  • In this study , some factors such as mix proportion, type and dosage of high range water reducing admixture(HRWR) and natural pozzolanas influencing on the slump loss of high strength concrete(H.S.C) using HRWR were investigated for reducing the slump loss. The acquired results indicated that the slump loss of H.S.C was affected according to cement content, sand percentage and type and dosage of HRWR and fly ash was superior to ground granulated blast furance slag in reducing the slump loss of H.S.C.

  • PDF

광물질 혼화재 및 석고를 사용한 고강도 콘크리트의 슬럼프 손실 (Slump Loss of High Strength Concrete Containing Mineral Admixture and Gypsum)

  • 김기형;최재진
    • 한국안전학회지
    • /
    • 제12권1호
    • /
    • pp.101-107
    • /
    • 1997
  • High strength concrete(HSC) using high range water reducing admixture (HRWR) has the defect which severe slump loss occurs according to elapsed time. For using HSC without any trouble, special caution and countermeasure against this problem are necessary. In this study, for minimizing the slump loss of HSC, mineral admixture( flyash, ground granulated blast furnace slag ) and gypsum were used experimentally. Flyash and ground granulated blast furnace slag are effective in reducing the slump loss of HSC. Especially, the slump loss of HSC containing mineral admixture and gypsum Is minimized by the aggregation inhibiting action of gypsum. Cement substituted with flyash 30% or ground granulated blast furnace slag 50% by weight are very effective in minimizing the slump loss.

  • PDF

고성능감수제(高性能減水劑)를 사용한 콘크리트의 유동성(流動性) 손실(損失)을 저감(低減)시키기 위한 연구(硏究) (A Study for Reducing the Slump Loss of Concrete Using High Range Water Reducing Admixture)

  • 문한영;김기형
    • 대한토목학회논문집
    • /
    • 제12권3호
    • /
    • pp.81-90
    • /
    • 1992
  • 고성능감수제를 사용한 콘크리트의 유동성 손실을 저감시키기 위한 연구의 일환으로 시멘트의 종류, 고성능감수제의 종류, 사용방법 및 사용량이 굳지않은 콘크리트의 유동성 손실에 미치는 영향을 파악하기 위하여 시멘트풀, 모르터 및 콘크리트의 유동성 손실과 관련된 실험을 통하여 얻어진 결과에 대하여 고찰하였다. 본 연구결과 고성능감수제의 첨가시기는 시멘트 및 고성능감수제의 종류에 따라 다소 차이가 있으나 30분후 첨가방법이 유동성 손실을 줄이는데 유효하였으며, 대체로 고성능감수제 사용량이 많을수록 유동성 손실이 크게 나타났으며 보통포틀랜드시멘트 콘크리트가 유동성 손실이 가장 크고 플라이애쉬 20% 혼합시멘트 콘크리트에 나프탈린계 고성능감수제를 30분후 첨가한 경우 유동성 손실이 매우 작은 효과가 있었다.

  • PDF

레드믹스트 콘크리트의 슬럼프손실량(損失量)의 추정(推定) 및 슬펌프손실(損失)에 영향을 미치는 요인분석(要因分析) (Estimation and Analysis of Slump Loss in Ready Mixed Concrete)

  • 문한영;최재진
    • 대한토목학회논문집
    • /
    • 제6권2호
    • /
    • pp.23-34
    • /
    • 1986
  • 레미콘의 슬럼프 손실량(損失量)을 추정(推定)할 수 있는 중회귀식(重回歸式)을 유도하였으며, 이 식의 실용성(實用性)을 현장실험을 통하여 확인하므로써 레미콘 생산관리(生産管理)에 응용할 수 있도록 하였다. 레미콘의 슬럼프 손실에 영향을 미치는 요인(要因) 중에서 운반거리와 운반시간에 대하여 조사 분석하고, 레미콘 트럭의 대기시간과 배출시간이 슬럼프 관리면에서 문제시되고 있음을 지적하였다. 그리고 콘크리트의 배합, 온도 및 혼화제의 종류와 사용량이 슬럼프 손실에 미치는 영향을 검토한 결과, 일반적으로 단위시멘트량 및 믹싱직후의 슬럼프값의 크기에 따른 슬럼프 손실은 큰 차이가 없는 것으로 분석되었다. 또한 혼화제의 종류에 따라 슬럼프 손실을 크게 하는 경우도 있었으나, 혼화제의 사용량에 따른 차이는 거의 없었다.

  • PDF

고강도 콘크리트의 배합방법과 운반특성에 관한 실험적 연구 (An Experimental Study on the High Strength Concrete Properties for Mixing Methods and Elapsed time)

  • 권녕호;안재현;박칠림
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1992년도 봄 학술발표회 논문집
    • /
    • pp.7-12
    • /
    • 1992
  • The aim of this study is to develop economical High-Strength and High-Quality Concrete, and to assure quality control of Concrete in the field. For this purpose, Five types of Mixing Methods are examined and the relationship between slump loss and slump recovery by transport is studied. As a result, workability and strength are dependent on the Mixing Method, although the Mixing proportions are same, Also, adding admixture in the field is proposed as an alternative to consider the relationship between slump loss and slump recovery.

  • PDF

실리카흄 사용 고강도콘크리트의 기초적 성질에 대한 연구 (A Study on the Fundamental Properties of High Strength Concrete Using Silica Fume)

  • 문한영;김기형;문대중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1993년도 가을 학술발표회 논문집
    • /
    • pp.11-17
    • /
    • 1993
  • In this study, the fundamental properties of High-Strength Concrete(HSC), such as the slump loss, the temperature increment, the strength development, are considered by experiment. In reducing the temperature and the slump loss, and developing the strength of HSC, the application of silica fume as an admixtures is very effective. And when gypsum is added, the slump loss is reduced and the strength of HSC is improved remarkably, but the temperature of concrete is increased, thus a more study to reduce the temperature increment is required

  • PDF

플라이 애시 및 석고를 활용한 고강도 콘크리트의 성능개선 (Improvement of Properties of High Strength Concrete Using Fly Ash and Gypsum)

  • 김기형;최재진;최연왕
    • 콘크리트학회논문집
    • /
    • 제11권5호
    • /
    • pp.99-105
    • /
    • 1999
  • In producing high strength concrete, the most practical method is to use high range water reducing admixture(HRWR). Workabili쇼 of concrete using HRWR varies rapidly with elapsed time after mixing. Effects of fly ash and gypsum on slump loss and compressive strength of concrete were examined by experiment in this study. The slump loss of high strength concrete was reduced with increase of substitution ratio of fly ash. When 2~4% gypsum of cement weight was applied, the reduction of slump loss was not prominent and strength increase appeared at all test ages.

고성능 AE감수제를 사용한 콘크리트의 기초적 성질 (Properties of Concrete Using Slump Retentive Superplasticizer)

  • 최재진;김은겸;신치범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 봄 학술발표회 논문집(I)
    • /
    • pp.638-644
    • /
    • 1999
  • Workability time of superplasticized concrete is maintained generally for 30-60 minutes only. Therefore it is of great advantage for the concrete producer to use a high range water reducer which provides an extended slump life. Recently slump retentive srperplasticizer has been developed. Concrete mixing tests were done to know slump, setting, air content, bleeding and hardening characteristics of concrete using slump retentive superplasticizer. With slump retentive superplasticizer, high quality concrete was produced and slump loss of concrete was reduced in big way, making long transportation time possible as a practical alternative to on-site addition.

  • PDF

재생 골재 콘크리트의 슬럼프 손실 개선을 위한 분말형 감수제의 활용 (Application of Powdered Superplasticizer to Improve of Slump Loss Rate in Recycled Aggregate Concrete)

  • 양근혁;심재일;이재삼;정헌수
    • 콘크리트학회논문집
    • /
    • 제18권5호
    • /
    • pp.649-656
    • /
    • 2006
  • 본 연구에서는 재생 골재 콘크리트의 현장적용성을 높이기 위해 보통 콘크리트에 비해 큰 슬럼프 손실을 개선할 수 있는 분말형 감수제(PSP제)를 개발하였다. 이 PSP제가 혼입된 콘크리트의 유동성 및 역학적 성질들을 평가하기 위하여 재생 굵은골재와 재생 잔골재 혼입조건에 24배합이 실험되었다. 액상형 고성능 감수제를 투입한 콘크리트의 슬럼프는 시간경과와 함께 급격히 감소하며 120분 후에는 초기 슬럼프의 50% 이하로 떨어졌다. 하지만 PSP 제를 혼입한 콘크리트의 슬럼프는 배합 후 30분 까지는 거의 변화가 없으며 1시간 경과 후에도 초기 슬럼프의 85% 이상을 유지하였다. 뿐만 아니라 PSP제는 콘크리트의 압축강도, 할렬인장강도, 휨강도 및 탄성계수들도 향상시켰으며 건조수축 변형률을 감소시켰다. 콘크리트의 성능향상을 고려하였을 때 PSP제의 최적 혼입률은 시멘트 양 대비 5%이었다.

콘크리트의 제 성질 향상을 위한 혼화재 활용에 대한 연구 (A Study on the Utilization of mineral Admixture to Improve the Properties of Concrete)

  • 문한영;문대중;신화철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 봄 학술발표회 논문집
    • /
    • pp.124-128
    • /
    • 1997
  • In order tohave a betterunderstanding of thefavorable effect ofground granulated blast-furnace slag and fly ash, slump loss, temperature risingand compressive strength of concrete were investigated into diffrent conditions. When slag was mixed with ordinary portland cement as30%, slump loss gotto some 18% at 60min, maximum temperatureto some $43^{\cire}C$ at 180min, compressive strength similar to that of ordinary portland concrete at 28 days. Therefore it wasnoted thatslump loss andmaximum teaperaturerising of concrete were very reduced according to ground granulated blast-furnace slag and fly ash mixed with ordinary portland cement.