• 제목/요약/키워드: Temperature dependence of dielectric constant

검색결과 93건 처리시간 0.027초

용매 증발법에 의한 $Pb(Mg_{1/3}Nb_{2/3})O_3$ 분말 합성 및 유전 성질 (Synthesis of $Pb(Mg_{1/3}Nb_{2/3})O_3$ powder by Solvent Evaporation and its Dielectric Property)

  • 이종필;이종국;강상구;김환
    • 한국세라믹학회지
    • /
    • 제33권1호
    • /
    • pp.17-24
    • /
    • 1996
  • Pb(Mg1/3Nb2/3)O3 powder with high purity chemical homogeniety and reactivity was prepared by solvent eva-poration of common solution. The common solution was fabricated using a Pb(NO3)2 Mg(NO)3 and NB solution which was prepared by dissolving NbC in H2O2 acquous solution. In precusor powder prepared by solvent evaporation method the synthetic temperature of Pb(Mg1/3 Nb2/3)O3 phase was lowered. And the formation of homogeneous Pb(Mg1/3Nb2/3)O3 phase was enhanced but the formation of pyrochlore phase was reduced. The dielectric constant of PMN ceramics from the synthesized powder was found to increase with both sintering temperature and excess MgO and subsequent analysis of the microstructures confirmed that this was due to an increase in grain size. The grain size dependence is explained as a consequence of low-permittivity grain boundaries.

  • PDF

(001) Pb(Mg1/3Nb2/3)O3-x%PbTiO3 단결정의 도메인 구조 및 상전이 (Domain Structure and Phase Transformation of (001) Pb(Mg1/3Nb2/3)O3-x%PbTiO3 Single Crystals)

  • 이은구
    • 한국세라믹학회지
    • /
    • 제51권3호
    • /
    • pp.218-223
    • /
    • 2014
  • The domain structures, dielectric properties, and phase transformation of (001)-oriented $Pb(Mg_{1/3}Nb_{2/3})O_3-x%PbTiO_3$ (PMN-x%PT) crystals for x=20, 30, 35, and 40 mole% have been investigated. PMN-20%PT consists of polar nano-domains (PND) which do not self-assemble into macro-domain plates. PMN-30%PT consists of PNDs which begin to self-assemble into colonies along preferred {110} planes. PMN-35PT consists of miniature polar domains on the nm scale. PMN-40%PT consists of {001} oriented lamella domains on the mm scale that have internal nano-scale heterogeneities. The dielectric properties of poled (001) PMN-x%PT single crystals have been measured for orientations both parallel and perpendicular to the [001] poling direction. The results of the temperature dependence of the dielectric constant and mesh scans for the 30%PT sample demonstrate that the initial monoclinic phase changes to single domain tetragonal phase and to cubic phase with increasing temperature.

Perovskite PMT-PT계의 강유전 특성 및 확산상전이 (Ferroelectric Properties and DPT in the Perovskite PMT-PT System)

  • 김연중
    • 한국진공학회지
    • /
    • 제17권2호
    • /
    • pp.122-129
    • /
    • 2008
  • Perovskite 구조의 PMT-PT계 고용체를 precursor columbite를 이용한 산화물 혼합법으로 제작하여 결정립의 성장과 상전이 현상을 분석하였다. $1250^{\circ}C$에서 4시간 유지하여 제작한 시편의 소결밀도는 이론밀도의 97% 이상이었고, 완전한 perovskite phase를 형성하였다. 치밀하게 소결 처리된 시편의 결정립의 크기는 $6\sim8{\mu}m$로 측정되었다. PMT-PT 고용체계는 복합 강유전 고용체의 전형적인 P-E 이력현상과 강한 진동수 분산특성이 관찰되었다. 특히 PMT가 70% 이하인 조성은 상전이 온도 이상에서도 자발분극이 완전히 소멸하지 않는 relaxor 특성을 보였으며, 유전상수와 유전손실의 큰 진동수 의존성을 보였다.

고에너지밀도 캐패시터를 위해 PET 기판에 증착한 TiO2 박막의 특성 (Properties of TiO2 Thin Films Deposited on PET Substrate for High Energy Density Capacitor)

  • 박상식
    • 한국재료학회지
    • /
    • 제22권8호
    • /
    • pp.409-415
    • /
    • 2012
  • $TiO_2$ thin films for high energy density capacitors were prepared by r.f. magnetron sputtering at room temperature. Flexible PET (Polyethylene terephtalate) substrate was used to maintain the structure of the commercial film capacitors. The effects of deposition pressure on the crystallization and electrical properties of $TiO_2$ films were investigated. The crystal structure of $TiO_2$ films deposited on PET substrate at room temperature was unrelated to deposition pressure and showed an amorphous structure unlike that of films on Si substrate. The grain size and surface roughness of films decreased with increasing deposition pressure due to the difference of mean free path. X-ray photoelectron spectroscopy (XPS) analysis revealed the formation of chemically stable $TiO_2$ films. The dielectric constant of $TiO_2$ films was significantly changed with deposition pressure. $TiO_2$ films deposited at low pressure showed high dissipation factor due to the surface microstructure. The dielectric constant and dissipation factor of films deposited at 70 mTorr were found to be 100~120 and 0.83 at 1 kHz, respectively. The temperature dependence of the capacitance of $TiO_2$ films showed the properties of class I ceramic capacitors. $TiO_2$ films deposited at 10~30 mTorr showed dielectric breakdown at applied voltage of 7 V. However, the films of 500~300 nm thickness deposited at 50 and 70 mTorr showed a leakage current of ${\sim}10^{-8}{\sim}10^{-9}$ A at 100 V.

Epoxy Molding Compound의 경화거동에 관한 연구 (A Study on the Cure Behavior of Epoxy Molding Compound)

  • 윤상영;오명숙;박내정
    • 폴리머
    • /
    • 제24권6호
    • /
    • pp.837-844
    • /
    • 2000
  • 본 연구에서는 반도체 봉지제로 사용되는 상용 EMC중 가속제의 함량이 다른 두 종류의 프리프레그에 대하여 그 경화거동을 등온 및 승온조건에서 시차 주사 역량계, 점도계 및 유전율 측정계를 이용하여 분석하였다. 경화반응 속도변수는 Kamal의 자동촉매 반응식을 이용하여 m+n을 2로 가정한 후 Ryan Dutta의 방법에 따라 계산에 의한 경화반응 속도의 예측 치와 실제 실험 데이터가 10$0^{\circ}C$를 제외한 나머지 온도에서는 잘 일치하는 경향을 나타내었다. 경화과정 중 겔화와 유리화와 같은 상 전이를 관찰하였으며 각각의 등온 경화온도에서 경화시간에 따른 유리전이 온도 ($T_{g}$ )를 측정하여 경화온도와 유리전이 온도가 같아지는 유리화점을 구할 수 있었고 절대온도와의 사이에 Arrhenius관계가 성립함을 확인하였다. 또한 평판형 전극을 이용한 DEA는 EMC의 경화 과정을 동정하는데 효과적으로 이용될 수 있음을 알 수 있었다. 같은 종류의 수지 시스템에서는 TTT diagram상에서 $_{gel}$$T_{g}$ 가속제의 농도에 상관없이 일정한 온도에서 나타남을 확인하였다.

  • PDF

Pb(Zn, Nb)$O_3$-Pb(Ni, Nb))$O_3$-$PbTiO_3$-$PbZrO_3$계 세라믹스의 소결 및 전기적 특성 (Sintering and Electric Prooperties of Pb(Zn, Nb)$O_3$-Pb(Ni, Nb))$O_3$-$PbTiO_3$-$PbZrO_3$ System)

  • 박재성;이기태;남효덕
    • 한국세라믹학회지
    • /
    • 제27권7호
    • /
    • pp.934-942
    • /
    • 1990
  • The quarternary system ceramics 0.5[yPb(Zn1/3Nb2/3)O3-(1-y)Pb(Ni1/3Nb2/3)O3]-0.5[xPbTiO3-(1-x)PbZrO3](PZN-PNN-PT-PZ) was fabricated by the columbite precursor method to obtain a stabilized perovskite structure and by conventional method to evaluate the efficiency of the former methd. Dielectric and piezoelectric properties were investigated and the stability of the perovskite phase was studied as a function of PZN and PT contents and firing temperature. In the samples prepared by the columbite precursor method, the pyrochlore phase, which is detrimental to both the dielectric and piezoelectric properties, was not observed in the absence of PZN, and electric properties were improved even when fabricated at low temperature. By adding PZN, some pyrochlore phase appeared and the morphotropic phase boundary of the samples shifted to more Zr-rich composition. The temperature dependence of piezoelectric constant decreased with the addition of PZN, due to the rising of the Curie point.

  • PDF

Photoionization of N,N,N',N'-Tetramethyl-p-phenylenediamine in Polar Solvents

  • Min Yeong Lee;Du Jeon Jang;Minyung Lee;Du-Jeon Jang;Dongho Kim;Sun Sook Lee;Bong Hyun Boo
    • Bulletin of the Korean Chemical Society
    • /
    • 제12권4호
    • /
    • pp.429-433
    • /
    • 1991
  • The photoinduced electron transfer reactions of N,N,N',N'-tetramethyl-p-phenylenediamine (TMPD) in various polar solvents were studied by measuring time-resolved fluorescence. The temperature dependence on the fluorescence decay rate in acetonitrile, methanol, ethanol and buthanol was carried out to obtain the activation energy and Arrehnius factor for the photoinduced electron transfer reaction. It was found that as the dielectric constant of the solvent increases, the activation energy and the reaction rate increase. This implys that the Arrehnius factor is important in controlling the photoinduced electron transfer reaction rate. In water, TMPD exists in three forms (cationic, protonated and neutral forms) due to the high dielectric constant and strong proton donating power of water. The photoinduced electron transfer reaction was found to be very fast (< 50 ps) and also the long liverd component in the fluorescence decay profile attributable to the photoexcited protonated form of TMPD was observed. Probably, the reaction pathway and the reaction coordinate seem to be different depending on the solvents studied here.

상업용 오존촉매와 광촉매를 이용한 오존제거특성 (Characteristics of Residual Ozone Decomposition with Commercial Ozone Decomposition Catalyst (ODC) and Photo catalyst)

  • 변정훈;박재홍;황정호
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.1255-1260
    • /
    • 2004
  • Decomposition of ozone at room temperature was investigated comparatively with commercial monolithic ozone decomposition catalyst (ODC, $MnO_2$) and monolithic photo catalyst ($TiO_2$). The effects of residence time, UV (ultraviolet) light dependence and ozone concentration on the conversion was presented. UV ray was irradiated using BLB (black light blue) lamp ($315{\sim}400$ nm), supplied with a constant intensity in the reactor. The concentration of ozone in the square-shape reactor can be controlled by combining the DBD (dielectric barrier discharge) reactor with an AC high voltage supply system. The catalytic performance, in presence of UV irradiation did not show significant changes for $MnO_2$ catalyst. $TiO_2$ catalyst was the different case, which showed higher decomposition activity in presence of UV irradiation. Deactivation of catalyst detected by real-time ozone monitor for 120 hours with a constant inlet ozone concentration.

  • PDF

압전 PMN-PZT 단결정의 유전 및 압전 특성에 미치는 전극 종류의 영향 (Effect of the Electrode Type on the Dielectric and Piezoelectric Properties of Piezoelectric PMN-PZT Single Crystals)

  • 이종엽;오현택;최균;이호용
    • 한국세라믹학회지
    • /
    • 제52권1호
    • /
    • pp.77-82
    • /
    • 2015
  • The effect of the electrode type on the dielectric and piezoelectric properties of $Pb(Mg_{1/3}Nb_{2/3})O_3-PbZrO_3-PbTiO_3$ (PMN-PZT) single crystals was investigated in an effort to improve their properties for various piezoelectric applications. First, three different types of PMN-PZT single crystals [PMN-PZT-A (piezoelectrically soft type; dielectric constant ~ 10,000), PMN-PZT-B (piezoelectrically soft type; phase-transition temperature between the rhombohedral and tetragonal phases ($T_{RT}$) ~ $145^{\circ}C$), PMN-PZT-C (piezoelectrically hard type; high mechanical quality factor ($Q_m$) ~ 1,000)] were fabricated using the solid-state single crystal growth (SSCG) method. Then, four different types of electrodes [sputtered Au, sputtered Cr/Au, sputtered Ti/Au, and fired Ag] were formed on the single crystals, and their dielectric and piezoelectric properties were measured. The single crystals with a sputtered Ti/Au electrode showed the highest dielectric and piezoelectric constants but the lowest coercive electric field ($E_C$). The single crystals with a fired Ag electrode showed the lowest dielectric and piezoelectric constants but the highest coercive electric field ($E_C$). This dependence on the type of electrode was most significant in the piezoelectrically hard PMN-PZT-C single crystals. However, the effects of the electrode type on the phase transition temperatures ($T_C$, $T_{RT}$) and dielectric loss were negligible. These results clearly demonstrate that it is important to select an appropriate electrode so as to maximize the dielectric and piezoelectric properties of single crystals in each type of piezoelectric application.

Microstructure of the Oriented Hexagonal HoMnO3 Thin Films by PLD

  • Choi, Dong-Hyeok;Shim, In-Bo;Kouh, Tae-Joon;Kim, Chul-Sung
    • Journal of Magnetics
    • /
    • 제12권4호
    • /
    • pp.141-143
    • /
    • 2007
  • We have fabricated (0001) oriented hexagonal $HoMnO_3$ thin films with thickness of 300 nm using Pulsed Laser Deposition (PLD) technique on $Pt(111)/Ti/SiO_2/Si$ substrates. The XRD $\theta-2\theta$ pattern shows only (0002), (0004), and (0008) reflection of a hexagonal phase, and the full width at half maximum (FWHM) of (0004) peak is under $1.6^{\circ}$. The chemical state of Mn from XPS spectra of the films reveals the presence of $Mn^{3+}$ only. The temperature dependence of dielectric constant shows a weak anomaly at magnetic $N\acute{e}el$ temperature $(T_N)$, which is about 70 K.