• 제목/요약/키워드: anodization

검색결과 333건 처리시간 0.034초

Formation of Niobium Oxide Film with Duplex Layers by Galvanostatic Anodization

  • Kim, Hyun-Kee;Yoo, Jeong-Eun;Park, Ji-Young;Seo, Eul-Won;Choi, Jin-Sub
    • Bulletin of the Korean Chemical Society
    • /
    • 제33권8호
    • /
    • pp.2675-2678
    • /
    • 2012
  • Studies on niobium anodization in the mixture of 1 M $H_3PO_4$ and 1 wt % HF at galvanostatic anodization are described here in detail. Interestingly, duplex niobium oxide consisting of thick barrier oxide and correspondingly thick porous oxide was prepared at a constant current density of higher than 0.3 $mAcm^{-2}$, whereas simple porous type oxide was formed at a current density of lower than 0.3 $mAcm^{-2}$. In addition, simple barrier or porous type oxide was obtained by galvanostatic anodization at a single electrolyte of either 1 M $H_3PO_4$ or 1 wt % HF, respectively. The formation mechanism of duplex type structures was ascribed to different forming voltages required for moving anions.

실리콘 양극산화 방법에 의한 실리콘내의 보론과 아세닉 확산분포의 측정 (Measurement of diffusion Profiles of Boron and Arsenic in Silicon by Silicon Anodization Method)

  • 박형무;김충기
    • 대한전자공학회논문지
    • /
    • 제18권1호
    • /
    • pp.7-19
    • /
    • 1981
  • 실리콘 양극산화방법으로 실리콘에서의 불순물 분포를 측정하였다. 전해액으로 Ethylene Glycol-KNO3(0.04N)을 사용하였고, 200V의 전압을 가했을 때 한번의 양극산화에 의하여 삭감되는 실리콘 두께는 웨이퍼 타이프에 관계없이 460±40A이다. Predeposition후의 보론과 아세닉의 분포를 구하였고 이 분포에 의하여 불순물 농도에 따른 확산계수를 계산하였다. 또한 npn트란지스터 구조에서 아세닉 에미터와 브론 베이스간의 상호작용에 의한 베이스 pull-in 현상을 관찰하였다.

  • PDF

NaF 전해질 양극산화에 의한 마이크로콘 구조 니오븀 산화물 제조 (Formation of Nb2O5 Microcone Structure in NaF Electrolyte by Anodization)

  • 정봉용;정은혜
    • 한국세라믹학회지
    • /
    • 제48권6호
    • /
    • pp.625-629
    • /
    • 2011
  • In this study, we show that by anodization of Nb in NaF electrolytes microcone niobium oxide layers can be formed under a range of experimental conditions. It is found that a single NaF electrolyte leads to the formation of microcones. At 1 M NaF, 40 V, 1 h, well-ordered microcones were generated on Nb discs. XRD results show that the initially formed anodic oxide is amorphous, but an amorphous to crystalline transition occurs during anodization. For the formation of favorable microcones, it is considered that proper parameters such as electrolyte concentration, voltage, anodizing time are necessary according to the kind of electrolytes.

TiO2 나노튜브 내경 확장을 위한 양극산화 조건 (Anodic Growth of Large Inner Diameter TiO2 Nanotubes)

  • 이현권;오현철;이기영
    • 한국표면공학회지
    • /
    • 제51권1호
    • /
    • pp.27-33
    • /
    • 2018
  • In the present work, we demonstrate the feasibility to form large inner diameter $TiO_2$ nanotubes by anodization of Ti in a HF/ethylene glycol electrolyte. In order to achieve the large inner diameter $TiO_2$ nanotubes, optimization of the anodization condition is required. We discover the key factors in the formation of large inner diameter $TiO_2$ nanotubes are concentration of water in the electrolyte, anodization temperatures, and high-applied potential. Under optimum conditions, the inner diameters of $TiO_2$ nanotubes are 379 nm. The results are approximately 3 folders larger than the general case.

Formation of One-dimensional Nb2O5 Nanostructures by Anodization

  • Lee, Kiyoung
    • 한국표면공학회지
    • /
    • 제49권6호
    • /
    • pp.486-489
    • /
    • 2016
  • In the present work, we investigate the anodization of Nb in a $K_2HPO_4$ containing glycerol electrolyte at elevated temperatures ($180^{\circ}C$). Under optimized conditions, uniformly over the entire anodized surface, self-organized porous $Nb_2O_5$ structures can be formed. The growth rate of highly ordered $Nb_2O_5$ is $1.7{\mu}m/min$ at beginning stage of anodization and the overall current efficiency is 70 %.

Anodic Aluminum Oxide (AAO) for Nanotechnology Applications

  • 이우
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.33-33
    • /
    • 2010
  • Recently, a self-organizing process that occurs during the anodization of aluminum in acidic electrolytes has attracted a vast amount of research attentions, coupled with the ever-increasing demand for the development of effective, inexpensive and technologically simple methods for the synthesis of low-dimensional nanostructures over a macroscopic area overcoming many of the drawbacks of conventional lithographic techniques. In this presentation, recent progress in the fabrication of ordered nanoporous anodic aluminum oxide (AAO), including conventional anodization techniques, newly developed pulse anodization, hard anodization processes, and generic approaches to three-dimensional pore structures with periodically modulated diameters. Discussion will also cover the applications of AAO for the development of structurally well-defined extended arrays of low-dimensional nanostructures, such as nanodots, nanotubes, and nanowires, which could be model systems in investigating a diverse range of research problems in chemistry and physics and also be starting materials in realizing advanced electronic devices.

  • PDF

Electrochemical Anodic Formation of VO2 Nanotubes and Hydrogen Sorption Property

  • Lee, Hyeonkwon;Jung, Minji;Oh, Hyunchul;Lee, Kiyoung
    • Journal of Electrochemical Science and Technology
    • /
    • 제12권2호
    • /
    • pp.212-216
    • /
    • 2021
  • We investigated the feasibility of hydrogen storage with electrochemically formed VO2 nanotubes. The VO2 nanotubes were fabricated through the anodization of vanadium metal in fluoride ion-containing organic electrolyte followed by an annealing process in an Ar-saturated atmosphere at 673 K for 3 h at a heating rate of 3 K /min. During anodization, the current density significantly increased up to 7.93 mA/cm2 for approximately 500 s owing to heat generation, which led to a fast-electrochemical etching reaction of the outermost part of the nanotubes. By controlling the anodization temperature, highly ordered VO2 nanotubes were grown on the metal substrate without using any binders or adhesives. Furthermore, we demonstrated the hydrogen sorption properties of the anodic VO2 nanotubes.

알루미늄 양극산화를 사용한 LED COB 패키지 (ED COB Package Using Aluminum Anodization)

  • 김문정
    • 한국산학기술학회논문지
    • /
    • 제13권10호
    • /
    • pp.4757-4761
    • /
    • 2012
  • 알루미늄 기판 및 양극산화 공정을 사용하여 LED Chip on Board(COB) 패키지를 제작하였다. 선택적 양극산화 공정을 적용하여 알루미늄 기판 상에 알루미나를 형성하고 이를 COB 패키지 절연층으로 사용하였으며, 비아홀 내부가 충진된 구조의 Thermal Via를 구현하였다. 패키지 기판 종류에 따른 열저항 및 발광효율 변화를 파악하기 위해 알루미늄 기판과 알루미나 기판을 제작하고 이를 각각 비교 분석하였다. Thermal Via가 적용된 알루미늄 기판이 51%의 열저항 개선 및 14%의 발광효율 향상 특성을 보여주었다. 이러한 결과는 선택적 양극산화 공정 및 Thermal Via 구조적용으로 COB 패키지의 방열 특성이 향상되었음을 의미한다. 또한 동일한 전력 소모시 LED 칩 개수에 따른 COB 패키지의 열저항 및 발광효율 변화를 분석함으로써 다수 칩의 효율적인 배치가 열저항 및 발광효율을 증가시킬 수 있음을 확인하였다.

카복실산 용액에서 양극산화에 의해 형성된 나노다공성 금 표면상의 전기화학적 글루코오스 산화 (Electrochemical Oxidation of Glucose at Nanoporous Gold Surfaces Prepared by Anodization in Carboxylic Acid Solutions)

  • 노성진;정화경;이금섭;김민주;김종원
    • 전기화학회지
    • /
    • 제16권2호
    • /
    • pp.74-80
    • /
    • 2013
  • 세 가지 종류의 카복실산(포름산, 아세트산, 프로피온산) 용액 하에서 양극산화 반응을 통한 나노 다공성 금(nanoporous gold, NPG) 구조의 형성과 NPG 전극 표면 상의 전기화학적 글루코오스 산화반응을 관찰하였다. 세 가지 카복실산 용액 조건 중에서 포름산 용액 조건하의 양극산화를 통해 형성된 NPG 전극에서 글루코오스의 산화 활성이 가장 우수하였다. 포름산 용액 조건하의 양극산화 과정에서 가장 우수한 글루코오스 산화 활성을 얻기 위한 최적 조건은 인가전위 5.0 V와 반응시간 4시간이었다. 카복실산 용액 하에서 형성된 NPG 상의 전기화학적 글루코오스 산화 활성을 염소이온의 부재 및 존재 하 조건에서 관찰하고, 이를 옥살산 용액 하에서 형성된 NPG 상의 거동과 비교 분석하였다. 포름산 용액 하에서 최적 조건으로 형성된 NPG 전극상에서 글루코오스의 전류법 검출 응용을 제시하였다.