강 기판위에 아크이온 플레이팅된 CrN박막의 산화 (The Oxidation of CrN Films Arc-ion Plated on a Steel Substrate)

  • 이동복;이영찬
    • 한국재료학회지
    • /
    • 제11권4호
    • /
    • pp.324-328
    • /
    • 2001
  • 아크이온 플레이팅 장치를 이용하여 STD61강 기판 위에 이온질화 전처리를 행하거나 하지 않은 후, CrN 박막을 증착하고, 대기중 $700~900^{\circ}C$의 온도에서 40시간동안 이들에 대한 산화거동을 연구하였다. 산화거동은 열중량분석기, X선회절기, EDS, SEM을 이용하여 조사하였다. 증착된 CrN박막은 CrN과 $Cr_2$N의 두 상으로 구성되어 있었다. CrN박막은 보호적 $Cr_2$O$_3$층을 형성하여 기판을 산화로부터 보호하였다. 이온질화처리는 CrN박막의 내산화성에 영향을 주지 않았다.

  • PDF

난분해성 산업폐수 처리를 위한 고도산화기술 (Advanced oxidation technologies for the treatment of nonbiodegradable industrial wastewater)

  • 김민식;이기명;이창하
    • 상하수도학회지
    • /
    • 제34권6호
    • /
    • pp.445-462
    • /
    • 2020
  • Industrial wastewater often contains a number of recalcitrant organic contaminants. These contaminants are hardly degradable by biological wastewater treatment processes, which requires a more powerful treatment method based on chemical oxidation. Advanced oxidation technology (AOT) has been extensively studied for the treatment of nonbiodegradable organics in water and wastewater. Among different AOTs developed up to date, ozonation and the Fenton process are the representative technologies that widely used in the field. Based on the traditional ozonation and the Fenton process, several modified processes have been also developed to accelerate the production of reactive radicals. This article reviews the chemistry of ozonation and the Fenton process as well as the cases of application of these two AOTs to industrial wastewater treatment. In addition, research needs to improve the cost efficiency of ozonation and the Fenton process were discussed.

High-temperature Oxidation of Nano-multilayered AlTiSiN Thin Films deposited on WC-based carbides

  • Hwang, Yeon Sang;Lee, Dong Bok
    • Corrosion Science and Technology
    • /
    • 제12권3호
    • /
    • pp.119-124
    • /
    • 2013
  • Nano-multilayered, crystalline AlTiSiN thin films were deposited on WC-TiC-Co substrates by the cathodic arc plasma deposition. The deposited film consisted of wurtzite-type AlN, NaCl-type TiN, and tetragonal $Ti_2N$ phases. Their oxidation characteristics were studied at 800 and $900^{\circ}C$ for up to 20 h in air. The WC-TiC-Co oxidized fast with large weight gains. By contrast, the AlTiSiN film displayed superior oxidation resistance, due mainly to formation of the ${\alpha}-Al_2O_3$-rich surface oxide layer, below which an ($Al_2O_3$, $TiO_2$, $SiO_2$)-intermixed scale existed. Their oxidation progressed primarily by the outward diffusion of nitrogen, combined with the inward transport of oxygen that gradually reacted with Al, Ti, and Si in the film.

방전플라즈마 소결법에 의해 제조된 Fe-Ni 합금의 미세조직 및 고온산화특성 (Microstructure and High Temperature Oxidation Behaviors of Fe-Ni Alloys by Spark Plasma Sintering)

  • 임채홍;박종석;양상선;윤중열;이진규
    • 한국분말재료학회지
    • /
    • 제24권1호
    • /
    • pp.53-57
    • /
    • 2017
  • In this study, we report the microstructure and the high-temperature oxidation behavior of Fe-Ni alloys by spark plasma sintering. Structural characterization is performed by scanning electron microscopy and X-ray diffraction. The oxidation behavior of Fe-Ni alloys is studied by means of a high-temperature oxidation test at $1000^{\circ}C$ in air. The effect of Ni content of Fe-Ni alloys on the microstructure and on the oxidation characteristics is investigated in detail. In the case of Fe-2Ni and Fe-5Ni alloys, the microstructure is a ferrite (${\alpha}$) phase with body centered cubic (BCC) structure, and the microstructure of Fe-10Ni and Fe-20Ni alloys is considered to be a massive martensite (${\alpha}^{\prime}$) phase with the same BCC structure as that of the ferrite phase. As the Ni content increases, the micro-Vickers hardness of the alloys also increases. It can also be seen that the oxidation resistance is improved by decreasing the thickness of the oxide film.

H2O2 촉매 전환에 의해 생성된 건식산화제를 이용한 NO 산화에 관한 연구 (A study on the NO oxidation using dry oxidant produced by the catalytic conversion of H2O2)

  • 장정희;한기보
    • 한국응용과학기술학회지
    • /
    • 제33권1호
    • /
    • pp.100-109
    • /
    • 2016
  • 본 연구에서는 촉매 상 $H_2O_2$ 전환에 의해 건식산화제가 생성되었으며, 이를 이용한 NO 산화 공정에 대한 연구를 진행하였다. 건식산화제를 생성하기 위한 $H_2O_2$ 촉매 전환에 관한 실험을 수행한 결과, Mn계 촉매의 성능이 가장 우수하였으며, 이를 통해 생성된 건식산화제를 NO 산화공정에 주입하여 다양한 운전조건에서 NO 산화특성을 조사하였다. 그 결과, $H_2O_2$ 주입량, 산화반응온도, 그리고 공간속도가 NO 산화율에 크게 영향을 미치는 것을 확인하였다. 그리고, 산화반응온도와 $H_2O_2$ 주입량이 증가할수록 NO 산화효율이 증가하였으며, 공간속도가 증가할수록 NO 산화효율이 감소하였다.

Characteristics of Oxide Layers Formed on Al2021 Alloys by Plasma Electrolytic Oxidation in Aluminate Fluorosilicate Electrolyte

  • Wang, Kai;Koo, Bon-Heun;Lee, Chan-Gyu;Kim, Young-Joo;Lee, Sung-Hun;Byon, Eung-Sun
    • 한국표면공학회지
    • /
    • 제41권6호
    • /
    • pp.308-311
    • /
    • 2008
  • Oxide layers were prepared on Al2021 alloys substrate under a hybrid voltage of AC 200 V (60 Hz) combined with DC 260 V value at room temperature within $5{\sim}60\;min$ by plasma electrolytic oxidation (PEO). An optimized aluminate-fluorosilicate solution was used as the electrolytes. The surface morphology, thickness and composition of layers on Al2021 alloys at different reaction times were studied. The results showed that it is possible to generate oxide layers of good properties on Al2021 alloys in aluminate-fluorosilicate electrolytes. Analysis show that the double-layer structure oxide layers consist of different states such as ${\alpha}-{Al_2}{O_3}$ and ${\gamma}-{Al_2}{O_3}$. For short treatment times, the formation process of oxide layers follows a linear kinetics, while for longer times the formation process slows down and becomes a steady stage. During the PEO processes, the average size of the discharge channels increased gradually as the PEO treatment time increased.

팔라듐-은 막반응기를 이용한 메탄의 부분산화반응 (Partial Oxidation of Methane in Palladium-silver Alloy Membrane Reactor)

  • 최태호;김광제;문상진;서정철;백영순
    • 공업화학
    • /
    • 제16권5호
    • /
    • pp.641-647
    • /
    • 2005
  • 메탄의 부분산화반응은 수소 제조의 중요한 반응 중의 하나이다. 무전해 도금방법에 의해 제조된 팔라듐-은 막을 막반응기(membrane reactor)로서 메탄의 부분산화반응에 적용하여 반응온도, $O_2/CH_4$ 몰비, $CH_4$ 공급속도, $N_2$ 운반 가스 흐름속도 등의 변화에 따라 실험을 수행하였다. 막반응기의 메탄 전환율은 알루미나에 담지된 니켈 촉매를 사용하는 반응조건하에서 $350{\sim}730^{\circ}C$의 반응온도에 따라 증가하는 경향을 보였으며, 특히 $730^{\circ}C$$O_2/CH_4$ 몰비 0.5에서 메탄 전환율과 CO 선택도가 가장 높았다. 막반응기의 메탄 전환율은 전통적인 관형반응기와 비교한 결과 반응조건에 따라 10~40% 정도 높았다.

The Influence of Surface Modification of Gold Nanoparticles Supported on TiO2 in the Catalytic Activity of CO Oxidation

  • Park, Da-Hee;Reddy, A.S.;Eah, Sang-Kee;Park, Jeong-Young
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제41회 하계 정기 학술대회 초록집
    • /
    • pp.213-213
    • /
    • 2011
  • Gold catalysts supported on TiO2 have shown a unique catalytic behavior on CO oxidation, depending on surface effects. Particle size has an influence on the surface activity. To make monodisperse Au nanoparticles, organic capping ligands, such as alkylthiols, were used by a "greener" synthesis method [1,2] and Au nanoparticles were deposited on TiO2. However, organic capping ligands must be removed for high catalytic activities by the Au nanoparticles without changing the Au size [3]. We used UV ozone treatment to decompose thiol ligands. The samples have been characterized by X-ray photoelectron spectroscopy to examine the surface modification by UV ozone treatment. We show the size distribution of the gold nanoparticles by light scattering analysis and transmission electron microscopy. Au/TiO2 have been prepared using the wetness impregnation method. The catalytic performance of CO oxidation over Au supported on TiO2 under oxidizing reaction conditions (40 Torr CO and 100 Torr O2) were tested. The results show that the catalytic activity depends on particle size and the time of UV ozone exposure, which suggests the role of sulfur bonding in determining the catalytic activity of Au/TiO2 catalysts.

  • PDF

$Ag/{\alpha}-Al_2O_3Ag/SnO_2$ 촉매상에서의 에틸렌 산화반응 (Oxidation of Ethylene over $Ag/{\alpha}-Al_2O_3Ag/SnO_2$)

  • 전기원;한종수;전학제
    • 대한화학회지
    • /
    • 제28권2호
    • /
    • pp.109-113
    • /
    • 1984
  • 여러가지 함량으로 은을 입힌$ Ag/{\alpha}-Al_2O_3$$Ag/SnO_2$상에서의 반응실험과 촉매의 Auger spectra, $SnO_2$에 흡착된 산소의 EPR spectra를 비교하여 담체의 종류가 에틸렌 산화반응의 활성과 선택성에 미치는 영향을 조사하였다. $SnO_2$상에서는 흡착산소중 O-가 반응에 참여하여 ethylene를 완전 산화하는 방향으로 유도하므로써 ethylene oxide 생성의 선택성을 저하시키는 것 같다.

  • PDF

Growth of Al2O3/Al Composite by Directed Metal Oxidation of Al Surface Doped with Sodium Source

  • Park, Hong Sik;Kim, Dong Seok;Kim, Do Kyung
    • 한국세라믹학회지
    • /
    • 제50권6호
    • /
    • pp.439-445
    • /
    • 2013
  • Both an unreinforced $Al_2O_3$/Al matrix and a ${\alpha}-Al_2O_3$ particulate reinforced composite have been produced by the oxidation of an Al surface doped with NaOH in the absence of any other dopant. Fabrication of the matrix was initiated by the formation of $NaAlO_2$, which provides a favorable surface structure for the matrix formation by breaking the protective $Al_2O_3$ layer on Al. During the matrix growth, the external surface of the growth front was covered with a very thin sodium-rich oxide. A cyclic formation process of the sodium-rich oxide on the growth surface was proposed for the sodium-induced directed metal oxidation process. This process involves dissolution of the sodium-rich oxide, motion of Na to the growth front, and re-formation of the oxide on the surface. Near-net-shape composites were fabricated by infiltrating an $Al_2O_3$/Al matrix into a ${\alpha}-Al_2O_3$ particulate preform, without growth barrier materials. The infiltration distance increased almost linearly in the NaOH-doped preform.