A comparative study on the tensile bonding strength of gold alloy solder joints by dental soldering method (치과용 납착 방법에 따른 금합금 납착 연결부의 인장 결합강도 비교 연구)

  • Cho, Mi-Hyang;Lee, Myung-Kon
    • Journal of Technologic Dentistry
    • /
    • v.30 no.1
    • /
    • pp.49-55
    • /
    • 2008
  • In this study, to provide the fundamental data on stable connection method for successful implants prosthesis, We fabricated the solder joint of gold alloy bar specimens by gas flame soldering method and laser welding and soldering method. It compared and studied the tensile strength of two soldering method by universal testing machine. The results using universal testing machine were as follow : The mean of tensile strength of solder joint bar in gas flame soldering method specimens was 363.89 $\pm$17.62 MPa, and the mean strength of laser welding and soldering method was 125.91 $\pm$ 19.66 MPa, so gas flame soldering method was better than laser welding and soldering method and the finding better way to improve tensile strength is needed in laser welding method. On weak loading condition and the part which is needed an accuracy, laser welding method is more effective and on long-span prosthesis and frequent chewing loading part, laser welding technique is recommended first and applying additional gas flame soldering technique would be better for making much more successful prosthesis.

  • PDF

Mechanical Characteristic Evaluation of Sn-Ag-Cu Lead Free Solder Ball Joint on The Pad Geometry (패드 구조에 따른 Sn-Ag-Cu계 무연 솔더볼 접합부의 기계적 특성평가)

  • Jang, Im-Nam;Park, Jai-Hyun;Ahn, Yong-Sik
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.17 no.2
    • /
    • pp.41-47
    • /
    • 2010
  • The effect of PCB and BGA pad designs was investigated on the mechanical property of Pb-free solder joints. The mechanical property of solder joint was tested by three different test methods of drop impact tests, bending impact test, and high speed shear test. Two kinds of pad design such as NSMD (Non-Solder Mask Defined) and SMD (Solder Mask Defined) were applied with the OSP finished Pb-free solder (Sn-3.0Ag-0.5Cu, Sn-1.2Ag-0.5Cu). in the drop impact test and bending impact test, the characterized lifetime showed the same tendency, and SMD design showed better mechanical property of solder joint than NSMD regardless of test method, which was due to the different crack path. The fracture crack on SMD pad was propagated along the intermetallic compound (IMC) layer of solder joint, while the fracture crack on NSMD pad propagated through upper edge of land which shields pattern. In the high speed shear test, pad lift occurred on the solder joint of NSMD. SMD/SMD combination of pad design consequently illustrated the best mechanical property of BGA/PCB solder joint, followed by SMD/NSMD, NSMD/SMD, and NSMD/NSMD.

Evaluation and Test Method Characterization for Mechanical and Electrical Properties in BGA Package (BGA 패키지의 기계적${\cdot}$전기적 특성 평가 및 평가법)

  • Koo Ja-Myeong;Kim Jong-Woong;Kim Dae-Gon;Yoon Jeong-Won;Lee Chang-Yong;Jung Seung-Boo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.4 s.37
    • /
    • pp.289-299
    • /
    • 2005
  • The ball shear force was investigated in terms of test parameters, i.e. displacement rate and probe height, with an experimental and non-linear finite element analysis for evaluation of the solder joint integrity in area array packages. The increase in the displacement rate and the decrease in the probe height led to the increase in the shear force. Excessive probe height could cause some detrimental effects on the test results such as unexpected high standard deviation and probe sliding from the solder ball surface. The low shear height conditions were favorable for assessing the mechanical integrity of the solder joints. The mechanical and electrical properties of the Sn-37Pb/Cu and Sn-3.5Ag/Cu BGA solder joints were also investigated with the number of reflows. The total thickness of the intermetallic compound (IMC) layers, consisting of Cu6Sn5 and Cu3Sn, was increased as a function of cubic root of reflow time. The shear force was increased up to 3 or 4 reflows, and then was decreased with the number of reflows. The fracture occurred along the bulk solder, in irrespective of the number of reflows. The electrical resistivity was increased with increasing the number of reflows.

  • PDF

A Study on the Microstructure and Adhesion Properties of Sn-3.5Ag/Alloy42 Lead-Frame Solder Joint (Sn-3.5Ag/Alloy42 리드프레임 땜납접합의 미세조직과 접합특성에 관한 연구)

  • Kim, Si-Jung;Bae, Gyu-Sik
    • Korean Journal of Materials Research
    • /
    • v.9 no.9
    • /
    • pp.926-931
    • /
    • 1999
  • The microstructure, wettability, shear strength and aging effect of Sn-3.5Ag/Cu and Alloy42 lead-frame solder joints were measured for comparison. In the case of Sn-3.5Ag/Cu, $Ag_3Sn and Cu_6Sn_5$ phases in the matrix Sn and $1~2\mu\textrm{m}$ thick $Cu_6Sn_5$ phase at the interface of solder/lead-frame were formed. In the case of Sn-3.5Agl Alloy42, only AgJSn phase of low density in the matrix Sn and $0.5~1.5\mu\textrm{m}$ thick $FeSn_2$, phase at the interface of solder/leadframe were formed. Comparing to Cu, Alloy42 showed wider area of spread and smaller contact angle, thus better wet­tability. But shear strength and ductility of Alloy 42 solder joints were only 33% and 75% of those of Cu, respectively After aging at $180^{\circ}C$ for 1 week, $\xi-Cu_3Sn$ layer on $\eta-Cu_6Sn_5$ layer was formed on Cu lead-frame, while coarsened cir­cular $Ag_3Sn$ phase in the matrix and thickened $FeSn_2$, at the interface were formed on Alloy42 lead- frame.

  • PDF

Effects of Temperature and Mechanical Deformation on the Microhardness of Lead free and Composite Solders (무연 복합 솔더의 미소경도에 미치는 기계적 변형과 온도의 영향)

  • Lee Joo Won;Kang Sung K.;Lee Hyuck Mo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.2 s.35
    • /
    • pp.121-128
    • /
    • 2005
  • Solder joints in microelectronic devices are frequently operated at an elevated temperature in service. They also experience plastic deformation caused by temperature excursion and difference in thermal expansion coefficients. Deformed solders can go through a recovery and recrystallization process at an elevated temperature, which would alter their microstructure and mechanical properties. In this study, to predict the changes in mechanical properties of Pb-free solder joints at high temperatures, the high temperature microhardness of several Pb-free and composite solders was measured as a function of temperature, deformation, and annealing condition. Solder alleys investigated include pure Sn, Sn-0.7Cu, Sn-3.5Ag, Sn-3.8Ag-0.7Cu, Sn-2.8Ag-7.0Cu (composite), and Sn-2.7Ag-4.9Cu-2.9Ni (composite). Numbers are all in wt.$\%$ unless specified otherwise. Solder pellets were cast at two cooling rates (0.4 and $7^{\circ}C$/s). The pellets were compressively deformed by $30\%$ and $50\%$ and annealed at $150^{\circ}C$ for 2 days. The microhardness was measured as a function of indentation temperature from 25 to $130^{\circ}C$. Their microstructure was also evaluated to correlate with the changes in microhardness.

  • PDF

Applications of neural networks in manufacturing process monitoring and control

  • Cho, Hyung-Suck
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 1992.10b
    • /
    • pp.11-21
    • /
    • 1992
  • Modern manufacturing process requires machine intelligence to meet the demands for high technology products as well as intelligence-based operating skills to lessen human worker's intervene. To meet this trend there has been wide spread interest in applying artificial neural network(ANN) to the areas of manufacturing process monitoring and control. This paper addresses application problems in such processes as welding, assembly, hydroforming process and inspection of solder joints.

  • PDF

Evaluation of Mechanical Property for Pb-free Solder/Ni Plate Joints with Artificial Aging Time (인공시효시간에 따른 Ni 기판 Pb-free 솔더접합부의 기계적 물성평가)

  • Park, So Young;Yang, Sung Mo;Yu, Hyo Sun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.5
    • /
    • pp.467-471
    • /
    • 2015
  • Thus far, solders used in electronics remain lead-based. Pb-free solutions in electronic components and systems are receiving increased attention in the semiconductor and electronics industries. Pb-free materials currently in used are Sn-37Pb, Sn-4Ag and Sn-4Ag-0.5Cu/Ni plate joints. In this study, solder alloys were used at high temperatures for artificial aging processing that was performed at $150^{\circ}C$ for 0hr, 100hr, 200hr, 400hr, 600hr and 1000hr. The SP test was conducted at $30^{\circ}C$ and $50^{\circ}C$. As a result, the maximum shear strength of all the specimens decreased with the increase in artificial aging time and temperature of the SP test. In addition, Pb-free solders showed higher total fracture energy compared with Sn-37Pb at high temperatures. The mechanical properties of Sn-4Ag-0.5Cu solder/Ni plate joints remained in excellent conditions in electronic parking systems at high temperatures.

Electromigration and Thermomigration in Flip-Chip Joints in a High Wiring Density Semiconductor Package

  • Yamanaka, Kimihiro
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.18 no.3
    • /
    • pp.67-74
    • /
    • 2011
  • Keys to high wiring density semiconductor packages include flip-chip bonding and build-up substrate technologies. The current issues are the establishment of a fine pitch flip-chip bonding technology and a low coefficient of thermal expansion (CTE) substrate technology. In particular, electromigration and thermomigration in fine pitch flipchip joints have been recognized as a major reliability issue. In this paper, electromigration and thermomigration in Cu/Sn-3Ag-0.5Cu (SAC305)/Cu flip-chip joints and electromigration in Cu/In/Cu flip chip joints are investigated. In the electromigration test, a large electromigration void nucleation at the cathode, large growth of intermetallic compounds (IMCs) at the anode, a unique solder bump deformation towards the cathode, and the significantly prolonged electromigration lifetime with the underfill were observed in both types of joints. In addition, the effects of crystallographic orientation of Sn on electromigration were observed in the Cu/SAC305/Cu joints. In the thermomigration test, Cu dissolution was accelerated on the hot side, and formation of IMCs was enhanced on the cold side at a thermal gradient of about $60^{\circ}C$/cm, which was lower than previously reported. The rate of Cu atom migration was found comparable to that of electromigration under current conditions.