An Experimental Study on the Bond Strength after Surface Treatment of Non-precious Metal Alloy for porcelain Crown

도재용 비금속합금의 표면처리에 따른 결합강도에 관한 실험적 연구

  • So, Myung-Sub (Department of Dental Laboratory technology Dea Jeon Medical Junior College)
  • 소명섭 (대전보건전문대학 치과기공과)
  • Published : 1987.06.01

Abstract

This study done to evaluate some surface treatment methods in metal coping which can increase the bond strength between porcelain and metal. Therefore this experiment was performed according to the Mc Lean's Theory of bond strength between porcelain and strength between porcelain and metal. In the experiment the author measured respective thermal expansion coefficents in three types of metal(Tallasium, Vera Bond and Rexillium) and Vita Porcelain to get the differences in the coefficents between porcelain and metals. And using insteron testing machine, the author also performed Planar interface shear bond tests on the 45 specimens(15 specimens in oxide surface, rough surface and fine surface treatment methods respectively) to measure bond strength between metal and porcelain. The results Were as follows, 1. The differences in thermal expansion coefficients between three types of metal and Vita procelain: Talladium - $1.2\;10^{-6/0}\;C$, Vera Bond - $1.6\;10^{-6/0}\;C$, Rexillium - $1.9\;10^{-6/0}\;C$. 2. The bond strength in oxide surface on the Shear bond test was the lowest among the treatment methods. 3. There was no significant differences in treatment methods of rough surface of fine surface. 4. In the oxide surface treatment method, there were significant differences(P<0.05)between Vera bond and Rexillium, and between Talladium and Rexillium. 5. In the fine surface treatment, there was a significant difference(P<0.05)between Talladium and Rexillium.

Keywords