The objective of this study is to investigate the properties of fresh concrete with recycled coarse and fine aggregates. Four different kinds of aggregate with natural, recycled aggregates were prepared. The concrete mixtures were produced with test parameters of replacement ratio of recycled aggregate. The properties of the fresh concrete were measured by means of slump and air content according to elapsed time. Quality control method to maintain the constant total mixing water for recycled aggregate concrete was suggested. The all concrete mixtures were produced with approximately the same slump on the job site after an hour. Test results indicated that compressive strength of concrete with constant slump is not affected by the replacement ratio of recycled aggregate. Also the practical way for the quality control of recycled aggregate concrete is to maintain the constant total mixing water.
Journal of the Korean Recycled Construction Resources Institute
/
v.10
no.4
/
pp.367-375
/
2022
In this study, the characteristics of recycled aggregate concrete according to the mixing ratio of recycled fine aggregate were analyzed by design strength to explore its use in the production of ready-mixed concrete. The results show that, depending on the ratio of recycled aggregate, the compressive strength is similar to that of normal concrete and does not deteriorate. Therefore, it is possible to achieve a strength similar to the target design strength. Furthermore, if the ratio of recycled fine aggregate for concrete is up to 25 % of the total aggregate amount (50 % of the to-tal fine aggregate), slump does not cause problems. Our findings show that the higher the de-sign standard strength, the greater the amount of powder, and management of slump reduction, unit quantity, and performance system is necessary. The obtained results show that recycled ag-gregate can be used for the production of ready-mixed concrete after adjusting its mixing ratio and concrete mix proportions.
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.1
/
pp.125-130
/
2010
It is necessary to re-establish the code and to control the quality of the recycled aggregate itself for ensuring the useability of the recycled aggregate using waste concrete. Generally, adhering mortar cause of the water absorption ratio increment and strength decreased at the surface of the aggregate of the recycled aggregate using waste concrete, thus removing the adhering mortar could increase the useability of the recycled aggregate in the concrete industry. In this study, as a quality control method of the recycled aggregate using waste concrete, the quality characteristic of the recycled aggregate according to the mixing proportion between the recycled and the natural aggregate is obtained Therefore, a system is established to reuse the recycled aggregate in the construction industry.
Journal of the Korean Recycled Construction Resources Institute
/
v.6
no.1
/
pp.8-15
/
2018
Waste concrete accounts for the largest portion of construction waste, and the supply of natural aggregate is unstable. Therefore, importance of using recycled aggregate is emphasized. The purpose of this study is to investigate the mechanical properties of high strength concrete according to the replacement rate of recycled coarse aggregate. For this purpose, the target design compressive strength was set to 40MPa, and the substitution rates of the recycled coarse aggregate were set to 0%, 30%, 60%, and 100%, respectively. Through experiments on the unreinforced concrete and hardened concrete, The validity of the use was confirmed. In addition, LCA method was used to evaluate the environmental impact of recycled aggregates and to compare and analyze the environmental impacts of the aggregates.
Journal of the Korean Recycled Construction Resources Institute
/
v.10
no.1
/
pp.1-8
/
2022
In this study, the mechanical properties of concrete with recycled coarse aggregate (RG) selected by multi-stage wind pressure (MSWP) treatment were evaluated. After evaluating the basic properties of natural and recycled coarse aggregates, the mechanical performance of the recycled coarse aggregates concrete was experimentally investigated. As a result, it was found that the MSWP technique could improve the fundamental properties such as density and water absorption of RG. In addition, the concrete with RG selected by MSWP showed a better mechanical performance, indicating a higher strength values, surface electric resistivity and a lower absorption. Thus, it seems that the MSWP technique can be effective for the production of high-quality RG.
Journal of the Korea Academia-Industrial cooperation Society
/
v.18
no.11
/
pp.7-15
/
2017
The purpose of this study was to evaluate the properties of recycled aggregate concrete (RAC) using low quality recycled aggregate with or without washing before usage. The recycled aggregate concrete evaluated in this study contained various amounts of low quality recycled aggregate, viz. 30%, 60% and 100%. To evaluate the performance of the recycled aggregate concrete, various test methods were employed to assess its compressive strength, absorption, surface resistance, ultrasound velocity, chloride ion resistance, etc. The properties of the RAC with 30% and 60% washed recycled aggregate were similar those of the natural aggregate. However, the properties of the RAC with 100% washed recycled aggregate were slightly lower than those of the other versions. Also, the RAC with the non-washed recycled aggregate exhibited lower performance results. The results showed that the RAC with washed recycled aggregate had similar properties to normal concrete (concrete using natural aggregate). This implies that the recycled aggregate should be washed to improve the RCA.
Kim, Jung-Ho;Sung, Jong-Hyun;Kim, Choong-Gyum;Lee, Sea-Hyun;Kim, Han-Soo
Journal of the Korean Recycled Construction Resources Institute
/
v.6
no.4
/
pp.229-235
/
2018
In this study, recycled aggregate and natural aggregate were mixed in advance using an aggregate mixing facility that was developed to improve the quality of recycled aggregate concrete. Then the mixed aggregate was applied and concrete characteristics before and after a mix were considered. Based on the findings extracted, this study aimed to suggest a new direction for quality stabilization and application activation of recycled aggregate. The test results of change rates of mortars and coarse aggregates in fresh concrete mixed by a concrete mixer, before and after mixing aggregates showed that the variations of the mortars and coarse aggregates in the concrete mixed with the aggregates beforehand were decreased than those in the concrete before mixing them. The variation of compressive strength and the mean compressive strength at the ages of 3 and 7 days showed similar results before and after the aggregates were mixed, and the strength at the age of 28 days before and after mixing them showed larger deviation than that at the ages of 3 and 7 days. The use of the mixed aggregates after mixing aggregates beforehand reduced the variation in strength and is believed that it is advantageous for long-age strength development. The above results show that the variations of coarse aggregates and compressive strength in the concrete using the mixed aggregates produced by mixing recycled aggregates and natural aggregates beforehand are reduced so it will be possible to produce the homogeneous concrete by mixing aggregates beforehand.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.1
/
pp.26-32
/
2020
Concrete recycling is becoming mandatory rather selective due to depletion of constructional materials and increase of concrete waste. Studies on recycling concrete are conducted in various point of view for long time. However, standard or guideline of many countries for the application of recycled aggregate concrete(RAC) has restrictions such as low replacement rate of coarse aggregate and no fine aggregate allowed due to inferior material properties of recycled aggregate. This study intends to figure out the feasibility of casting natural aggregate concrete(NAC) and RAC separately in a structural member. In making RAC, replacement rate of coarse aggregate was 50, 100% in RAC and treatment of interface of two concretes is introduced. RAC treatment of recycled aggregate or inclusion of additives was not done as it can increase embodied energy of concrete work. Double-shear test with uniformly distributed loading was adopted to evaluate shear strength at the interface of two concretes. After curing it was hard to distinguish interface of two concretes. Experimental result revealed that specimen with higher replacement rate showed higher shear-to-compressive strength ratio, which is possibly attributed to coarse aggregate size and roughness of sheared section. Further study on the effect of various parameters is required and subsequent research activity is on-going.
Ha, Jung-Soo;Shin, Jin-Hak;Chung, Lan;Kim, Han-Sic
Journal of the Korea Concrete Institute
/
v.28
no.4
/
pp.445-454
/
2016
With the increase of decrepit facilities, construction waste increased to a certain level and now the increase is more or less stabilized. Yet construction waste still constitutes the largest portion of the overall wastes. Also, it is inevitable to spend a huge amount of the national budget due to the aggravating shortage of aggregate caused by prohibition on collection of natural aggregates as well as due to the damage to the land and environment caused by development of the sources of aggregates. As a countermeasure to the situation, the Ministry of Land, Infrastructure and Transport promulgated the quality standard for recycled aggregate to manage the usage of recycled aggregate according to its quality. But use of recycled aggregate for the purpose of high added value still remains nominal. Therefore, this research aims to study the applicability of recycled aggregate concrete as structural concrete by evaluating the quality improvement effects and the performance of the recycled aggregate concrete including recycled fine aggregate and recycled coarse aggregate that have undergone carbonation for 4 days and 14 days respectively in the condition of 60% RH, 20% $CO_2$ and $20^{\circ}C$ temperature, suggested for carbonation modifying from the advance research. The result shows carbonation modify contributed to quality improvement with 0.91% decrease in absorption rate for recycled fine aggregate and 0.7% decrease in absorption rate for recycled coarse aggregate. The physical properties and durability of the recycled aggregate made of aggregate modified by carbonation showed results similar to general concrete, which confirmed the possibility of applying the recycled aggregate made of recycled aggregate modified by carbonation to structural concrete.
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.1
/
pp.117-124
/
2010
The aggregate, which does not satisfy the standard of KS F 2573, was selected for this investigation. The 28day compressive strength of recycled aggregate concrete without pozzolan material was 21.7MPa, which was less than the strength of concrete made with crushed stone. However, the compressive strength at 28 days was improved by mixing early rapid hardening cement to the cement at the weight ratio of 2.5%. Furthermore, the compressive strength at 91 days and 180 days increased significantly by adding fly ash, slag powder, and diatom powder. The tensile strength of recycled aggregate concrete with pozzolan material also increased about 40% compared to the general concrete. Futhermore, the shrinkage and creep of recycled aggregate concrete with fly ash and slag powder was a little decreased that of recycled aggregate concrete with fly ash and diatom powder. Relationship between compressive strength and creep coefficient was shown to the linear relation like as ${\sigma}_c=-30CF+404$.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.