• Title/Summary/Keyword: Ceria Slurry

Search Result 56, Processing Time 0.026 seconds

Experimental and Numerical Analysis of A Novel Ceria Based Abrasive Slurry for Interlayer Dielectric Chemical Mechanical Planarization

  • Zhuanga, Yun;Borucki, Leonard;Philipossian, Ara;Dien, Eric;Ennahali, Mohamed;Michel, George;Laborie, Bernard;Zhuang, Yun;Keswani, Manish;Rosales-Yeomans, Daniel;Lee, Hyo-Sang;Philipossian, Ara
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.2
    • /
    • pp.53-57
    • /
    • 2007
  • In this study, a novel slurry containing ceria as the abrasive particles was analyzed in terms of its frictional, thermal and kinetic attributes for interlayer dielectric (ILD) CMP application. The novel slurry was used to polish 200-mm blanket ILD wafers on an $IC1000_{TM}$ K-groove pad with in-situ conditioning. Polishing pressures ranged from 1 to 5 PSI and the sliding velocity ranged from 0.5 to 1.5 m/s. Shear force and pad temperature were measured in real time during the polishing process. The frictional analysis indicated that boundary lubrication was the dominant tribological mechanism. The measured average pad leading edge temperature increased from 26.4 to $38.4\;^{\circ}C$ with the increase in polishing power. The ILD removal rate also increased with the polishing power, ranging from 400 to 4000 A/min. The ILD removal rate deviated from Prestonian behavior at the highest $p{\times}V$ polishing condition and exhibited a strong correlation with the measured average pad leading edge temperature. A modified two-step Langmuir-Hinshelwood kinetic model was used to simulate the ILD removal rate. In this model, transient flash heating temperature is assumed to dominate the chemical reaction temperature. The model successfully captured the variable removal rate behavior at the highest $p{\times}V$ polishing condition and indicates that the polishing process was mechanical limited in the low $p{\times}V$ polishing region and became chemically and mechanically balanced with increasing polishing power.

Polishing of Oxide film by colloidal silica coated with nano ceria (나노 세리아 입자가 표면 코팅된 콜로이달 실리카 슬러리의 Oxide film 연마특성)

  • Kim, Hwan-Chul;Lee, Seung-Ho;Kim, Dae-Sung;Lim, Hyung-Mi
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.35-37
    • /
    • 2005
  • 100, 200nm 크기의 colloidal silica 각각에 나노 ceria 입자를 수열합성법으로 코팅하였다. Colloidal silica 입자에 ceria를 코팅 시 slurry의 pH조절과 수열처리에 이용하여 silica에 ceria가 코팅됨을 TEM과 zeta-potential을 이용하여 확인하였다. 연마 슬러리의 분산 안정성과 연마효율을 높이기 위하여 슬러리의 pH 는 9로 하였으며, 이때의 zeta-potential 값은 -25 mV이었다. 1 wt%로 제조된 연마슬러리를 이용하여, 4 inch $SiO_2$, $Si_3N_4$ wafer를 압력변화에 따른 연마특성을 관찰 하였다. Ceria coated colloidal silica 100 nm, 200 nm와 commercial한 $CeO_2$입자를 연마압력 6 psi로 oxide film을 연마한 결과 연마율이 각각 2490 ${\AA}/min$, 4200 ${\AA}/min$, 4300 ${\AA}/min$으로 측정되었다. 또한 $SiO_2$, $Si_3N_4$ film의 6 psi압력에서 ceria coated colloidal silica 100 nm, 200 nm와 commercial 한 $CeO_2$입자의 선택비는 3, 3.8, 6.7 이었다. 입자크기가 클수록 연마율이 높으며, Preston equation을 따라 연마 압력과 연마율이 비례하였다.

  • PDF

Polishing Mechanism of TEOS-CMP with High-temperature Slurry by Surface Analysis

  • Kim, Nam-Hoon;Seo, Yong-Jin;Ko, Pil-Ju;Lee, Woo-Sun
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.4
    • /
    • pp.164-168
    • /
    • 2005
  • Effects of high-temperature slurry were investigated on the chemical mechanical polishing (CMP) performance of tetra-ethyl ortho-silicate (TEOS) film with silica and ceria slurries by the surface analysis of X-ray photoelectron spectroscopy (XPS). The pH showed a slight tendency to decrease with increasing slurry temperature, which means that the hydroxyl $(OH^-)$ groups increased in slurry as the slurry temperature increased and then they diffused into the TEOS film. The surface of TEOS film became hydro-carbonated by the diffused hydroxyl groups. The hydro-carbonated surface of TEOS film could be removed more easily. Consequently, the removal rate of TEOS film improved dramatically with increasing slurry temperature.

A Study on the CMP of Lithium Tantalate Wafer (Lithium Tantalate (LiTaO3) 웨이퍼의 CMP에 관한 연구)

  • Lee, Hyun-Seop;Park, Boum-Young;Seo, Heon-Deok;Chang, One-Moon;Jeong, Hae-Do
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.9 s.240
    • /
    • pp.1276-1281
    • /
    • 2005
  • Compound semiconductors are the semiconductors composed of more than two chemical elements. Lithium Tantalate$K_I$ wafer is used for several optical devices, especially surface acoustic wave(SAW) device. Because of the lithography in SAW device process, $LiTaO_3$ polishing is needed. In this paper, the commercial slurries $(NALC02371^{TM},\; ILD1300^{TM},\;ceria slurry)$ used for chemical mechanical polishing(CMP) were tested, and the most suitable slurry was selected by measuring material removal rate and average centerline roughness$(R_a)$. From these result, it was proven that $ILD1300^{TM}$ was the most suitable slurry for $LiTaO_3$ wafer CMP due to the chemical reaction between solution in slurry and material.

Global planarization Characteristic of $WO_3$ ($WO_3$ 박막의 광역평탄화 특성)

  • Lee, Woo-Sun;Ko, Pi-Ju;Choi, Gwon-Woo;Kim, Tae-Wan;Seo, Yong-Jin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.04b
    • /
    • pp.89-92
    • /
    • 2004
  • Chemical mechanical polishing (CMP) process has been widely used to planarize dielectric layers, which can be applied to the integrated circuits for sub-micron technology. Despite the increased use of CMP process, it is difficult to accomplish the global planarization of in the defect-free inter-level dielectrics (ILD). we investigated the performance of $WO_3$ CMP used silica slurry, ceria slurry, tungsten slurry. In this paper, the effects of addition oxidizer on the $WO_3$ CMP characteristics were investigated to obtain the higher removal rate and lower non-uniformity.

  • PDF