  • ln this work, we studied electrical characteristics and leakage current mechanism of $Ta_2O_{5}$ MOS(Metal-Oxide-Semiconductor) devices. $Ta_2O_{5}$ thin film (63 nm) was deposited by ALD(Atomic Layer Deposition) method at temperature of 235 $^{\circ}C$. The structures of the $Ta_2O_{5}$ thin films were examined by XRD(X-Ray Diffraction). From XRD, it is found that the structure of $Ta_2O_{5}$ is single phase and orthorhombic. From capacitance-voltage (C-V) anaysis, the dielectric constant was 19.4. The temperature dependence of current density-electric field (J-E) characteristics of $Ta_2O_{5}$ thin film was studied at temperature range of 300 - 423 K. In ohmic region (<0.5 MV/cm), the resistivity was 2.456${\times}10^{14}$ ($\omega{\cdot}cm$ at 348 K. The Schottky emission is dominant at lower temperature range from 300 to 323 K and Poole-Frenkel emission is dominant at higher temperature range from 348 to 423 K.

원자층 증착 방법에 의한 $Ta_2O_5$ 박막의 전기적 특성 (The Electrical Properties of $Ta_2O_5$ Thin Films by Atomic Layer Deposition Method)

  • 이형석;장진민;장용운;이승봉;문병무
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 일렉트렛트 및 응용기술
    • /
    • pp.41-46
    • /
    • 2002
  • In this work, we studied electrical characteristics and leakage current mechanism of Au/$Ta_2O_5$/Si metal-oxide-semiconductor (MOS) devices. $Ta_2O_5$ thin film (63nm) was deposited by atomic layer deposition (ALD) method at temperature of $235^{\circ}C$. The structures of the $Ta_2O_5$ thin films were examined by X-Ray Diffraction (XRD). From XRD, the structure of $Ta_2O_5$ was single phase and orthorhombic. From capacitance-voltage (C-V) analysis, the dielectric constant was 19.4. The temperature dependence of current-voltage (I-V) characteristics of $Ta_2O_5$ thin film was studied from 300 to 423 K. In ohmic region (<0.5 MVcm${-1}$), the resistivity was $2.4056{\times}10^{14}({\Omega}cm)$ at 348 K. The Schottky emission is dominant in lower temperature range from 300 to 323 K and Poole-Frenkel emission dominant in higher temperature range from 348 to 423 K.

  • PDF

초정밀 다층 Cermet 박막저항체 제조에 관한 연구 (A study on the manufacturing of super precision multilayer cermet thin film resistor)

  • 허명수;최승우;천희곤;권식철;이건환;조동율
    • 한국진공학회지
    • /
    • 제6권1호
    • /
    • pp.77-84
    • /
    • 1997
  • DC Magnetron Sputtering 방법으로 원기둥형 Alumina기판(직경 4mm, 길이 11mm) 상에 부(-)의 TCR특성의 TaN0.1(부도체)와 정(+)의 TCR특성의 Cr(금속)박막두께를 적절히 조절하므로써 초정밀 저항기를 제조하였다. 그리고 면저항(Rs)을 1k$\Omega$/수준으로 높이고 보 호막을 형성키 위하여 상부에 $Ta_2O_5$막을 입형 $Ta_2O_5/TaN_{0.1}/Cr/Al_2O_3$(substrate)의 다층 박 막저항체를 제조하였다. 적절한 조건(기판온도, $N_2$(g), Ar(g)의 유속 등)으로 상기 다층박막 내 각 막의 두께를 약10,100과 500nm두께로 증착했을 때, $Rs\approx 1k\Omega/\Box$$TCR\approx 20$\pm 5ppm/^{\circ}C$ 의 초정밀 저항체가 제조되었다.

  • PDF

Sol-gel Self-patterning 기술을 이용한 광감응성 Sr0.9Bi2.1Ta2O9 박막의 제조기술에 관한 연구 (A Study on Fabrication of Photosensitive Sr0.9Bi2.1Ta2O9 Thin Film by Sol-gel Self-patterning Technique)

  • 양기호;박태호;임태영;오근호;김병호
    • 한국세라믹학회지
    • /
    • 제39권8호
    • /
    • pp.750-757
    • /
    • 2002
  • Photosensitive sol solution을 이용한 self pattern된 박막은 photoresist/dry etching process에 비해 박막의 제조과정이 간단하다는 장점을 가지고 있다. 이 연구에서는 photosensitive sol solution을 이용하여 spin coating법에 의해 $Sr_{0.9}Bi_{2.1}Ta_2O_9$의 조성을 갖는 강유전체 박막을 제조하였으며 출발원료는 $Sr(OC_2H_5)_2,\;Bi(TMHD)_3$$Ta(OC_2H_5)_5$를 사용하였다. SBT 박막에 UV 노광시간을 증가시킴에 따라 M-O-M 결합이 생성되면서 metal ${\beta}$-diketonate의 UV 흡수 피크 강도는 감소되었고 SBT 박막에 UV 조사에 따른 용해도 차이가 생기면서 fine patterning을 얻을 수 있었다. 또한 UV가 조사된 SBT 박막의 강유전 특성이 UV가 조사되지 않은 것보다 우수하였다.

MOD법에 의한 강유전성 $Sr_xBi_yTa_2O_{9+\alpha}$(SBT) 박막의 제조 및 후열처리 효과에 관한 연구 (Fabrication and Post-Annealing Effects of Ferroelectric $Sr_xBi_yTa_2O_{9+\alpha}$(SBT) Thin Films by MOD Process)

  • 정병직;신동석;윤희성;김병호
    • 한국전기전자재료학회논문지
    • /
    • 제11권3호
    • /
    • pp.229-236
    • /
    • 1998
  • Ferroelectric $Sr_xBi_yTa_2O_{9+\alpha}$/(0.7$\leqSr\leq1.0,\; 2.0\leqBi\leq2.6)$ solutions were prepared by MOD (Metalorganic Deposition) process. These solutions were made into thin films with thickness ranging from 1500~2000${\AA}$ by spin coating. The phase transformation of the SBT thin films by variation of annealing temperature and annealing time were observed using high temperature XRD and SEM. The crystallization and grain growth of SBT thin film were accomplished at $800^{\circ}C$ for 30 minutes after deposition of Pt top electrode by sputtering to prevent electrical breakdown. Ferroelectric properties of the SBT thin films were measured in the range of $\pm$3V\; and\; \pm5V$. The specimen with composition ratio of Sr/Bi/Ta (0.8/2.4/2.0) has the excellent ferroelectric properties ; $2P_r = 10.5,\; 13.2\muC/cm^2 \;at\; \pm3V\; and\; \pm5V$ respectively. Observing the post annealed Pt/SBT/Pt interface by SEM, it was found that Pt electrode sputtered on to the SBT thin film penetrated into the hollow on the SBT thin film, thus decreasing the effective insulation thickness. The effective insulation thickness recovered by post annealing, and this was confirmed by leakage current density measurement.

  • PDF

플라스틱 필름 LCD용 연성 박막 다이오드 소자 제작 (Fabrication of Flexible Thin Film Diode Devices for Plastics film LCO)

  • 이찬재;홍성제;한정인;김원근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.218-221
    • /
    • 2002
  • We have successfully developed the high performance flexible thin film diode device for flexible plastic film LCD. For flexible LCD, TFD device must be normally operated under any deformation state. Two type devices, Ti/Ta$_2$O$\sub$5//Ta and Al/Ta$_2$O$\sub$5//Al were fabricated and the symmetry and reliability of those were estimated under various measurement conditions including severely bending states.

  • PDF

ECR-플라즈마 화학 증착법에 의해 제조된 $Ta_2O_5$ 박막의 유전 특성 (Dielectric Characteristics of $Ta_2O_5$ Thin Films Prepared by ECR-PECVD)

  • 조복원;안성덕;이원종
    • 한국세라믹학회지
    • /
    • 제31권11호
    • /
    • pp.1330-1336
    • /
    • 1994
  • Ta2O5 films were deposited on the p-Si(100) substrates by ECR-PECVD and annealed in O2 atmosphere. The thicknesses of Ta2O5/SiO2 layers were measured by an ellipsometer and a cross-sectional TEM. Annealing in O2 atmosphere enhanced the stoichiometry of the Ta2O5 film and reduced the impurity carbon content. Ta2O5 films were crystallized at the annealing temperatures above 75$0^{\circ}C$. The best leakage current characteristics and the maximum dielectric constant of Ta2O5/SiO2 film capacitor were observed in the specimen annealed at $700^{\circ}C$ and 75$0^{\circ}C$, respectively. The flat band voltage of the Al/Ta2O5/SiO2/p-Si MOS capacitor was varied in the range of -0.6~-1.6 V with the annealing temperature. The conduction mechanism in the Ta2O5 film, the variation of the effective oxide charge density with the annealing temperature, and the effective electric field distribution in the Ta2O5/SiO2 double layer were also discussed.

  • PDF

열처리 조건이 PECVD 방식으로 증착된 $Ta_2$$O_5$ 박막 특성에 미치는 영향 (Effect of Annealing Conditions on $Ta_2$$O_5$ Thin Films Deposited By PECVD System)

  • 백용구;은용석;박영진;김종철;최수한
    • 전자공학회논문지A
    • /
    • 제30A권8호
    • /
    • pp.34-41
    • /
    • 1993
  • Effect of high temperature annealing conditions on Ta$_{2}O_{5}$ thin films was investigated. Ta$_{2}O_{5}$ thin films were deposited on P-type silicon substrates by plasma-enhanced chemical vapor deposition (PECVD) using tantalum ethylate. Ta(C$_{2}H_{5}O)_{5}$, and nitrous oxide. N$_{2}$O. The microstructure changed from amorphous to polycrystalline above 700.deg. C annealing temperature. The refractive index, dielectric onstant and leakage current of the film increased as annealing temperature increased. However, annealing in oxygen ambient reduced leakage currents and dielectric constant due to the formation of interfacial SiO$_{2}$ layer. By optimizing annealing temperature and ambient, leakage current lower than 10$^{-8}$ A/cm$^{2}$ and maximum capacitance of 9 fF/${\mu}m^{2}$ could be obtained.

  • PDF

$IrO_2$를 하부전극으로 사용한 $Sr_{0.9}Bi_{2+x}Ta_2O_9$ 박막의 유전 및 전기적 특성 (Dielectric and Electrical Properties of $Sr_{0.9}Bi_{2+x}Ta_2O_9$ Thin Films on $IrO_2$ Electrode)

  • 박보민;송석표;정병직;김병호
    • 한국세라믹학회지
    • /
    • 제37권3호
    • /
    • pp.233-239
    • /
    • 2000
  • Sr0.9Bi2+xTa2O9(x=0, 0.1, 0.2, 0.3) thin films on IrO2/SiO2/Si or Pt/Ti/SiO2/Si substrate were prepared by spin coating method using SBT stock solutions synthesized by MOD process. SBT thin films on IrO2 transformed to layered perovskite phase at $700^{\circ}C$, but showed low breakdown voltage due to their porous microstructure. The smaple of Sr0.9Bi2+xTa2O9 composition showed the best dielectric and electrical properties. When the sample of the same composition was annealed at 80$0^{\circ}C$, the dielectric and electric properties were improved due to the grian growth and dense surface. the remanent polarization values(2Pr) at $\pm$3 V for IrO2 and Pt electrodes were 10.5, 7.15$\mu$C/$\textrm{cm}^2$, respectively. The SBT thin film with IrO2 electrode showed the lower coercive field. The leakage current density and breakdown voltage of SBT thin films on IrO2 were higher than those on Pt.

  • PDF