• 제목/요약/키워드: Silver powder size

검색결과 42건 처리시간 0.03초

은 플레이크 분말의 입자크기에 미치는 기계적 밀링 공정변수의 영향 (Effect of Mechanical Milling Parameters on the Particle Size of Silver Flake)

  • 이길근;정해영
    • 한국분말재료학회지
    • /
    • 제21권4호
    • /
    • pp.307-312
    • /
    • 2014
  • This study is focused on investigating the relation between the particle size of silver flake powder and mechanical milling parameters. Mechanical milling parameters such as ball size, impeller rotation speed and milling time of the attrition ball-mill were controlled to produce silver flake powder. The particle size of the silver flake powder increased with increasing ball size and impeller rotation speed. The change of the particle size of the silver flake powder with mechanical milling parameters was analyzed based on balls motion in the mill container of the attrition ball-mill. The silver flake particles were formed at the elastic deformation area of the ball due to the collision between balls. The change of the particle size of the silver flake powder with mechanical milling parameters well consists with the change of the collision energy of ball with parameters mentioned above.

기계적 밀링공정에 의한 은 플레이크 분말 제조 (Fabrication of Silver Flake Powder by the Mechanical Milling Process)

  • 정해영;이길근
    • 한국분말재료학회지
    • /
    • 제23권1호
    • /
    • pp.54-60
    • /
    • 2016
  • This study focuses on fabricating silver flake powder by a mechanical milling process and investigating the formation of flake-shaped particles during milling. The silver flake powder is fabricated by varying the mechanical milling parameters such as the amount of powder, ball size, impeller rotation speed, and milling time of the attrition ballmill. The particle size of the silver flake powder decreases with increasing amount of powder; however, it increases with increasing impeller rotation speed. The change in the particle size of the silver flake powder is analyzed based on elastic collision between the balls, taking energy loss of the balls due to the powder into consideration. The change in the particle size of the silver flake powder with mechanical milling parameters is consistent with the change in the diameter of the elastic deformation contact area of the ball, due to the collision between the balls, with milling parameters. The flake-shaped silver particles are formed at the elastic deformation contact area of the ball due to the collision.

패각분말을 이용한 살균성 메디아의 제조 및 정수기용 필터에 대한 응용 (Manufacture of Sterilizing Media with Shell Powder and It's Application to the Filter of Water Clarifier)

  • 신춘환
    • 한국환경과학회지
    • /
    • 제15권11호
    • /
    • pp.1027-1034
    • /
    • 2006
  • Antimicrobial powder was made by exchanging silver ion on calcined oyster shell. On the purpose of application to water clarifier, bail-type media mixed with antimicrobial powder and $0{\sim}30%$ white kaoline were made. The sterilization effect, pore size distribution and zeta potential was tested to indicate the condition for the media of water clarifier. From these tests, it was confirmed that this media have an excellent sterilization power on $G^-\;and\;G^+$ germs. As the concentration of the exchanged silver ion increased, the surface charge density of the anions on the surface of the media also increased. The surface pore size decreased with the concentration of silver ion and 20% more white kaoline ratio. Consequently, mixing ratio of white kaoline would appear to indicate the optimun condition as media have sterilization power.

환원침전법을 이용한 수용액으로부터 은 나노분말의 제조 연구 (Preparation of Ag Nano-Powder from Aqueous Silver Solution through Reductive Precipitation Method)

  • 이화영;오종기
    • 자원리싸이클링
    • /
    • 제14권6호
    • /
    • pp.21-27
    • /
    • 2005
  • 국내 은 함유 폐자원의 고부가가치 제품화를 위한 연구의 일환으로써 sodium formaldehydesulfoxy와 ascorbic acid를 각각 환원제로 사용한 Ag 나노분발의 제조실험을 수행하였다. Ag수용액은 질산은을 소정 농도로 증류수에 용해시켜 사용하였으며, Ag미립자의 응집방지를 위한 분산제로는 Tamol NN8906, PVP, SDS 및 caprylic acid를 각각 사용하었다. 환원반응을 통하여 제조한 Ag 미립자는 입도분석기 및 TEM측정을 통하여 morphology와 평균입도를 측정하였다. sodium formaldehydesulfoxylate 에 의한 은의 환원을 위해서는 이론치의 1.4배를 첨가해 주어야 하는 것으로 나타났으며, ascorbic acid와는 달리 생성된 Ag 입자가 너무 크게 성장하는 문제점이 있었다. 분산제에 따른 Ag 입자의 특성을 살펴본 결과, Tamol 및 PVP를 사용한 경우에는 bimodal distribution을 보였으나, SDS 와 caprylic acid의 경우에는 수십 nm에서 $100{\mu}m$에 이르는 매우 broad한 입도분포를 보였다.

Flake-type Ag분말의 입자크기에 따른 신축성 전극 특성 연구 (Stretchable Electrode Properties Study According to Particle Size of Flake-type Ag Powders)

  • 남현민;서민호;남수용
    • 마이크로전자및패키징학회지
    • /
    • 제29권4호
    • /
    • pp.35-40
    • /
    • 2022
  • 본 연구에서는 실버 파우더의 입자 크기, 즉 평균입자 크기가 2㎛, 7㎛, 이들의 혼합(50:50wt%), 이렇게 3가지 실버 페이스트를 제조하여 점도 및 점탄성, 경화후에 잔류용제 유무 확인을 위한 TGA측정, Strain에 따른 저항변화 및 전극 표면구조 변화에 대해서 검토한 결과 다음과 같은 결론을 얻을 수 있었다. 이러한 결과를 정리하면 Strain에 따른 저항변화를 최소화하기 위해서는 실버 파우더의 입자를 2㎛정도인 것이 가장 바람직함을 알 수 있었다.

불활성 증발 응축방법으로 제조된 금과 은 나노입자의 소결특성 (Sintering Characteristics of Au and Ag Nanoparticles Prepared by Inert Gas Condensation)

  • 이승현;민동열;이광민
    • 한국분말재료학회지
    • /
    • 제14권3호
    • /
    • pp.165-172
    • /
    • 2007
  • The purpose of this study was to analyze the sintering characteristics of gold and silver nanoparticles. In this study, gold and silver nanoparticles were prepared by using Inert Gas Cndensation (IGC). The sintering temperatures for gold and silver nanoparticles were $100{\sim}1000^{\circ}C\;and\'100{\sim}500^{\circ}C$, respectively. The sintering characteristics of gold and silver nanoparticles prepared by IGC were evaluated by X-ray diffraction(XRD), transmission electron microscopy (TEM), and scanning electron microscopy (SEM). Gold and silver nanoparticles with the size of $1{\sim}100\;nm\;and\;10{\sim}100\;nm$, respectively, were obtained. The size of sintered gold and silver nanoparticles increased with an increase in the sintering temperature. XRD data showed that silver nanoparticles were similar with polycrystal single-phase.

전도성 실버 페이스트의 미세구조 발달에 미치는 glass-frit 크기의 영향 (Influence of Glass-Frit Size on the Microstructural Evolution of Conductive Silver Paste)

  • 한현근;서동석;이종국
    • 대한금속재료학회지
    • /
    • 제46권8호
    • /
    • pp.516-523
    • /
    • 2008
  • The effect of glass-frit size on microstructural evolution and electrical resistance of conductive silver paste was investigated. Silver paste was prepared by mixing 70 wt% commercial silver powder with $1.6{\mu}m$, 3 wt% Bi based glass-frit and 27 wt% organic vehicle. Two different sizes of glass-frit were obtained by ball-milling of commercial glass-frit ($3{\mu}m$) for 3 and 5 days, which had an average particle size of 1.0 and $0.5{\mu}m$. The smaller glass-frit was melt at low sintered temperature and rapidly spread between the silver particles, which is induced the dense networking among silver particles and strong adhesiveness to $Al_2O_3$ substrate. The silver film with smaller glass-frit sintered at $500^{\circ}C$ showed the small pore size and low porosity resulting in low electrical resistivity of $4{\mu}{\Omega}cm$.

Hydrazine Hydrate 환원(還元)에 의한 질산은(窒酸銀) 수용액(水溶液)으로부터 은(銀) 나노분말(粉末)의 제조(製造) 연구(硏究) (Preparation of Ag Nano-Powder from Aqueous Silver Nitrate Solution through Reduction with Hydrazine Hydrate)

  • 이화영
    • 자원리싸이클링
    • /
    • 제15권4호
    • /
    • pp.19-26
    • /
    • 2006
  • 함은 폐재의 리싸이클링을 위한 연구의 일환으로써 Hydrazine Hydrate을 환원제로 사용하여 질산은 수용액으로부터 Ag 나노분말을 제조하기 위한 실험을 수행하였다. 이를 위해 질산은을 소정 농도로 증류수에 용해시킨 수용액에 Ag 미립자의 응집방지를 위한 분산제로써 Tamol NN8906 혹은 Tween 20을 미리 혼합한 다음 환원제인 Hydrazine Hydrate 용액을 첨가하는 방법으로 환원반응을 실시하였다. 환원반응을 통하여 제조한 Ag 미립자는 입도분석기 및 TEM 측정을 통하여 형상과 평균입도를 측정하였다. Hydrazine Hydrate에 의한 은의 환원을 위해서는 이론치의 약 2배를 첨가해 주어야 하는 것으로 나타났으며, Tamol NN8906을 분산제로 사용하여 제조한 Ag 나노분발은 매우 좁은 입도범위의 분포특성을 보여 주었다. Tween 20을 분산제로 사용한 경우의 입도 분포는 bimodal 혹은 multimodal distribution을 보였으며, 입자 모양에 있어서는 Tamol NN8906과 Tween 20이 모두 비슷하게 표면이 매끄러운 불규칙한 모양의 입자들로 구성되어 있었다.

LTCC 전극공정부산물 침출 용액으로부터 은 회수 및 은 나노입자 제조 (Recovery and Synthesis of Silver Nanoparticles from Leaching Solution of LTCC Electrode By-Products)

  • 유주연;강유빈;박진주;류호진;윤진호;이근재
    • 한국분말재료학회지
    • /
    • 제24권4호
    • /
    • pp.315-320
    • /
    • 2017
  • There has been much interest in recycling electronic wastes in order to mitigate environmental problems and to recover the large amount of constituent metals. Silver recovery from electronic waste is extensively studied because of environmental and economic benefits and the use of silver in fabricating nanodevices. Hydrometallurgical processing is often used for silver recovery because it has the advantages of low cost and ease of control. Research on synthesis recovered silver into nanoparticles is needed for application to transistors and solar cells. In this study, silver is selectively recovered from the by-product of electrodes. Silver precursors are prepared using the dissolution characteristics of the leaching solution. In the liquid reduction process, silver nanoparticles are synthesized under various surfactant conditions and then analyzed. The purity of the recovered silver is 99.24%, and the average particle size of the silver nanoparticles is 68 nm.

Ag 파우더 특성에 따른 터치 패널용 그라비어 오프셋 인쇄의 전도성 페이스트의 제조 및 물성 연구 (A Study on the Characteristics and Property of Gravure Off-set Printing Conductive Paste for Touch Panel by Ag Powder Characteristic)

  • 송재형;장아람;김성빈;남수용
    • 한국인쇄학회지
    • /
    • 제29권2호
    • /
    • pp.45-58
    • /
    • 2011
  • Gravure off-set printing recently is used in electronics display market. This method has advantages of mass production and high printing speed. It is also fine pattern can be implemented. We have manufactured low-curable conductive Ag pastes for gravure off-set printing. When printing, the pastes be used different silver powder shape because of the printing characteristics. The pastes were prepared with silver powder by silver powder shape and size, epoxy resin, solvent and homogenized on a standard three-roll mill. And the pastes exhibited a shear-thinning flow at viscosity profile. Moreover the adhesive strength and resistivity of silver film had a good characteristics. With the manufactured paste in this study, touch panel had is manufactured and it had $4{\times}10-5{\Omega}.cm$.