Si_3N_4$ whiskers was investigated with the silicon addition content. In the composites containing of 10 wt% Si, a large number of $Si_3N_4$ whiskers was found at the continuous pore regions. In the sample to which 15 wt% Si powder was added, maximum values of about 101 MPa bending strength and 57.5% relative density were obtained.

SiC Whisker의 분산과 $Al_2O_3-SiC Whisker$ 복합재료의 기계적 성질 (SiC-Whisker Dispersion and Mechanical Properties of $Al_2O_3-SiC Whisker$ Whisker Composite)

  • 정수종;이주완;김득중;신유선;강석중
    • 한국세라믹학회지
    • /
    • 제30권6호
    • /
    • pp.492-498
    • /
    • 1993
  • The pretreatment condition for uniform distribution of SiC whisker in A2O3-SiCw composites has been determined and the mechanical properties of the composites with various whisker contents have been measured. Good dispersion of the whisker can be obtained in a solution of pH=10.45 by ball milling and ultrasonic treatment. The relative density of hot pressed composites decreases with the whisker content up to 40vol%, but is found to be satisfactory, over 98% for all samples. The mechanical property of the composites is sensitive to the whisker dispersion. Uniform distributjion of the whisker is critical in order to guarantee good mechanical property.The samples containing 20~30vol% whisker show the best mechanical property within the studied range.

  • PDF

Sinter Plus HIP에 의한 $Al_2$$O_3$-SiC 나노복합재료의 치밀화 거동 (Densification Behavior of Fine SiC Particle-Dispersed $Al_2$$O_3$-SiCComposite by Sinter Plus HIP)

  • 채기웅
    • 한국세라믹학회지
    • /
    • 제38권2호
    • /
    • pp.179-182
    • /
    • 2001
  • Al$_2$O$_3$-5 vol% SiC 나노복합재료의 sinter plus HIP에 의한 치밀화시 일어나는 기공의 변화에 초점을 두어 치밀화 거동을 관찰하였다. $Al_2$O$_3$-SiC 시편은 질소분위기 중의 상압소결과 이후의 열간정수압소결(HIP)에 의해 완전치밀화가 이루어졌다. 155$0^{\circ}C$의 상압소결에 의해서는 90%의 비교적 낮은 상대밀도가 얻어졌으나, 기공의 폐기공화로 이후의 열간정수압소결(HIP)에 의해 99.6%의 완전치밀화가 가능하였다. 상압소결한 시편을 X-선 회절기와 주사전자현미경(SEM)으로 관찰한 결과, 선택적으로 시편 표면부에서만 SiAl$_{6}$O$_2$N$_{6}$과 AlN 등으로 이루어진 치밀화된 반응층을 확인할 수 있었으며, 이러한 표면 반응층이 비교적 낮은 상대밀도의 시편내의 모든 기공을 폐기공화하는 효과를 주는 것을 알 수 있었다.

  • PDF

Y2O3 첨가 탄소 프리폼에 Si 용융 침투에 의해 제조한 반응 소결 탄화규소 (RBSC Prepared by Si Melt Infiltration into the Y2O3 Added Carbon Preform)

  • 장민호;조경식
    • 한국분말재료학회지
    • /
    • 제28권1호
    • /
    • pp.51-58
    • /
    • 2021
  • The conversion of carbon preforms to dense SiC by liquid infiltration is a prospectively low-cost and reliable method of forming SiC-Si composites with complex shapes and high densities. Si powder was coated on top of a 2.0wt.% Y2O3-added carbon preform, and reaction bonded silicon carbide (RBSC) was prepared by infiltrating molten Si at 1,450℃ for 1-8 h. Reactive sintering of the Y2O3-free carbon preform caused Si to be pushed to one side, thereby forming cracking defects. However, when prepared from the Y2O3-added carbon preform, a SiC-Si composite in which Si is homogeneously distributed in the SiC matrix without cracking can be produced. Using the Si + C → SiC reaction at 1,450℃, 3C and 6H SiC phases, crystalline Si, and Y2O3 were generated based on XRD analysis, without the appearance of graphite. The RBSC prepared from the Y2O3-added carbon preform was densified by increasing the density and decreasing the porosity as the holding time increased at 1,450℃. Dense RBSC, which was reaction sintered at 1,450℃ for 4 h from the 2.0wt.% Y2O3-added carbon preform, had an apparent porosity of 0.11% and a relative density of 96.8%.

리튬 이온 전지용 음극으로서의 Si@C/rGO의 합성 (Si@C/rGO Composite Anode Material for Lithium Ion Batteries)

  • 김채현;김성훈;안욱
    • 전기화학회지
    • /
    • 제27권2호
    • /
    • pp.73-79
    • /
    • 2024
  • 화석 연료의 사용이 증가함에 따라 이산화탄소와 같은 온실 가스의 배출량이 함께 증가하며 발생하는 환경 문제의 해결을 위해 이차전지와 같은 친환경 에너지 저장 기술이 주목받고 있다. 리튬 이온 전지의 중대형 전지를 제작하기 위해서는 고용량과 고효율 뿐만 아니라 우수한 안정성을 지니는 배터리의 전극 소재의 개발이 필수적이다. 이를 위해 고분자의 합성을 토대로 고용량을 얻을 수 있는 실리콘과 합성한 후 reduced Graphene Oxide (rGO)를 첨가하여 전극 활 물질을 제조해 물리적 특성과 전기화학적 성능을 분석하였다. 제조한 전극은 실리콘에 고분자를 탄화시켜 코팅하고 기계적 강도와 높은 안정성을 보이는 rGO를 첨가해 실리콘에 탄소를 코팅하는 Si@C 복합체에 비해 개선된 용량과 향상된 안정성을 보이는 것을 확인했다.

액상소결 시의 β-SiC의 입자성장 방지 (Prevention of Grain Growth during the Liquid-Phase Assisted Sintering of β-SiC)

  • 길건영;노비얀토 알피안;한영환;윤당혁
    • 한국세라믹학회지
    • /
    • 제47권6호
    • /
    • pp.485-490
    • /
    • 2010
  • In our previous studies, continuous SiC fiber-reinforced SiC-matrix composites ($SiC_f$/SiC) had been fabricated by two different slurry infiltration methods: vacuum infiltration and electrophoretic deposition (EPD). 12 wt% of $Al_2O_3-Y_2O_3$-MgO with respect to SiC powder was used as additives for liquid-phase assisted sintering. After hot pressing at $1750^{\circ}C$ under 20 MPa for 2 h in Ar atmosphere, a high composite density could be achieved for both cases, whereas the problems such as large grain size and non-uniform distribution of liquid phase were observed, which was resulted in the relatively poor mechanical properties of composites. Therefore, efforts have been made to reduce the grain growth during the sintering, including the optimization for hot pressing condition and utilization of spark plasma sintering using a SiC monolith. Based on the results, spark plasma sintering was found to be effective method in decreasing the amount of sintering additive, time and grain growth, which will be explained in comparison to the results of hot pressing in this paper.

방전플라즈마 소결에 의한 자기 통전식 SiC계 세라믹 발열체 개발 (Development of Electroconductive SiC Ceramic Heater by Spark Plasma Sintering)

  • 신용덕;최원석;고태헌;이정훈;주진영
    • 전기학회논문지
    • /
    • 제58권4호
    • /
    • pp.770-776
    • /
    • 2009
  • The composites were fabricated by adding 0, 15, 30, 45[vol.%] $ZrB_2$ powders as a second phase to SiC matrix. The physical, mechanical and electrical properties of electroconductive SiC ceramic composites by spark plasma sintering(SPS) were investigated. Reactions between ${\beta}$-SiC and $ZrB_2$ were not observed in the XRD and the phase analysis of the electroconductive SiC ceramic composites. The relative density of mono ${\beta}$-SiC, ${\beta}$-SiC+15[vol.%]$ZrB_2$, ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]$ZrB_2$ composites are respectively 99.24[%], 87.53[%], 96.41[%] and 98.11[%] Phase analysis of the electroconductive SiC ceramic composites by XRD revealed mostly of ${\beta}$-SiC, $ZrB_2$ and weakly of $ZrO_2$ phase. The flexural strength showed the lowest of 114.44[MPa] for ${\beta}$-SiC+15[vol.%]$ZrB_2$ powders and showed the highest of 210.75[MPa] for composite no added with $ZrB_2$ powders at room temperature. The trend of the mechanical properties of the electroconductive SiC ceramic composites is accorded with the trend of the relative density. The electrical resistivity of the electroconductive SiC ceramic composites decreased with increased $ZrB_2$ contents. The electrical resistivity of mono ${\beta}$-SiC, ${\beta}$-SiC+15[vol.%]$ZrB_2$, ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]$ZrB_2$ composites are respectively $4.57{\times}10^{-1},\;2.13{\times}10^{-1},\;2.68{\times}10^{-2}\;and\;1.99{\times}10^{-2}[{\Omega}{\cdot}cm]$ at room temperature. The electrical resistivity of mono ${\beta}$-SiC and ${\beta}$-SiC+15[vol.%]$ZrB_2$ are negative temperature coefficient resistance(NTCR) in temperature ranges from $25[^{\circ}C]\;to\; 100[^{\circ}C]$. The electrical resistivity of ${\beta}$-SiC+30[vol.%]$ZrB_2$ and ${\beta}$-SiC+45[vol.%]ZrB_2$ are positive temperature coefficient resistance(PTCR) in temperature ranges from $25[^{\circ}C]\;to\;100[^{\circ}C]$. It is convinced that ${\beta}$-SiC+30[vol.%]$ZrB_2$ composites by SPS for heater or ignitors can be applied.

Biomorphic C/SiC 복합재료의 기계적 물성 연구 (Prediction of Mechanical Property of Biomorphic Composites)

  • 정재연;우경식;이동주;홍순형;김연철
    • 한국항공우주학회지
    • /
    • 제40권8호
    • /
    • pp.670-677
    • /
    • 2012
  • 본 논문에서는 Biomorphic C/SiC 복합재료에 대하여 단위구조해석을 수행하였다. 소나무와 뉴송을 탄화하고 실리콘을 함침해 제조한 복합재료의 미세조직을 사각배열과 육각배열로 가정해 단위구조를 정의하고 등가물성치를 계산하였다. 단위구조의 크기가 동일하지 않은 경우도 고려하였고, 또한 공극의 배열에 따른 물성치의 변화를 몬테카를로 시뮬레이션을 통해 조사하였다.

반응소결 SiC/Graphite 복합체에서 Graphite 입자의 크기에 따른 마찰마모특성 (Tribological Properties of Reaction-Bonded SiC/Graphite Composite According to Particle Size of Graphite)

  • 백용혁;서영현;최웅;이종호
    • 한국세라믹학회지
    • /
    • 제34권8호
    • /
    • pp.854-860
    • /
    • 1997
  • The tribological property of ceramics is very important for use in seal rings, pump parts, thread guides and mechanical seal, etc. In the present study, which RBSC/graphite composites were manufactured by adding graphite powders with different particle sizes to mixtures of SiC powder, metallic silicon, carbon black and alumina, effects on the tribological property of each RBSC/graphite composite was investigated in accordance with the particle size of the added graphite powder. The water absorption, the bending strength and the resistance for the friction and wear were measured, and the crystalline phase and the microstructure were respectively examined by using XRD and SEM. In case that the particle size of the graphite powder was fine(2${\mu}{\textrm}{m}$), the formation of $\beta$-SiC was accelerated, thereby making the increase of the bending strength and the decrease of the water absorption, but no improvement for the tribological properties. Furthermore, in case that the particle size of the graphite powder was some large(88~149${\mu}{\textrm}{m}$), the formation of $\beta$-SiC was not accelerated, to thereby make the decrease of the bending strength and the increase of the water absorption, but the improvement for the tribological property of only the composite having the graphite powder of 20 vol%. In addition, in case that the particle size distribution of the graphite powder was large (under 53 ${\mu}{\textrm}{m}$), there was no improvement for every properties. However, the composites, which the graphite powder with the particle size of 53~88 ${\mu}{\textrm}{m}$ was added in 10~15 vol%, had the most increased resistance for the friction and wear which show the worn out amount of 0.4~0.6$\times$10-3 $\textrm{cm}^2$, and the value of the bending strength is 380~520 kg/$\textrm{cm}^2$.