Defect assessment of a weld zone is important in fitness-for-service evaluation of plant components. Typically a J and $C^*$ estimation method for a defective homogeneous component is extended to a mismatched component, by incorporating the effect due to the strength mismatch between the weld metal and the base material. The key element is a mismatch limit load. For instance, the R6/R5 procedure employs an equivalent material concept, defined by a mismatch limit load. A premise is that if a proper mismatch limit load solution is available, the same concept can be used for any defect location (either a weld centre defect or a heat affected zone (HAZ) defect) and for any material combination (either two-material or multi-material combinations; either similar or dissimilar joints). However, validation is still limited, and thus a more systematic investigation is needed to generalise the suggestion to any geometry, any defect location and any material combination. This paper describes the effect of structural geometry on the $C^*$ integral for defective similar welds, based on systematic elastic-creep 2-D and 3-D finite element (FE) analyses, to attempt to elucidate the questions given above. It is found that the existing 'equivalent material' concept is valid only for limited cases, although it provides conservative estimates of $C^*$ for most of cases. A modification to the existing equivalent material concept is suggested to improve accuracy.
Recently, fatigue problem become a critical issue in the design of prestressed concrete bridges due to the increase of traffic volumes and use of high-strength materials. Most existing studies are mainly concerned with the fatigue behavior of component materials only such as concrete, reinforcing bars, and prestressing steels and few studies exist that deals with the fatigue behavior of bridge members. An improved analytic formulation for both uncracked and cracked prestressed concrete composite section with cyclic creep effect is developed to take into account the change of neutral axis with crack propagation. The procedure also enables to investigate serviceability limit states, deflection and crack width. The present study allows more realistic analysis and design of prestressed concrete composite girder bridges under fatigue loadings.
In this study, we used a stochastic approach for guaranteeing the reliability and robustness of the performance with regard to the design of polymer components, while taking into consideration the degradation properties and operating conditions in automobiles. Creep and tensile tests were performed for obtaining degradation properties. The Prony series, which described the viscoelastic models, were calculated to use the creep data by the Maxwell fluid model. We obtained the stress data from the frequency response analysis of the polymer components while considering the degradation properties. Limit state functions are generated by using these data. Reliability assessments are conducted under the variation of the degradation properties and area of frequency at peak response. For this study, the input parameters are assumed to be a normal distribution, and the reliability under the yield stress criteria is evaluated by using the Monte Carlo Simulation. As a result, the reliabilities, according to the three types of polymer materials in automotive components, are compared to each other and suggested the applicable possibility of polymeric materials in automobiles.
철근콘크리트 구조물은 일반적으로 재료적 특성에 따른 크리프 및 건조수축으로 인하여 장기변형이 발생하며, 이러한 변형으로 인한 구조물의 처짐을 허용 한계 이하로 유지시키는 것이 사용성 확보 측면에서 중요하다 할 수 있다. 노후된 RC보의 성능 개선을 위하여 다양항 보수 보강 방법이 사용되고 있으며 이중 대표적인 방법으로 FRP 외부부착 공법이 있다. 재료적인 성질이 우수한 FRP는 RC구조물의 보강 재료로써 현재 널리 사용되고 있으며, 일시적인 하중 뿐만 아니라 지속 하중 하에서도 향상된 보강 성능을 제공해야 한다. 따라서 FRP가 외부 부착된 RC 부재에 지속 하중이 작용할 때 콘크리트의 크리프 및 건조수축의 영향으로 인한 시간 의존적 장기 거동을 정확히 예측하는 방법이 필요하다. 본 논문에서는 FRP가 외부 부착된 RC보의 장기 처짐 예측을 위해서, CFRP와 GFRP로 보강된 실험체를 제작하고, 25 kN의 지속하중을 470일간 가하여 시간 변화에 따른 처짐을 측정하였다. 또한, 이러한 처짐의 예측을 위하여 ACI-209 code 및 CEB-FIP code에 근거하여 크리프계수와 건조수축변형률을 산정하였으며, EMM과 AEMM을 사용한 ACI-318기준, Branson's method 그리고, Mayer's method를 사용하여 FRP가 외부 부착된 RC보의 장기 처짐을 예측하였다. 실험 결과, CFRP보 보강된 실험체가 가장 높은 장기 사용성을 보였으며, Mayer's method가 장기처짐에 대한 실험값을 가장 근사하게 예측한다는 것을 확인할 수 있었다.
Due to creep and shrinkage of the concrete core, concrete-filled steel tubular (CFST) arches continue to deform in the long-term under sustained loads. This paper presents analytical investigations of the effects of geometric nonlinearity on the long-term in-plane structural performance and stability of three-pinned CFST circular arches under a sustained uniform radial load. Non-linear long-term analysis is conducted and compared with its linear counterpart. It is found that the linear analysis predicts long-term increases of deformations of the CFST arches, but does not predict any long-term changes of the internal actions. However, non-linear analysis predicts not only more significant long-term increases of deformations, but also significant long-term increases of internal actions under the same sustained load. As a result, a three-pinned CFST arch satisfying the serviceability limit state predicted by the linear analysis may violate the serviceability requirement when its geometric nonlinearity is considered. It is also shown that the geometric nonlinearity greatly reduces the long-term in-plane stability of three-pinned CFST arches under the sustained load. A three-pinned CFST arch satisfying the stability limit state predicted by linear analysis in the long-term may lose its stability because of its geometric nonlinearity. Hence, non-linear analysis is needed for correctly predicting the long-term structural behaviour and stability of three-pinned CFST arches under the sustained load. The non-linear long-term behaviour and stability of three-pinned CFST arches are compared with those of two-pinned counterparts. The linear and non-linear analyses for the long-term behaviour and stability are validated by the finite element method.
The Kanweoldo Deposit in the Cheonsoo Bay western coast of Korean Peninsula is considered to be influenced by severe freezing condition under cold humid environment of the last glacial age. The evidence of severe freezing in the some upper part of the fine-grained Kanweoldo Deposit is characteristically irregular wavy la-mellar structure with the interval of 2∼8mm. In particular lamina show very compacted fabrics composed of rounded or spheroidal discrete aggregates covered by silt caps. Such laminar structure and associated micro-fabrics might owe to soil freezing such as ice segregation in lens form cryophoresis pressure from growing ice and disturbance by frost-creep. Furthermore pedogenesis of cold-humid type such as gleyzation or peseudo-gleyzation also might af-fect the kanweoldo Deposit in the priod of severe cold-humid cli-mate of the Wrm. The Kanweoldo sediment and organic remnant(16,708 B.P. with error limit of 250 years) affected by severe cryogenic activities sug-gest that the paleoclimate of Late Wrm in Korea might be so cold and humid as to engender the cryogenic structure in subaerial silty and sandy silt deposits.
Journal of Advanced Marine Engineering and Technology
/
제29권4호
/
pp.399-406
/
2005
Alloy 625 is used widely in industrial applications such as aeronautical aerospace, chemical, petrochemical and marine applications. Because of a good combination of yield strength. tensile strength, creep strength, excellent fabricability, weldability and good resistance to high temperature corrosion on prolonged exposure to aggressive environments. High qualify weldments for this material are readily produced by commonly used processes. But all of processes are not applicable to this material by reason of unavailability of matching, position or suitable welding filler metals and fluxes may limit the choice of welding processes. Recently, the flux cored wire is developed and applied for the better productivity in several welding position including the vortical position. In this study. the weldability and weldment characteristics of Alloy 625 are evaluated in FCAW weld associated with the several shielding gases($80\%Ar+20\%\;CO_2,\;50\%Ar+50\%\;CO_2.\;100\%\;CO_2$) in viewpoint of welding productivity. The results of the experimental study on corrosive characteristics of Alloy 625 are as follows; There is no remarkable difference among shielding gases. however they has a striking difference among corrosive solutions by results of distinguished density and time of corrosive solution. Generally, the shielding gases($80\%Ar+20\%\;CO_2$) was superior to the other gases on high temperature tensile and a low temperature impact. but all of the shield gases were making satisfactory results on corrosion test.
지오그리드의 장기허용강도를 산출할 때 사용되는 총 감소계수는 내시공성 감소계수($RF_{ID}$), 내화학성 감소계수($RF_D$), 크리프 감소계수($RF_{CR}$) 등이 적용된다. 지오그리드의 단기인장강도에 대한 감소계수를 고려한 허용인장강도 산출 모델의 경우 감소계수들 사이의 상호 작용력을 고려하지 않는 한계를 가지고 있다. 접점강도는 인장강도와 마찬가지로 시공 시 손상이나 화학적 분해에 의하여 감소하게 된다. 기존의 단일접점강도 시험 방법은 치수효과를 고려할 수 없기에 결과의 편차가 큰 시공 시 손상된 시험편의 접점강도를 측정하는데 적합하지 않다. 또한 시공 시 손상에 의한 전단강도 변화에 대한 연구도 전혀 이루어지지 않은 실정이다. 따라서 본 연구에서는 다양한 조건을 고려하여 지오그리드의 장기성능에 영향을 미치는 감소계수들을 재평가하고 감소계수 사이의 상호 작용을 고려하여 정확한 장기허용강도를 구하려고 한다. 내시공성 시험과 내화학성 시험 후 크리프 시험결과 총 감소계수는 GRI GG-4 시험값보다 작게 나타났다. 내시공성 시험과 내화학성 시험 후 접점강도의 감소계수는 인장강도 감소계수보다 더 작게 나타났다. 내시공성 시험후 전단강도 차이가 나타나지 않거나 증가함을 나타내었다.
Clamping force of a high strength bolt is reduced by a certain period of time after the initial set-up. In case of special treatments on faying surfaces such as protective coating, clamping force is relaxed more severely. Tests for slip critical joints subject to various faying surface parameters were conducted. Five different surface treatments were tested including mill scale surface, blast surface, rust surface and coated surfaces. Each specimen was composed of F10T M20 of high strength bolts and steel plates. Based on the result of slip coefficient test, blast treatment surface showed 0.59, rust treatment surface showed 0.54 and inorganic zinc treatment surface exhibited 0.44. Clean mill treatment surface and red lead paint treatment surface were 0.23, 0.21 respectively. It is identified that the slip coefficient in Korean structural design guide should be determined for various surface conditions. Subsequently from long term relaxation test of ASTM A 490 high strength bolts, relaxation of no-coated surfaces such as blast, clean mill, rust treatment, the loss of initial clamping load was 10.5%, 13.6% and 7.9% for 1,000 hours, while the loss of initial clamping force was reached as 15.0%, 18.7% more than the required redundancy 10% in case of inorganic zinc and red lead painted treatment. It is required that the limit of relaxation on coated faying surface should be established separately for various surfaces.
본 연구에서는 암석과 콘크리트의 정적 및 동적 장기강도시험을 통해 이들 재료의 시간 의존적 거동에 대해 연구했으며, 특히 장기강도시험 중 발생한 미소파괴음 신호를 분석하여 장기 안정성 평가에 활용하고자 하였다. 정적 장기강도시험의 경우 임계하 균열성장시험을 활용하여 Mode I과 Mode II에 대한 장기거동과 미소파괴음 발생특성을 분석하였으며, 동적 장기강도시험의 경우, 반복재하 4점 굴곡시험을 통한 장기강도의 한계와 미소파괴음 발생특성을 분석하였다. 미소파괴음 분석결과, 미소파괴음 히트 누적곡선 대 시간에 따른 곡선은 1차, 2차, 3차 구간이 있는 크립곡선의 모양과 유사한 모양을 보였다. 선형구간에 해당하는 미소파괴음 히트 누적곡선의 2차 구간의 기울기와 지연파괴시간과의 로그-로그 관계로부터 암석과 콘크리트의 정적 및 동적 장기 안정성을 평가하는 방안에 대한 가능성을 제시하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.