• Title/Summary/Keyword: Lead-free solder

Search Result 199, Processing Time 0.026 seconds

Simulation of Thermal Fatigue Life Prediction of Flip Chip with Lead-free Solder Joints by Variation in Bump Pitch and Underfill (무연 솔더 접합부을 갖는 플립칩에서의 언더필 및 범프 피치 변화에 의한 열 피로 수명 예측 해석)

  • Kim, Seong-Keol;Kim, Joo-Young
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.19 no.2
    • /
    • pp.157-162
    • /
    • 2010
  • This paper describes the thermal fatigue life prediction models for 95.5Sn-4.0Ag-0.5Cu solder joints of Flip chip package considering Under Bump Metallurgy(UBM). A 3D Finite element slice model was used to simulate the viscoplastic behavior of the solder. For two types of solder bump pitches, simulations were analyzed and the effects of underfill packages were studied. Consequently, it was found out that solder joints with underfill had much better fatigue life than solder joints without underfill, and solder joints with $300{\mu}m$ bump pitch had a longer thermal fatigue life than solder joints with $150{\mu}m$ bump pitch. Through the simulations, flip chip with lead-free solder joints should be designed with underfill and a longer bump pitch.

Evaluation of Shear Strength of a Miniature Lead-free Single Solder Ball Joint (초소형 무연 단일 솔더볼 연결부의 전단강도 평가)

  • Joo, Se-Min;Kim, Ho-Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.25 no.6
    • /
    • pp.14-21
    • /
    • 2010
  • A miniature single solder ball joint is designed to mimic the actual solder joints used in the micro-electric industries. Shear tests were conducted to evaluate the mechanical behavior of miniature single solder joints at intermediate strain rates from $0.019\;s^{-1}$ to $2.16\;s^{-1}$ at room temperature. The shear fracture strength of the present solder ball joints generally increased with increasing shear strain rate, ranging from 32 to 51MPa. This behavior is affected by the sensitivity of bulk solder strength to strain rate. Shear fracture mode changed from brittle to partial ductile (failure inside the bulk solder) with an increase of shear speed. The unloading shear fracture toughness is generally consistent with the measure of the amount of bulk solder on the fractured surface.

Lead-free Solder Technology and Reliability for Automotive Electronics (자동차 전장용 무연 솔더 기술)

  • Lee, Soon-Jae;Jung, Jae-Pil
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.22 no.3
    • /
    • pp.1-7
    • /
    • 2015
  • In this study, properties of Pb-free solders for automotive electronics parts were discussed. Lead-free solders for electronics became important after RoHS (Restriction of the use of certain Hazardous Substances) to avoid environmental pollution. Also the growing electronic rate in automotive parts and ELV (End-of Life Vehicles) make Pb-free solder for automotive electronics to be inevitable trend. Definitely, Pb-free solder for automotive electronics should have good wettability, basic strength, but need more reliability than other solders, since it has harsh condition like high temperature, humidity and engine vibration. Thus, shear strength test, thermal shock, drop test and many others are needed to ensure the high reliability. This study describes the properties and requirements of Pb-free solders for automotive electronics.

Reliability Appraisal Standard for Lead-free Solder Bar (무연 솔더바에 대한 신뢰성 평가기준에 관한 연구)

  • Choi, Jai-Kyoung;Park, Jai-Hyun;Park, Hwa-Soon;Ahn, Yong-Sik
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.14 no.2 s.43
    • /
    • pp.23-33
    • /
    • 2007
  • The growing environmental regulation governs the use of lead by RoHS, WEEE, and then. The electronic industry is moving to replace Pb-bearing solder with Pb-free solder. To use the Pb-free solder, microelectronic industry needs consequently the new reliability appraisal such as the packaging for high temperature process, various mechanical change caused by new solder, and the development of Pb-free sloder for long life of product. The evaluation of solder bar and mechanical properties of joint were performed compared with international standard, and new appraisal standard was established. The solderability and spread ability of Sn-0.7Cu solder material showed up to the standard. Shear test of solder joint using by the solder resulted that the shear strengths after thermal shock or after aging were not much lower than the shear strength of as-soldered and that they were also up to the standard.

  • PDF

Reliability of Fine Pitch Solder Joint with Sn-3.5wt%Ag Lead-Free Solder (Sn-3.5wt%Ag 비납솔더를 이용한 미세피치 솔더접합부의 신뢰성에 관한 연구)

  • 하범용;이준환;신영의;정재필;한현주
    • Journal of Welding and Joining
    • /
    • v.18 no.3
    • /
    • pp.89-96
    • /
    • 2000
  • As solder becomes small and fine, the reliability and solderability of solder joint are the critical issue in present electronic packaging industry. Besides the use of lead(Pb) containing solders for the interconnections of microelectronic subsystem assembly and packaging has enviromental problem. In this study, using Sn/Pb and Sn/Ag eutectic solder paste, in order to obtain decrease of solder joint strength with increasing aging time, initial solder joint strength and aging strength after 1000 hour aging at $100^{\circ}C$ were measured by peel test. And in order to obtain the growth of intermetallic compound(IMC) layer thickness, IMC layer thickness was measured by scanning electron microscope(SEM). As a result, solder joint strength was decreased with increasing aging time. The mean IMC layer thickness was increased linearly with the square root of aging time. The diffusion coefficient(D) of IMC layer was found to $1.29{\times}10^{-13}{\;}cm^2/s$ at using Sn/Pb solder paste, 7.56{\times}10^{-14}{\textrm}{cm}^2/s$ at using Sn/Ag solder paste.

  • PDF

Analysis of Output Characteristics of Lead-free Ribbon based PV Module Using Conductive Paste (전도성 페이스트를 이용한 무연 리본계 PV 모듈의 출력 특성 분석)

  • Yoon, Hee-Sang;Song, Hyung-Jun;Go, Seok-Whan;Ju, Young-Chul;Chang, Hyo Sik;Kang, Gi-Hwan
    • Journal of the Korean Solar Energy Society
    • /
    • v.38 no.1
    • /
    • pp.45-55
    • /
    • 2018
  • Environmentally benign lead-free solder coated ribbon (e. g. SnCu, SnZn, SnBi${\cdots}$) has been intensively studied to interconnect cells without lead mixed ribbon (e. g. SnPb) in the crystalline silicon(c-Si) photovoltaic modules. However, high melting point (> $200^{\circ}C$) of non-lead based solder provokes increased thermo-mechanical stress during its soldering process, which causes early degradation of PV module with it. Hence, we proposed low-temperature conductive paste (CP) based tabbing method for lead-free ribbon. Modules, interconnected by the lead-free solder (SnCu) employing CP approach, exhibits similar output without increased resistivity losses at initial condition, in comparison with traditional high temperature soldering method. Moreover, 400 cycles (2,000 hour) of thermal cycle test reveals that the module integrated by CP approach withstands thermo-mechanical stress. Furthermore, this approach guarantees strong mechanical adhesion (peel strength of ~ 2 N) between cell and lead-free ribbons. Therefore, the CP based tabbing process for lead free ribbons enables to interconnect cells in c-Si PV module, without deteriorating its performance.

Thermal Fatigue Life Prediction of ${\mu}BGA$ Solder Joint Using Sn-37mass%Pb Solder and Sn-3.5mass%Ag Lead-free Solder (Sn-37mass%Pb 솔더 및 Sn-3.5mass%Ag 무연솔더를 이용한 ${\mu}BGA$ 솔더접합부의 열피로수명 예측)

  • 신영의;이준환;하범용;정승부;정재필
    • Journal of Welding and Joining
    • /
    • v.19 no.4
    • /
    • pp.406-412
    • /
    • 2001
  • This study is focussed on the numerical prediction of the thermal fatigue life of a ${\mu}BGA$(Micro Ball Grid Array) solder joint. Numerical method is used to perform three-dimensional finite element analysis for Sn-37mass%Pb. Sn-3.5mass%Ag solder alloys during the given thermal cycling. Strain values, along with the result of mechanical fatigue tests for solder alloys were then used to predict the solder joint fatigue life using the Coffin-Manson equation. In this study, a practical correlation for the prediction of the thermal fatigue life is suggested by using the dimensionless variable $\gamma$. As a result. it could be found that Sn-3.5mass%Ag has longer fatigue life than Sn-37mass%Pb in low cycle fatigue. In addition. the result with ${\gamm}ashow$a good agreement with the FEA results.

  • PDF

Effects of Ag on the Characteristics of Sn43Bi57Agx(wt%) Lead-free Solder for Photovoltaic Ribbon (태양광 리본용 Sn43Bi57Agx(wt%) 무연 솔더의 특성에 미치는 Ag의 영향)

  • Jeong, Joo-Hyeon;Cho, Tae-Sik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.2
    • /
    • pp.119-125
    • /
    • 2017
  • We have studied the effects of Ag on the characteristics of $Sn_{43}Bi_{57}Ag_x$(wt%) lead-free solders for photovoltaic ribbon. Ag atoms in the solder formed an alloy phase of Ag3Sn after reacting with some part of Sn atoms, while they did not react with Bi atoms, but decreased the mean size of Bi solid phase and the thickness of solder. When Ag atoms of 3.0 wt% was added to eutectic $Sn_{43}Bi_{57}$(wt%) solder, it showed the optimally useful results that the peel strength of photovoltaic ribbon greatly increased and the sheet resistance of the solder decreased. In the meanwhile, the eutectic $Sn_{43}Bi_{57}$(wt%) solder showed a low melting temperature of $138.9^{\circ}C$, and showed a very similar result regardless of the added amount of Ag atoms.

Evaluation of the Impact Shear Strength of Thermal Aged Lead-Free Solder Ball Joints (열시효 처리된 무연 솔더 볼 연결부의 충격 전단강도 평가)

  • Chung, Chin Sung;Kim, Ho Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.30 no.6
    • /
    • pp.7-11
    • /
    • 2015
  • The present study investigates the impact shear strength of thermal aged Sn-3Ag-0.5Cu lead-free solder joints at impact speeds ranging from 0.5 m/s to 2.5 m/s. The specimens were thermal aged for 24, 100, 250 and 1000 hours at $100^{\circ}C$. The experimental results demonstrate that the shear strength of the solder joint decreases with an increase in the load speed and aging time. The shear strength of the solder joint aged averagely decreased by 43% with an increase in the strain rate. For the as-reflowed specimens, the mode II stress intensity factor ($K_{II}$) of interfacial IMC between Sn-3.0Ag-0.5Cu and a copper substrate also was found to decrease from $1.63MPa.m^{0.5}$ to $0.97MPa.m^{0.5}$ in the speed range tested here. The degradations in the shear strength and fracture toughness of the aged solder joints are mainly caused by the growth of IMC layers at the solder/substrate interface.

Evaluation of the Joint Strength of Lead-free Solder Ball Joints at High Strain Rates (고속 변형률 속도에서의 무연 솔더 볼 연결부의 강도 평가)

  • Joo, Se-Min;Kim, Taek-Young;Lim, Woong;Kim, Ho-Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.27 no.6
    • /
    • pp.7-13
    • /
    • 2012
  • A lack of study on the dynamic tensile strengths of Sn-based solder joints at high strain rates was the motivation for the present study. A modified miniature Charpy impact testing machine instrumented with an impact sensor was built to quantitatively evaluate the dynamic impact strength of a solder joint under tensile impact loading. This study evaluated the tensile strength of lead-free solder ball joints at strain rates from $1.8{\times}10^3s^{-1}$ and $8.5{\times}10^3s^{-1}$. The maximum tensile strength of the solder ball joint decreases as the load speed increases in the testing range. This tensile strength represented that of the interface because of the interfacial fracture site. The tensile strengths of solder joints between Sn-3.0Ag-0.5Cu and copper substrate were between 21.7 MPa and 8.6 MPa in the high strain range.