$SrZrO_3 $박막의 접착강도에 미치는 Sr/Zr 몰비와 유기화합물 첨가효과 (Effect of Sr/Zr Ratio and Organic Vehicle Addition on Bond Strength of $SrZrO_3 $ Thin Films)

  • 이세종;이득용;예경환;송요승
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제4권1호
    • /
    • pp.13-16
    • /
    • 2002
  • $SrZrO_3 $resistive oxide barriers on Ag sheathed Bi2223 tapes were prepared by the sol-gel and dip coating method to reduce AC coupling loss. The performance of the dip-coated $SrZrO_3 $ thin films was evaluated in terms of bond strength by varying the Sr/Zr mol ratio and the amount of organic vehicle (ethyl cellulose and a-terpineol) additives. The bond strength of the coatings increased as the Sr/Zr ratio decreased and the amount of organic vehicle rose, respectively. It was found that the effect of organic vehicle addition was more pronounced, suggesting that the adherence of the $SrZrO_3 $ films on Bi2223 tapes was governed primarily by the amount of organic vehicle additive.

폴리카본산계 고성능감수제를 사용한 콘크리트의 특성연구 (Study on The Properties of The Concrete with Polycarboxylate Superplasticizer)

  • 오병환;김기완;박대균
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.277-280
    • /
    • 2004
  • Recently, as structure is more higher and bigger, we need high strength and high performance concrete. Therefore it is necessary superplasticizer for high strength and high performance concrete. In this study, it is examined the properties of flow, air content and strength of concrete with polycarboxylate superplasticizer in comparison with existing superplasticizer. First, The slump loss of concrete used polycarboxylate superplasticizer showed 2cm until 120 minutes. Second, The air content loss of concrete used polycarboxylate superplasticizer showed $1\%$ until 120 minutes. Third, It is possible to manufacture $1000kgf/cm^2$ strength concrete using polycarboxylate superplasticizer with $806kg/m^3$ cement content, $18\%$ water-binder ratio, $15\%$ silica fume, $10\%$ fly-ash content.

  • PDF

프리믹스 및 포스트믹스 시멘트를 혼입시간이 콘크리트의 압축강도에 미치는 영향 (Effect of Mixing Time of Pre-Mixed Cement and Post-Mixed Cement on the Strength Development of the Concrete)

  • 백성진;이혁;한준희;김종;한민철
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2023년도 봄 학술논문 발표대회
    • /
    • pp.137-138
    • /
    • 2023
  • This study proposed the optimal mixing time for pre-mixed cement and post mixed cement using the statistical analysis method of box plots. Pre-mixed cement can prevent material seegregation, strength loss, and quality variation if mixed for at least 60 seconds, and the data median is shown to be within the box range. Post-mixed cement should be mixed for at least 180 seconds to prevent material segregation, strength loss, and quality variation, and compressive strength tends to increase with longer vibrating times. Therefore, it is suggested that using pre-mixed cement can shorten the vibrating time and increase the productivity of the concrete.

  • PDF

Primary user localization using Bayesian compressive sensing and path-loss exponent estimation for cognitive radio networks

  • Anh, Hoang;Koo, Insoo
    • KSII Transactions on Internet and Information Systems (TIIS)
    • /
    • 제7권10호
    • /
    • pp.2338-2356
    • /
    • 2013
  • In cognitive radio networks, acquiring the position information of the primary user is critical to the communication of the secondary user. Localization of primary users can help improve the efficiency with which the spectrum is reused, because the information can be used to avoid harmful interference to the network while simultaneity is exploited to improve the spectrum utilization. Despite its inherent inaccuracy, received signal strength based on range has been used as the standard tool for distance measurements in the location detection process. Most previous works have employed the path-loss propagation model with a fixed value of the path loss exponent. However, in actual environments, the path loss exponent for each channel is different. Moreover, due to the complexity of the radio channel, when the number of channel increases, a larger number of RSS measurements are needed, and this results in additional energy consumption. In this paper, to overcome this problem, we propose using the Bayesian compressive sensing method with a calibrated path loss exponent to improve the performance of the PU localization method.

저발열시멘트 콘크리트의 기초적 성질에 대한 연구 (A Study on the Properties of Low-Heat Cement Concrete)

  • 문한영;김성수;신화철;강석화
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.57-60
    • /
    • 1997
  • The properties of Low-heat cement are especially in lower heat of hydration than that of other types of cement. In other respect, Low-heat concrete is more advantageous than OPC concrete in chemical resistance, long term age compressive strength, slump loss and resistance to seawater. This paper deals with 28 days age compressive strength and slump loss by elapsed time of mortar and concrete that made with Low-heat cement and 3 types of other cement.

  • PDF

고온을 받은 고강도 콘크리트의 역학적 특성에 관한 실험적 연구 (An Experimental Study on the Mechanical Behavior of High-Strength Concretes Subjected to High Temperature)

  • 양근혁;홍성우
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.25-28
    • /
    • 2005
  • The experimental results on the mechanical behavior of high-strength concretes subjected to high temperature were presented. Main variables were heating temperature, heating continuance time, and cooling condition. The compressive strength properties of high strength concrete(HSC) varied differently with temperature than those of normal strength concrete(NSC). HSC had higher rates of strength loss than NSC in the temperature range of between $20^{circ}C$ and $400^{circ}C$. Especially, HSC exploded in $400^{circ}C$ of high temperature.

  • PDF

실리카흄 혼합 고강도 콘크리트의 기초물성에 관한 연구 (A Study on the Fundamental Properties of High-Strength Concrete using Silica Fume)

  • 문한영;김진철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1991년도 가을 학술발표회 논문집
    • /
    • pp.21-25
    • /
    • 1991
  • For the purpose of improving the compressive strength of concrete, the high strength concrete which have the compressive strength about 800kg/$\textrm{cm}^2$ were made by using silica fume and high range water reducing admixture on reducing the water-cement ratio. But the facts that the slump loss of high strength concrete was high and the tensile strength and elastic modulus were not improved enough are indicated to problems which must be solved.

  • PDF

Assessment of strength and durability of bagasse ash and Silica fume concrete

  • Singaram, Jayanthi;Kowsik, Radhika
    • Computers and Concrete
    • /
    • 제17권6호
    • /
    • pp.801-814
    • /
    • 2016
  • An alternative type of building system with masonry units is extensively used nowadays to reduce the emission of CO2 and embodied energy. Long-term performance of such structures has become essential for sustaining the building technology. This study aims to assess the strength and durability properties of concrete prepared with unprocessed bagasse ash (BA) and silica fume (SF). A mix proportion of 1:3:3 was used to cast concrete cubes of size $100mm{\times}100mm{\times}100mm$ with various replacement levels of cement and tested. The cubes were cast with zero slump normally adopted in the manufacturing of hollow blocks. The cubes were exposed to acid attack, alkaline attack and sulphate attack to evaluate their durability. The mass loss and damages to concrete for all cases of exposures were determined at 30, 60, and 90 days, respectively. Then, the residual compressive strength for all cases was determined at the end of 90 days of durability test. The results showed that there was slight difference in mass loss before and after exposure to chemical attack in all the cases. Though the appearance was slightly different than the normal concrete the residual weight was not affected. The compressive strength of 10% bagasse ash (BA) as a replacement for cement, with 10% SF as admixture resulted in better strength than the normal concrete. Hence concrete with 10% replacement with BA along with 10% SF as admixture was considered to be durable. Besides solid concrete cubes, hollow blocks using the same concrete were casted and tested simultaneously to explore the possibility of production of masonry units.

모래 지반 내에 형성된 공극이 전단강도에 미치는 영향 (Effect of Void Formation on Shear Strength of Sand)

  • 최현석;박성식;김창우
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2010년도 춘계 학술발표회
    • /
    • pp.577-583
    • /
    • 2010
  • In this study, the effect of void formation resulting from gas hydrate dissociation or loss of some particles within soil structure on the strength of soil is examined. Beag-ma river sands with uniform gradation were used to simulate a gas hydrate bearing or washable soil structure. Empty capsules for medicine are used to mimic large voids, which are bigger than soil particle. Beag-ma river sand was miced with 8% cement ratio and 14% water content and compacted into a shear box. The number and direction embedded into a specimen. After 4 hours curing, a series of direct shear test is performed on the capsule embedded cemented sands. Shear strength of cemented sands with capsules depends on the volume and direction. The volume and direction formed by voids are most important factors in strength. A shear strength of a specimen with large voids decreases up to 39% of a specimen without void. The results of this study can be used to predict the strength degradation of gas hydrate bearing sediments after dissociation and loss of fine particles within soil structure.

  • PDF

혼화재를 사용한 고강도 경량콘크리트에 관한 실험적 연구 (An Experimental Study on High Strength Lightweight Concrete Using Compound Materials)

  • 김종인;최영화;김정훈
    • 한국산업융합학회 논문집
    • /
    • 제6권2호
    • /
    • pp.115-122
    • /
    • 2003
  • This experimental study on high strength lightweight concrete using compound materials has been performed. In which, expanded clay was used as coarse aggregate, and silica fume and fly ash as admixtures varying by 0, 10% and 0, 5, 10, 15, 20% of cement amount respectively were added. Thus, the properties of fresh and hardened concrete have been investigated. The results of this study can be summarized as follows ; Each slump loss of mixtures replaced fly ash has been decreased by increasing replacement rate. The compressive strength have shown 465, 428 and $401kgf/cm^2$ at 30, 40 and 50% of W/B in 28days respectively, all of which have satisfied the criterion $270kgf/cm^2$ of high strength lightweight concrete. The unit volume weight of hardened concrete has been decreased by increasing replacement rate of silica fume and fly ash, values of which have satisfied the criterion $2000kgf/cm^3$of light weight concrete.