• Title/Summary/Keyword: $ZrO_2$ Formation

Search Result 197, Processing Time 0.023 seconds

Effects of Mechanical Alloying Treatment on Age Hardening Behavior of Rapidly Solidified Al-5Cr-2Zr Alloy (급속냉각한 Al-5Cr-2Zr 합금의 시효경화에 미치는 기계적 합금화 처리효과)

  • 김완철
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.18 no.5
    • /
    • pp.29-35
    • /
    • 1994
  • The microstructual refinement process of Al-5Cr-2Zr alloys mechanical alloying 30h can be divided in five stages ; initial stage, welding predomminance stage, spherical partical formation stage, convolution welding predominance stage, and steady state. The rate of structural of aluminium splats was roughly logarithmic with processing time ; ${\in}$=k/0.78 ln(1+0.0028t). The age hardening in rapidly solidified Al-5Cr-2Zr alloys is ascribed to the coherency and dispersion hardening. Coherency hardening is occurred by matastable cubic Al3Zr precipitates in Al-Cr-Zr alloys. Dispersion hardening after mechanical alloying is attributed to the finely-dispersed $Al_2O_3$ and $Al_4C_3$ in Al-5Cr-2Zr alloys.

  • PDF

Fabrication and Machinability of Mullite-ZrO2-Al2TiO5 Ceramics

  • Shin, Young Been;Lee, Won Jae;Kim, Il Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.6
    • /
    • pp.423-428
    • /
    • 2015
  • The machinability of materials is an important factor in engineering applications. Many ceramic components that have complex shapes require machining, typically using diamond tools, which leads to high production cost. Machinable ceramics containing h-BN have recently been developed, but these materials are very expensive because of high cost of raw materials and machining. Therefore the development of low-cost machinable ceramics is desirable. In this study, mullite-$ZrO_2$ ceramics were prepared additions of $Al_2TiO_5$. $ZrSiO_4$, $Al_2O_3$, and $Al_2TiO_5$ powders mixed at various molar ratios with sintering at 1400, 1500, and $1600^{\circ}C$ for 1 hr. Phase formation and microstructure of the sintered ceramics were observed by XRD and SEM, respectively. The machinability of each specimen was tested using the micro-hole machining method. The machinability results show that the ceramics sintered at temperatures over $1500^{\circ}C$ can be used as good low-cost machinable mullite-$ZrO_2-Al_2TiO_5$ ceramics.

An Efficient and Green Approach for the Esterification of Aromatic Acids with Various Alcohols over H3PO4/TiO2-ZrO2

  • Kalbasi, Roozbeh Javad;Massah, Ahmad Reza;Barkhordari, Zeynab
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.8
    • /
    • pp.2361-2367
    • /
    • 2010
  • $TiO_2-ZrO_2$ was prepared with surfactant through a sol-gel method. Catalysts containing 5 - 35% $H_3PO_4$ were prepared using these oxides. Subsequently the catalytic performance of prepared catalysts was determined for liquid phase esterification of aromatic acids. $H_3PO_4/TiO_2-ZrO_2$ has been used as catalyst to synthesize various novel esters by esterification of some aromatic acids with aliphatic alcohols (2-propanol, 1-butanol, iso butanol, 3-pentanol, 1-hexanol, heptanol, cyclo heptanol, octanol and decanol). Under optimized conditions, maximum yields and selectivity (100%) to the corresponding ester, was obtained by using 25 wt % $H_3PO_4/TiO_2-ZrO_2$ as catalyst. The Catalyst can be easily recycled after reaction and can be reused without any significant loss of activity/selectivity performance. No by-product formation, high yields, short reaction times, mild reaction conditions, operational simplicity with reusability of the catalyst are the salient features of the present synthetic protocol. The reaction was carried out under solvent-free condition.

Characterization by Solid-State $^51V$ NMRand X-ray Diffraction of Vanadium Oxide Supported on ZrO₂

  • 손종락;박만영;배영일
    • Bulletin of the Korean Chemical Society
    • /
    • v.17 no.3
    • /
    • pp.274-278
    • /
    • 1996
  • Vanadium oxide-zirconia catalysts were prepared by dry impregnation of powdered Zr(OH)4 with aqueous solution of NH4VO3. The characterization of prepared catalysts was performed using 51V solid state NMR, XRD, and DSC. The addition of vanadium oxide up to 9 mol% to zirconia shifted the phase transitions of ZrO2 from amorphous to tetragonal toward higher temperatures due to the interaction between vanadium oxide and zirconia. On the basis of results of XRD and DSC, it is concluded that the content of V2O5 monolayer covering most of the available zirconia was 9 mol%. The crystalline V2O5 was observed only with the samples containing V2O5 content exceeding the formation of complete monolayer (9 mol%) on the surface of ZrO2.

Catalytic Gasification of Mandarin Waste Residue using Ni/CeO2-ZrO2

  • Kim, Seong-Soo;Kim, Jeong Wook;Park, Sung Hoon;Jung, Sang-Chul;Jeon, Jong-Ki;Ryu, Changkook;Park, Young-Kwon
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.11
    • /
    • pp.3387-3390
    • /
    • 2013
  • Catalytic gasification of mandarin waste residue was carried out using direct and indirect catalyst-contact methods for the first time. In the indirect method, non-catalytic reaction in a reactor was followed by catalytic upgrading of vapor product in another reactor. Two different catalysts, $Ni/{\gamma}-Al_2O_3$ and $Ni/CeO_2-ZrO_2$, were employed. $CeO_2-ZrO_2$ support was prepared using hydrothermal synthesis in supercritical water. The catalysts were characterized by $H_2$-temperature programmed reduction and Brunauer-Emmett-Teller analyses. Under the condition of equivalent ratio (ER) = 0, the indirect catalyst-contact method led to a higher gas yield than the direct method. Under ER = 0.2, the yield of biogas obtained over $Ni/CeO_2-ZrO_2$ was higher than that obtained over $Ni/{\gamma}-Al_2O_3$. Also, the coke formation of $Ni/CeO_2-ZrO_2$ was lower than that of $Ni/{\gamma}-Al_2O_3$. Such results were attributed to the higher reducibility and better lattice oxygen mobility of $Ni/CeO_2-ZrO_2$, which were advantageous for partial oxidation reaction.

FABRICATION OF ZrO2-BASED NANOCOMPOSITES FOR TRANSURANIC ELEMENT-BURNING INERT MATRIX FUEL

  • MISTARIHI, QUSAI;UMER, MALIK A.;KIM, JOON HUI;HONG, SOON HYUNG;RYU, HO JIN
    • Nuclear Engineering and Technology
    • /
    • v.47 no.5
    • /
    • pp.617-623
    • /
    • 2015
  • $ZrO_2$-based composites reinforced with 6.5 vol.% of carbon foam, carbon fiber, and graphite were fabricated using spark plasma sintering, and characterized using scanning electron microscopy and X-ray diffractometry. Their thermal properties were also investigated. The microstructures of the reinforced composites showed that carbon fiber fully reacted with $ZrO_2$, whereas carbon foam and graphite did not. The carbothermal reaction of carbon fiber had a negative effect on the thermal properties of the reinforced $ZrO_2$ composites because of the formation of zirconium oxycarbide. Meanwhile, the addition of carbon foam had a positive effect, increasing the thermal conductivity from 2.86 to $3.38Wm^{-1}K^{-1}$ at $1,100^{\circ}C$. These findings suggest that the homogenous distribution and chemical stability of reinforcement material affect the thermal properties of $ZrO_2$-based composites.

Preparation of $Li_2O-ZrO_2-P_2O_5-SiO_2$ based Glassy Solid Electrolytes by Sol-Gel Process and Their Ionic Conduction (솔-젤법에 의한 $Li_2O-ZrO_2-P_2O_5-SiO_2$계 유리 고체전해질의 제조와 그의 이온전도성)

  • 박강석;김기원;강은태
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.6
    • /
    • pp.660-670
    • /
    • 1994
  • Transparent, crack-free dried gel monoliths with a composition of LiZr1.5Si2P2O12.5 have been synthesized by the low temperature polymerization of the Sol-Gel technique using metal alkoxides as starting materials. After initial reaction (20~40 min), each metal alkoxide closely paralleled each other during the hydrolysis reactions. The safe drying conditions of gels with no creaks the control of the shrinkage rate. The gels converted into the glass by heat treatment at 75$0^{\circ}C$. FTIR data indicated that the gels were phase separated into silicarich and phosphate-rich regions with the lithium. XRD results showed the formation of crystalline LiH2PO4. The gels dried at 15$0^{\circ}C$ or fired at 75$0^{\circ}C$ contained the residual water. The high ionic conductivity at room temperature for these gels was attributed to the motion of protons.

  • PDF

Synthesis and Crystal Chemistry of New Actinide Pyrochlores (새로운 파이로클로어의 합성 및 결정화학적 특징)

  • ;;;Sergey V. Yudintsev
    • Journal of the Mineralogical Society of Korea
    • /
    • v.15 no.1
    • /
    • pp.78-84
    • /
    • 2002
  • New pyrochlore-type phases($A_2$$B_2$$O_{7}$) were synthesized in the systems: CaO-C$eO_2$-T$iO_2$, CaO-$UO_2$(T$hO_2$)-Z$rO_2$, CaO-$UO_2$(T$hO_2$)-$Gd_2$$O_3$-T$iO_2$-Z$rO_2$, 및 CaO-T$hO_2$-S$nO_2$. The starting materials were pressed with the pressure of 200~400 MPa and sintered at 1500~ 155$0^{\circ}C$ for 4~8 hours in air and at 1300~ 135$0^{\circ}C$ for 5 ~50 hours under oxygen atmosphere. The products were characterized using XRD, SEM/EDS and TEM. In the bulk compositions of CaCe$Ti_2$$O_{7}$, CaTh$Zr_2$$O_{7}$,($Ca_{0.5}$ Gd$Th_{0.5}$)(ZrTi)$O_{7}$) ($Ca_{0.5}$Gd$Th_{0.5}$)(ZrTi)$O_{7}$, ($Ca_{0.5}$G$dU_{0.5}$)(ZrTi)$O_{7}$ and CaTh$Sn_2$$O_{7}$ , pyrochlore was the major phase, together with other oxide phase $of_2$$O_{7}$ fluorite structure. In the samples with target compositions CaU$Zr_2$$O_2$$Ca_{0.5}$ G$dU_{0.5}$)$Zr_2$T$iO_{7}$ pyrochlore was not identified, but a fluorite-structured phase was detected. The formation factor as the stable phase depended on crystal chemical characteristics of the actinide and lanthanide elements of the system concerned.

Effect of Oxidation of Bond Coat on Failure of Thermal Barrier Coating (Bond Coat의 산화가 Thermal Barrier Coating의 파괴에 미치는 영향)

  • 최동구;최함메;강병성;최원경;최시경;김재철;박영규;김길무
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.1
    • /
    • pp.88-94
    • /
    • 1997
  • The oxidation behavior of the NiCrAlY bond coat and thermal fatigue failure in the plasma-sprayed thermal barrier coating system, ZrO2.8wt%Y2O3 top coat/Ni-26Cr-5Al-0.5Y bond coat/Hastelloy X superalloy substrate, in commercial use for finned segment of gas turbine burner were investigated. The main oxides formed in the bond coat were NiO, Cr2O3, and Al2O3. It divided the oxide distribution at this interface into two types whether an Al2O3 thin layer existed beneath ZrO2/bond coat interface before operation at high temperature or not. While a continuous layer of NiO was formed mainly in the region where the Al2O3 thin layer was present, the absence of it resulted in the formation of mixture of Cr2O3 and Al2O3 beneath NiO layer. Analyses on the fracture surface of specimen spalled by thermal cycling showed that spalling occurred mainly along the ceram-ic coat near ZrO2/bond coat oxide layer interface, but slightly in the oxide layer region.

  • PDF

Effect of SiC and WC additon on Oxidation Behavior of Spark-Plasma-Sintered ZrB2

  • Kim, Chang-Yeoul;Choi, Jae-Seok;Choi, Sung-Churl
    • Journal of Powder Materials
    • /
    • v.26 no.6
    • /
    • pp.455-462
    • /
    • 2019
  • ZrB2 ceramic and ZrB2 ceramic composites with the addition of SiC, WC, and SiC/WC are successfully synthesized by a spark plasma sintering method. During high-temperature oxidation, SiC additive form a SiO2 amorphous outer scale layer and SiC-deplete ZrO2 scale layer, which decrease the oxidation rate. WC addition forms WO3 during the oxidation process to result in a ZrO2/WO3 liquid sintering layer, which is known to improve the anti-oxidation effect. The addition of SiC and WC to ZrB2 reduces the oxygen effective diffusivity by one-fifth of that of ZrB2. The addition of both SiC and WC shows the formation of a SiO2 outer dense glass layer and ZrO2/WO3 layer so that the anti-oxidation effect is improved three times as much as that of ZrB2. Therefore, SiC- and WC-added ZrB2 has a lower two-order oxygen effective diffusivity than ZrB2; it improves the anti-oxidation performance 3 times as much as that of ZrB2.