마이크로 아크 산화 표면처리 기술을 활용한 치과도재 소부용 티타늄 인공치아 결합강도 연구 (A Study on the Bonding Strength of Titanium Artificial Teeth for Baking Dental Ceramics using Micro-arc Oxidation Surface Treatment Technology)

  • 송종법;박종민;김종순;정효경;최원식
    • 한국산업융합학회 논문집
    • /
    • 제25권2_2호
    • /
    • pp.309-314
    • /
    • 2022
  • The bonding strength [ISO22674] test was conducted by firing a dedicated ceramic powder on the surface of the dental titanium material treated with micro-arc oxidation. In the test group, an average result value of 34.34 MPa was obtained, and in the control group, a result value of 21.53 MPa was obtained. The bonding strength of the test group was higher than that of the control group by 12.81 MPa, resulting in a 37% improvement in durability of the dental artificial tooth ceramic restoration.

면 수초지의 지력 및 보류 향상을 위한 첨가제의 적용(제2보) -첨가제에 따른 면 수초지의 내구성 시험 (Improvements of Strength and Retention of Cotton Handsheet by Additives(II) -The durability test of cotton handsheet with additives)

  • 조유제;김강재;엄태진
    • 펄프종이기술
    • /
    • 제46권1호
    • /
    • pp.29-38
    • /
    • 2014
  • Guar gum is added to the pulp suspension at the suction side of the fan pump just before the sheet is formed on either a fourdrinier or cylinder machine. Guar gum replaced and supplements these hemicelluloses in paper bonding with many advantages, which include improved sheet formation with a more random distribution of pulp fibers. But, guar gum has serious storage problem. This material has easily decayed after High-temperature conditions such as summer. In this study, various properties of cotton handsheet were measured to solve the problem of deformation while storing guar gum and to improve the durability. After aging, which is one of the durability tests, cotton handsheet with 0.2% and 0.3% of A-PAM showed improved mechanical properties and bursting index and folding endurance of cotton handsheet with 0.3% of A-PAM were similar to those with guar gum. The yellowness loss of cotton handsheet with synthetic polymers was lower than those with guar gum.

고강력 직물의 열융착 라미네이팅을 통한 충격 완화용 에어쿠션 소재로의 적용 가능성 검토 연구 (Study on the Applicability of the Air Cushion Material for Impact Relief through Thermal Bonding of High Strength Fabrics)

  • 김지연;김훈민;민문홍
    • 한국염색가공학회지
    • /
    • 제32권3호
    • /
    • pp.176-183
    • /
    • 2020
  • In order to study wearable air cushion materials capable of responding to massive impact in high-altitude fall situation, high tenacity woven fabrics were bonded by heat only depending on various type of thermoplastic films and then mechanical properties were measured. Tensile strength, elongation, and 100% modulus measurement results for 4 types of films show that TPU-2 has higher impact resistance and easier expansion than PET-1. After thermal bonding, the combination with the highest tensile strength was a material with a TPU-2 film for nylon and a PET-2 film for PET, so there was a difference by type of fabric. The tear strength of the bonded materials were increased compared to the fabric alone, which shows that durability against damage such as tearing can be obtained through film adhesion. All of the peel strengths exceeded the values required by automobile airbags by about 5 times, and the TPU-2 bonded fabric showed the highest value. The air permeability was 0 L/dm2 /min. For both the film and the bonded material, which means tightness between the fabric and the film through thermal bonding. It is expected to be applied as a wearable air cushion material by achieving a level of mechanical properties similar to or superior to that of automobile airbags through the method of bonding film and fabric by thermal bonding.

Al 판재의 Adhesion Bonding에 미치는 전처리 영향 (Effects of Pretreatment on the Adhesive Bonding of Aluminium Plate)

  • 한성호;김만;장도연;노병호
    • 한국표면공학회지
    • /
    • 제25권2호
    • /
    • pp.97-102
    • /
    • 1992
  • Transimission electron microscope(TEM)/ultramicrotomy were used to characterize the detailed surface morphology of 2024-T3 Al alloy surfaces prepared by various pretreatment process. It was found that, for good and superior initial adhesive strength and durability, chemically pretreated substrates appeared essential. The film morphology developed after CSA etching treatment, ass revealed by TEM, suggested the present of irregular cell pattern with finely separated whisker-like protrusion with was responsible for increase of bond strength.

  • PDF

콘크리트 복개구조물용 보수재료의 성능 평가 (Evaluation of Performance on Repair Materials for Creek Concrete Structures)

  • 이창수
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제6권1호
    • /
    • pp.205-212
    • /
    • 2002
  • The deterioration rate of concrete structures in urban area is accelerated due to rapid urbanization and environmental pollution. Repair materials and methods newly introduced in Korea should be investigated whether they are appropriate for the urban environment in Korea. The creek concrete structures are exposed in severe environmental condition than others. Based on these background in mind, the study is focused on evaluation of performance on repair materials used to rehabilitate creek concrete structures. To evaluate the performance of repair materials, four kinds of repair materials were selected based on polymer emulsion. This experimental study was conducted on fundamental performance such as setting time, compressive strength, bending strength, bonding strength, thermal expansion coefficient, and durability performance such as chloride diffusion, carbonation, chemical attack, and steel corrosion rate. On the basis of this study, the optimal repair material which is proper to the environment condition can be selected and service life of creek concrete structures can be extended. As a result, the life cycle cost can be reduced and the waste of material resources will be cut down.

실리콘 고무와 내열접착 향상을 위한 Polyethylene Terephthalate 섬유 접착층의 제조 및 특성 (Treatment and Characterization of Polyethylene Terephthalate Fibers with Silicone Rubber Adhesive for Heat-Resistant Adhesion)

  • 김지효;이상오;이재웅
    • 한국염색가공학회지
    • /
    • 제31권2호
    • /
    • pp.107-117
    • /
    • 2019
  • In case of pure rubber materials, the initial quality of the rubber materials would be excellent, however, the durability against external impact might be poor. In order to overcome the relatively low durability, textile cord could be employed with silicone rubber. We have studied the improvement of heat-resistant adhesion properties of silicone adhesives between silicone rubber and PET fibers by applying various conditions including dip solution recipe. The silicone rubber used was a platinum catalyst curing type and platinum catalyst type silicone adhesive was used as an adhesive to obtain an optimum adhesive force. Furthermore, the bonding mechanism between silicone and PET fiber was established.

Effect of Joint Reformation on Adhesive Strength of 6061 Aluminum Alloy to Polycarbonate Lap Structures

  • D. W. Seo;Kim, H. J.;J. K. Lim
    • International Journal of Korean Welding Society
    • /
    • 제4권1호
    • /
    • pp.53-60
    • /
    • 2004
  • Adhesive-bonded joints are widely used in the industry. Recently, applications of adhesive bonding joints have been increased extensively in automobile and aircraft industry. The strength of adhesive joints is influenced by the surface roughness, adhesive shape, stress distribution, and etc. However, the magnitude of the influence has not yet been clarified because of the complexity of the phenomena. In this study, as the fundamental research of adhesive bonding joints, the effects of adhesive shape and loading speed on bonding strength properties and durability of aluminum to polycarbonate single-lap joints were studied. To evaluate the effect of adhesive shape, several modified shapes were used, and loading speeds were varied from 0.05 to 5mm/min. As a result, the load distribution showed a brittle fracture tendency. The trigonal edged single lap and bevelled lap joints showed the higher strength than the plain single lap, trigonal single lap, joggle lap and double lap joints in same adhesive area. The fractures of trigonal single lap and trigonal edged single lap joints that had the higher strength level were shown as the mixture type of the cohesive and interfacial-failure, mostly joggle lap joints that had the lower strength level were shown as the adhesive-failure.

  • PDF

에폭시 접착제 접합구조물의 강도향상을 위한 접착부 형상설계 (Shape Design of Adhesive Joints for Strength Improvement of Epoxy Adhesive Structures)

  • 서도원;김효진;임재규
    • 대한기계학회논문집A
    • /
    • 제28권6호
    • /
    • pp.783-790
    • /
    • 2004
  • Adhesive-bonded joints are widely used in the industry. Recently, applications of adhesive bonding joints have been increased extensively in automobile and aircraft industry. The strength of adhesive joints is influenced by the surface roughness, adhesive shape, stress distribution, and etc. However, the magnitude of the influence has not yet been clarified because of the complexity of the phenomena. In this study, as the fundamental research of adhesive bonding joints, the effects of adhesive shape and loading speed on bonding strength properties and durability of aluminum to polycarbonate single-lap joints were studied. To evaluate the effect of adhesive shape, several modified shapes were used, and loading speeds were varied from 0.05 to 5 mm/min. As a result, the load-displacement distribution was shown a brittle fracture tendency. The trigonal edged single lap and bevelled lap joints showed the higher strength than the plain single lap, trigonal single lap, joggle lap and double lap joints in same adhesive area. The fractures of trigonal single lap and trigonal edged single lap joints that had the higher strength level were shown as the mixture type of the cohesive and interfacial-failure, mostly joggle lap joints that had the lower strength level were shown as the adhesive-failure.

접착부 형상이 알루미늄/폴리카보네이트 접합재의 강도에 미치는 영향 (Effect of Adhesive Shape on the Strength of Aluminum/Polycarbonate Joint)

  • 서도원;김효진;최준용;;임재규
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 추계학술대회
    • /
    • pp.1039-1044
    • /
    • 2003
  • Adhesive-bonded joints are widely used in the industry. Recently aircraft applications of adhesive bonding joints have been increased extensively in automobile and air industry. Because adhesives which are available for structural applications have been developed a lot and understanding of adhesive bonding has been improved so much. In this study, as the fundamental research of design of adhesive bonding joints, this study considers specimen shape are affect strength and durability of Al/Polymer lap joints. In this research, cross head speed difference were concerned to evaluate their effects on the adhesive strength. Cross head speed makes a change 0.05mm/min, 0.5mm/min, 5mm/min. The result is load-displacement diagram showed brittleness fracture tendency. Fracture tendency that is shown enough on stress distribution of trigonal single lap joint and trigonal edged single lap joint occur the inside of adhesive.

  • PDF

Basalt 섬유쉬트의 철도시설 콘크리트구조물 보강재로서의 부착거동 연구 (Bonding Characteristics of Basalt Fiber Sheet as Strengthening Material for Railway Concrete Structures)

  • 박철우;심종성
    • 한국철도학회논문집
    • /
    • 제12권5호
    • /
    • pp.641-648
    • /
    • 2009
  • 최근 철도차량의 속도가 증가함에 따라 철도시설물에도 철근콘크리트 구조물이 많이 적용되고 있는 실정이다. 하지만 이러한 콘크리트 구조물은 공용년수의 증가에 따라 필연적으로 구조적인 보강이 요구된다. 강판보강법 및 섬유복합체(FRP)를 활용한 보강법 등이 가장 일반적으로 적용되는 실정이지만 각 공법마다 나름대로의 단점 역시 존재 한다. 최근 화재나 기타 환경적인 공격에 대하여 강한 내구성을 가진 재료의 개발이 요구되고 있으며 이에 따른 현무암으로부터 추출한 Basalt 섬유를 활용한 섬유보강재가 많은 관심을 받고 있다. 이에 본 연구에서는 Basalt 섬유쉬트를 보강재로 사용할 경우 중요한 특성인 콘크리트와의 부착특성에 관하여 연구를 수행하였다. 실험변수는 보강폭, 길이, 보강겹수를 포함한다. 실험결과, 파괴형태는 계면파괴, 섬유파단, 그리고 rip-off의 형태가 관측되었으며 보강길이보다는 보강폭이 보강강도에 더 많은 영향을 미치는 것으로 판단되었다. 또한 보강길이가 전부 유효하게 작용하지는 않았으며 이에 유효보강길이를 산정하고 이에 따른 부착강도를 산정하였다. 이를 다른 종류의 FRP재료를 활용한 경우에 유효 보강길이와 비교하여 Basalt 섬유쉬트의 부착특성을 분석하였다.