Evaluation of Tension Behavior in FRP Hybrid Bar Affected by UV Exposure and Freezing/Thawing Tests (UV 폭로 및 동결융해 시험을 거친 FRP Hybrid Bar의 인장거동 평가)

  • Yoon, Yong-Sik;Park, Jae-Sung;Park, Ki-Tae;Kwon, Seung-Jun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.130-136
    • /
    • 2017
  • The present work is for an evaluation of tension behavior and surface deterioration of FRP Hybrid Bar due to UV exposure and freezing/thawing(F/T) actions. For the work, FRP Hybrid Bar is subjected to UV exposure test, then F/T test is performed successively to 180 cycles. In FRP Hybrid Bar, no significant surface deterioration is evaluated after UV exposure. Tension hardening performance, a unique engineering advantage of FRP Hybrid Bar, is still maintained after F/T test. The performance in FRP Hybrid Bar exposed to UV is still effective. FRP Hybrid Bar exposed to UV have almost similar tension behavior of FRP Hybrid Bar without UV exposure. Although F/T cycles increase to 180, steel rebar, FRP Hybrid Bar, and FRP Hybrid Bar exposed to UV show no significant changes in tension behavior. In the work, UV exposure and F/T actions are evaluated to have little negative effect on surface deterioration and tensile performance in FRP Hybrid Bar, however spalling of silica coating due to impact should be considered since it affects bonding strength to outer concrete.

Comparative Study on Freeze-Thaw Durability of General Concrete and Pavement Concrete (일반콘크리트와 포장콘크리트의 동결융해 내구성에 대한 비교 연구)

  • Kim, Hyun-Joong;Lee, Beung-Duk;Lee, Ju-Gang
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.561-564
    • /
    • 2008
  • Concrete scaling is the progressive surface deterioration of susceptible subjected to freeze-thaw cycling in the presence of moisture. Particularly, it has been recognized that chlorides present in deicing agents can significantly increase concrete surface scaling. Domestic area of most be happened chloride deicer damage. Because daily mean temperature is below 0$^{\circ}C$ from the area of domestic most. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, not only the source of substantial cost penalties due to their corrosive action and ability to deterioration roadway surface materials but also the source of environmental damages. In this study, Use of (40, 27, 21MPa) pavement concrete analyze freeze-thaw test and scaling on the chlorides present.

  • PDF

Affecting Analysis of Air Content on the Freeze-Thaw Durability of Concrete (콘크리트의 동결융해 내구성에 공기량이 미치는 영향 분석)

  • Lee, Beung-Duk;Kim, Hyun-Joong;Kang, Hye-Jin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.565-568
    • /
    • 2008
  • Domestic area of most be happened chloride deicer damage. Because daily mean temperature is below 0$^{\circ}C$ from the area of domestic most. Concrete durability influence Air Content. Presently, We used to AE(air-entraining agent) for increase freeze-thaw durability. So, on concrete Air Spacing ratio used $200{\mu}m{\sim}230{\mu}m$ in Canada and under $250{\mu}m$ in Japan institution. Use of Air content has been and will continue to be a major part of concrete durability and scaling. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. The prepared optimum mix concrete in this study show that freeze-thaw and scaling resistance of Non-AE(air content 1.5%) and AE (air content 4.5%, 7.2%). Solution concentrations of deicing agent were good result, and the pore system and change of hydration products is not difference comparing before freeze-thaw test.

  • PDF

Effects of Micropores on the Freezing-Thawing Resistance of High Volume Slag Concrete (슬래그를 다량 치환한 콘크리트의 동결융해 저항성능에 미치는 미세공극의 영향)

  • Kim, Rae-Hwan;Kim, Gyu-Yong;Lee, Bo-Kyeong;Shin, Kyoung-Su;Song, Gwon-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.4
    • /
    • pp.67-74
    • /
    • 2015
  • In this study, effects of micropores on the freezing-thawing resistance of high volume slag concrete are reviewed. Concrete was made with slag which contains the ground granulated blast furnace slag(GGBS) and the pig iron preliminary treatment slag(PS) by replacing 0, 40, 70 %, then compressive strength, freezing-thawing resistance, micropores were reviewed. Also, specified design strength, target air contents were set. Deterioration was induced by using 14-day-age specimen which has low compressive strength for evaluating deterioration by freeze-thawing action. As results of the experiment, despite of specified design strength which has been set similarly and ensured target air contents, the pore size distribution of the concrete showed different results. Micropores in GGBS70 specimen have small amount of water which is likely to freeze because there is small amount of pore volume of 10~100 nm size at 0 cycle which has not been influenced by freezing-thawing. For these reasons, it was confirmed that the freezing-thawing resistance performance of GGBS70 is significantly superior than other specimens because relatively small expansion pressure is generated compared to the other specimens.

Analysis and Prediction of Highway Bridge Deck Slab Deterioration (고속도로 교량 바닥판 열화분석 및 추정)

  • Lee, Il-Keun;Kim, Woo-Seok;Kang, Hyeong-Taek;Seo, Jung-Wook
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.2
    • /
    • pp.68-75
    • /
    • 2015
  • This study established key factors causing deck slab deterioration based on GPR database of 747 highway bridges, and predicted deck slab damage rates with respect to bridge service life. To minimize the influence of bridge service life on deck slab deterioration, the deck slab damage rate database was corrected based on a linear regression model of bridge service life vs. deck slab damage rate. The corrected deck slab damage rates were analyzed to determine correlation considering the number of snowy days, the amount of snowfalls, the number of freeze-thaw days, average winter temperature, altitude, the amount of deicing chemicals and equivalent traffic volume, and then both the number of freeze-thaw days and the amount of deicing chemicals were determined to be key factors causing deck slab deterioration. The complex deterioration considering both key factors was represented deck slab damage rate charts, and the average deck slab life was derived. The results of this study will be used as a guideline for highway bridge maintenance to identify the progress of deck slab deterioration for a given bridge and predict the time required deck slab rehabilitation.

Calculation of Deterioration Depth of Major Rock Type Slopes caused by Freezing-Thawing in Korea (국내 주요 암종별 사면의 동결-융해에 의한 열화심도 계산)

  • Kwon, O-Il;Baek, Yong;Yim, Sung-Bin;Seo, Yong-Seok
    • The Journal of Engineering Geology
    • /
    • v.17 no.3
    • /
    • pp.359-365
    • /
    • 2007
  • Freezing and thawing cycle is one of the major weathering-induced factors in the mechanical weathering of the rock mass. This natural process accelerates rock weathering process by breaking down the parent rock materials and makes soil or weathered rock formation in a rock slope surface zone. It can also cause reduction of the shear strength in slopes. It is important to calculate the deterioration depth caused by freezing-thawing for a slope stability analysis. In this study, deterioration depths of rock slope due to freezing-thawing were calculated using the 1-D heat conductivity equation. The temperature distribution analysis was also carried out using collected temperature distribution data for last five years of several major cities in Korea. The analysis was performed based on the distributed rock types in study areas. Thermal conductivities, specific heats and densities of the calculation rocks are tested in the laboratory. They are thermal properties of rocks as input parameters for calculating deterioration depths. Finally, the paper is showing the calculated deterioration depths of each rock type slopes in several major cities of Korea.

Evaluation of Bond Strength in FRP Hybrid Bar Affected by Freezing/thawing Test and UV Rays (동결융해 및 UV 폭로시험을 거친 FRP Hybrid Bar의 인발거동특성 평가)

  • Park, Jae-Sung;Yoon, Yong-Sik;Park, Ki-Tae;Kwon, Sung-Jun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.1
    • /
    • pp.53-58
    • /
    • 2017
  • FRP Hybrid Bar, composed of an embedded steel and the coated composites with epoxy and glass fiber, is an effective construction material with tension-hardening performance and lightweight. The epoxy exposed to UV(Ultra Violet Rays) and FT(Freezing and Thawing) action easily shows a surface deterioration, which can cause degradation of bonding strength between inside-steel and outside-concrete. In the present work, surface inspection for 3 different samples of normal steel, FRP Hybrid Bar before UV, and FRP Hybrid Bar after UV test was performed, then concrete samples with 3 reinforcement types were prepared for accelerated FT test. Through visual inspection on 3 typed reinforcement, no significant deterioration like chalking was evaluated. The results from FT test to 120 and 180 cycles showed FRP Hybrid Bar exposed to UV test has higher bonding strength than normal steel by 106.3% due to enlarged bond area by silica coating. The 3 cases showed a similar bond strength tendency with increasing FT cycles, however a relatively big deviations of bond strength were evaluated in FRP Hybrid Bar after UV test due to loss of silica coating.

Performance Evaluation of Various Concrete Repair Materials to Corrosion Prevent of Rebar (철근의 부식 방지를 위한 다양한 콘크리트 보수재료들의 성능평가)

  • Tae-Kyun Kim;Jong-Sub Park
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.4
    • /
    • pp.458-466
    • /
    • 2023
  • Structures in our surroundings deteriorate over time due to environmental and chemical factors, resulting in a decrease in their performance. The primary causes of degradation in concrete structures are carbonation, salt damage, and freeze-thaw cycles. Various maintenance methods exist to address these degradation issues. However, research and technological development for existing maintenance methods have been ongoing, but the accuracy and effectiveness of repair materials and techniques have not been extensively validated. Therefore, in this study, we conducted a material performance evaluation of various manufacturers' repair materials. Based on this evaluation, we applied corrosion inhibitors and epoxy, which are the methods most closely related to crack repair, to assess the durability performance against carbonation, salt damage, and freeze-thaw cycles. The results show approximately a two-fold performance improvement against carbonation and salt damage, and a 5% enhancement in repair performance against freeze-thaw cycles. Thus, it is considered effective in preventing rebar corrosion when appropriate maintenance is carried out according to environmental and chemical factors during structural repairs.

Estimation of Deterioration Depth of Rock Slope due to Freezing-thawing (동결융해에 의한 암반사면의 열화심도 산정)

  • Baek Yong;Seo Yong-Seok;Jeong Ja-Hyea;Kwon O-Ii
    • The Journal of Engineering Geology
    • /
    • v.15 no.3
    • /
    • pp.325-335
    • /
    • 2005
  • Deterioration depths of rock slope due to freezing-thawing were calculated using the 1-D heat conductivity equation. The temperature distribution analysis was carried out using temperature distribution data for last two years of the five major cities such as Seoul, Daejeon, Pohang, Gwangju and Cangneung. The analysis was performed based on three different types of rocks, sandstone, granite and gneiss. This study has found that the deterioration depths tend to be greater with the increase of the thermal conductivity coefficient in Seoul, Daejeon and Pohang where showing relatively greater temperature deviations. Regarding the influence of rock types, deterioration depths turned out to be greater in Gwangju and Gangneung where show relatively smaller temperature deviations among the five cities, assuming these cities are on the granite with thermal conductivity of $55,200\;cal/m\timesday\times^{\circ}C$. In contrast, for the other rock types, cities of relatively geater temperature deviations show deeper deterioration depth than the others. Deterioration depths of rock slope in Korea due to freezing-thawing fumed out to be around 8.4 m to 10.7 m.

A Study on the Durability Improvement of Highway-Subsidiary Concrete Structure Exposed to Deicing Salt and Freeze-Thaw (동결융해 및 제설제에 노출된 고속도로 소구조물 콘크리트의 내구성 개선 연구)

  • Lee, Byung-Duk;Choi, Yoon-Suk;Kim, Young-Geun;Choi, Jae-Seok;Kim, Il-Sun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.4
    • /
    • pp.128-135
    • /
    • 2016
  • In the current concrete structure of the highway is still the major problem most of concrete deterioration caused by the freeze-thaw and deicing salt, which is of issues that are not completely resolved. In particular, a single freezing event does not cause much harm, durability of concrete under multi-deterioration environment by repeated freeze-thaw and deicing salt is rapidly degraded and reduce its service life. In this study, the exposure environmental condition according the regional highway points were established. The damage condition and chloride content of the concrete at general and severe environmental exposure condition were also investigated. In addition, the experimental test of chloride ion permeability, scaling resistant and freeze-thaw resistance were carried out to improve the durability of the mechanical placing concrete of subsidiary structure. According to the results of this study, in observation of concrete surface condition, the concrete exposed by severe environmental condition showed broad ranges of damage with high chloride contents. Meanwhile, the water-binder(W/B) ratio and the less water content, and fly ash concrete than the specified existing mix proportion is significantly improved the durability. Also, the optimal mix proportion derived for test is satisfied the strength and air contents, water-binder ratio, and durability criteria of concrete specifications, as well as service life seems greatly improved.