• 제목/요약/키워드: Thin film thickness

검색결과 1,951건 처리시간 0.031초

Secondary Phase and Defects in Cu2ZnSnSe4 Solar Cells with Decreasing Absorber Layer Thickness

  • Kim, Young-Ill;Son, Dae-Ho;Lee, Jaebaek;Sung, Shi-Joon;Kang, Jin-Kyu;Kim, Dae-Hwan;Yang, Kee-Jeong
    • Current Photovoltaic Research
    • /
    • 제9권3호
    • /
    • pp.84-95
    • /
    • 2021
  • The power conversion efficiency of Cu2ZnSnSe4 (CZTSe) solar cells depends on the absorber layer thickness; however, changes in the characteristics of the cells with varying absorber layer thickness are unclear. In this study, we investigated the changes in the characteristics of CZTSe solar cells for varying absorber layer thickness. Five absorber thicknesses were employed: CZTSe1 2.78 ㎛, CZTSe2 1.01 ㎛, CZTSe3 0.55 ㎛, CZTSe4 0.29 ㎛, and CZTSe5 0.15-0.23 ㎛. The efficiency of the CZTSe solar cells decreased as the absorber thickness decreased, resulting in power conversion efficiencies of 10.45% (CZTSe1), 8.67% (CZTSe2), 7.14% (CZTSe3), 3.44% (CZTSe4), and 1.54% (CZTSe5). As the thickness of the CZTSe absorber layer decreased, the electron-hole recombination at the grain boundaries and the absorber-back-contact interface increased. This caused an increase in the current loss, owing to light loss in the long-wavelength region. In addition, as the thickness of the CZTSe absorber layer decreased, more ZnSe was produced, and the resulting defects and defect clusters led to an open-circuit voltage loss.

ZnO/Ag Multilayer의 투과율과 전도성에 관한 연구 (The Study of Transmittance and Conductivity in ZnO/Ag Multilayer Films)

  • 김윤해;김도완;무라카미 리이치;문경만;이성열
    • 한국해양공학회지
    • /
    • 제25권1호
    • /
    • pp.39-43
    • /
    • 2011
  • This study has lowered the specific resistance by coating a thin film layer of Ag, playing the role of the electron donor on the ZnO that is used usefully for the transparent conductive oxides. Presently, this study has examined the transmittance and electric characteristics according to the thickness of the Ag thin film layer. Also, this study has observed the transmittance and electric characteristics according to the uppermost ZnO thin film layer of ZnO/Ag/ZnO symmetric film and has conducted the theoretical investigation. In order to observe the transmittance and electric characteristics according to the thickness of the Ag thin film layer and the uppermost ZnO thin film layer, this study conducted the film deposition at room temperature while making use of the DC magnetron sputtering system. In order to see the changes in the thickness of the Ag thin film layer, this study coated a thin film while increasing by 4nm; and, in order to see the changes in the thickness of uppermost ZnO thin film layer, it performed the thin film coating by increasing by 5nm. From the experimental result, the researchers observed that the best transmittance could be obtained when the thickness of the Ag thin film layer was 8nm, but the resistance and mobility increased as the thickness got larger. On the other hand, when the thickness of the uppermost ZnO thin film layer was 20nm, the experiment yielded the best transmittance with excellent electric characteristics. Also, when compared the ZnO/Ag asymmetric film with the ZnO/Ag/ZnO symmetric film, the ZnO/Ag asymmetric film showed better transmittance and electric characteristics.

P(VDF/TrFE) 필름의 두께에 따른 인체 감지형 초전형 PIR 적외선 센서의 특성 (Effect of P(VDF/TrFE) Film Thickness on the Characteristics of Pyroelectric Passive Infrared Ray Sensor for Human Body Detection)

  • 권성열
    • 센서학회지
    • /
    • 제20권2호
    • /
    • pp.114-117
    • /
    • 2011
  • A thick 25 ${\mu}m$ thickness poled P(VDF/TrFE) film pyroelectric infrared ray sensor has been fabricated and then thin 1.6 ${\mu}m$ thickness P(VDF/TrFE) film pyroelectric infrared ray sensor has been fabricated also. These thick and thin P(VDF/TrFE) film pyroelectric infrared ray sensor was mounted in TO-5 housing to detect infrared light of 5.5 ~ 14 ${\mu}m$ wavelength for human body detecting with each other. The noise output voltage of the thick P(VDF/TrFE) film pyroelectric infrared ray sensor were 380 mV and NEP(noise equivalent power) is $3.95{\times}10^{-7}$ W which is the similar value with the commercial pyroelectric infrared ray sensor using ceramic materials as a sensing material. The NEP and specific detectivity $D^*$ of the thin P(VDF/TrFE) film pyroelectric infrared ray sensor were $2.13{\times}10^{-8}$ W and $9.37{\times}106$ cm/W under emission energy of 13 ${\mu}W/cm^2$ respectively. These result caused by lower thermal diffusion coefficient of a thin 1.6 ${\mu}m$ thickness PVDF/TrFE film than the thick 25 ${\mu}m$ thickness poled P(VDF/TrFE) film pyroelectric infrared ray sensor.

파동간섭효과를 고려한 다층 박막 구조의 광학특성에 대한 수치해석 연구 (Numerical Study on Optical Characteristics of Multi-Layer Thin Film Structures Considering Wave Interference Effects)

  • 심형섭;이성혁
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권5호
    • /
    • pp.272-277
    • /
    • 2006
  • The present study is devoted to investigate numerically the optical characteristics of multi-layer thin film structures such as $Si/SiO_2\;and\;Ge/Si/SiO_2$ by using the characteristics transmission matrix method. The reflectivity and the absorptivity rate for thin film structures are estimated for different incident angles of rays and various film thicknesses. In addition, the influence of wavelength on optical characteristics related to complex refractive index is examined. It is found that such wave-like characteristics are observed in predicting reflectivities and depends mainly on film thickness. Moreover, the present study predicts the film thickness for ignoring wave interference effects, and it also discusses the fundamental physics behind optical and energy absorption characteristics appearing in multi-layer thin film structures.

표면파의 분산 특성을 이용한 Ni 박막의 두께 측정 (Thickness Measurement of Ni Thin Film Using Dispersion Characteristics of a Surface Acoustic Wave)

  • 박태성;곽동열;박익근;김미소;이승석
    • 비파괴검사학회지
    • /
    • 제34권2호
    • /
    • pp.171-175
    • /
    • 2014
  • 본 연구에서는 박막 표면을 따라 전파하는 표면파의 속도 분산성을 이용하여 박막의 두께를 비파괴적으로 측정할 수 있는 기법을 제안하였다. 표면파의 분산성을 이용하여 박막의 두께를 측정하기 위하여 전자빔증착법(E-beam evaporation)을 이용하여 Si(100) 웨이퍼 위에 니켈의 증착시간을 제어함으로서 두께가 다른 니켈 박막시험편을 제작하였다. 제작된 시험편의 실제 증착된 박막의 두께를 확인하기 위하여 SEM(scanning electron microscope)을 이용하여 박막의 단면사진을 촬영하여 두께를 확인하였다. 그 후에 두께가 다른 시험편에서의 표면파의 속도를 초음파현미경(scanning acoustic microscope)의 V(z) 곡선법을 이용하여 표면파의 속도를 측정하고 실제 측정된 두께와 표면파 속도와의 상관성을 확인하였다. 박막의 두께가 증가함에 따라 표면파의 속도는 감소하는 경향성을 나타내었다. 결론적으로 본 연구에서 제안한 표면파의 속도 분산성을 이용하여 나노 스케일 니켈 박막의 두께를 측정하는 기법이 가능성이 있음을 확인하였다.

p-Si 기판에 성장한 BaTiO3 박막의 두께와 구조적 특성과의 관계 (Relationship between Thin Film Thickness and Structural Properties of BaTiO3 Thin Films Grown on p-Si Substrates)

  • 민기득;이종원;김선진
    • 한국재료학회지
    • /
    • 제23권6호
    • /
    • pp.334-338
    • /
    • 2013
  • In this study, $BaTiO_3$ thin films were grown by RF-magnetron sputtering, and the effects of the thin film thickness on the structural characteristics of $BaTiO_3$ thin films were systematically investigated. Instead of the oxide substrates generally used for the growth of $BaTiO_3$ thin films, p-Si substrates which are widely used in the current semiconductor processing, were used in this study in order to pursue high efficiency in device integration processing. For the crystallization of the grown thin films, annealing was carried out in air, and the annealing temperature was varied from $700^{\circ}C$. The changed thickness was within 200 nm~1200 nm. The XRD results showed that the best crystal quality was obtained for ample thicknesses 700 nm~1200 nm. The SEM analysis revealed that Si/$BaTiO_3$ are good quality interface characteristics within 300 nm when observed thickness. And surface roughness observed of $BaTiO_3$ thin films from AFM measurement are good quality surface characteristics within 300 nm. Depth-profiling analysis through GDS (glow discharge spectrometer) showed that the stoichiometric composition could be maintained. The results obtained in this study clearly revealed $BaTiO_3$ thin films grown on a p-Si substrate such as thin film thickness. The optimum thickness was 300 nm, the thin film was found to have the characteristics of thin film with good electrical properties.

RF magnetron reactive sputtering 법으로 제작한 BST 박막의 전기적 및 계면 특성에 관한 연구 (Electrical and interface characteristics of BST thin films grown by RF magnetron reactive sputtering)

  • 강성준;장동훈;유영섭
    • 전자공학회논문지D
    • /
    • 제35D권5호
    • /
    • pp.33-39
    • /
    • 1998
  • The BST (Ba$_{1-x}$ Sr$_{x}$TiO$_{3}$)(50/50) thin film has been grown by RF magnetron reactive sputtering and its characteristics such as crystallization, surface roughness, and electrical properties have been investigated with varying the film thickness. The crystallization and surface roughness of BST thin film are investigated by using XRD and AFM, respectively The BST thin film anealed at 800.deg. C for 2 min has pure perovskite structure and good surface roughness of 16.1.angs.. We estimate that the thickness and dielectric constant of interface layer between BST film and electrode are 3nm and 18.9, respectively, by measuring the capacitance with various film thickness. As the film thickness increases form 80nm to 240nm, the dielectric constant at 10kHz increases from 199 to 265 and the leakage current density at 200kV/cm decreases from 0.682.mu.A/cm$^{2}$ to 0.181 .mu.A/cm$^{2}$. In the case of 240nm-thick BST thin film, the charge storage density and leakage current density at 5V are 50.5fC/.mu.m$^{2}$ and 0.182.mu.A/cm$^{2}$, respectively. The values indicate that the BST thin film is a very useful dielectric material for the DRAM capacitor.or.

  • PDF

Metal-insulator Transition in $(Sr_{0.75},\;La_{0.25})TiO_3$ Ultra-thin Films

  • Choi, Jae-Du;Choi, Eui-Young;Lee, Yun-Sang;Lee, Jai-Chan
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2011년도 추계학술발표대회
    • /
    • pp.19.2-19.2
    • /
    • 2011
  • The $(Sr_{0.75},\;La_{0.25})TiO_3$ (SLTO) ultra-thin films with various thicknesses have been grown on Ti-O terminated $SrTiO_3$(100) substrate using Laser-Molecular Beam Epitaxy (Laser MBE). By monitoring the in-situ specular spot intensity oscillation of reflection high energy electron diffraction (RHEED), we controlled the layer-by-layer film growth. The film structure and topography were verified by atomic force microscopy (AFM) and high resolution thin film x-ray diffraction by the synchrotron x-ray radiation. We have also investigated the electronic band structure using x-ray absorption spectroscopy (XAS). The ultra thin SLTO film exhibits thickness driven metal-insulator transition around 8 unit cell thickness when the film thickness progressively reduced to 2 unit cell. The SLTO thin films with an insulating character showed band splitting in Ti $L_3-L_2$ edge XAS spectrum which is attributed to Ti 3d band splitting. This narrow d band splitting could drive the metal-insulator transition along with Anderson Localization. In optical conductivity, we have found the spectral weight transfer from coherent part to incoherent part when the film thickness was reduced. This result indicates the possibility of enhanced electron correlation in ultra thin films.

  • PDF

유기반도체 박막증착을 위한 선형증착원의 유체유동해석 (Analysis of Fluid Flow in the Linear Cell Source for Organic Semiconductor Thin Film Deposition)

  • 곽인철;양영수;최범호;김영미
    • 한국정밀공학회지
    • /
    • 제26권10호
    • /
    • pp.74-80
    • /
    • 2009
  • This paper presents a study on fluid flow analysis of organic semiconductor thin film deposition process using the computational numerical method. In the production process, the thickness of deposited organic thin film depends on distribution of nozzle size in the linear cell system, so we analyze to decide the optimal nozzle system for uniform thickness of organic thin film. The results of deposited thickness of thin film by numerical analysis are in good agreement with those of the experimental measurements.

The Effect of Thickness on Flexible, Electrical and Optical properties of Ti- ZnO films on Flexible Glass by Atomic Layer Deposition

  • 이우재;윤은영;권세훈
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.196.1-196.1
    • /
    • 2016
  • TCO(Transparent Conducting Oxide) on flat glass is used in thin-film photovoltaic cell, flat-panel display. Nowadays, Corning(R) Willow Glass(R), known as flexible substrate, has attracted much attention due to its many advantages such as reliable roll-to-roll glass processing, high-quality flexible electronic devices, high temperature process. Also, it can be an alternative to flexible polymer substrates which have their poor stability and degradation of electrical and optical qualities. For application on willow glass, the flexibility, electrical, optical properties can be greatly influenced by the TCO thin film thickness due to the inherent characterization of thin film in nanoscale. It can be expected that while thick TCO layer causes poor transparency, its sheet resistance become low. Also, rarely reports were focusing on the influence of flexible properties by varying TCO thickness on flexible glass. Therefore, it is very important to optimize TCO thickness on flexible Willow glass. In this study, Ti-ZnO thin films, with different thickness varied from 0 nm to 50 nm, were deposited on the flexible willow glass by atomic layer deposition (ALD). The flexible, electrical and optical properties were investigated, respectively. Also, these properties of Ti-doped ZnO thin films were compared with un-doped ZnO thin film. Based on the results, when Ti-ZnO thin films thickness increased, resistivity decreased and then saturated; transmittance decreased. The Figure of Merit (FoM) and flexibility was the highest when Ti-ZnO thickness was 40nm. The flexible, electrical and optical properties of Ti-ZnO thin films were better than ZnO thin film at the same thickness.

  • PDF