• Title/Summary/Keyword: sccm

Search Result 658, Processing Time 0.023 seconds

Deposition of β-SiC by a LPCVD Method and the Effect of the Crystallographic Orientation on Mechanical Properties (저압 화학기상증착법을 이용한 β-SiC의 증착 및 결정 성장 방위에 따른 기계적 특성 변화)

  • Kim, Daejong;Lee, Jongmin;Kim, Weon-Ju;Yoon, Soon Gil;Park, Ji Yeon
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.1
    • /
    • pp.43-49
    • /
    • 2013
  • ${\beta}$-SiC was deposited onto a graphite substrate by a LPCVD method and the effect of the crystallographic orientation on mechanical properties of the deposited SiC was investigated. The deposition was performed at $1300^{\circ}C$ in a cylindrical hot-wall LPCVD system by varying the deposition pressure and total flow rate. The texture and crystallographic orientation of the SiC were evaluated by XRD. The deposition rate increased linearly with the gas flow rate from 800 sccm to 1600 sccm. It also increased with the pressure but became saturated above a total pressure of 3.3 kPa. In the range of 3.3 - 10 kPa, the preferred orientation changed from the (220) and (311) planes to the (111) plane. The hardness and elastic modulus showed maximum values when the SiC had the (111) preferred orientation, though it gradually decreased upon a change to the (220) and (311) preferred orientations.

Effect of Al Doping Concentration on Resistance Switching Behavior of Sputtered Al-doped MgOx Films

  • Lee, Gyu-Min;Kim, Jong-Gi;Park, Seong-Hun;Son, Hyeon-Cheol
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.307-307
    • /
    • 2012
  • In this study, we investigated that the resistance switching characteristics of Al-doped MgOx films with increasing Al doping concentration and increasing film thickness. The Al-doped MgOx based ReRAM devices with a TiN/Al-doped MgOx/Pt/Ti/SiO2 were fabricated on Si substrates. The 5 nm, 10 nm, and 15 nm thick Al-doped MgOx films were deposited by reactive dc magnetron co-sputtering at $300^{\circ}C$ and oxygen partial ratio of 60% (Ar: 16 sccm, O2: 24 sccm). Micro-structure of Al-doped MgOx films and atomic concentration were investigated by XRD and XPS, respectively. The Al-doped MgOx films showed set/reset resistance switching behavior at various Al doping concentrations. The process voltage of forming/set is decreased and whereas the initial current level is increased with decreasing thickness of Al-doped MgOx films. Besides, the initial current of Al-doped MgOx films is increased with increasing Al doping concentration in MgOx films. The change of resistance switching behavior depending on doping concentration was discussed in terms of concentration of non-lattice oxygen of Al-doped MgOx.

  • PDF

Synthesis of Graphene on Ni/SiO2/Si Substrate by Inductively-Coupled Plasma-Enhanced Chemical Vapor Deposition (유도결합 플라즈마 화학기상증착법을 이용한 Ni/SiO2/Si 기판에서 그라핀 제조)

  • Park, Young-Soo;Huh, Hoon-Hoe;Kim, Eui-Tae
    • Korean Journal of Materials Research
    • /
    • v.19 no.10
    • /
    • pp.522-526
    • /
    • 2009
  • Graphene has been effectively synthesized on Ni/SiO$_2$/Si substrates with CH$_4$ (1 SCCM) diluted in Ar/H$_2$(10%) (99 SCCM) by using an inductively-coupled plasma-enhanced chemical vapor deposition. Graphene was formed on the entire surface of the 500 nm thick Ni substrate even at 700 $^{\circ}C$, although CH$_4$ and Ar/H$_2$ gas were supplied under plasma of 600 W for 1 second. The Raman spectrum showed typical graphene features with D, G, and 2D peaks at 1356, 1584, and 2710 cm$^{-1}$, respectively. With increase of growth temperature to 900 $^{\circ}C$, the ratios of the D band intensity to the G band intensity and the 2D band intensity to the G band intensity were increased and decreased, respectively. The results were strongly correlated to a rougher and coarser Ni surface due to the enhanced recrystallization process at higher temperatures. In contrast, highquality graphene was synthesized at 1000 $^{\circ}C$ on smooth and large Ni grains, which were formed by decreasing Ni deposition thickness to 300 nm.

Fabrication and Properties of Diamond Thin-Film from N-Hexane by Using Microwave Plasma Process (Microwave Plasma Process에 의한 N-Hexane으로부터 다이아몬드 박막제작 및 특성)

  • Han, Sang-Bo;Kwon, Tae-Jin;Park, Sang-Hyun;Park, Jae-Youn;Lee, Seung-Ji
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.25 no.4
    • /
    • pp.79-87
    • /
    • 2011
  • In this paper, the best conditions for the deposition of the high quality diamond thin-film from N-hexane as a carbon source in the microwave plasma process was carried out. Major parameters are the deposition time, flow rates of oxygen and hexane. The deposition time for the steady state thin-film was required more than 4[h], and the suitable flow rates of hexane and oxygen for the high-quality thin-film are 0.4[sccm] and 0.1~0.2[sccm], respectively. In addition, amorphous carbons such as DLC and graphite were grown by increasing the flow rate of hexane, and it decreased by increasing the flow rate of oxygen. Specifically, the growth rate is about 1.5[${\mu}mh-1$] under no addition of oxygen and it decreased about 60[%] as ca. 1.0[${\mu}mh-1$] with oxygen.

The Characteristics of $Cu_2O$ Thin Films Deposited Using RF-Magnetron Sputtering Method with Nitrogen-Ambient

  • Lee, Seong Hyun;Yun, Sun Jin;Lim, Jung Wook
    • ETRI Journal
    • /
    • v.35 no.6
    • /
    • pp.1156-1159
    • /
    • 2013
  • We investigate the characteristics of $Cu_2O$ thin films deposited through the addition of $N_2$ gas. The addition of $N_2$ gas has remarkable effects on the phase changes, resulting in improved electrical and optical properties. An intermediate phase ($6CuO{\cdot}Cu_2O$) appears at a $N_2$ flow rate of 1 sccm, and a $Cu_2O$ (200) phase is then preferentially grown at a higher feeding amount of $N_2$. The optical and electrical properties of $Cu_2O$ thin films are improved with a sufficient $N_2$ flow rate of more than 15 sccm, as confirmed through various analyses. Under this condition, a high bandgap energy of 2.58 eV and a conductivity of $1.5{\times}10^{-2}$ S/cm are obtained. These high-quality $Cu_2O$ thin films are expected to be applied to $Cu_2O$-based heterojunction solar cells and optical functional films.

Studies on the Optimization of Contact Oxide Etching Process Using Taguchi Method (Taguchi 방법을 사용한 콘택 산호막 식각 공정 최적화 연구)

  • Jeon, Yeong-Jin;Kim, Chang-Il;Gu, Jin-Geun;Yu, Hyeong-Jun
    • Korean Journal of Materials Research
    • /
    • v.5 no.1
    • /
    • pp.63-74
    • /
    • 1995
  • Process optimization experiments based on the Taguchi method were performed in order to set up the optimal process conditions for the contact oxide etching process module which was built in order to be attached to the cluster system of multi-processing purpose. From the two times experiments of Taguchi method, the overall behaviors of the etchmg characteristics depending upon the equipment parameters were understood at the 1st Taguchi experiment, the detail and optimal process conditions were extracted from the 2nd Taguchi experiment. As a final analysis of experimental results, the optimal etching characteristics were obtalned at the process conditions of $CHF_{3}/CF_{4}$ gas flow rate=72/8 sccm, chamber pressure=50 mTorr, RF power=300 Watts, magnetic field intensity=90 Gauss.

  • PDF

The Plasma Modification of Polycarbonate and Polyethersulphone Substrates for Ta2O5 Thin Film Deposition (Ta2O5 박막증착에서 플라즈마 전 처리를 통한 Polycarbonate와 Polyethersulphone 기판의 표면 개질)

  • Kang, Sam-Mook;Yoon, Seok-Gyu;Jung, Won-Suk;Yoon, Dae-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.1 s.284
    • /
    • pp.38-41
    • /
    • 2006
  • Surface of PC (Polycarbonate) and PES (Polyethersulphone) treated by plasma modification with rf power from 50 W to 200 W substrates in Ar (3 sccm), $O_2$ (12 sccm) atmosphere. From the results of modified substrates in XPS (X-ray Photoelectron Spectroscopy), the ratio of oxide containing bond increased with rf power. As the rf power was 200 W, the contact angle was the lowest value of 14.09 degree. And the datum from AFM (Atomic Force Microscopy), rms roughness value of PES and PC substrates increased with rf power. We could deposit $Ta_2O_5$ with good adhesion on plasma treated PES and PC substrates using by in-situ rf magnetron sputter.

Properties of TiO$_2$ Thin Film Deposited by LPMOCVD (LPMOCVD 법으로 증착된 TiO$_2$ 박막의 특성)

  • 이하용;박용환;고경현;박정훈;홍국선
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.9
    • /
    • pp.901-908
    • /
    • 1999
  • Effects of LPMOCVD process parameters on the properties of TiO2 thin film were investigated. Depositions were made in the range of temperature 300-67$0^{\circ}C$ with various TTIP(Titanium Tetraisopropoxide) concentrations by contrlling bubbler temperature(40-8$0^{\circ}C$) and/or flow rate(30-90 sccm). Post annealing treatments were carried out at 500-80$0^{\circ}C$ range in the air. Films deposited at 40$0^{\circ}C$ have denser morphology than those of films deposited at 50$0^{\circ}C$ and $600^{\circ}C$ due to slower deposition rate. Bubbler temperature can affect on the deposition rate in mass transfer controlled regime such as 50$0^{\circ}C$ or higher but not below 50$0^{\circ}C$ where surface reaction rate becomes important. On the contrary for films deposited above 50$0^{\circ}C$ flow rate can raise deposition rate but eventually saturate it at the 50 sccm and above due to retarded adhesion of decomposed species. But for films deposited at 40$0^{\circ}C$ deposition rate increases stadily with flow rate. As the film becomes more porous A(200) texture can not be developed and AnataselongrightarrowRutile transition kinetics increases.

  • PDF

Growth characteristics of 4H-SiC homoepitaxial layers grown by thermal CVD (화학기상증착법으로 성장시킨 4H-SiC 동종박막의 성장 특성)

  • Jang, Seong-Joo;Jeong, Moon-Taeg;Seol, Woon-Hag;Park, Ju-Hoon
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1999.06a
    • /
    • pp.271-284
    • /
    • 1999
  • As a semiconductor material for electronic devices operated under extreme environmental conditions, silicon carbides (SiCs) have been intensively studied because of their excellent electrical, thermal and other physical properties. The growth characteristics of single-crystalline 4H-SiC homoepitaxial layers grown by a thermal chemical vapor deposition (CVD) were investigated. Especially, the successful growth condition of 4H-SiC homoepitaxial layers using a SiC-uncoated graphite susceptor that utilized Mo-plates was obtained. The CVD growth was performed in an RF-induction heated atmospheric pressure chamber and carried out using off-oriented substrates prepared by a modified Lely method. In order to investigate the crystallinity of grown epilayers, Nomarski optical microscopy, Raman spectroscopy, photoluminescence(PL), scanning electron microscopy (SEM) and other techniques were utilized. The best quality of 4H-SiC homoepitaxial layers was observed in conditions of growth temperature 1500$^{\circ}C$ and C/Si flow ratio 2.0 of C3H3 0.2sccm & SiH4 0.3sccm. The growth rate of epilayers was about 1.0$\mu\textrm{m}$/h in the above growth condition.

  • PDF

Effect of Sputtering Parameter on the Deposition Behavior of TiO2 Thin Film (TiO2 박막의 증착거동에 미치는 스퍼터링 공정변수의 영향)

  • Kim, Eul-Soo;Lee, Gun-Hwan;Kwon, Sik-Chol;Ahn, Hyo-Jun
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.14 no.1
    • /
    • pp.8-16
    • /
    • 2003
  • $TiO_2$ thin films were deposited by DC reactive magnetron sputtering with variations in sputtering parameter such as Ar and $O_2$ flow rate, DC power, substrate temperature and magnetic field. Deposition rate, crystal structure, chemical bond of $TiO_2$ films on the deposition conditions were investigated by Alpha-step, X-ray Diffractometer(XRD), X-ray Photoelectron Spectroscopy(XPS). When the DC power was applied at 500watt, deposition rate of $TiO_2$ film was about 480A/min. $TiO_2$ films coated under the deposition condition of 15sccm Ar and 7~10sccm $O_2$ flow rate was only observed anatase phase. With increasing substrate temperature from RT to $300^{\circ}C$, crystal orientation of $TiO_2$ films variously became.