CuO와 ZnO 첨가에 따른 NKN-BZT 세라믹스의 압전 특성 (Piezoelectric Properties of NKN-BZT Ceramics Sintered with CuO and ZnO Additives)

  • 이승환;백상돈;이동현;이성갑;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제24권8호
    • /
    • pp.636-640
    • /
    • 2011
  • The lead-free $0.98(Na_{0.5},K_{0.5})NbO_3-0.02Ba(Zr_{0.52},Ti_{0.48})O_3$-(hereafter NKN-BZT) CuO, ZnO-doped ceramics were prepared using a conventional mixed oxide method. NKN-BZT ceramics doped CuO, ZnO have superior structural and electrical properties than pure NKN-BZT ceramics. For the NKN-BZT-ZnO ceramics sintered at $1,120^{\circ}C$, piezoelectric constant ($d_{33}$) of sample showed the optimum values of 172 pC/N. The $0.98(Na_{0.5},K_{0.5})NbO_3-0.02Ba(Zr_{0.52},Ti_{0.48})O_3$-ZnO ceramics are a promising candidate for lead-free piezoelectric materials.

$Li_2O$ 첨가에 따른 $(Na_{0.47}K_{0.47}Li_{0.06})NbO_3$ 세라믹스의 압전특성과 미세조직의 변화 (Piezoelectric Properties and Microstructures of $Li_2O$ excess $(Na_{0.47}K_{0.47}Li_{0.06})NbO_3$ Ceramics)

  • 김민수;전소현;박정주;전순종;민복기;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.256-256
    • /
    • 2007
  • As a candidate for lead-free piezoelectric materials, dense ($(Na_{0.47}K_{0.47}Li_{0.06})NbO_3$ (LNKN6) ceramics were developed by conventional sintering process. Sintering temperature was lowered by adding $Li_2O$ as a sintering aid. Abnormal grain growth in the LNKN6 ceramics was observed with varying $Li_2O$ content. The electrical properties of LNKN6 ceramics were investigated as a function of $Li_2O$ concentration. When the sample sintered at $1000^{\circ}C$ for 4h with the addition of 1 mol% $Li_2O$, electromechanical coupling factor ($k_p$) and piezoelectric coefficient ($d_{33}$) of LNKN6 ceramics were found to reach the highest values of 0.40 and 184 pC/N, respectively.

  • PDF

$Bi_2O_3$첨가에 따른 무연 NKNLTS계 세라믹스의 압전특성 (Piezoelectric properties of lead-free NKNLTS ceramics with $Bi_2O_3$ addition)

  • 이윤기;이은희;우덕현;안상기;권순용;류성림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.184-184
    • /
    • 2009
  • Lead-free Piezoelectric $[Li_{0.04}(Na_{0.44}K_{0.56})](Nb_{0.88}Ta_{0.1}Sb_{0.02})$ (abbreviated as NKNLTS) has been synthsized by conventional mixed oxide method traditional ceramics process without cold-isostatic pressing. Effect of $Bi_2O_3$ addition on NKNLTS ceramics was investigated. Piezoelectric properties of the ceramic were varied with the amount of $Bi_2O_3$ addition and showed the maximum Kp value at 0.4wt% $Bi_2O_3$ addition. The results show that the optimum poling condition for NKNLTS ceramics of 3.5kV/mm, poling temperature of $120^{\circ}C$ and poling time of 30min. At the sintering temperature of $1100^{\circ}C$ and the calcination temperature $800^{\circ}C$, the optimal values of density=$4.7g/cm^2$, Kp=0.44, $\varepsilon_r$=1309 were obtained. Consequently, lead free piezoelectric ceramics with the excellent piezoelectric could be fabricated using a conventional mixed oxide process and the optimal manuacturing condition of those was obtained.

  • PDF

NKN-(1-x)BNT-xBT 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Properties of NKN-(1-x)BNT-xBT Ceramics)

  • 이승환;남성필;이성갑;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제23권10호
    • /
    • pp.771-775
    • /
    • 2010
  • In this study, piezoelectric and dielectric properties of the $(Na_{0.5}K_{0.5})NbO_3-(1-x)(Bi_{0.5}Na_{0.5})TiO_3-xBaTiO_3$ [NKN-(1-x)BNT-xBT] ceramics were investigated. The lead-free NKN-(1-x)BNT-xBT ceramics were fabricated by a conventional mixed oxide method. The results indicate that the addition of $BaTiO_3$ significantly influences the sintering, microstructure, phase transition and electrical properties of NKN-BNT ceramics. A gradual change in the piezoelectric and dielectric properties was observed with the increase of BT contents. The dielectric constant, piezoelectric constant ($d_{33}$) and electromechanical coupling factor ($k_p$) increased at the morphotropic phase boundary (MPB). The $d_{33}$=184 pC/N, $k_p$=0.38, dielectric constant=1455 with dielectric loss value of less than 1% were obtained for the NKN-0.95BNT-0.05BT ceramics sintered at $1150^{\circ}C$ for 2h. These results demonstrate that the NKN-(1-x)BNT-xBT ceramics is an attractive candidate for lead-free piezoelectric materials.

소결온도에 따른 PMN-PNN-PZT 세라믹스의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of PMN-PNN-PZT with the Sintering Temperature)

  • 이유형;류주현;이상호;윤현상;류성림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.290-291
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, sensers, transducers, PMN-PNN-PZT ceramics were manufacrtured with the sintering temperature, and their piezoelectric and dielectric properties were investigated. At the composition ceramics sintered at $900^{\circ}C$, desity, dielectric constant$({\varepsilon}_r)$, electromechanical coupling factor(kp), piezoelectric constant$(d_{33})$ and mechanical quality factor(Qm) showed the optimal value of $7.86g/cm^3$, 1417, 0.634, 410pC/N and 1138, respectively.

  • PDF

PbO량에 따른 PMN-PNN-PZT 세라믹스의 유전 및 압전특성 (Piezoelectric and Dielectric Characteristics of PMN-PNN-PZT Ceramics According to the amount of PbO)

  • 김도형;김국진;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.219-220
    • /
    • 2006
  • In this study, m order to develop multilayer ceramics vibrator for ultrasonic nozzle, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3-Na_2CO_3$ as sintering aids and their piezoelectric and dielectric characteristics were investigated according to the aomunt of PbO. With increasing PbO contents. secondary phases were increased and phase structure were changed from tetragonal structure to rhombohedral structure and also electromechanical coupling factor were linearly decreased. At the composition ceramics with the sintering temperature of $870^{\circ}C$ and 1 mol% excess PbO, density, electromechanical coupling factor, dielectric constant, piezoelectric d constant and mechanical quality factor showed the optimum value of $7.879g/cm^2$, 0.55, 1149, 328pC/N, 1224, respectively for multilayer ceramics vibrator application for ultrasonic nozzle.

  • PDF

소결 온도에 따른 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3+0.01wt%ZnO 세라믹스의 압전 특성 (Piezoelectric Properties of 0.98(Na0.5K0.5)NbO3-0.02Li(Sb0.17Ta0.83)O3+0.01wt%ZnO Ceramics with a Sintering Temperature)

  • 이동현;이승환;이성갑;이규탁;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제24권7호
    • /
    • pp.543-546
    • /
    • 2011
  • We studied sintering temperature to enhance the piezoelectric properties of $0.98(Na_{0.5}K_{0.5})NbO_3-0.02Li(Sb_{0.17}Ta_{0.83})O_3$+0.01wt%ZnO (hereafter NKN-LST+ZnO) lead free piezoelectric ceramics. The synthesis and sintering method were the conventional solid state reaction method and sintering was executed at $1,080\sim1,120^{\circ}C$. We found that NKN-LST+ZnO ceramics at optimal sintering temperature showed the improved piezoelectric properties at the optimal sintering temperature. The NKN-LST+ZnO ceramics show good performance with piezoelectric constant $d_{33}$= 153 pC/N sintered at $1,090^{\circ}C$. The results reveal that NKN-LST+ZnO ceramics are promising candidate materials for lead-free piezoelectric application.

소결조제 변화에 따른 PCW-PMN-PZT세라믹스의 저온소결 및 압전특성 (Low Temperature Sintering and Piezoelectric Properties of PCW-PMN-PZT Ceramics with the Variation of Sintering Aids)

  • 정광현;이덕출;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제17권12호
    • /
    • pp.1320-1325
    • /
    • 2004
  • In this study, in order to develop the low temperature sintering ceramics for multilayer piezoelectric transformer, PCW-PMN-PZT ceramics added with Li$_2$CO$_3$, Bi$_2$O$_3$ and CuO as sintering aids were manufactured, and their microstructural, dielectric and piezoelectric properties were investigated. When the only CuO was added, specimens could not be sintered below 98$0^{\circ}C$. However, when Li$_2$CO$_3$ and Bi$_2$O$_3$ were added, specimens could be sintered below 98$0^{\circ}C$. Li$_2$CO$_3$ and Bi$_2$O$_3$ addition were proved to lower sintering temperature of piezoelectric ceramics due to the effect of Li$_2$O-Bi$_2$O$_3$ liquid phase. Li$_2$CO$_3$ and Bi$_2$O$_3$ added specimens showed higher piezoelectric properties than those of the only CuO added specimens. At 0.2 wt% Li$_2$CO$_3$ and 0.3 wt% Bi$_2$O$_3$ added specimen sintered at 92$0^{\circ}C$, the dielectric constant of 1457, electromechanical coupling factor of 0.56 and mechanical quality factor of 1000 were shown, respectively. These values are suitable for multilayer piezoelectric transformer application.

압전 세라믹/Polymer 1-3 Composites의 압전 및 음향 특성 (Piezoelectric and acoustic properties of piezoceramic/polymer 1-3 composites)

  • 최헌일;사공건
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1992년도 하계학술대회 논문집 B
    • /
    • pp.727-729
    • /
    • 1992
  • In this study, the piezoelectric composites with 1-3 connectivity have been studied. A piezoelectric ceramics PZT prepared by Flux method is used as a filler in a epoxy Eccogel polymer matrix. The piezoelectric coefficients were increased as PZT volume% increases, and resonance frequency was moved to lower frequency as the sample thickness increased. The acoustic matching impedance with water is lowered than single phase PZT ceramics.

  • PDF

BCTZ첨가가 NKLN-AS계 압전세라믹스의 미세구조와 압전/유전특성 및 상전이현상에 미치는 효과 (BCTZ Addition on the Microstructure, Piezoelectric/Dielectric Properties and Phase Transition of NKLN-AS Piezoelectric Ceramics)

  • 이웅재;어순철;이영근;윤만순
    • 한국재료학회지
    • /
    • 제22권1호
    • /
    • pp.35-41
    • /
    • 2012
  • Presently, the most promising family of lead-free piezoelectric ceramics is based on $K_{0.5}Na_{0.5}NbO_3$(KNN). Lithium, silver and antimony co-doped KNN ceramics show high piezoelectric properties at room temperature, but often suffer from abnormal grain growth. In the present work, the $(Ba_{0.85}Ca_{0.15})(Ti_{0.88}Zr_{0.12})O_3$ component, which has relaxor ferroelectric characteristics, was doped to suppress the abnormal grain growth. To investigate this effect, Lead-Free $0.95(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}NbO_3-(0.05-x)AgSbO_3-x(Ba_{0.85}Ca_{0.15})(Ti_{0.88}Zr_{0.12})O_3$[KNLN-AS-xBCTZ] piezoelectric ceramics were synthesized by ball mill and nanosized-milling processes in lead-Free $0.95(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}NbO_3-(0.05-x)AgSbO_3$ in order to suppress the abnormal grain growth. The nanosized milling process of calcined powders enhanced the sintering density. The phase structure, microstructure, and ferroelectric and piezoelectric properties of the KNLN-AS ceramics were systematically investigated. XRD patterns for the doped and undoped samples showed perovskite phase while tetragonality was increased with increasing BCZT content, which increase was closely related to the decrease of TO-T. Dense and uniform microstructures were observed for all of the doped BCZT ceramics. After the addition of BCTZ, the tetragonal-cubic and orthorhombic-tetragonal phase transitions shifted to lower temperatures compared to those for the pure KNNL-AS. A coexistence of the orthorhombic and tetragonal phases was hence formed in the ceramics with x = 0.02 mol at room temperature, leading to a significant enhancement of the piezoelectric properties. For the composition with x = 0.02 mol, the piezoelectric properties showed optimum values of: $d_{33}$ = 185 pC/N, $k_P$ = 41%, $T_C=325^{\circ}C$, $T_{O-T}=-4^{\circ}C$.