Porcelain Bonding Strength and Mechanical Properties of Sintered Ni-Cr-Ti Alloy for Dental Prosthodontics (치과보철용 Ni-Cr-Ti 소결체합금의 포셀린결합력 및 기계적 특성)

  • Choe, Han-Cheol;Park, Seon-Yeong;Shim, Myung-Sub
    • Journal of the Korean institute of surface engineering
    • /
    • v.49 no.6
    • /
    • pp.560-566
    • /
    • 2016
  • In this study, porcelain bonding strength and mechanical properties of sintered Ni-Cr-Ti alloy for dental prosthodontics have been researched experimentally. Mechanical and morphological characteristics of the alloys were examined by Vickers hardness test, tensile and bonding strength test, surface roughness test, field-emission scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. In the sintered Ni-13Cr-xTi alloys, morphology of sintered alloy showed porous matrix diffused with alloying elements of Cr and Ti, and showed dendritic structure after melting process. From the XRD results, the second phases of NiCr, $Ni_3Cr$, and $Ni_3Ti$ were formed in the case of sintered and melted Ni-13Cr-xTi alloys. The tensile strength and hardness of Ni-13Cr-xTi alloys increased, as Ti content increased. Surface roughness increased, as Ti content increased. The bonding strength between metal and porcelain of Ni-13Cr-5Ti alloy was higher than those of Ni-13Cr and Ni-13Cr-10Ti alloys

Effect of metal conditioner on bonding of porcelain to cobalt-chromium alloy

  • Minesaki, Yoshito;Murahara, Sadaaki;Kajihara, Yutaro;Takenouchi, Yoshihisa;Tanaka, Takuo;Suzuki, Shiro;Minami, Hiroyuki
    • The Journal of Advanced Prosthodontics
    • /
    • v.8 no.1
    • /
    • pp.1-8
    • /
    • 2016
  • PURPOSE. The purpose of this study was to evaluate the efficacy of two different metal conditioners for non-precious metal alloys for the bonding of porcelain to a cobalt-chromium (Co-Cr) alloy. MATERIALS AND METHODS. Disk-shaped specimens ($2.5{\times}10.0mm$) were cast with Co-Cr alloy and used as adherend materials. The bonding surfaces were polished with a 600-grid silicon carbide paper and airborne-particle abraded using $110{\mu}m$ alumina particles. Bonding specimens were fabricated by applying and firing either of the metal conditioners on the airborne-particle abraded surface, followed by firing porcelain into 5 mm in diameter and 3 mm in height. Specimens without metal conditioner were also fabricated. Shear bond strength for each group (n=8) were measured and compared (${\alpha}=.05$). Sectional view of bonding interface was observed by SEM. EDS analysis was performed to determine the chemical elements of metal conditioners and to determine the failure modes after shear test. RESULTS. There were significant differences among three groups, and two metal conditioner-applied groups showed significantly higher values compared to the non-metal conditioner group. The SEM observation of the sectional view at bonding interface revealed loose contact at porcelain-alloy surface for non-metal conditioner group, however, close contact at both alloy-metal conditioner and metal conditioner-porcelain interfaces for both metal conditioner-applied groups. All the specimens showed mixed failures. EDS analysis showed that one metal conditioner was Si-based material, and another was Ti-based material. Si-based metal conditioner showed higher bond strengths compared to the Ti-based metal conditioner, but exhibited more porous failure surface failure. CONCLUSION. Based on the results of this study, it can be stated that the application of metal conditioner is recommended for the bonding of porcelain to cobalt-chromium alloys.

Study of the Bond Strength Between Dental Ceramic Alloys and Porcelain (치과 도재용 합금과 도재간의 결합력에 관한 연구)

  • Yoon, Il-Joong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.19 no.1
    • /
    • pp.29-37
    • /
    • 1981
  • The bond strengths with ceramco porcelain were compared between precious alloy S, and non-precious alloys V.U. and R. And the changes in bond strengths of non-precious alloys with ceramco porcelain, according to surface preparations by sand blasting, longitudinal grinding, transverse grinding, and high polishing, were studied. The test specimens were prepared by firing porcelain doughnuts on the surface prepared alloy rods, and investing in dental stone. The specimens were subjected to shear loading forces. The conclusions drawn from the investigation are as follows: 1. The bond strengths with ceramco porcelain were higher in the non-precious alloys U and R, than in the precious alloy S. 2. The bond strengths were in descending order for R alloy, U alloy, V alloy, and S alloy. 3. The bond strengths were highest when the R alloy and U alloy were surface prepared by sand blasting. 4. All bond strength values were lowest when the alloy surfaces were prepared by high polishing.

  • PDF

A Study of Bond Strength of Nickel-Chromium Alloys with Porcelain in Ceramometal System (상이(霜異)한 Ceramometal System에 있어서 Nickel-Chromium합금과 도재(陶材)와의 결합강도(結合强度)에 관(關)한 비교실험연구(比較實驗硏究))

  • Kim, Chee-Young
    • Journal of Technologic Dentistry
    • /
    • v.7 no.1
    • /
    • pp.19-25
    • /
    • 1985
  • In oder to compare and measure bond strength of ceramometal system with use of ceramco porcelain powder including SnO2 and uni metal, Rexillium III, Vera Bond as non precious alloys manufactured for porecelain-metal restorations. Total 24 test sample were constructed. All Test sample were measured with a Mitutoyo micrometer graduated to 0.01mm. It is as follows measured of thickness 3.3mm(metal : 1.1mm, porcelain: 2.2mm), width 12mm, length 30mm(porcelain 12mm x 12mm), Compared maximum bending stress test. The results obtained were as follows: 1. Bond strength of each metal with ceramco porcelain powder showed statistical significance.(P<0.05) 2. Vera Bond and uni metal, uni metal and Rexillium III revealed no statistical Significance.(P>0.05) Vera Bond and Rexillium III showed statistical significance.(P<0.05) 3. The order of maximum bending stress was Rexillium III, uni metal, vera Bond. The order of bond strength ratio making bending stress was Vera bond, uni metal, Rexillium III.

  • PDF

Spectrophotometic analysis of the influence of substrate on the color of dental ceramics (하부구조물 및 두께에 따른 치과 수복용 세라믹의 색조에 대한 분광측색분석)

  • Song, Young-Gyun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.31 no.2
    • /
    • pp.96-103
    • /
    • 2015
  • Purpose: The purpose of this study was to spectrophotometrically evaluate the influence of porcelain layer thickness and substructure. Materials and Methods: Four groups of porcelain specimens (metal and ceramic substructure) was prepared for analysis. Color parameters were measured with spectrophotometer and color difference (${\Delta}E*$) were calculated. T-test and one-way ANOVA test were used to find out significant difference and Tukey test was used to identify where the difference ware. Results: Increasing the thickness of porcelain decreased values (P < 0.05). Increasing the thickness of porcelain on ceramic substructure decreased the $a^*$ (P < 0.05) but, the $b^*$ were not statistically different. Total color difference (${\Delta}E*$) were below 1 when the difference of porcelain thickness were 0.5 mm. Conclusion: The thickness of porcelain are the factor effecting on color. This study will help the color are controlled by changing the thickness of porcelain clinically.

Comparison of Surface Roughness according to Porcelain Materials and Condensation (도재의 재료와 축성방법에 따른 표면거칠기의 비교)

  • Lee, Cheong-Hee
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.18 no.3
    • /
    • pp.179-184
    • /
    • 2002
  • To compare surface roughness in various porcelains and know effects of condensation, We used Ceramco dentin porcelain, Creation dentin porcelain, Creation margin porcelain, Vintage margin porcelain, Vintage dentin porcelain, and Vita dentin porcelain, and built up the powders with condensation or not, and then fired according to the instructions with porcelain furnace( Dekema, Germany ). We polished the samples step by step using the porcelain adjustment kit( Shofu Inc., Japan ), and then measured, compared and analysed Ra, Rz, and Rmax with Surftest SV-400( Mitutoyo Co., Japan ). 1. With condensation, roughness is significantly increased in Ceramco dentin porcelain (p<0.05) and decreased in Vita dentin porcelain(p<0.05). 2. In Ra, Vita dentin porcelain is significantly the roughest and Creation margin porcelain is rougher than others in no condensation, (p<0.05), and there is no difference under condensation. 3. In Rz, Vita dentin porcelain is significantly the roughest and Creation margin porcelain is rougher than others in no condensation, and Creation margin porcelain is significantly the roughest and Creation dentin porcelain is rougher than others under condensation(p<0.05). 4. In Rmax, Vintage dentin porcelain is significantly the roughest and Creation margin porcelain is rougher than others in no condensation, and Creation margin porcelain is significantly the roughest than others under condensation(p<0.05).

An Experimental Study on the Bond Strength after Surface Treatment of Non-precious Metal Alloy for porcelain Crown (도재용 비금속합금의 표면처리에 따른 결합강도에 관한 실험적 연구)

  • So, Myung-Sub
    • Journal of Technologic Dentistry
    • /
    • v.9 no.1
    • /
    • pp.39-49
    • /
    • 1987
  • This study done to evaluate some surface treatment methods in metal coping which can increase the bond strength between porcelain and metal. Therefore this experiment was performed according to the Mc Lean's Theory of bond strength between porcelain and strength between porcelain and metal. In the experiment the author measured respective thermal expansion coefficents in three types of metal(Tallasium, Vera Bond and Rexillium) and Vita Porcelain to get the differences in the coefficents between porcelain and metals. And using insteron testing machine, the author also performed Planar interface shear bond tests on the 45 specimens(15 specimens in oxide surface, rough surface and fine surface treatment methods respectively) to measure bond strength between metal and porcelain. The results Were as follows, 1. The differences in thermal expansion coefficients between three types of metal and Vita procelain: Talladium - $1.2\;10^{-6/0}\;C$, Vera Bond - $1.6\;10^{-6/0}\;C$, Rexillium - $1.9\;10^{-6/0}\;C$. 2. The bond strength in oxide surface on the Shear bond test was the lowest among the treatment methods. 3. There was no significant differences in treatment methods of rough surface of fine surface. 4. In the oxide surface treatment method, there were significant differences(P<0.05)between Vera bond and Rexillium, and between Talladium and Rexillium. 5. In the fine surface treatment, there was a significant difference(P<0.05)between Talladium and Rexillium.

  • PDF

An Experimental Study on Wear of Porcelain Surface to Natural Teeth and Crown Metal Alloys (자연치아 및 치과용 합금에 대한 도재표면 마모에 관한 실험적 연구)

  • Lee, Nung-Soo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.19 no.1
    • /
    • pp.47-54
    • /
    • 1981
  • Dental porcelains are widely used for restorative material because of its excellent esthetic property. But according to contact with natural teeth or metal in oral cavity, the porcelain may be worn and may effect on masticatory physiology and prosthetic function. The purpose of this experiment was to study on wear of porcelain surface which treated in different method. Using the abrasion device which was designed and constructed by myself, the different porcelain surface were abraded by gold alloy, nickel-chrome alloy and natural teeth in order to compare roughness. Results were as follows. 1. The group of porcelain abraded by gold alloy showed less surface roughness change (t=2.92, p<0.05), and the group of porcelain abraded by natural teeth had high surface roughness. change (t=6.84, p<0.05). 2. According to the method of surface treatment, the surface roughness were very significant (F=9.12, p<0.05). 3. After abrading, the porcelain surface roughness change was very significant (F=54.49, p<0.05). 4. There was no significant between surface treatment method and the kind of abrading materials. (F=1.01, p>0..05). 5. The group of natural glazing had the most smooth surface ($2.1{\pm}1.13{\mu}m$).