• Title/Summary/Keyword: Ag-free solder

Search Result 190, Processing Time 0.024 seconds

Activation Energy and Interface Reaction of Sn-40Pb/Cu & Sn-3.0Ag-0.5Cu/Cu (Sn-40Pb/Cu 및 Sn-3.0Ag-0.5Cu/Cu 접합부 계면반응 및 활성화에너지)

  • Kim, Whee-Sung;Hong, Won-Sik;Park, Sung-Hun;Kim, Kwang-Bae
    • Korean Journal of Materials Research
    • /
    • v.17 no.8
    • /
    • pp.402-407
    • /
    • 2007
  • In electronics manufacturing processes, soldering process has generally been used in surface mounting technology. Because of environmental restriction, lead free solders as like a SnAgCu ternary system are being used widely. After soldering process, the formation and growth of intermetalic compounds(IMCs) are formed in the interface between solder and Cu substrate as follows isothermal temperature and time. In this studies, therefore, we investigated the effects of the Cu substrate thickness on the IMC formation and growth of Sn-40Pb/Cu and Sn-3.0Ag-0.5Cu/Cu solder joints, respectively. The effect of the Cu thickness in PCB Cu pad and pure Cu plate was analyzed as measuring of thickness of each IMC. After solder was soldered on PCB and Cu plate which have different Cu thickness, we measured the IMC thickness in solder joints respectively. Also we compared with the effectiveness of Cu thickness on the IMC growth. From these results, we calculated the activation energy.

Development of the Copper Core Balls Electroplated with the Solder of Sn-Ag-Cu

  • Imae, Shinya;Sugitani, Yuji;Nishida, Motonori;kajita, Osamu;Takeuchi, Takao
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1207-1208
    • /
    • 2006
  • We developed the copper core ball electroplated with Sn-Ag-Cu of the eutectic composition which used mostly as Pb free solder ball with high reliability. In order to search for the practicality of this developed copper core ball, the evaluation was executed by measuring the initial joint strength of the sample mounted on the substrate and reflowed and by measuring the joint strength of the sample after the high temperature leaving test and the constant temperature and the humidity leaving test. This evaluation was compered with those of the usual other copper core balls electroplated with (Sn,Sn-Ag,Sn-Cu,Sn-Bi) and the Sn-Ag-Cu solder ball.

  • PDF

Evaluation of the Impact Shear Strength of Thermal Aged Lead-Free Solder Ball Joints (열시효 처리된 무연 솔더 볼 연결부의 충격 전단강도 평가)

  • Chung, Chin Sung;Kim, Ho Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.30 no.6
    • /
    • pp.7-11
    • /
    • 2015
  • The present study investigates the impact shear strength of thermal aged Sn-3Ag-0.5Cu lead-free solder joints at impact speeds ranging from 0.5 m/s to 2.5 m/s. The specimens were thermal aged for 24, 100, 250 and 1000 hours at $100^{\circ}C$. The experimental results demonstrate that the shear strength of the solder joint decreases with an increase in the load speed and aging time. The shear strength of the solder joint aged averagely decreased by 43% with an increase in the strain rate. For the as-reflowed specimens, the mode II stress intensity factor ($K_{II}$) of interfacial IMC between Sn-3.0Ag-0.5Cu and a copper substrate also was found to decrease from $1.63MPa.m^{0.5}$ to $0.97MPa.m^{0.5}$ in the speed range tested here. The degradations in the shear strength and fracture toughness of the aged solder joints are mainly caused by the growth of IMC layers at the solder/substrate interface.

Electromigration and Thermomigration Characteristics in Flip Chip Sn-3.5Ag Solder Bump (플립칩 Sn-3.5Ag 솔더범프의 Electromigration과 Thermomigration 특성)

  • Lee, Jang-Hee;Lim, Gi-Tae;Yang, Seung-Taek;Suh, Min-Suk;Chung, Qwan-Ho;Byun, Kwang-Yoo;Park, Young-Bae
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.5
    • /
    • pp.310-314
    • /
    • 2008
  • Electromigration test of flip chip solder bump is performed at $140^{\circ}C$ C and $4.6{\times}10^4A/cm^2$ conditions in order to compare electromigration with thermomigration behaviors by using electroplated Sn-3.5Ag solder bump with Cu under-bump-metallurgy. As a result of measuring resistance with stressing time, failure mechanism of solder bump was evaluated to have four steps by the fail time. Discrete steps of resistance change during electromigration test are directly compared with microstructural evolution of cross-sectioned solder bump at each step. Thermal gradient in solder bump is very high and the contribution of thermomigration to atomic flux is comparable with pure electromigration effect.

Assessment of Viscoplastic Deformation Behavior of Eutectic Solder and Lead-free Solder (유연 솔더와 무연 솔더의 점소성 변형거동 평가)

  • Lee, Bong-Hee;Joo, Jin-Won
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.18 no.2
    • /
    • pp.17-27
    • /
    • 2011
  • This paper describes an experimental study and finite element analysis (FEA) carried out for investigating thermal deformation behavior of solders, resulting from temperature change in the solder. With such a goal in mind, a shear specimen that was composed of two metal bars having different coefficient of thermal expansion and solder blocks placed between two bars was designed and fabricated. Two different types of solder blocks, eutectic solder (Sn/36Pb/ 2Ag) and lead-free solder (Sn/3.0Ag/0.5Cu) were tested as well. Fringe patterns for several temperature steps were recorded and analyzed for three temperature cycles using a real-time moir$\acute{e}$ setup. The experimental data was verified with FEA and used to evaluate the suitability for numerous solder constitutive models available in literatures. FEA employing Anand material model suggested by Darveaux et al. and Chang et al. were found to be in an excellent agreement with the experimental results for the eutectic solder and the lead-free solder, respectively. In addition, numerical predictions on bending displacement, shear strain and viscoplastic distortion energy are documented and viscoplastic deformation behavior of two types of solder material are compared.

Characteristic of Intermetallic Compounds for Aging of Lead Free Solders Applied to 48 $\mu$BGA (48 $\mu$BGA에 적용한 무연솔더의 시효처리에 대한 금속간화합물의 특성)

  • Shin, Young-Eui;Lee, Suk;Fujimoto, Kozo;Kim, Jong-Min
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.8 no.3
    • /
    • pp.37-42
    • /
    • 2001
  • The concerns of the toxicity and health hazard of lead in solders have demanded the research to find suitable lead-free solder alloys. It was discussed that effect of the intermetallic formation and structure on the reliability of solder joints. In this study, lead-free solder alloys with compositions of Sn/3.5Ag/0.75Cu, Sn/2.0Ag/0.5Cu/2.0Bi were applied to the 48 $\mu$BGA packages. Also, the lead-free solder alloys compared with eutectic Sn/37Pb solder using shear test under various aging temperature. Common $\mu$BGA with solder components was aged at $130^{\circ}C$, $150^{\circ}C$ and $170^{\circ}C$. And the each temperature applied to 300, 600 and 900 hours. The thickness of the intermetallics was measured for each condition and the activation energy for their growth was computed. The fracture surfaces were analyzed using SEM (Scanning Electron Microscope) with EDS (Energy Dispersive Spectroscopy). These results for reliability of lead-free interconnections are discussed.

  • PDF

Study on Thermal Stability of the Interface between Electroless Ni-W-P Deposits and BGA Lead-Free Solder (Sn-3.0Ag-0.5Cu) (BGA 무연솔더(Sn-3.0Ag-0.5Cu)와 무전해 Ni-W-P 도금층 계면의 열 안정성에 대한 연구)

  • Shin, Dong-Hee;Cho, Jin-Ki;Kang, Seung-Goon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.17 no.1
    • /
    • pp.25-31
    • /
    • 2010
  • In this study, we investigated the morphology and thermal stability of interfacial phases in joint between lead free solder(Sn-3.0Ag-0.5Cu) and electroless Ni-W-P under bump metallizations(UBM) with different tungsten contents as a function of thermal aging. Content of phosphorus of each deposits was fixed at 8 wt.%, and content of tungsten was variated each 0, 3, 6 and 9 wt.%. Specimens were prepared by reflowing at $255^{\circ}C$, aging range was $200^{\circ}C$ and up to 2 weeks. After reflow process, in the electroless Ni(W)-P/solder joint, the interfacial intermetallic compound(IMC) was showed both $(Cu,Ni)_6Sn_5$ and $(Ni,Cu)_3Sn_4$. UBM and generated IMC at the interface of lead free solder was proportionally increased with aging time. The thickness of IMC was increased because the generation rate of $Ni(W)_3P$ decreased with increasing contents of W.