Ir-Re thin films with Ti interlayer were deposited onto the tungsten carbide substrate by ion beam assisted DC magnetron sputtering. The Ir-Re films were prepared with targets of having two atomic percent of 7:3 and 5:5. The microstructure and surface analysis of the specimen were conducted by using SEM, XRD and AFM. Mechanical properties such as hardness and adhesion strength of Ir-Re thin film also were examined. The interlayer of pure titanium was formed with 100 nm thickness. The film growth of Ir-30at.%Re was faster than that of Ir-50at.%Re in the same deposition conditions. Ir-Re thin films consisted of dense and columnar structure irrespective of the different target compositions. The values of hardness and adhesion strength of Ir-30at.%Re thin film coated on WC substrate were higher than those of Ir-50at.%Re thin film.
Oskomov, Konstantin V.;Chun, Hui-Gon;You, Yong-Zoo;Lee, Jing-Hyuk;Kim, Kwang-Bok;Cho, Tong-Yul;Sochogov, Nikolay S.;Zakharov, Alexender N.
한국표면공학회지
/
제36권1호
/
pp.27-33
/
2003
Pulsed magnetron sputtering of graphite target was employed for deposition of diamond-like carbon (DLC) films. Time-resolved probe measurements of magnetron discharge plasma have been performed. It was shown that the pulsed magnetron discharge plasma density ($∼10^{17}$$m^{-3}$ ) is close to that of vacuum arc cathode sputtering of graphite. Raman spectroscopy was sed to examine DLC films produced at low ( $U_{sub}$ / < 1 kV) pulsed bias voltages applied to the substrate. It has been shown that maximum content of diamond-like carbon in the coating (50-60%) is achieved at energy per deposited carbon atom of $E_{c}$ =100 eV. In spite of rather high percentage of $sp^3$-bonded carbon atoms and good scratch-resistance, the films showed poor adhesion because of absence of ion mixing between the film and the substrates. Electric breakdowns occurring during the deposition of the insulating DLC film also thought to decrease its adhesion.
RF 마크네트론 스퍼터법으로 Ce의 일부를 희토류 원소로 치환한 Ce$_{1-x}$RE$_{x}$O$_{2-y}$(0.1$\leq$x$\leq$0.4, RE=Y, Nd) 박막을 Si(111), $Al_2$O$_3$(1012) 기판 위에 1450~1$600^{\circ}C$로 소결한 target을 이용하여 성장시켰다. Ce$_{1-x}$RE$_{x}$O$_{2-y}$ 박막의 성장시 기판온도 및 증착시간 등을 변화시켜 성장시켰으며, 성장된 박막의 특성분석은 XRD, SEM, TEM으로 행하였다. 증착된 박막의 방향성 및 결정성장 거동은 증착온도 및 시간에 따라 차이를 보였다. Si(111) 기판 위에 증착된 Ce$_{1-x}$Y$_{x}$O$_{2-y}$(x=0.3) 박막의 경우, 80$0^{\circ}C$에 비해 7$50^{\circ}C$에서 증착 시간에 따른 (111) 우선배향성의 정도가 나은 결과를 보였으며, $Al_2$O$_3$(1012) 기판 위에 증착한 Ce$_{1-x}$Nd$_{x}$O$_{2-y}$(x=0.3) 박막 또는 (111) 우선배향성을 나타내었다.을 나타내었다.
Chun, Hui-Gon;Sochugov, Nikolay S.;You, Yong-Zoo;Soloviv, Andrew A.;Zakharov, Alexander N,
반도체디스플레이기술학회지
/
제2권3호
/
pp.19-23
/
2003
Extended unbalanced magnetron sputtering system based on the cylindrical magnetron with a rotating cathode was developed. The unbalanced configuration of magnetic field was realized by means of additional lines of permanent magnets, placed along both sides of a 89 mm outer diameter and 600 mm long cylindrical cathode. The performance of the unbalanced magnetron was assessed in terms of the ion current density and the ion-to-atom ratio incident at the substrate. Furthermore, the paper presents the comparison of the internal plasma parameters, such as the electron temperature, electron density, plasma and floating potentials, measured by a Langmuir probe in various positions from the cathode, for conventional and unbalanced constructions of the cylindrical magnetron. The plasma density and ion current density are about 3-5 times higher than those of conventional one, in the unbalanced magnetron in a 0.24 Pa Ar atmosphere with a DC cathode power of 3 kW.
AZO (ZnO:Al) were fabricated by RF magnetron sputtering In $H_2/Ar(5%\;H_2)$ atmosphere, and structural, electrical and optical properties were investigated. The substrate temperatures were varied at RT, $100^{\circ}C,\;150^{\circ}C$ and$200^{\circ}C$. The resistivity of the films grown in $H_2/Ar(5%\;H_2)$ were reduced from $7.67{\times}10^{-4}{\Omega}\;cm$ to $5.95{\times}10^{-4}{\Omega}\;cm$ comparing that Ar (100%) and the transmittance of the ZnO:Al films in the visible range was 85%.
Chun, Hui-Gon;You, Yong-Zoo;Nikolay S. Sochugov;Sergey V. Rabotkin
한국표면공학회지
/
제36권4호
/
pp.296-300
/
2003
Extended cylindrical magnetron sputtering system with rotating 600-mm long and 90-mm diameter graphite cathode and pulsed power supply voltage generator were developed and fabricated. Time-dependent Langmuir probe characteristics as well as carbon films thickness were measured. It was shown that ratio of ions flux to carbon atoms flux for pulsed magnetron discharge mode was equal to $\Phi_{i}$$\Phi$sub C/ = 0.2. It did not depend on the discharge current in the range of $I_{d}$ / = 10∼60 A since both the plasma density and the film deposition rate were found approximately proportional to the discharge current. In spite of this fact carbon film structure was found to be strongly dependent on the discharge current. Grain size increased from 100 nm at $I_{d}$ = 10∼20 A to 500 nm at $I_{d}$ = 40∼60 A. To deposit fine-grained hard nanocrystalline or amorphous carbon coating current regime with $I_{d}$ = 20 A was chosen. Pulsed negative bias voltage ($\tau$= 40 ${\mu}\textrm{s}$, $U_{b}$ = 0∼10 ㎸) synchronized with magnetron discharge pulses was applied to a substrate and voltage of $U_{b}$ = 3.4 ㎸ was shown to be optimum for a hard carbon film deposition. Lower voltages were not sufficient for amorphization of a growing graphite film, while higher voltages led to excessive ion bombardment and effects of recrystalization and graphitization.
In nitride and oxide film deposition, sputtered metals react with nitrogen or oxygen gas in a vacuum chamber to form metal nitride or oxide films on a substrate. The physical properties of sputtered films (metals, oxides, and nitrides) are strongly influenced by magnetron plasma density during the deposition process. Typical target power densities on the magnetron during the deposition process are ~ (5-30) W/cm2, which gives a relatively low plasma density. The main challenge in reactive sputtering is the ability to generate a stable, arc free discharge at high plasma densities. Arcs occur due to formation of an insulating layer on the target surface caused by the re-deposition effect. One current method of generating an arc free discharge is to use the commercially available Pinnacle Plus+ Pulsed DC plasma generator manufactured by Advanced Energy Inc. This plasma generator uses a positive voltage pulse between negative pulses to attract electrons and discharge the target surface, thus preventing arc formation. However, this method can only generate low density plasma and therefore cannot allow full control of film properties. Also, after long runs ~ (1-3) hours, depends on duty cycle the stability of the reactive process is reduced due to increased probability of arc formation. Between 1995 and 1999, a new way of magnetron sputtering called HIPIMS (highly ionized pulse impulse magnetron sputtering) was developed. The main idea of this approach is to apply short ${\sim}(50-100){\mu}s$ high power pulses with a target power densities during the pulse between ~ (1-3) kW/cm2. These high power pulses generate high-density magnetron plasma that can significantly improve and control film properties. From the beginning, HIPIMS method has been applied to reactive sputtering processes for deposition of conductive and nonconductive films. However, commercially available HIPIMS plasma generators have not been able to create a stable, arc-free discharge in most reactive magnetron sputtering processes. HIPIMS plasma generators have been successfully used in reactive sputtering of nitrides for hard coating applications and for Al2O3 films. But until now there has been no HIPIMS data presented on reactive sputtering in cluster tools for semiconductors and MEMs applications. In this presentation, a new method of generating an arc free discharge for reactive HIPIMS using the new Cyprium plasma generator from Zpulser LLC will be introduced. Data (or evidence) will be presented showing that arc formation in reactive HIPIMS can be controlled without applying a positive voltage pulse between high power pulses. Arc-free reactive HIPIMS processes for sputtering AlN, TiO2, TiN and Si3N4 on the Applied Materials ENDURA 200 mm cluster tool will be presented. A direct comparison of the properties of films sputtered with the Advanced Energy Pinnacle Plus + plasma generator and the Zpulser Cyprium plasma generator will be presented.
RF magnetron sputtering법에 의해 단상의 하이드록시아파타이트와 하이드록시아파타이트은 복합코팅층을 ZrO$_2$와 Si 웨이퍼 기판에 코팅하였다. 이들 코팅층들의 두께 0.7∼1.0$\mu\textrm{m}$ 범위였으며 또한 거칠기(roughness)는 3∼4nm였다. 열처리된 HAp 코팅층은 나노크기의 결정들로 구성되어 있었으며, 반면 Ag가 함유된 복합코팅층의 경우 결정질과 비결정질이 혼재되어 있었다. 열처리 전 HAp 코팅층의 Ca/P비는 1.9였고, Ag의 함량이 증가함에 따라 비는 감소하는 경향을 나타내었다. 또한 Ag 함량이 증가함에 따라 HAp코팅층의 미소 경도는 감소하였다.
NiO 산화물 타겟을 이용한 RF 마그네트론 스퍼터로 상온에서 Si(100) 기판 위에 NiO 박막을 증착시켜, 스퍼터 가스의 산소 유량비가 NiO 박막의 결정 배향성과 표면 형상에 미치는 영향을 조사하였다. Ar 가스에서 증착된 NiO 박막은 높은결정화도와 (100)면의 우선 배향성을 나타내었으나, $O_2$ 가스에서 증착된 경우에는 (111)면의 우선 배향성을 보였으며 그 증착속도도 감소하였다. 스퍼터 가스의 $O_2$ 함량에 따른 NiO 박막의 결정성과 우선배향성 변화에 대한 요인을 고찰하였으며, 박막의 표면 형상과 거칠기의 변화를 조사하였다.
TSV(through silicon via)는 긴 종횡비를 갖는 패턴에 Cu, Ta, Ti을 높은 conformality를 갖도록 증착하는 공정이다. Magnetron cathode의 자석 배열 설계는 target 물질 종류에 따라서 multitrack, water drop type등이 있으며 target과 substrate 사이의 공간에 플라즈마를 형성시켜서 기판에 이온 입사량을 늘린 후 기판 바이어스를 이용하여 이온 충돌, re-sputtering을 통한 재증착 과정을 통해 치밀한 금속 박막을 연속적으로 형성할 수 있도록 하는 것이 목적이다. 또한 sputter가 사용되고 있는 분야에 효율을 증대시키고, 증착되는 막의 품질향상을 위해 UBMS를 사용하고 있으며, 산업에 사용되어 지는 300 mm wafer용 시스템은 제작비가 약 10억 원 정도 소요되며 다양한 테스트를 진행하기 위해선 많은 비용이 소요된다. 따라서 비용과 소요시간을 줄여 다양한 테스트를 위해 소규모 플라즈마 시스템을 설계하게 되었다. 61 l/sec 터보 분자 펌프와 다이아프램 펌프를 기초로한 TMP station에 2.75 인치 CF flange가 장착된 6 way cross를 main 챔버로 활용하고, 작은 size의 unbalanced magnetron cathode를 제작, 장착한 다음 6 way cross 주변에 전자석을 적절히 배치하여 300 mm wafer system에서와 동일한 물리적 현상을 테스트 할 수 있도록 하였다. Fig1. (a) UBMS system의 사진을 나타내었고, (b)에는 6 way cross 내부에 발생된 플라즈마의 형상을 나타내었다. 전원 장치는 Advanced Energy사의 MDX-1.5K DC power supply를 사용하였고, 방전 전압 - 전류 관계의 가스 압력에 따른 plasma 현상과 magnetron 배율에 따른 plasma 현상 그리고 전자석에 의한 영향을 주로 관찰 하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.