Hydroxyapatite (HAp) powders with different crystallinities were synthesized at various calcination temperatures through the co-precipitation of $Ca(OH)_2$ and $H_3PO_4$. The degradation behavior of these HAp powders with different crystallinities was assessed in a simulated body fluid solution (SBF) for 8 weeks. Below $800^{\circ}C$, the powders were nonstochiometric HAp, and the single HAp phase was successfully synthesized at $800^{\circ}C$. The degree of crystallinity of the HAp powders increased with an increasing calcination temperature and varied in a range from 39.6% to 92.5%. In the low crystallinity HAp powders, the Ca and P ion concentrations of the SBF solution increased with an increasing soaking time, which indicated that the low crystallinity HAp degraded in the SBF solution. The mass of the HAp powders linearly decreased with respect to the soaking time, and the mass loss was higher at lower crystallinities. The mass loss ranged from 0.8% to 13.2% after 8 weeks. The crystallinity of the HAp powders increased with an increasing soaking time up to 4 weeks and then decreased because of HAp degradation. The pH of the SBF solution did not change much throughout the course of these experiments. These results suggested that the crystallinity of HAp can be used to control the degradation.
Im W. S.;Yoon T. S.;Yu F. C.;Gao C. X.;Kim D. J.;Ibm Y. E.;Kim H. J.;Kim C. S.;Kim C. O.
Korean Journal of Materials Research
/
v.15
no.1
/
pp.73-77
/
2005
Motivated by the enhanced magnetic properties of Mg-codoped GaMnN ferromagnetic semiconductors, Be-codoped GaMnAs films were grown via molecular beam epitaxy with varying Mn flux at a fixed Be flux. The structural, electrical, and magnetic properties were investigated. GaAs:(Mn,Be) films showed metallic behavior while GaAs:Mn films showed semiconducting behavior as determined by the temperature dependent resistivity measurements. The Hall-effect measurements with varying magnetic field showed clear anomalous Hall effect up to room temperature proving ferromagnetism and magnetotransport in the GaAs:(Mn,Be) films. Planar Hall resistance measurement also confirmed the properties. The dramatic enhancement of the Curie temperature in GaMnAs system was attributed to Be codoping in the GaMnAs films as well as MnAs precipitation.
In this study, leaching process to extract phosphorus from the steelmaking slag was investigated for using the fertilizer resources of agriculture. In general, the phosphorus of steelmaking slag is formed as $C_2S-C_3P$ solid solution, and also, this solid solution is soluble in water more than the other phase in slag, and less than free CaO phase. In the present experiment, the influence of pH on the leaching behavior of various elements from the steelmaking slag was investigated by using multi-component steelmaking slag. When the pH was decreased, the concentration of Ca, Si, P and Fe in solution from the steelmaking slag was increased. Furthermore, at a pH of 3, the concentration of P ion in solution was decreased as leaching time increased. It is considered that the decrement of P was caused from the precipitation reaction between P ion and Fe ion in solution.
Kim, Jun Hwan;Baek, Jong Hyuk;Lee, Byoung Oon;Lee, Chan Bock;Yoon, Young Soo
Korean Journal of Metals and Materials
/
v.48
no.8
/
pp.691-698
/
2010
A study has been carried out to evaluate the interaction behavior between a lanthanide element and clad material in order to analyze the effect of the lanthanide element on the fuel cladding chemical interaction (FCCI). A diffusion couple test between Misch metal (70Ce-30La) and ferritic-martensitic steel (Gr.92) was performed at $660^{\circ}C$, followed by a microstructural analysis of the coupled sample. The results showed that Ce in the Misch metal, rather than La, reacted with the ferritic-martensitic steel (FMS) to form an interaction layer that penetrated the clad thickness. Fe diffused outside the clad interface to form an $Fe_2Ce$ compound, leaving a depletion of Fe caused by excess diffusion as well as by the formation of Cr-rich precipitation inside the interaction layer. The rate of growth followed the cubic rate law, which indicated that Fe depletion was caused by the diffusion of Fe and that the associated Cr-rich phase formation controlled the whole diffusion process.
Kim, Hyeju;Lee, Hyoungrok;Kim, Kyeong-A;Lee, Joodong;Oh, Kyung-sik;Kwon, Sang-Hum;Kim, Donggyu
Journal of Korea Foundry Society
/
v.39
no.1
/
pp.7-13
/
2019
Few studies of large blooms over 700 mm thick among those used for the forging of raw materials have been reported. The cooling rate difference between the surface and the center of a large bloom is large, and the degradation of the mechanical properties is likely in cases involving excessively coarse precipitates resulted from the slow cooling rate of a large bloom after casting. Therefore, a schematic investigation of the growth behaviors of precipitates while varying their locations in blooms is necessary. The dissolution behaviors of precipitates were investigated by simulating a reheating process during which the bloom is heated to a high temperature. The segregation behavior of the as-cast large bloom was also investigated. Reheating specimens were obtained after an isothermal heat treatment at $1150^{\circ}C$ with various holding times to simulate the reheating process, with the samples undergoing a subsequent water quenching step. The precipitates were extracted using an electrolytic extractor and a particle size analysis was conducted with the aid of SEM, EDS, and TEM. In the present work, Al oxide, MnS and Nb carbide were mainly observed.
Application of a stronger and more durable material for reactor pressure vessels (RPVs) might be an effective way to insure the integrity and increase the efficiency of nuclear power plants. A series of research projects to apply the SA508 Gr.4 steel in ASME code to RPVs are in progress because of its excellent strength and durability compared to commercial RPV steel (SA508 Gr.3 steel). In this study, the microstructural characteristics and mechanical properties of SA508 Gr.3 Mn-Mo-Ni low alloy steel and SA508 Gr.4N Ni-Mo-Cr low alloy steel were investigated. The differences in the stable phases between these two low alloy steels were evaluated by means of a thermodynamic calculation using ThermoCalc. They were then compared to microstructural features and correlated with mechanical properties. Mn-Mo-Ni low alloy steel shows the upper bainite structure that has coarse cementite in the lath boundaries. However, Ni-Mo-Cr low alloy steel shows the mixture of lower bainite and tempered martensite structure that homogeneously precipitates the small carbides such as $M_{23}C_6$ and $M_7C_3$ due to an increase of hardenability and Cr addition. In the mechanical properties, Ni-Mo-Cr low alloy steel has higher strength and toughness than Mn-Mo-Ni low alloy steel. Ni and Cr additions increase the strength by solid solution hardening. In addition, microstructural changes from upper bainite to tempered martensite improve the strength of the low alloy steel by grain refining effect, and the changes in the precipitation behavior by Cr addition improve the ductile-brittle transition behavior along with a toughening effect of Ni addition.
Park, Sang Gyu;Kim, Min-Chul;Lee, Bong-Sang;Wee, Dang-Moon
Korean Journal of Metals and Materials
/
v.46
no.12
/
pp.771-779
/
2008
An effective way of increasing the strength and fracture toughness of reactor pressure vessel steels is to change the material specification from that of Mn-Mo-Ni low alloy steel(SA508 Gr.3) to Ni-Mo-Cr low alloy steel(SA508 Gr.4N). In this study, we evaluate the effects of alloying elements on the microstructural characteristics of Ni-Mo-Cr low alloy steel. The changes in the stable phase of the SA508 Gr.4N low alloy steel with alloying elements were evaluated by means of a thermodynamic calculation conducted with the software ThermoCalc. The changes were then compared with the observed microstructural results. The calculation of Ni-Mo-Cr low alloy steels confirms that the ferrite formation temperature decreases as the Ni content increases because of the austenite stabilization effect. Consequently, in the microscopic observation, the lath martensitic structure becomes finer as the Ni content increases. However, Ni does not affect the carbide phases such as $M_{23}C_6 $ and $M_7C_3$. When the Cr content decreases, the carbide phases become unstable and carbide coarsening can be observed. With an increase in the Mo content, the $M_2C$ phase becomes stable instead of the $M_7C_3$ phase. This behavior is also observed in TEM. From the calculation results and the observation results of the microstructure, the thermodynamic calculation can be used to predict the precipitation behavior.
The purpose of this study was to examine the influence of conditions for quenching and/or tempering on the corrosion and hydrogen diffusion behavior of ultra-strong automotive steel in terms of the localized plastic strain related to the dislocation density, and the precipitation of iron carbide. In this study, a range of analytical and experimental methods were deployed, such as field emission-scanning electron microscopy, electron back scatter diffraction, electrochemical permeation technique, slow-strain rate test (SSRT), and electrochemical polarization test. The results showed that the hydrogen diffusion parameters involving the diffusion kinetics and hydrogen solubility, obtained from the permeation experiment, could not be directly indicative of the resistance to hydrogen embrittlement (HE) occurring under the condition with low hydrogen concentration. The SSRT results showed that the partitioning process, leading to decrease in localized plastic strain and dislocation density in the sample, results in a high resistance to HE-induced by aqueous corrosion. Conversely, coarse iron carbide, precipitated during heat treatment, weakened the long-term corrosion resistance. This can also be a controlling factor for the development of ultra-strong steel with superior corrosion and HE resistance.
Since amorphous alloys have been known to have better mechanical and chemical properties than crystalline alloys of the same composition, a great number of studies on the formation of Al-based amorphous alloys have been carried out actively. However, little has been obtained about the effect of Rare-Earth metal and Transition metal addition on amorphous phase formed by melt spinning method. This study included fabrication of amorphous alloy $Al_{85}Ce_5Ni_{10}$ by melt spinning methods and DTA, XRD, TEM analysis to determine crystalization behavoir. Annealing treatments were carried out in Ar atmosphere under isothermal and nonisothermal conditions. The diffraction pattern of non-heated ribbons showed broad form characteristic of glass metallic alloy. The crystallization of amorphous $Al_{85}Ce_5Ni_{10}$ takes place eutedtoidly by homogeneous formation of Al and MS-1, followed by precipitation of the $Al_{11}Ce_3$ and later $MS-1{\rightarrow}Al_3Ni$ transformation.
Proceedings of the Korean Society of Soil and Groundwater Environment Conference
/
2004.04a
/
pp.380-383
/
2004
Heavy metal release from wastewater is a serious environmental problem, and therefore, various wastewater treatment techniques have been developed. Among the techniques, sorption technique is most attractive. Considerable researches have been recently focused on finding out inexpensive sorbents, especially from various natural materials. In order to evaluate the applicability of the scoria taken from the Jeju Island, Korea to remove heavy metals (Pb, Cu, Zn, Cd) from aqueous solutions, equilibrium sorption experiments were conducted in this study. In equilibrium tests, powdered activated carbon (PAC), one of the most commonly used sorbents, was also tested to compare the effectiveness of the Jeju scoria with that of PAC. The Jeju scoria had larger adsorption capacity and affinity for metal ions (Pb(II), Cu(II), Zn(II), Cd(II)) than PAC. The sorption parameters of the two sorbents were evaluated by using both the Langmuir and Freundlich isotherms, and the sorption data were better fitted to the Freundlich isotherm. In addition, the sorption behavior of metal ions (Pb(II), Cu(II), Zn(II), Cd(II)) onto the scoria displayed a typical characteristic of the cation sorption. The removal of metal ions decreased at a lower pH condition due to competition with hydrogen ions for the sorption sites of Jeju scoria, while the removal increased at a high pH condition due to hydroxide precipitation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.