실리카 슬러리의 에이징 효과 및 산화막 CMP 특성 (Aging Effects of Silica Slurry and Oxide CMP Characteristics)

  • 이우선;고필주;이영식;서용진;홍광준
    • 한국전기전자재료학회논문지
    • /
    • 제17권2호
    • /
    • pp.138-143
    • /
    • 2004
  • CMP (Chemical Mechanical Polishing) technology for global planarization of multilevel interconnection structure has been widely studied for the next generation devices. Among the consumables for CMP process, especially, slurry and their chemical compositions play a very important role in the removal rates and within-wafer non-uniformity (WIWNU) for global planarization ability of CMP process. However, CMP slurries contain abrasive particles exceeding 1 ${\mu}{\textrm}{m}$ size, which can cause micro-scratch on the wafer surface after CMP process. Such a large size particle in these slurries may be caused by particle agglomeration in slurry supply-line. In this work, to investigate the effects of agglomeration on the performance of oxide CMP slurry, we have studied an aging effect of silica slurry as a function of particle size distribution and aging time during one month. We Prepared and compared the self-developed silica slurry by adding of alumina powders. Also, we have investigated the oxide CMP characteristics. As an experimental result, we could be obtained the relatively stable slurry characteristics comparable to aging effect of original silica slurry. Consequently, we can expect the saving of high-cost slurry.

Effect of Particle Size of Ceria Coated Silica and Polishing Pressure on Chemical Mechanical Polishing of Oxide Film

  • Kim, Hwan-Chul;Lim, Hyung-Mi;Kim, Dae-Sung;Lee, Seung-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • 제7권4호
    • /
    • pp.167-172
    • /
    • 2006
  • Submicron colloidal silica coated with ceria were prepared by mixing of silica and nano ceria particles and modified by hydrothermal reaction. The polishing efficiency of the ceria coated silica slurry was tested over oxide film on silicon wafer. By changing the polishing pressure in the range of $140{\sim}420g/cm^2$ with the ceria coated silica slurries in $100{\sim}300nm$, rates, WIWNU and friction force were measured. The removal rate was in the order of 200, 100, and 300 nm size silica coated with ceria. It was known that the smaller particle size gives the higher removal rate with higher contact area in Cu slurry. In the case of oxide film, the indentation volume as well as contact area gives effect on the removal rate depending on the size of abrasives. The indentation volume increase with the size of abrasive particles, which results to higher removal rate. The highest removal rate in 200 nm silica core coated with ceria is discussed as proper combination of indentation and contact area effect.

$Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) 박막의 CMP 메커니즘 연구 (A Study on CMP Mechanism of $Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) Thin Films)

  • 신상헌;고필주;김남훈;이우선
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1450-1451
    • /
    • 2006
  • In this paper, we first applied the chemical mechanical polishing (CMP) process to the planarization of ferroelectric film in order to obtain a good planarity of electrode/ferroelectric film interface. $Bi_{3.25}La_{0.75}Ti_{3}O_{12}$ (BLT) ferroelectric fan was fabricated by the sol-gel method. Removal rate and non-uniformity (WIWNU%) were examined by change of silica slurries pH(10.3, 11.3, 12.3). Surface roughness of BLT thin films before and after CMP process was inquired into by atomic force microscopy (AFM). Effects of silica slurries pH(10.3, 11.3, 12.3) were investigated on the CMP performance of BLT film by the surface analysis of X-ray photoelectron spectroscopy(XPS).

  • PDF

고유전율막의 CMP 특성 (Chemical Mechanical Polishing Characteristics of High-k Thin Film)

  • 박성우;서용진;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.55-56
    • /
    • 2006
  • In this paper, we first applied the chemical mechanical polishing (CMP) process to the planarization of ferroelectric film in order to obtain a good planarity of electrode/ferroelectric film interface. BST ($Ba_{0.6}Sr_{0.4}TiO_3$), PZT ($Pb_{1.1}(Zr_{0.52}TiO_{0.48})O_3$) and BTO ($BaTiO_3$) ferroelectric film are fabricated by the sol-gel method. And then, we compared the structural characteristics before and after CMP process of BST, PZT, BTO films. Their dependence on slurry composition was also investigated. We expect that our results will be useful promise of global planarization for ferroelectric random access memories (FRAM) application in the near future.

  • PDF

A Study on Pressure Distribution for Uniform Polishing of Sapphire Substrate

  • Park, Chul jin;Jeong, Haedo;Lee, Sangjik;Kim, Doyeon;Kim, Hyoungjae
    • Tribology and Lubricants
    • /
    • 제32권2호
    • /
    • pp.61-66
    • /
    • 2016
  • Total thickness variation (TTV), BOW, and surface roughness are essential characteristics for high quality sapphire substrates. Many researchers have attempted to increase removal rate by controlling the key process parameters like pressure and velocity owing to the high cost of consumables in sapphire chemical mechanical polishing (CMP). In case of the pressure approach, increased pressure owing to higher deviation of pressure over the wafer leads to significant degradation of the TTV. In this study, the authors focused on reducing TTV under the high-pressure conditions. When the production equipment polishes multiple wafers attached on a carrier, higher loads seem to be concentrated around the leading edge of the head; this occurs because of frictional force generated by the combination of table rotation and the height of the gimbal of the polishing head. We believe the skewed pressure distribution during polishing to be the main reason of within-wafer non-uniformity (WIWNU). The insertion of a hub ring between the polishing head and substrate carrier helped reduce the pressure deviation. Adjusting the location of the hub ring enables tuning of the pressure distribution. The results indicated that the position of the hub ring strongly affected the removal profile, which confirmed that the position of the hub ring changes the pressure distribution. Furthermore, we analyzed the deformation of the head via finite element method (FEM) to verify the pressure non-uniformity over the contact area Based on experiment and FEM results, we determined the optimal position of hub ring for achieving uniform polishing of the substrate.

DHF를 적용한 웨이퍼의 층간 절연막 평탄화에 관한 연구 (A Study on ILD(Interlayer Dielectric) Planarization of Wafer by DHF)

  • 김도윤;김형재;정해도;이은상
    • 한국정밀공학회지
    • /
    • 제19권5호
    • /
    • pp.149-158
    • /
    • 2002
  • Recently, the minimum line width shows a tendency to decrease and the multi-level increases in semiconductor. Therefore, a planarization technique is needed and chemical mechanical polishing(CMP) is considered as one of the most suitable process. CMP accomplishes a high polishing performance and a global planarization of high quality. However there are several defects in CMF, such as micro-scratches, abrasive contaminations and non-uniformity of polished wafer edges. Wet etching process including spin-etching can eliminate the defects of CMP. It uses abrasive-free chemical solution instead of slurry. On this study, ILD(Interlayer-Dielectric) was removed by CMP and wet etching process using DHF(Diluted HF) in order to investigate the possibility of planrization by wet etching mechanism. In the thin film wafer, the results were evaluated from the viewpoint of material removal rate(MRR) and within wafer non-uniformity(WIWNU). And the pattern step heights were also compared for the purpose of planarity characterization of the patterned wafer. Moreover, Chemical polishing process which is the wet etching process with mechanical energy was introduced and evaluated for examining the characteristics of planarization.

$BaTiO_3$$TiO_2$ 연마제 첨가를 통한 BTO박막의 CMP (CMP of BTO Thin Films using $TiO_2$ and $BaTiO_3$ Mixed Abrasive slurry)

  • 서용진;고필주;김남훈;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.68-69
    • /
    • 2005
  • BTO ($BaTiO_3$) thin film is one of the high dielectric materials for high-density dynamic random access memories (DRAMs) due to its relatively high dielectric constant. It is generally known that BTO film is difficult to be etched by plasma etching, but high etch rate with good selectivity to pattern mask was required. The problem of sidewall angle also still remained to be solved in plasma etching of BTO thin film. In this study, we first examined the patterning possibility of BTO film by chemical mechanical polishing (CMP) process instead of plasma etching. The sputtered BTO film on TEOS film as a stopper layer was polished by CMP process with the self-developed $BaTiO_3$- and $TiO_2$-mixed abrasives slurries (MAS), respectively. The removal rate of BTO thin film using the$ BaTiO_3$-mixed abrasive slurry ($BaTiO_3$-MAS) was higher than that using the $TiO_2$-mixed abrasive slurry ($TiO_2$-MAS) in the same concentrations. The maximum removal rate of BTO thin film was 848 nm/min with an addition of $BaTiO_3$ abrasive at the concentration of 3 wt%. The sufficient within-wafer non-uniformity (WIWNU%)below 5% was obtained in each abrasive at all concentrations. The surface morphology of polished BTO thin film was investigated by atomic force microscopy (AFM).

  • PDF

수열처리법을 이용한 $Al_2O_3/CeO_2$ composite 연마재 제조 및 연마 특성 (Preparation of $Al_2O_3/CeO_2$ Composite Abrasives by using Hydrothermal Treatment and its Polishing Properties)

  • 최성현;이승호;임형미;길재수;최귀돈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.1278-1282
    • /
    • 2004
  • 수열처리법으로 nano-sized $CeO_2$ 입자를 $Al_3O_3$ 입자의 표면에 균일하게 코팅하여 $AL_2O_3/O_2$ composite 연마 입자를 제조하었다. 제조된 $Al_2O_3\CeO_2$ composite 입자의 뭍성을 TEM, XRD, zeta potential analyzer 및 particle size analyzer로 측징하였다. $Al_2O_3/CeO_2$ composite 입자와 구성된 슬러리와 비교 시료로서 $Al_2O_3$$CeO_2$ 입자를 혼합한 슬러리를 사용하여 thermal oxide film에 대한 연마특성을 평가하였다. 연마슬러리에 포함된 $A1_2O_3/CeO_2$ composite 입자와 $Al_2O_3$$CeO_2$ 혼합입자에서 나노 크기의 세리아 입자가 sub-micron 크기의 알루미나 입자의 표면에 균일하게 코팅되므로서 $Al_2O_3$ 단일 성분의 슬러리에 비해 removal rate(RR)는 106 nm/min, WIWNU는 $8\sim9%$, roughness는 $2.6{\AA}$의 향상된 연마 특성을 나타내었다. 알루미나 입자의 불규칙한 형상 때문에 $Al_2O3/CeO_2$ composite 슬러리와 $Al_2O_3$$CeO_2$ 혼합슬러리의 연마 특성이 비슷한 수준을 나타내었다.

  • PDF

스퍼터링 증확 CdTe 박막의 두께 불균일 현상 개선을 위한 화학적기계적연마 공정 적용 및 광특성 향상 (Application of CMP Process to Improving Thickness-Uniformity of Sputtering-deposited CdTe Thin Film for Improvement of Optical Properties)

  • 박주선;임채현;류승한;명국도;김남훈;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.375-375
    • /
    • 2010
  • CdTe as an absorber material is widely used in thin film solar cells with the heterostructure due to its almost ideal band gap energy of 1.45 eV, high photovoltaic conversion efficiency, low cost and stable performance. The deposition methods and preparation conditions for the fabrication of CdTe are very important for the achievement of high solar cell conversion efficiency. There are some rearranged reports about the deposition methods available for the preparation of CdTe thin films such as close spaced sublimation (CSS), physical vapor deposition (PVD), vacuum evaporation, vapor transport deposition (VTD), closed space vapor transport, electrodeposition, screen printing, spray pyrolysis, metalorganic chemical vapor deposition (MOCVD), and RF sputtering. The RF sputtering method for the preparation of CdTe thin films has important advantages in that the thin films can be prepared at low growth temperatures with large-area deposition suitable for mass-production. The authors reported that the optical and electrical properties of CdTe thin film were closely connected by the thickness-uniformity of the film in the previous study [1], which means that the better optical absorbance and the higher carrier concentration could be obtained in the better condition of thickness-uniformity for CdTe thin film. The thickness-uniformity could be controlled and improved by the some process parameters such as vacuum level and RF power in the sputtering process of CdTe thin films. However, there is a limitation to improve the thickness-uniformity only in the preparation process [1]. So it is necessary to introduce the external or additional method for improving the thickness-uniformity of CdTe thin film because the cell size of thin film solar cell will be enlarged. Therefore, the authors firstly applied the chemical mechanical polishing (CMP) process to improving the thickness-uniformity of CdTe thin films with a G&P POLI-450 CMP polisher [2]. CMP process is the most important process in semiconductor manufacturing processes in order to planarize the surface of the wafer even over 300 mm and to form the copper interconnects with damascene process. Some important CMP characteristics for CdTe were obtained including removal rate (RR), WIWNU%, RMS roughness, and peak-to-valley roughness [2]. With these important results, the CMP process for CdTe thin films was performed to improve the thickness-uniformity of the sputtering-deposited CdTe thin film which had the worst two thickness-uniformities of them. Some optical properties including optical transmittance and absorbance of the CdTe thin films were measured by using a UV-Visible spectrophotometer (Varian Techtron, Cary500scan) in the range of 400 - 800 nm. After CMP process, the thickness-uniformities became better than that of the best condition in the previous sputtering process of CdTe thin films. Consequently, the optical properties were directly affected by the thickness-uniformity of CdTe thin film. The absorbance of CdTe thin films was improved although the thickness of CdTe thin film was not changed.