• Title/Summary/Keyword: 상아질 결합제

Search Result 43, Processing Time 0.024 seconds

THE STUDY ON SHEAR BOND STRENGTH OF VARIOUS DENTIN BONDING SYSTEMS IN PRIMARY DENTIN (유치 상아질에 대한 수종의 상아질 결합제의 전단결합강도에 대한 연구)

  • Kang, Sun-Hee;Lee, Kwang-Hee;Kim, Dae-Eup
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.32 no.2
    • /
    • pp.293-299
    • /
    • 2005
  • It is important to reduce chair time and procedure in restorative treatment for children. Composite resin is not only used in esthetic restoration of anterior teeth but also posterior teeth by its improved physical property. The 7th generation dentin bonding system was recently developed in order to simplify three steps which is needed to bond composite resin to tooth surface-etchant, primer, adhesive. We compared shear bond strengths of 4, 5, 6, 7th generations dentin bonding systems. The primary dentin was pretreated with 4, 5, 6, 7th generation dentin bonding systems. Then composite resin was cured to the specimen using molds 2.5mm in diameter and 2mm in height. Thermocycling was performed and shear bond strength was finally measured. The results were as follow; 1. The mean values of shear bond strengths in 5th generation dentin bonding system(group 2) were greater than those of 4, 6, 7th generation dentin bonding system(group 1, 3, 4). The differences were statistically significant. 2. The mean values of shear bond strengths in 4th generation dentin bonding system(group 2) were greater than those of 6, 7th generation dentin bonding system(group 1, 3, 4). But, the differences were not statistically significant. 3. Between the mean values of shear bond strengths in 6, 7th generation dentin bonding system(group 3, 4) were similar.

  • PDF

THE STUDY ON SHEAR BOND STRENGTHS OF VARIOUS ONE-BOTTLE DENTIN ADHESIVES (수종의 One-bottle 상아질 결합제의 전단 결합 강도에 관한 연구)

  • Oh, So-Hee;Kim, Jong-Soo;Kwon, Soon-Won
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.4
    • /
    • pp.553-565
    • /
    • 2001
  • One-bottle adhesive system was recently developed in order to simplify the clinical skills and save chair time after continuous improvements on dentin bonding agents. To test the shear bond strength of a new "one-bottle adhesive" system to bovine dentin various commercially available one-bottle adhesives(Prime & Bond $2.1^{(R)}$, One Coat $Bond^{(R)}$, Syntac $Sprint^{(R)}$, Single $Bond^{(R)}$) were included for comparison. And we observe the interfacial morphology by scanning electron microscope. The results were as follows; 1. Group II (One Coat $Bond^{(R)}$) showed higher shear bond strength than group I (Prime & Bond $2.1^{(R)}$), group III(Syntac $Sprint^{(R)}$), and group IV(Single $Bond^{(R)}$), but no statistically significant difference was founded between groups(p>.05). 2. Relating reverse-cone shape resin tags were observed in samples of all groups under SEM. We could observed hybrid layer, resin tag and many lateral branches in every group. But, we observed in group III rare lateral branched than other three groups, and discontinuous hybrid layer.

  • PDF

A STUDY ON THE EFFECT OF DENTIN ADHESIVE TO FLUORIDE RELEASE OF COMPOMER (상아질 결합제가 컴포머의 불소유리에 미치는 영향에 관한 연구)

  • Yoon, Yeo-Sang;Kim, Jong-Soo;Kwon, Soon-Won;Kim, Yong-Kee
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.2
    • /
    • pp.228-237
    • /
    • 2001
  • It is well known that glass-ionomer cement and compomer can release fluoride which can inhibit the progression of dental caries. The purposes of this study were to evaluate whether the fluoride from fluoride-containing filling materials can penetrate the dentin bonding adhesive and the dentin bonding adhesive can increase the bond strength of resin-modified glass ionomer. The amount of fluoride release from resin-modified glass ionomer and compomer was measured during 28 days of period and statistically analyzed by t-test. The bond strength of each material with/without dentin bonding adhesive was measured and also statistically analyzed by t-test. The distribution of fluoride from each material into the tooth was explored by electron probe microanalysis system(EPMA). The experimental teeth used were second primary molars about to exfoliate. The amount of fluoride release from each material was diminished by dentin bonding adhesive during 28 days(p<0.05) and the bond strength was not increased by dentin adhesive in resin-modified glass ionomer. The bond strength of group VI was not detectable. The distribution of fluoride from each material into teeth was according to dentino-enamel junction and dispersed into pulp from pulpal floor. The widest distribution was shown in resin-modified glass ionomer cement filled without the application of dentin bonding adhesive.

  • PDF

Comparative evaluation of micro-shear bond strength between two different luting methods of resin cement to dentin (합착 술식에 따른 레진 합착제의 상아질에 대한 미세전단결합강도의 비교 연구)

  • Lee, Yoon-Jeong;Park, Sang-Jin;Choi, Kyoung-Kyu
    • Restorative Dentistry and Endodontics
    • /
    • v.30 no.4
    • /
    • pp.283-293
    • /
    • 2005
  • The purpose of this study was to evaluate the effect of dual bonding technique by comparing microshear bond strength between two different luting methods of resin cement to tooth dentin. Three dentin bonding systems(All-Bond 2, One-Step, Clearfil SE Bond), two temporary cements (Propac, Freegenol) were used in this study. In groups used conventional luting procedure, dentin surfaces were left untreated. In groups used dual bonding technique, three dentin bonding systems were applied to each dentin surface. All specimens were covered with each temporary cement. The temporary cements were removed and each group was treated using one of three different dentin bonding system. A resin cement was applied to the glass cylinder surface and the cylinder was bonded to the dentin surface. Then, micro-shear bond strength test was performed. For the evaluation of the morphology at the resin/dentin interface, SEM examination was also performed. 1. Conventional luting procedure showed higher micro-shear bond strengths than dual boning technique. However, there were no significant differences. 2. Freegenol showed higher micro-shear bond strengths than Propac, but there were no significant differences. 3. In groups used dual bonding technique, SE Bond showed significantly higher micro-shear bond strengths in One-Step and All-Bond 2 (p<0.05), but there was no significant difference between One-Step and All-Bond 2. 4. In SEM observation, with the use of All-Bond 2 and One-Step, very long and numerous resin tags were observed. This study suggests that there were no findings that the dual bonding technique would be better than the conventional luting procedure.

EFFECT OF SELF-ETCHING PRIMER APPLICATION ON THE CHARACTERISTICS & STRENGTH OF DENTIN BONDING IN PRIMARY TOOTH (자가부식 프라이머의 처리가 유치의 상아질과 레진 간의 결합 형태와 강도에 미치는 효과)

  • Lee, Jun-Haeng;Kim, Yong-Kee;Kim, Jong-Soo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.26 no.4
    • /
    • pp.595-607
    • /
    • 1999
  • The purpose of this in vitro study was to evaluate the efficacy of self-etching primer which was developed to simplify the bonding procedures by measuring the shear bond strength and observing the interfacial morphology. 90 flat dentinal surfaces were prepared by grinding the buccal and lingual areas of caries-free human deciduous molars. After bonding of composite resin to sample surfaces according to the manufacturer's direction and thermocycling, shear bond strengths were measured using Universal testing machine(Instron). Another groups of specimens were treated by hydrochloric acid to secure the resin only and those tags were evaluated under SEM for their length and forms and the morphology of the bonding sites were also observed. The result as follows. 1. Group III showed higher shear bond strength than group I and II but no statistically significant difference was founded between group I and II(p>.05). 2. Adhesive failure was predominant in group II whereas dentin detachment was the main failure pattern in group I and III. 3. Relating long resin tags of $100-200{\mu}m$ were observed in samples of all groups under SEM. In group I, homogeneously long resin tags were arranged rather tight whereas rather loosely arranged resin tags of various length were found in group II. Lateral branching of resin tags was the characteristic finding observed in group III.

  • PDF

A COMPARATIVE STUDY OF THE EFFECT OF CHLORHEXIDINE ON THE BOND STRENGTH OF ADHESIVE RESTORATION (클로르헥시딘이 접착성 수복재의 결합에 미치는 영향에 관한 비교 연구)

  • Yeom, Hae-Woong;Kim, Jong-Soo;Kwon, Soon-Won
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.29 no.1
    • /
    • pp.30-37
    • /
    • 2002
  • Bacterial microleakage around restorations is considered the principal cause of pulpal inflammation associated with restorations. The rationale for using cavity disinfectant is based on its antimicrobial properties but the cavity disinfectant may leave debris on dentin surfaces. The purpose of this study was to evaluate the effect of 2% chlorhexidine on shear bond strength and microleakage of adhesive restoration. 45 sound bovine teeth were used for the shear bond strength test and 30 for the micorleakage. For the experimental groups, 2% chlorhexidine was applied before the restorations, and was not for the control groups. The result from the this study can be summarized as follows; 1. No significant difference could be found in shear bond strength of each group. 2. No significant difference could be found in microleakage of each group.

  • PDF

MICROTENSILE BOND STRENGTH OF DENTIN BONDING ADHESIVES ON BOVINE TEETH (Bovine teeth에 대한 수 종 상아질 접착제의 미세인장결합강도)

  • Song, Eun-Ju;Kim, Jae-Moon;Kim, Shin;Jeong, Tae-Sung
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.34 no.3
    • /
    • pp.420-429
    • /
    • 2007
  • The purpose of this study was to compare the micro ensile bond strength to bovine dentin of several adhesives (SM, Scotch $Bond^{TM}$ Multipurpose; SB, $Adper^{TM}$ Single Bond 2; SE, $Clearfil^{(R)}$ SE Bond; AQ, AQ $Bond^{TM}$; TS, $Clearfil^{(R)}$ tri-S Bond). Except SM and SB, they have a simplified one- or two-step application protocols in compare with the dentin adhesives conventional three-step protocols. For the microtensile bond strength test, the labial surfaces of bovine incisors were used. Following exposure of dentin layer, according to their manufacturer's directions, each dentin adhesives were applied and composite resin blocks were constructed. The teeth were sectioned for specimen and tested microtensile bond strength. Also observed the fracture mode of interface. The obtained results were as follows : 1. The microtensile bond strength values ranged from 51.34 to 24.04 MPa on dentin(in decreasing order, SE, SM, SB, AQ and TS). 2. The highest microtensile bond strength was by SE and SM on bovine dentin, and the lowest by AQ and TS. 3. SM, SB and SE showed cohesive failures and adhesive failure but AQ, TS presented almost adhesive failures. In summary, microtensile bond strengths of single-step adhesives (AQ and TS) on bovine dentin were significantly lower than those of multi-step adhesives (SM, SB and SE) (p<0.05).

  • PDF

SHEAR BOND STRENGTH OF "ONE-BOTTLE ADHESIVE" SYSTEM IN PRIMARY DENTIN. (One-Bottle 상아질 결합제의 유치 상아질에 대한 전단 결합 강도에 관한 연구)

  • Kim, Jong-Bin;Kim, Jong-Soo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.27 no.3
    • /
    • pp.444-456
    • /
    • 2000
  • To test the shear bond strength of a new "one-bottle adhesive" system to primary dentin two commercially available one-bottle adhesives (Prime & Bond NT, Single bond) and conventional three step system(Scotchbond Multi-Purpose Plus) were included for comparison. And We observe the interfacial morphology by scanning electron microscope. 90 primary molar teeth were embedded in acrylic and buccal and lingual surface were polished to 320 grit to create standardized dentin surface for testing. After bonding of composite resin to sample surfaces according to the manufacturer s direction and 1000 times thermocycling in dwell time 30 second, Shear bond strengths of adhesives to dentin were determined using universal testing machine and analyzed by ANOVA test. Another groups of specimens were treated by hydrochloric acid to secure the resin only and those tags were evaluated under SEM for their length and forms and the morphology of the bonding sites were also observed. The result are as follows. 1. Group I(Prime & Bond NT) showed higher shear bond strength than group iI(Single Bond) and III(Scotchbond Multi Purpose Plus) but no statistically significant difference was founded between groups(p>.05). 2. Relating long resin tags of $70-120{\mu}m$ were observed in samples of all groups under SEM. We could observed hybrid layer, resin tag and many lateral branches in every group. But, we observed in group III rare lateral branched than other two group and discontinuous hybrid layer.

  • PDF

EFFECT OF CHLORHEXIDINE ON MICROTENSILE BOND STRENGTH OF DENTIN BONDING SYSTEMS (Chlorhexidine 처리가 상아질 접착제의 미세인장결합강도에 미치는 영향)

  • Oh, Eun-Hwa;Choi, Kyoung-Kyu;Kim, Jong-Ryul;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.33 no.2
    • /
    • pp.148-161
    • /
    • 2008
  • The purpose of this study was to evaluate the effect of chlorhexidine (CHX) on microtensile bond strength (${\mu}TBS$) of dentin bonding systems. Dentin collagenolytic and gelatinolytic activities can be suppressed by protease inhibitors, indicating that MMPs (Matrix metalloproteinases) inhibition could be beneficial in the preservation of hybrid layers. Chlorhexidine (CHX) is known as an inhibitor of MMPs activity in vitro. The experiment was proceeded as follows: At first, flat occlusal surfaces were prepared on mid-coronal dentin of extracted third molars. GI (Glass Ionomer) group was treated with dentin conditioner, and then, applied with 2 % CHX. Both SM (Scotchbond Multipurpose) and SB (Single Bond) group were applied with CHX after acid-etched with 37% phosphoric acid. TS (Clearfil Tri-S) group was applied with CHX, and then, with adhesives. Hybrid composite Z-250 and resin-modified glass ionomer Fuji-II LC was built up on experimental dentin surfaces. Half of them were subjected to 10,000 thermocycle, while the others were tested immediately. With the resulting data, statistically two-way ANOVA was performed to assess the ${\mu}TBS$ before and after thermo cycling and the effect of CHX. All statistical tests were carried out at the 95 % level of confidence. The failure mode of the testing samples was observed under a scanning electron microscopy (SEM). Within limited results, the results of this study were as follows; 1. In all experimental groups applied with 2 % chlorhexidine, the microtensile bond strength increased, and thermo cycling decreased the micro tensile bond strength (P > 0.05). 2. Compared to the thermocycling groups without chlorhexidine, those with both thermocycling and chlorhexidine showed higher microtensile bond strength, and there was significant difference especially in GI and TS groups. 3. SEM analysis of failure mode distribution revealed the adhesive failure at hybrid layer in most of the specimen. and the shift of the failure site from bottom to top of the hybrid layer with chlorhexidine groups. 2 % chlorhexidine application after acid-etching proved to preserve the durability of the hybrid layer and microtensile bond strength of dentin bonding systems.

Effects of activators contained in adhesives on dentin bond strengths (상아질 접착제에 포함된 활성제의 사용 유무가 자가중합 복합레진의 상아질에 대한 전단결합강도에 미치는 영향)

  • Kang, Hye-Kyung;Shin, Joo-Hee;Suh, Kyu-Won;Ryu, Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.5
    • /
    • pp.511-519
    • /
    • 2008
  • Statement of problem: An incompatibility between the initiator systems of self-curing composite resins and light-curing adhesives was supposed recently. Purpose: The purpose of the study was to evaluate the influence of activators for self/dual bonding on dentin shear bonding strengths. Material and methods: Fifty human molars were divided into 5 groups. A flat dentin surface was created for each tooth. A self-curing composite resin (Luxacore) was bonded with the following adhesives (n = 10); One-Step, Prime&Bond NT, AdheSE, Prime&Bond NT and AdheSE were also used in combination with activators. Shear bond strengths were measured after 24 hours of water storage. The specimens were loaded in shear in the Instron until failure at a 1 mm/min crosshead speed. Data were compared using one-way ANOVA and Tukey HSD test (${\alpha}$= 0.05). Results: The dentin adhesive systems in order of decreasing median bond strength were One-Step > Prime&Bond NT with activator, AdheSE with activator > Prime&Bond NT, AdheSE. Among adhesives, One-Step had the highest bond strength. Prime&Bond NT with activator had higher bond strengths than Prime&Bond NT that was used alone, and so was AdheSE. Conclusion: Shear bond strengths were increased in Prime&Bond NT and AdheSE when these were used with activators comparing used without activators. But using activators was not effective clinically comparing One-Step.