An STI(Shallow Trench Isolation) by using a CMP(Chemical Mechanical Polishing) process has been one of the key issues in the device isolation[1] In this paper we fabricated N, P-MOSFEET tall analyse hump characteristics in various rounding oxdation thickness(ex : Skip, 500, 800, 1000$\AA$). As a result we found that hump occurred at STI channel edge region by field oxide recess. and boron segregation(early turn on due to boron segregatiorn at channel edge). Therefore we improved that hump occurrence by increased oxidation thickness, and control field oxide recess( 20nm), wet oxidation etch time(19HF,30sec), STI nitride wet cleaning time(99HF, 60sec+P 90min) and fate pre-oxidation cleaning time (U10min+19HF, 60sec) to prevent hump occurring at STI channel edge.