• 제목/요약/키워드: ZrC

Search Result 1,787, Processing Time 0.023 seconds

Platinum Nano-Dispersion via In Situ Processing - Preparation and catalytic Property of Porous $CaZrO_3/MgO/Pt$ Nanocomposite

  • Yoshikazu;Hwang, Hae-Jin;Naoki Kondo;Tatsuki Ohji
    • Journal of Powder Materials
    • /
    • v.8 no.3
    • /
    • pp.163-167
    • /
    • 2001
  • A bulk porous $CaZrO_3/MgO$ composite with plantinum nano-dispersion was synthesized in air atmosphere through the combination of several in situ reactions, including the pyrolysis of $PtO_2$. A mixture of $CaMg(CO_3)_2$(dolomite), $ZrO_2$, $PtO_2$ and LiF (0.5 wt%, as an additive) was cold isostatically pressed at 200 MPa and sintered at $1100^{\circ}C$ for 2 h. The porous $CaZrO_3/MgO/Pt$ composite ($CaZrO_3/MgO$ : Pt=99 : 1 in volume) had a uniformly open-porous structure (porosity: 56%) with three-dimensional (3-D) network and a narrow pore-size distribution, similarly to the porous $CaZrO_3/MgO$ composites reported before. Catalytic Properties (viz., NO direct decomposition and NO reduction by $C_2H_4$) of the $CaZrO_3/MgO/Pt$ composite were investigated up to $900^{\circ}C$. In the absence of oxygen, the NO conversion rate reached ~52% for the direct decomposition and ~100% for the reduction by $C_2H_4$, respectively. The results suggest the possibility of the porous composite as a multifunctional filter, i.e., simultaneous hot gas-filtering and $de-NO_x$ in one component.

  • PDF

Copolymerizations of Ethylene with 1-Hexene over ansa-Metallocene Diamide Complexes

  • Kim, Il;Kwak, Chang-Hun;Son, Gi-Wan;Kim, Jae-Sung;Sinoj Abraham;Bijal K. B.;Ha, Chang-Sik;Kim, Bu-Ung;Jo, Nam-Ju
    • Macromolecular Research
    • /
    • v.12 no.3
    • /
    • pp.316-321
    • /
    • 2004
  • We have performed copolymerizations of ethylene with 1-hexene using various ansa-metallocene compounds in the presence of the non-coordinative [CPh$_3$][B(C$\_$6/F$\_$5/)$_4$ion pair as a cocatalyst. The metallocenes chosen for this study are isospecific metallocene diamide compounds, rac-(EBI)Zr(NMe$_2$)$_2$ [1, EBI = ethylene-l ,2-bis(1-indenyl)], rac-(EBI)Hf(NMe$_2$)$_2$ (2), rac-(EBI)Zr(NC$_4$H$\_$8/)$_2$ (3), and rac-(CH$_3$)$_3$Si(1-C$\_$5/H$_2$-2-CH$_3$-4-$\^$t/C$_4$H$\_$9/)2 Zr(NMe$_2$)$_2$ (4), and syndiospecific metallocene dimethyl compounds, ethylidene(cyclopentadienyl)(9-fluorenyl) ZrMe$_2$ [5, Et(Flu)(Cp )ZrMe$_2$] and isopropylidence (cyclopentadienyl)(9-fluorenyl)ZrMe$_2$ [6, iPr(Flu)(Cp)ZrMe$_2$]. The copolymerization rate decreased in the order 4 >1-3>2 >5>6. The reactivity of I -hexene decreased in the order 2 >6>1- 3-5> 4. We characterized the microstructure of the resulting poly(ethylene-co-l-hexene) by $\^$l3/C NMR spectroscopy and investigated various other properties of the copolymers in detail.

Dielectric Properties in the Pb1-3x/2Lax[(Mg1/3Ta2/3)0.66Zr0.34]O3 Systems

  • Kim, Yeon Jung
    • Applied Science and Convergence Technology
    • /
    • v.26 no.4
    • /
    • pp.70-73
    • /
    • 2017
  • The dielectric constant and loss of poling/non-poling was measured in the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ samples. The addition of $La^{3+}$ to the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ did not cause a large change in grain size. But the addition of $La^{3+}$ did show transition temperature, which shifted toward low temperature in the $Pb[(Mg_{1/3}Ta_{2/3})Zr]O_3$ systems. In addition, the dielectric and pyroelectric properties (${\varepsilon}{\sim}20000$, $p{\sim}0.03C/m^2K$) of this system using $La^{3+}$ have been greatly improved. Pyroelectrics $Pb_{0.97}La_{0.02}(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ system was found to have a relatively high ferroelectric FOMs ($F_V{\sim}0.035m^2/C$, $F_D{\sim}0.52{\times}10^{-4}Pa^{-1/2}$) at room temperature. Spontaneous polarization showed a value of $0.27{\sim}0.35C/m^2$ in the composition added to $La^{3+}$. The piezoelectric constant ($d_{33}=350{\sim}490pC/N$) and electromechanical coupling factor ($k_P=0.25{\sim}0.35$) are obtained in $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ compositions with $La^{3+}$ dopant.

Functional LTCC Substrate with Near Zero Temperature Coefficient of the Resonant Frequency (Near Zero TCF 특성을 가지는 기능성 LTCC 기판)

  • Choi, Young-Jin;Park, Jeong-Hyun;Ko, Won-Jun;Park, Jae-Hwan;Park, Jae-Gwan;Nahm, Sahn
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.635-638
    • /
    • 2004
  • 페로브스카이트 구조를 가지는 $CaZrO_3$ 유전체 세라믹스에 $CaTiO_3$를 부피 비율로 첨가하여 첨가량 변동에 따른 마이크로파 유전 특성을 조사하였다. 또한 저온 동시소성 기능성 LTCC 기판용 유전체 소재로서 활용하기 위하여 저융점의 borosilicate계 유리 프리트를 첨가하여 $CaZrO_3-CaTiO_3$ 복합 유전체 세라믹스의 저온 소결 거동과 마이크로파 유전 특성을 평가하였다. 알칼리가 첨가된 저융점의 borosilicate계 유리 프리트를 $10\sim30$ wt% 범위로 첨가함으로서 $CaZrO_3-CaTiO_3$ 복합 유전체 세라믹스의 소결온도를 $1450^{\circ}C$에서 $900^{\circ}C$이하로 낮출 수 있었으며, 유리 프리트의 첨가량으로 공진 주파수 온도계수 특성을 조절할 수 있었다. 유리 프리트의 첨가량이 15 wt% 첨가시 $875^{\circ}C$에서 충분한 소결이 이루어졌으며, 이 경우 $CaZrO_3-CaTiO_3$ 복합 유전체 세라믹스는 유전율(k) 23, 품질계수(Qxf) 2500, 공진 주파수 온도계수 ($\tau_{cf}$) -3 ppm/$^{\circ}C$의 매우 양호한 마이크로파 유전 특성을 나타내었다. 유리 프리트의 첨가에 의하여 소결 과정에서 주상인 $CaZrO_3$$CaZr_4O_9$ 상으로의 변화가 뚜렷이 나타났는데, 이러한 상전이 현상과 함께 미세구조의 변화에 대해서도 고찰하였다.

  • PDF

Dielectric properties and microstructures of (CaxSr1-x)ZrO3 ceramics

  • Li, Yu-De;Chen, Jian-Ming;Lee, Ying-Chieh
    • Journal of Ceramic Processing Research
    • /
    • v.19 no.6
    • /
    • pp.461-466
    • /
    • 2018
  • The effects of Ca/Sr ratio and the sintering temperature on the properties of $(Ca_xSr_{(1-x)})ZrO_3$ (CSZ) ceramics were investigated in this study. CSZ ceramics were prepared using solid-state reaction process, which were sintered in air at temperatures ranging from $1350^{\circ}C$ to $1450^{\circ}C$. Their structures were characterized by X-ray Diffraction (XRD), Scanning Electron Microscopy (SEM), and Transmission Electron Microscopy (TEM). The change in Ca/Sr ratio significantly affected the crystalline phase and the dielectric properties of the $(Ca_xSr_{(1-x)})ZrO_3$ ceramics. The secondary phase, $Ca_{0.15}Zr_{0.85}O_{1.85}$, was observed and increased correspondingly with the rising of sintering temperatures. In order to understand the effects of secondary phase on the dielectric properties of CSZ ceramics, the $Ca_{0.15}Zr_{0.85}O_{1.85}$ phase was prepared individually using solidstate method. The $Ca_{0.15}Zr_{0.85}O_{1.85}$ ceramics sintered at $1500^{\circ}C$ for 2 hours possessed a dielectric constant (${\varepsilon}_r$) of 21.7, a dielectric loss ($tan{\delta}$) of $49.510^{-4}$ and an Insulation Resistance (IR) of $2.1{\times}10^{10}{\Omega}$. The ($Ca_{0.7}Sr_{0.3})ZrO_3$ ceramics exhibited the best dielectric properties, with a permittivity of 29, a dielectric loss ($tan{\delta}$) of $2.7{\times}10^{-4}$, and an Insulation Resistance (IR) of $2.6{\times}10^{12}{\Omega}$.

Study on Microstructure and Corrosion Characteristics of Zr-0.8Sn-xNb Ternary Alloys (Nb 첨가량에 따른 Zr-0.8Sn-xNb 3원계 합금의 미세조직 및 부식특성 연구)

  • Kim, Hyeon-Gil;Jeong, Yong-Hwan;Wi, Myeong-Yong
    • Korean Journal of Materials Research
    • /
    • v.9 no.5
    • /
    • pp.452-459
    • /
    • 1999
  • To develop advanced cladding materials, the effect of Nb addition on the microstructure and corrosion characteristics of Zr-0.8Sn-xNb alloys was investigated. As the Nb content increased, the grain size decreased and the volume fraction of precipitates increased. It was observed from the corrosion test at $360^{\circ}C$ that the corrosion resistance increased with decreasing Nb content. The best corrosion resistance was obtained in Zr-0.8Sn-0.2Nb alloy with high volume fraction of tetra-$ZrO_2$in the oxide. Therefore, it is suggested that Nb in theZr-0.85Sn-xNb system should be added within the solubility limit of Nb from the viewpoint of alloy design.

  • PDF

Effect of Zr Addition on the Mechanical Properties and MnS Morphology of Cr-Mo Plastic Mold Steel (Cr-Mo계 금형강의 기계적 성질과 MnS 형상 변화에 미치는 Zr첨가의 영향)

  • Kim, Nam-Kyu;Jeon, Ho-Sung;Lee, Oh-Yeon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.23 no.4
    • /
    • pp.191-197
    • /
    • 2010
  • Zr addition is known as effective method to improve the anisotropy of steel due to the elongated MnS inclusions which are observed in hot forged steels. The aim of this research is to investigate the effect of Zr addition on the mechanical properties and manganese sulphide morphology of 0.27%C-Cr-Mo plastic mold steel. The ingots were prepared by vacuum induction melting and forged to ${\Phi}35mm$ round bar. Forged bars were quenched and tempered at $560{\sim}640^{\circ}C$ for 1 hour. Jominy test, microstructual observation, tensile test and Charpy impact test were conducted. The morphology of MnS inclusions was changed by Zr addition. The shape of MnS inclusions was not so much lengthened and controlled not to be elongated by Zr inclusions which surround the MnS inclusions. Tensile strength and yield strength of the tempered steels were not nearly affected by the addition of Zr, but elongation and reduction of area were decreased. Especially, the toughness of Zr added steels was deteriorated with increasing of Zr content. From the results of this study, it is assumed that anisotropy of steels was improved by the addition of Zr. However, impact toughness of the steel was significantly decreased by the excessive Zr addition (over 0.066%).

Property Comparison of Ru-Zr Alloy Metal Gate Electrode on ZrO2 and SiO2 (ZrO2와 SiO2 절연막에 따른 Ru-Zr 금속 게이트 전극의 특성 비교)

  • Seo, Hyun-Sang;Lee, Jeong-Min;Son, Ki-Min;Hong, Shin-Nam;Lee, In-Gyu;Song, Yo-Seung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.9
    • /
    • pp.808-812
    • /
    • 2006
  • In this dissertation, Ru-Zr metal gate electrode deposited on two kinds of dielectric were formed for MOS capacitor. Sample co-sputtering method was used as a alloy deposition method. Various atomic composition was achieved when metal film was deposited by controlling sputtering power. To study the characteristics of metal gate electrode, C-V(capacitance-voltage) and I-V(current-voltage) measurements were performed. Work function and equivalent oxide thickness were extracted from C-V curves by using NCSU(North Carolina State University) quantum model. After the annealing at various temperature, thermal/chemical stability was verified by measuring the variation of effective oxide thickness and work function. This dissertation verified that Ru-Zr gate electrodes deposited on $SiO_{2}\;and\;ZrO_{2}$ have compatible work functions for NMOS at the specified atomic composition and this metal alloys are thermally stable. Ru-Zr metal gate electrode deposited on $SiO_{2}\;and\;ZrO_{2}$ exhibit low sheet resistance and this values were varied with temperature. Metal alloy deposited on two kinds of dielectric proposed in this dissertation will be used in company with high-k dielectric replacing polysilicon and will lead improvement of CMOS properties.

Magnetic Properties of Fe-Zr-N Soft Magnetic Thin Films (Fe-Zr-N 연자성 박막의 자기적 성질)

  • 김택수;김종오;이중환;윤선진;김좌연
    • Journal of the Korean Magnetics Society
    • /
    • v.6 no.5
    • /
    • pp.317-322
    • /
    • 1996
  • Thin films of Fe-Zr-N were fabricated by rf magnetron reactive sputtering method. The saturation magnetization and coercivity as functions of annealing temperature and partial pressure of nitrogen gas, effective permeability at high frequencies, and thermal stability were investigated. Magnetic softness was exhibited in the composition range of $Fe_{72-78}Zr_{7-10}N_{15-18}$ which was boundary between polycrystalline and amorphous structure. These films exhibited magnetic softness with saturation magentic flux density of 1.55 T and effective permeability of about 3000 at 1 MHz. These films also exhibited thermal stability by sustaining effective permeability of 2500 or above as the temperature was raised to $550^{\circ}C$. It is asswned that good magnetic softness is obtained because grain growth of $\alpha-Fe$ is prohibited due to the precipitation of ZrN nanocrystals. The grain sizes of $\alpha-Fe$ films were $40~50\AA$ and the grain sizes of ZrN nanocrystals were $10~15\AA$.

  • PDF

High-temperature Oxidation of CrZrN Films in Air (CrZrN 박막의 대기 중 고온산화)

  • Kim, Min-Jeong;Hwang, Yeon-Sang;Bong, Seong-Jun;Lee, Sang-Yul;Lee, Dong-Bok
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.05a
    • /
    • pp.167-168
    • /
    • 2012
  • Films of CrN, $Cr_{40}Zr_9N$, and $Cr_{31}Zr_{16}N$ were deposited on a steel substrate by closed field unbalanced magnetron sputtering, and their oxidation behaviors at $700^{\circ}C$ and $800^{\circ}C$ for up to 60h in air were investigated. All the deposited films were composed of the CrN phase. Zirconium atoms in $Cr_{40}Zr_9N$ and $Cr_{31}Zr_{16}N$ films partially dissolved in the CrN phase. They advantageously refined the columnar structure, reduced the surface roughness, and increased the microhardness. The CrN film displayed relatively good oxidation resistance, owing to the formation of the highly protective $Cr_2O_3$ on its surface. The $Cr_{40}Zr_9N$ and $Cr_{31}Zr_{16}N$ films oxidized to $Cr_2O_3$ as the major phase and ${\alpha}-ZrO_2$ as the minor one. They oxidized primarily by the inward transport of oxygen. The addition of Zr could not increase the oxidation resistance of the CrN film, because the formed $ZrO_2$ that was intermixed in the $Cr_2O_3$-rich oxide layer was oxygen permeable, and developed the compressive stress in the oxide scale owing to the volume expansion during its formation.

  • PDF