• 제목/요약/키워드: p-doped

검색결과 801건 처리시간 0.039초

Characteristic in Mg-doped p-type GaN changing activation temperature in $N_2$ gas ambient

  • Lee, Sung-Ho;Kim, Chul-Joo;Seo, Yong-Gon;Seo, Mun-Suek;Hwang, Sung-Min
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.113-114
    • /
    • 2008
  • Conventional furnace annealing (CFA) for activating Mg-doped p-type GaN films had been performed in pure $N_2$ ambient. All sample activated the same gas ambient. The annealing process change temperature: the first process is performed at $550^{\circ}C$ for 10 min. but, the first process is the same bulk. From second to five process increase activation temperature to change $50^{\circ}C$ and annealing time keeping for 10 min. It is found that the samples characteristic measure hall measurement. Similar results were also evidenced by photoluminescence (PL) measurement.

  • PDF

Characterization of Monocrystalline $\beta-SiC$ Thin Film Grown by Chemical Vapor Deposition

  • 김형준
    • 한국세라믹학회:학술대회논문집
    • /
    • 한국세라믹학회 1986년도 Priceedings Of The Third Korea-Japan Seminar On New Ceramics
    • /
    • pp.287-304
    • /
    • 1986
  • High quality monocrystalline $\beta$-SiC thin films were grown via two-step process of conversion of the Si(100) surface by reaction with $C_2H_4$ and the subsequent chemical vapor deposition (CVD) at $1360^{\circ}C$ and 1 atm total pressure. Four dopants, B and Al and p-type, and N and P for n-type, were also incorporated into monocrystalline $\beta$-SiC thin films during the CVD growth process. IR and Raman spectroscopies were used to evaluate the quality of the undoped $\beta$-SiC thin films and to investigate the effects of dopants on the structure of the doped $\beta$-SiC thin films. The changes in the shape of IR and Raman spectra of the doped thin films due to dopants were observed. But the XTEM micrographs except for the B-doped and annealed films showed the same density and distribution of stacking faults and dislocations as was seen in the undoped samples, The IR and Raman spectra of the B-doped and annealed films showed the broad and weak bands and one extra peak at the 850 $cm^{-1}$ respectively. The SAD pattern and XTEM micrograph of the B-doped and annealed film provided the evidence for twinning.

  • PDF

펄스 레이저 증착법에 의해 증착된 Phosphorus 도핑된 ZnO 박막의 특성 분석 (Characterization of Phosphorus Doped ZnO Thin Films grown by Pulsed Laser Deposition Method)

  • 임성훈;강홍성;김건희;장현우;이상렬
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.55-56
    • /
    • 2005
  • The properties of phosphorus doped ZnO thin films deposited on (001) sapphire substrates by pulsed laser deposition (PLD) were investigated depending on various deposition conditions. The phosphorus (P) doped ZnO target was composed of ZnO + x wt% Al (x=1, 3, 5). The structural, electrical and optical properties of the ZnO thin films were measured by X-ray diffraction (XRD), Hall measurements and photoluminescence (PL). As the deposition temperature optimized, the electrical properties of the phosphorus doped ZnO (ZnO:P) layer showed a electron concentration of $7.76\times10^{16}/cm^3$, a mobility of 10.225 $cm^2/Vs$, a resistivity of 7.932 $\Omega$cm. It was observed the electrical property of the film was changed by dopant activation effect as target variations and deposition conditions.

  • PDF

PLD법을 이용한 Buffer Layer 증착온도에 따른 As-doped ZnO 박막의 특성 (Characteristics of As-doped ZnO thin films with various buffer layer temperatures prepared by PLD method)

  • 이홍찬;심광보;오영제
    • 센서학회지
    • /
    • 제15권2호
    • /
    • pp.84-89
    • /
    • 2006
  • Highly concentrated p-type ZnO thin films can be obtained by doping of N, P and As elements. In this study, undoped ZnO buffer layers were prepared on a (0001) sapphire substrate by a ultra high vaccum pulsed laser deposition(UHV-PLD) method. ZnO buffer layers were deposited with various deposition temperature($400{\sim}700^{\circ}C$) at 350 mtorr of oxygen working pressure. Arsenic doped(1 wt%) ZnO thin films were deposited on the ZnO buffer layers by UHV-PLD. Crystallinity of the samples were evaluated by X-ray diffractometer and scanning electron microscopy. Optical, electrical properties of the ZnO thin films were estimated by photoluminescence(PL) and Hall measurements. The optimal condition of the undoped ZnO buffer layer for the deposition of As-doped ZnO thin films was at $600^{\circ}C$ of deposition temperature.

HVPE에 의한 불순물이 첨가된 GaN 박막의 제작 (The preparation of the doped GaN thin films by HVPE)

  • 정성훈;송복식;문동찬;김선태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 춘계학술대회 논문집
    • /
    • pp.66-69
    • /
    • 1997
  • The p-GaN fins doped with the impurity of Zn were grown on n-GaN films to prevent the defects from the lattice mismatch with sapphire substrates by HVPE. For growth of the high quality n-GaN, the optimized conditions were at first deduced from the results of various HCI gas flow rates and growth temperatures. On the basis of these conditions, p-GaN films were grown and investigated of the characteristics. The FWHM of the double crystal rocking curve of n-GaN was decreased and the hexagonal phases on the surface of GaN films were tend to be vivid with the inoement of HCI gas flow rates. Finally the n-type GaN films with FWHM of 648arcsec were obtained at 10cc/min of HCI gas. As the GaN films were grown with the above conditions, Zn was introduced in the form of vapor as a dopant for p-GaN films. But when Zn vaporized at 77$0^{\circ}C$ was doped to the films, the crystallites of Zn were distributed uniformly on the surface of the GaN film due to the over-doped.

  • PDF

Highly Sensitive and Selective Trimethylamine Sensor Using Yolk-shell Structured Mo-doped Co3O4 Spheres

  • Kim, Tae-Hyung;Kim, Ki Beom;Lee, Jong-Heun
    • 센서학회지
    • /
    • 제28권5호
    • /
    • pp.271-276
    • /
    • 2019
  • Pure and 0.5, 1, 2, 5, and 10 at% of Mo-doped $Co_3O_4$ yolk-shell spheres were synthesized by ultrasonic spray pyrolysis of droplets containing Co nitrate, ammonium molybdate, and sucrose and their gas sensing characteristics to 5 ppm trimethylamine (TMA), ethanol, p-xylene, toluene, ammonia, carbon monoxide, and benzene were measured at $225-325^{\circ}C$. The sensor using pure $Co_3O_4$ yolk-shell spheres showed the highest response to p-xylene and very low response to TMA at $250^{\circ}C$, while the doping of Mo into $Co_3O_4$ tended to increase the overall responses of gas sensors. In particular, the sensor using 5 at% Mo-doped $Co_3O_4$ yolk-shell spheres exhibited the high response to TMA with low cross-responses to other interfering gases. The high response and selectivity of Mo-doped $Co_3O_4$ yolk-shell spheres to TMA are attributed to the electronic sensitization by higher valent Mo doping and acid-base interaction between TMA and Mo components.

전자상자성공명을 이용한 $Poly-Si/SiO_2$ 박막의 결함연구 : 플라즈마 수소화처리에 따른 결함밀도의 변화 (A Study of Defects in $Poly-Si/SiO_2$ Thin Films Using Electron Paramagnetic Resonance : Defect Density Changes due to Plasma Hydrogenation Treatment)

  • 노승정;장혁규
    • 한국자기학회지
    • /
    • 제8권6호
    • /
    • pp.346-349
    • /
    • 1998
  • Poly-Si 활성층이 도핑되지 않은 도는 BF2 이온주입으로 도핑된 poly-Si/SiO2 박막에 존재하는 결함을 효과적으로 감소시키기 위하여 저온 rf 수소플라즈마 처리를 수행하였고, 결합의 변화를 전자상자성공명을 이용하여 조사하엿다. 활성층이 도핑되지 않은 시편과 도핑된 시편에서 모두 관측되었던 Pb center와 E' center가 30분의 수소화처리 결과, Pb center의 경우에 각각 80%(도핑되지 않은 시편)와 76% (되핑된 시편)의 큰 결함 감소효과를 얻었으며 E center는 제거되어 관측되지 않았다. 90분의 처리공정에서는 두 시편에서 모두 감소되었던 Pbcenter의 밀도가 다시 증가하였으며, 제거되었던 E' center가 재생되엇다. 특히 도핑된 시편에서의 Pbcenter의 밀도증가가 더욱 민감하게 나타났다.

  • PDF

Optimization of $p^+$ seeding layer for thin film silicon solar cell by liquid phase epitaxy

  • Lee, Eun-Joo;Lee, Soo-Hong
    • 한국결정성장학회지
    • /
    • 제15권6호
    • /
    • pp.260-262
    • /
    • 2005
  • Thickness optimization of heavily doped p-type seeding layer was studied to improve performance of thin film silicon solar cell. We used liquid phase epitaxy (LPE) to grow active layer of $25{\mu}m$ thickness on $p^+$ seeding layer. The cells with $p^+$ seeding layer of $10{\mu}m\;to\;50{\mu}m$ thickness were fabricated. The highest efficiency of a cell is 12.95%, with $V_{oc}=633mV,\;J_{sc}=26.5mA/cm^2$, FF = 77.15%. The $p^+$ seeding layer of the cell is $20{\mu}m$ thick. As thicker seeding layer than $20{\mu}m$, the performance of the cell was degraded. The results demonstrate that the part of the recombination current is due to the heavily doped seeding layer. Thickness of heavily doped p-type seeding layer was optimized to $20{\mu}m$. The performance of solar cell is expected to improve with the incorporation of light trapping as texturing and AR coating.

NH3 분위기에서 후속 열처리에 의한 p형 ZnO 형성 (Formation of N Doped, p-type ZnO Films by Post-annealing in NH3 Ambient)

  • 정은수;김홍승;조형균
    • 한국전기전자재료학회논문지
    • /
    • 제19권7호
    • /
    • pp.611-617
    • /
    • 2006
  • We report the preparation of N doped, p-type ZnO films by post-annealing in $NH_3$ ambient. The properties were examined by XRD, Hall-effect measurement, PL, and SIMS. ZnO films showed better crystallinity and electron concentration of $10^{15}-10^{17}/cm^3$ with post-annealing in $NH_3$ ambient. These films were converted to p-type ZnO by activation thermal annealing process at $800^{\circ}C$ under $N_2$ ambient. The electrical properties of the p-type ZnO showed a hole concentration of $1.06\times10^{16}/cm^3$, a mobility of $15.8cm^2/V{\cdot}s$, and a resistivity of $40.18\Omega{\cdot}cm$. The N doped ZnO films showed a strong photoluminescence peak at 3.306 eV at 13 K, which is closely related to neutral acceptor bound excitons of the p-type ZnO:N. In the SIMS spectra, the incorporation of nitrogen was confirmed.

질소 도핑된 P/P- Epitaxial Silicon Wafer의 Slip 및 강도 평가 (Evaluation of Slip and Strength of Nitrogen doped P/P- Epitaxial Silicon Wafers)

  • 최은석;배소익
    • 한국재료학회지
    • /
    • 제15권5호
    • /
    • pp.313-317
    • /
    • 2005
  • The relation between bulk microdefect (BMD) and mechanical strength of $P/P^-$ epitaxial silicon wafers (Epitaxial wafer) as a function of nitrogen concentrations was studied. After 2 step anneal$(800^{\circ}C/4hrs+1000^{\circ}C/16hrs)$, BMD was not observed in nitrogen undoped epitaxial silicon wafer while BMD existed and increased up to $3.83\times10^5\;ea/cm^2$ by addition of $1.04\times10^{14}\;atoms/cm^3$ nitrogen doping. The slip occurred for nitrogen undoped and low level nitrogen doped epitaxial wafers. However, there was no slip occurrence above $7.37\times10^{13}\;atoms/cm^3$ nitrogen doped epitaxial wafer. Mechanical strength was improved from 40 to 57 MPa as nitrogen concentrations were increased. Therefore, the nitrogen doping in silicon wafer plays an important role to improve BMD density, slip occurrence and mechanical strength of the epitaxial silicon wafers.