• 제목/요약/키워드: hydroxyapatite (HA)

검색결과 244건 처리시간 0.026초

RF 스퍼터링용 Hydroxyapatite 타겟의 제조 및 Hydroxyapatite/Ti-6Al-4V 합금 박막의 특성(I) (The Fabrication of Hydroxyapatite Targets and the Characteristics of Hydroxyapatite/Ti-6Al-4V Alloy Thin Films by RF Sputtering(I))

  • 정찬회;김명한
    • 한국재료학회지
    • /
    • 제13권4호
    • /
    • pp.205-212
    • /
    • 2003
  • RF sputtering process was applied to produce thin hydroxyapatite[HA, Ca10($PO_4$)$_{6}$ $ (OH)_2$films on Ti-6Al-4V alloy substrates. To make a 101.6 mm dia.${\times}$5 mm HA target, the commercial HA powder was first calcinated for 3h at $200^{\circ}C$. A certain amount of the calcinated HA powder was pressed under a pressure of 20,000 psi by the cold isostatic press(CIP) and the pressed HA target was sintered for 6 h at $1,200^{\circ}C$. The effects of different heat treating conditions on the bonding strength between HA thin films and Ti-6Al-4V alloy substrates were studied. Before deposition, the alloy substrates were annealed for 1 h at $850^{\circ}C$ under $3.0${\times}$10^{-3}$ Xtorr, and after deposition, the hydroxyapatite/Ti-6Al-4V alloy thin films were annealed for 1 h at 400, 600 and $800^{\circ}C$ under the atmosphere, respectively. Experimental results represented that the HA thin films on the annealed substrates had higher hardness than non-heat treated substrates before the deposition.

천연 및 인공원료로부터 제조한 생체친화형 하이드록시아파타이트 세라믹스 (Biocompatible Hydroxyapatite Ceramics Prepared from Natural Bones and Synthetic Materials)

  • 이종국;고영화;이난희
    • 한국재료학회지
    • /
    • 제22권6호
    • /
    • pp.285-291
    • /
    • 2012
  • Hydroxyapatite (HA) is well known as a biocompatible and bioactive material. HA has been practically applied as bone graft materials in a range of medical and dental fields. In this study, two types of dense hydroxyapatite ceramics were prepared from natural bones and synthetic materials. The biocompatibility of HA ceramics for supporting osteoblast cell growth and cytotoxicity using an in vitro MG-63 cell line model were respectively evaluated. Artificial hydroxyapatite shows relative density of 93% with 1-2 ${\mu}m$ after sintering, but a hydroxyapatite compact derived from bovine bone has low sintered density of 85% with a small content of MgO. Irrespective of the starting raw materials, both types of sintered hydroxyapatite displayed similar biocompatibility in the tests. FE-SEM observations showed that most MG-63 cells had a stellar shape and formed an intercellular matrix containing fibers on sintered HA. The cells were well attached and grown over the HA surface, indicating that there was no toxicity.

플라즈마 용사법에 의한 Hydroxyapatite 코팅의 용사조건에 관한 연구 (Study on the Spraying Parameters of a Plasma-sprayed Hydroxyapatite Coating)

  • 여인웅;안효석
    • 한국세라믹학회지
    • /
    • 제36권4호
    • /
    • pp.444-450
    • /
    • 1999
  • Hydroxyapatite(HA) was spray-coated to alloy substrate(Ti-6Al-4V) using plasma-spray process for bioceramic application The coating morphology composition and crystallinity were influenced by following process parameters ; stand-off distance spray power level and auxiliary gas pressure. These parameters have been systematically varied in the present study to evaluate their relative influence on the coating qual-ity and to seek an optimum spraying condition. Amorphicity and decomposition of HA increased with stand-off distance and the imperfect coating layer was obtained at the short stant-off distance (55mm). The cry-stallinity of HA coating decreased with spray power level and auxiliary gas pressure but the bond strength between the HA coated layer and Ti alloy substrate increased with the spray power level.

  • PDF

Enhanced Hemolytic Biocompatibility of Hydroxyapatite by Chromium (Cr3+) Doping in Hydroxyapatite Nanoparticles Synthesized by Solution Combustion Method

  • Bandgar, Sneha S.;Yadav, Hemraj M.;Shirguppikar, Shailesh S.;Shinde, Mahesh A;Shejawal, Rajendra V.;Kolekar, Tanaji V.;Bamane, Sambhaji R.
    • 한국세라믹학회지
    • /
    • 제54권2호
    • /
    • pp.158-166
    • /
    • 2017
  • For the better success of biomedical implant surgery, we used a modified solution combustion method to synthesize Hydroxyapatite (HA) and Chromium ($Cr^{3+}$) modified Cr-HA with different concentrations of 0.5, 1.0, 1.5, 2.0 and 2.5. The Cr-HA nanopowder was characterized by TGA, XRD, SEM-EDS and TEM. The HA and Cr-HA powders were subjected to in vitro biological studies to determine their biocompatibility and hemocompatibility. The cytotoxicity of HA and Cr-HA were evaluated on Hela (Cervical cancer) cells and L929 (mouse fibroblast) cells by using MTT assay. Hemocompatibility studies demonstrated a noticeable haemolytic ratio below 5%, which confirms that these materials are compatible in nature with human blood. The results of the present work confirm that the synthesised HA and Cr-HA are biocompatible and can be extensively used in the biomedical field to improve overall material biological properties.

참치 뼈로부터 수산화아파타이트 분말의 제조 및 소결 특성 (Preparation of Hydroxyapatite Powder Derived from Tuna Bone and Its Sintering Property)

  • 서동석;김용국;황규홍;이종국
    • 한국세라믹학회지
    • /
    • 제45권10호
    • /
    • pp.594-599
    • /
    • 2008
  • Hydroxyapatite(HA) was prepared from waste tuna bone, and its sintering property and dissolution behavior were investigated. Tuna bone derived-HA powder consisted of mainly HA and small amount of MgO. Porous HA ceramics with sintered density of 79% was obtained by pressureless sintering at $1200^{\circ}C$. Meanwhile, HA ceramics prepared by hot pressing at $1000^{\circ}C$ showed dense microstructure with sintered density of 95%. Immersion test revealed that both porous and dense HA ceramics were stable in liquid environment without distinct evidence of surface dissolution. It may be assumed that the presence of Mg in tuna bone-derived HA may improve dissolution resistance of HA.

수산화인회석 코팅 임프란트의 골치유과정에 관한 실험적 연구 (Experimental study about the bony healing of hydroxyapatite coating implants)

  • 엄태관;김종화;조인희;정창모;조용석;김영균
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제37권4호
    • /
    • pp.295-300
    • /
    • 2011
  • Introduction: Hydroxyapatite(HA) coating implant can accelerate osseointegration, however, there are many controversies. Materials and Methods: This study examined the early osseointegration of two types of hydroxyapatite coated implants. Twelve adult male miniature pigs (Medi Kinetics Micropigs, Medi Kinetics Co., Ltd., Busan, Korea) were used in this study. In the implants placed in the mandible, a histomorphometric evaluation was performed to evaluate the bone-implant contact (BIC) ratio. Results: The BIC ratio increased with time. TS III HA and Zimmer HA were not significantly different (P>0.05). At 8 weeks, the BIC of Zimmer HA was higher than TS III HA, but there was no significant difference (P>0.05). Conclusion: HA coated implants will accelerate early osseointegration.

수산화인회석과 폴리락타이드 복합체에서 상호작용력의 도입 (Introduction of Specific Interaction of Hydroxyapatite/Polylactide Composites)

  • 강진규;임준혁;문명준;이원기;김미라;이진국
    • 폴리머
    • /
    • 제33권1호
    • /
    • pp.13-18
    • /
    • 2009
  • 인공뼈의 잠재적인 재료로서 주목을 받는 hydroxyapatite(HA)와 Poly(L-lactide)(PLLA) 복합체의 물성을 개선하기 위하여 HA에 D-lactide(DLA)를 표면 그래프트(g-HA)하여 PLLA 사이의 스테레오 콤프렉스 형성을 도입하였다. 복합체 필름은 건조단계에서 HA의 침전을 최소화하기 위하여 용매-비용매법으로 제조하였다. 복합체의 구조와 물성은 thermal gravimetric analysis(TGA), differential scanning calorimeter, scanning electron microscopy 및 mechanical property 측정으로 확인하였다. TGA분석으로부터 HA에 대한 DLA의 표면 그래프트율은 6 wt%였고 HA에 비하여 유기용매에 대한 분산성이 증가하였다. 복합체의 스테레오 콤프렉스 형성은 용융온도의 변화로써 확인하고 HA/PLLA 복합체에 비하여 우수한 기계적 물성을 나타내었다.

Facile Synthesis of Hydroxyapatite by Hydrothermal and Solvent Combustion Methods

  • Bramhe, Sachin N;Lee, Hyun Chul;Chu, Min Cheol;Ryu, Jae-Kyung;Balakrishnan, Avinash;Kim, Taik Nam
    • 한국재료학회지
    • /
    • 제25권9호
    • /
    • pp.492-496
    • /
    • 2015
  • Hydroxyapatite (HA), which is an important calcium phosphate mineral, has been applied in orthopedics, dentistry, and many other fields depending upon its morphology. HA can be synthesized with different morphologies through controlling the synthesis method and several parameters. Here, we synthesize various morphologies of HA using two simple methods: hydrothermal combustion and solution combustion. The phase purity of the synthesized HA is confirmed using X-ray diffractometry. It demonstrates that pure phased hydroxyapatite can be synthesized using both methods. The morphology of the synthesized powder is examined using scanning electron microscopy. The effects of pH and temperature on the final powder are also investigated. At $140^{\circ}C$, using the hydrothermal method, nano-micro HA rods with a hexagonal crystal structure can be synthesized, whereas using solution combustion method at $600^{\circ}C$, a dense cubic morphology can be synthesized, which exhibits monoclinic crystal structures.

Ca/P 비에 따른 수산화아파타이트 생체재료의 표면용해 특성 (Surface dissolution of Hydroxyapatite Biomaterials with Ca/P Ratio)

  • 서동석;김환;이종국
    • 한국세라믹학회지
    • /
    • 제41권1호
    • /
    • pp.45-50
    • /
    • 2004
  • Ca/P 비가 각각 1.62, 1.67, 1.72인 수산화아파타이트(Hydroxyapatite, HA) 세라믹스를 제조하고, HA 표면에서 수용액에 의하여 일어나는 용해현상을 고찰하였다. 수용액에서 3일간 침적시킨 경우 입계에서부터 용해가 시작되었으며, 침적시간이 10일로 증가하면서 이러한 입계용해에 의한 HA 세라믹스의 미세구조적 분해 현상은 비화학양론적 조성, 즉 Ca/P 비가 1.62 또는 1.72인 시편에서 두드러지게 나타났다. 주목할만한 것은, 용해가 진행되는 동안 세라믹스의 표면에는 골식세포의 흡수 과정에서 흔히 볼 수 있는 표면 결함(lacunae)과 매우 유사한 모양을 갖는 원형의 빈 공간(cavity)이 형성되었다.

침적법에 의한 수산화아파타이트 코팅 금속재의 기초적 연구 (Hydroxyapatite Coating on Ti Plate by a Dipping Method)

  • 이준희;김석영;김영곤;이인섭
    • 대한의용생체공학회:의공학회지
    • /
    • 제18권3호
    • /
    • pp.217-222
    • /
    • 1997
  • Hydroxyapatite(HA)-coated metal composites were made by the dipping method. The specimen substrates were Ti plates with a thickness of 2 mm. The HA coating was carried out in HA-sol for 1 min by the dipping method. The concentration of HA-sol for the coating ranged from 3.28 to 9.99 wt%. Excellent coating was observed on Ti substrate dipped once in 9.99 wt% sol. Preparation of Ti plates by sandblasting provided the better environment for coating HA on Ti surface than non-treated surface. As the concentration of sol increased, the weight change and the coating thickness increased. Above 7 wt% sol, they increased sharply.

  • PDF