• 제목/요약/키워드: sea water immersion

검색결과 40건 처리시간 0.023초

점용접 아연도금강판의 강도특성에 미치는 온도 및 침수의 영향 (Effect of Temperature and Water Immersion on Strength Properties of Spot Welded Zincked Steel Plates)

  • 서도원;최준용;임재규
    • 대한기계학회논문집A
    • /
    • 제28권12호
    • /
    • pp.1864-1870
    • /
    • 2004
  • A spot welded structures have an influence on a diverse climatic situation, for instance temperature, humidity and precipitation. In addition factors of environmental pollution such as acid rain, that courses corrosion, have the tendency to increase. But spot welded structures strength is affected by humidity and environment temperature. Therefore, it is important to evaluate effect of temperature and water immersion on strength properties of spot welded part. In this study, the strength distribution of spot welded plates is evaluated the environmental temperature of zinc coated steel plates. Test is conducted with welded part immersed in distilled and synthetic sea water. Specimens are immersed into water for 10, 100, 500 and 1000 hours to evaluate the offsets of water immersion time on tensile-shear strength under the conditions of -40, 0, 20 and 5$0^{\circ}C$. From this result, spot welded specimens with 5 mm clearance have lower tensile-shear strength in the distilled water or synthetic sea water than without clearance. And they have lower tensile-shear strength under -4$0^{\circ}C$ and over 5$0^{\circ}C$.

해수의 건습반복 촉진열화에 따른 콘크리트의 내해수성 (Sea Water Resistance of the Concrte Deteriorated by Repeat of Immersing and Drying in Sea Water)

  • 박춘근;김병권;최재웅;고만기
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.307-312
    • /
    • 1997
  • The sea water resistance of cement and concrete must be compared when it used for construction in the ocean. The sea water resistance of the concrete specimens using three types of cements such as ordinary Portland cement, sulfate resistance Portland cement, blastfurnace slag cement were studied. In this study, an accelerated test for access sea water resistance by subjecting the concrete specimens to repeated cycles of concentrated sea water immersion and hot wind drying was employed. This study proved that sulfate resistance Portland cement had higher resistance for sea water.

  • PDF

침적식 온라인 굴절계를 이용한 해수의 염도 측정 (Salinity Determination for Sea Water Using Immersion-Type On-Line Refractometer)

  • 김병철;김영한;장상목
    • 한국항해항만학회지
    • /
    • 제26권5호
    • /
    • pp.571-575
    • /
    • 2002
  • 해수의 염도와 온도를 현장에서 측정할 수 있는 침적식 온라인 굴절계를 제작하고 실제 해수와 유사한 2 % 내지 4 %의 염수를 사용하여 그 성능을 조사하였다. 굴절률과 온도를 동시에 측정함으로 온도보상을 신속하게 할 수 있어 염도의 직접측정을 가능하게 하였다. 각기 다른 농도의 염용액에서 측정된 염도의 결과로부터 본 실험의 장치는 안정성과 재현성을 모두 갖는 염도 측정이 가능함을 알았다.

점용접 아연도금판의 강도특성에 대한 온도 및 침수의 영향 (Effect of Temperature and Water Assumtion on Strength of Spot Welded Zine Steel Plates)

  • 서도원;윤호철;최준용;임재규
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.358-363
    • /
    • 2003
  • Spot welded structure is operated in diverse situation because of temperature, humidity and precipitation. In addition factors of environmental pollution such as acid rain, that courses corrosion, have the tendency to increase, But spot welded structure strength is affected by dampness and environment temperatures. Therefore, it is important to evaluate effect of temperature of spot welded part, In this study, the strength distribution of spot welded plates is evaluated about the environmental temperature of zine coated steel plates and test is conducted with welded part immersed in distilled and synthetic sea water. Specimens are immersed into water for 10, 100, 500 and 1000hours to evaluate the effects of water immersion time on tensile-shear strength under the conditions of -40, 0, 20 and $50^{\circ}C$. Strength is evaluated by tensile-shear test. The conditions of spot welding are 240kgf electrode force, 10KA welding current with 0 and 5mm clearance. From this study, spot welded specimens with clearance have lower tensile-shear strength in the distilled water or synthetic sea water comparing with spot welded specimens without clearance. And they have lower tensile-shear strength under $-40^{\circ}C$ and over $50^{\circ}C$.

  • PDF

연근해 어선에 대한 방수복 비치기준 개정을 위한 기초연구 (A Basic Study on the Criteria of Immersion Suits for Fishing Vessels Engaged in Coastal and Inshore Fisheries)

  • 김기선;조장원;한세현;이창희
    • 수산해양교육연구
    • /
    • 제28권6호
    • /
    • pp.1581-1590
    • /
    • 2016
  • In order to reduce the risk of death from hypothermia for the fishing vessel's crew at sea, this paper suggests that the criteria of equipment of fishing vessels should be revised for fishing vessels engaged in coastal and inshore fisheries to be equipped with the immersion suit. The criteria of equipment of fishing vessels for immersion suits was amended to reflect the sinking of No.501 Oryongho but it was only reflected in ocean fisheries at Bering sea and Antarctic ocean that immersion suits must be provided with the same number of the total number of crew on board. Therefore, this paper analyses the relationship between maritime accident of fishing vessels and weather condition based on sea water temperature to find out the risk of hypothermia and also compares the international conventions(SFV Protocol 1993, Cape Town Agreement 2012, STCW-F 1995 and SOLAS 1974) and domestic law concerning criteria of equipment of fishing vessels. As a result, fishing vessels engaged in coastal and inshore fisheries are exposed to the risk of hypothermia when they are in distress and the criteria of equipment of fishing vessels should be amended to provide the immersion suits in accordance with the revision trend of international conventions.

바지락치패의 폐사에 관한 연구-II 바지락 치패의 온도, 염분, 노출에 대한 저항성 (Studies on the Natural Mortality of the Young Short Necked Clam, Tapes Japonica-II . Resistance to Temperature , Salinity and Exposure for the Young Short Necked Clam)

  • 최상
    • 한국동물학회지
    • /
    • 제9권1호
    • /
    • pp.7-15
    • /
    • 1966
  • In a previous paper, the dirunal and monthly changes of the tidal flat temperature and chlorinity were observed. In this paper the resistance of the young short necked clam in various growth stages to the temperature, to the chlorinity and to the exposure were studies. The young clam used were in early (E), medium (M) and late (L) young stages whose shell lengths were 2.0-3.5mm, 9.0-11.0mm. and 14.0-16.0mm., respectively. The results were : 1. At various sea water temperatures , the chlorinity resistance of the young clam was directly proportional to the shell length. 2. When both inadequate sea water temperature and abnormal chlorinity are simultaneously applied, the resistance of these young clams was more markedly reduced than the case of applying either one of these conditions. 3. In clams of M and L, no lethal effect were observed when daily immersion of four to eight hours for a week into the sea water of any concentration of chloriity at 26-34$^{\circ}C$, whereas in E, 37-90% of mortalities were obtained by immersion of eight hours daily into both the fresh water and the sea water of higher chloriniites (more than 23.5$\textperthousand$ Cl) at the same temperature above. 4. The lower critical thermal maximum for lethal to the young clam was 38$^{\circ}C$. With four hours immersion daily at the water temperature of 38$^{\circ}C$, the mortalities of E, M and L to the lower chlorinities (less than 6.7$\textperthousand$Cl) were 100, 70-100 and 27-37% respectively ; to the higher chlorinities (more than 23.5$\textperthousand$Cl) 10-70, 10-37 and 3 % respectively ; to the normal range of chlorinities (13.4-16.8$\textperthousand$Cl) 0-13, 3 and 0 % respectively. 5. No lethal effects were observed in E and M clams immersed continuously for seven days in sea water with chlornities of 7.2 -21.7$\textperthousand$Cl at 18-24$^{\circ}C$, while notable mortalities were observed in E which had been kept at lower (less than 4.8$\textperthousand$ Cl) and higher (more than 24.1$\textperthousand$ Cl) chlorinites. 6. Although the resistance of the young clam to the chlorinity may have to be related closely to the life history of the clam prior subject to the experiment, the adapted chlorinity range was 7.2-19.3$\textperthousand$ Cl and the optimum range was 13.4-16.8$\textperthousand$Cl. 7. Remarkable lethal effects were observed for the E and M clams to the exposure temperature of 38$^{\circ}C$ whereas the L and had no such fatal results.

  • PDF

해양 환경 폭로 시험을 통한 FA 콘크리트의 겉보기 염화물 확산계수 평가 (Evaluation of Apparent Chloride Diffusion Coefficient of Fly Ash Concrete by Marine Environment Exposure Tests)

  • 윤용식;임희섭;권성준
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제23권3호
    • /
    • pp.119-126
    • /
    • 2019
  • 해안 지역에 시공된 철근 콘크리트 구조물은 해수 중의 염소 이온에 의해 내부 철근이 부식하게 된다. 특히 해안지역에서는 해수에 침지되는 경우뿐만 아니라 조수간만 및 비래염분의 영향을 받기 때문에 이에 대한 고려가 필수적이다. 본 연구에서는 3가지 수준의 노출 환경(침지대, 간만대, 비말대)과 노출기간 180일, 365일, 730일을 고려하여 해양환경노출실험을 실시하였다. 대상 배합은 3가지 수준의 물-결합재비 및 2가지 수준의 플라이애시 치환률(0 %, 30 %)을 고려하여 설정하였다. 모든 노출조건에서 플라이 애시 치환 배합이 OPC 배합 대비 낮은 겉보기 염화물 확산계수를 나타내었으며, 이는 플라이애시의 포졸란 반응이 원인으로 사료된다. 플라이애시 배합은 노출 기간 180일에서는 플라이애시 치환 배합이 OPC 배합 대비 최대 63 5 %의 감소율을, 노출 기간 730일 에서는 최대 55.8 %의 감소율을 나타내었다. 노출 조건에 따른 확산계수 거동을 평가한 결과, 플라이애시 치환 배합에서는 간만대, 침지대, 비말대 순으로 확산계수가 평가되었다. 간만대에서는 건습이 반복되어 염화물 이온의 침투가 빠르게 일어나는 것으로 보인다.

성게 가시에 의하여 육아종이 발생한 1례 (A Case of Showing Granuloma Following a Sea Urchin Sting)

  • 임현술;김규회;김두희;김정란;김용민;이현경
    • 농촌의학ㆍ지역보건
    • /
    • 제20권2호
    • /
    • pp.169-174
    • /
    • 1995
  • The case was described of a 31 year old female who developed fusiform swelling of the right third finger at the site of puncture by sea urchin spine. We observed a radiopaque linear material suggesting a remnant spine which the size was 2.4 mm in sonography and mammography. We confirmed that it exhibits a urchin spine and distinct caseous necrosis with central calcification. Sea urchins(Echinoidea) are ubiquitous marine creatures that resemble pincushions and are covered by calcareous skeletons surrounded by numerous movable calcium carbonate spines. The sharp spines are brittle and easily detach when touched by the victim. Contact with sea urchin spines produces intense pain, some localized erythema and edema. Inflammation develops in response to retained fragments. Granulomas 1-5 mm in diameter develop rarely 2-12 months after envenomation. In treatment, hot water immersion and thorough wound cleansing are advisable. Analgesics may, be necessary after hot water immersion. Attempts to remove these spines should be performed with good lighting sources, preferably with radiological direction. Chronic granulomas usually require complete excision. Acetone has been suggested for rapid resolution of pain. No antidotes are available.

  • PDF

Theoretical Approach to Calculate Surface Chloride Content $C_s$ of Submerged Concrete under Sea Water Laden Environment

  • 윤인석
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.197-200
    • /
    • 2006
  • The ingress of chloride ions plays a crucial role for service life design of reinforced concrete structures. In view of durability design of concrete structures under marine environment, one of the most essential parameters is the surface chloride content of concrete. However, on the basis of the results of in-situ investigation, this value has been determining in the numerous studies on the durability design of concrete structures. Hence, it is necessary to confirm the range of the surface chloride content in order to establish a unified durability design system of concrete. This study suggests a rational and practical way to calculate the maximum surface chloride content of submerged concrete under marine environment. This approach starts with the calculation of the amount of chloride ingredients in normal sea water. The capillary pore structure is modeled by numerical simulation model HYMOSTRUC and it is assumed to be completely saturated by the salt ingredients of sea water. In order to validate this approach, the total chloride content of the mortar and concrete slim disc specimen was measured after the immersion into the artificial sea water solution. Additionally, the theoretical, the experimental and in-situ investigation results of other researchers are compiled and analyzed. Based on this approach, it will follow to calculate the maximum surface chloride content of concrete at tidal zone, where the environment can be considered as a condition of dry-wetting cycles.

  • PDF

Corrosion Property Evaluation of Copper Alloy Tubes against Sea Water

  • Pang, Beilli;Ong, Sang-Kil;Lee, Hong-Ro
    • 한국표면공학회지
    • /
    • 제42권6호
    • /
    • pp.280-286
    • /
    • 2009
  • In this study, the corrosion property of copper alloy tubes in seawater has been investigated. Three copper alloys of nominal composition Cu-20Zn-2Al(Al-Brass), Cu-30Ni(CN70/30) and Cu-10Ni(CN90/10) were considered. The samples were immersed in 3%NaCl flowing solution at $90^{\circ}C$ for 30, 50 and 80 days. Corrosion rate of copper alloy tubes in 3%NaCl flowing solution was investigated by weight-loss measurements and electrochemical test. The CN70/30 showed lowest corrosion rate among three copper alloy tubes. Because of passive films formation, corrosion rates of three types of copper tubes were decrease with time. Surface characteristics of copper alloy tubes were analyzed by optical micrograph(OM), scanning electronic microscopy (SEM), energy dispersive X-ray analysis(EDAX) and X-ray diffraction patterns(XRD). CN70/30 showed partly pitting problem on the surface owing to high Fe content, even though having high resistant against corrosion. Cracks appeared on the surface of CN90/10 and CN70/30 after more than 50 days immersion, which could be derived from high nickel contents.