• 제목/요약/키워드: manganese slag

검색결과 20건 처리시간 0.028초

콘크리트용 골재로서 실리콘 망간슬래그의 물리적 적합성 평가 (Physical Suitability Evaluation of Silicon manganese slag as Aggregate for Concrete)

  • 정의인;김봉주;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.41-42
    • /
    • 2015
  • The concrete aggregate generates carbon dioxide in production but its demanding is gradually increased in accordance with the depletion of natural resources. Therefore we evaluated compatibility and basic physical properties of Silicon manganese slag generated in iron production as an applicable concrete aggregate. In our test, the silicon maganese slag shows 2.8g/㎥ of density in 10mm of maximum particle size similar to a natural aggregate, and its absorption rate was 0.3% similar to the electric furnace slag. Unit volume weight and ratio of absolute volume was respectively 2,001㎏/㎥ and 51%. Strength properties of Silicon manganese slag will be evaluated with further studies and experiments.

  • PDF

FeO-MnO-CaO-SiO2-MgOsatd. 슬래그에서의 P의 열역학적 거동 (Thermodynamic of Phosphorus in FeO-MnO-CaO-SiO2-MgOsatd. Slag Systems)

  • 조문경;박경호;민동준
    • 대한금속재료학회지
    • /
    • 제47권3호
    • /
    • pp.188-194
    • /
    • 2009
  • Recently, new extraction technology for manganese nodule has been developed as alternative noble metallic resources. It is important to understand thermodynamic behaviors of phosphorus in low basic slag system from the viewpoint of the refining processing optimization. Thermodynamic behaviors of phosphorus in the $FeO-MnO-CaO-SiO_2-MgO_{satd.}$ slag system were investigated at 1723 K with various oxygen potential and slag composition of low basicity. The experimental results for dependence of phosphorus on oxygen potential and slag basicity indicated that the dissolution mechanism of phosphorus into slag of low basicity could be derived as follows; $[P]+5/4O_2+(O^{2-})=({PO_{3.5}}^{2-})$ Present experimental results implied that stability of phosphorus in slag would be depended on both of $O^{2-}$ (basicity) and content of $Ca^{2+}$ in molten slag. The thermodynamic effect of FeO, MnO and $Na_2O$ on low basicity on phosphate capacity was discussed.

망간단괴 용융환원 폐슬래그의 재활용 방안 (Survey on the Recycling of Waste Slag Generated by Smelting Reduction of Deep-Sea Manganese Nodules)

  • 박형규;남철우;김성돈
    • 자원리싸이클링
    • /
    • 제23권4호
    • /
    • pp.69-74
    • /
    • 2014
  • 심해저 망간단괴를 용융환원 제련시 발생된 슬래그에 규사와 cokes를 일정량 배합하여 아크로에서 재용융하여 Fe-Si-Mn 합금철을 제조하는 과정에서 발생하는 2차 슬래그는 아직 특정 용도가 개발되지 않은 폐슬래그로 취급되는데, 이 폐슬래그의 재활용 방안에 대하여 요업 원료로의 활용가능성과 건설재료로의 활용가능성을 검토하였다. 망간단괴 폐슬래그를 포틀랜드시멘트, 캐스타블내화물과 같은 요업원료로 사용하는 것은 조성 차이가 많아서 직접적인 활용이 곤란하고, 다른 활용방법으로서 폐슬래그를 도로 노반재나 성토재 및 복토재 등과 같은 건설재료로 활용하는 것이 무난하다고 판단된다. 도로 건설재료로 사용시 혹시 있을지도 모를 토양 오염에 대비하여 유해물질들에 대한 용출시험을 KS 기준에 따라 수행한 결과 폐슬래그의 무해성을 확인할 수 있었다. 따라서, 망간단괴 폐슬래그를 도로 성토재나 노반재와 같은 건설재료로 활용하는 방안을 제안코자 한다.

슬래그 원료를 사용해서 제조된 유리섬유의 점탄성 특성 (Visco-Elastic Properties of Glass Fiber Manufactured by Slag Material)

  • 이지선;김선욱;라용호;이영진;임태영;황종희;전대우;김진호
    • 한국전기전자재료학회논문지
    • /
    • 제32권6호
    • /
    • pp.477-482
    • /
    • 2019
  • This study investigated the influence of the viscoelastic property of slag when producing glass fiber, MFS631 with 60% of manganese slag, 30% of steel slag, and 10% of silica stone. To fabricate the MFS631 glass bulk, slag materials were placed in an alumina crucible, melted at $1,550^{\circ}C$ for 2 h, and then annealed at $600^{\circ}C$ for 2 h. It was found that glass is non-crystalline through X-ray diffraction analysis. MFS631 fiber was produced at speed in the range of 100~300 rpm at $1,150^{\circ}C$. The loss modulus (G") and storage modulus (G') of the produced glass fiber were evaluated at high temperatures. G' and G" of MFS631 were greater than $893^{\circ}C$, and the modulus value was 136,860 pa. This is similar to the results of a general E-glass fiber graph. Therefore, it was concluded that its spinnability is similar to that of E-glass fiber; therefore, it can be commercialized.

Properties of reduced and quenched converter slag

  • Ko, In-Yong;Ionescu Denisa;T. R. Meadowcroft
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.542-546
    • /
    • 2001
  • Converter slag has some compositional similarities to portland cement. But it has no hydration properties due to it's quite high concentrations of FeO(20-35%), MnO(4-6.5%). So it is needed to reduce the concentrations of iron and manganese of converter slag to use as cement additives by enhancing it's hydration properties. In this study, converter slag was modified it's composition by mixing of silica, alumina and quenched BF slag and reduced in induction furnace and quenched in running water. The hydraulic properties and structures of modified and quenched converter slag are significantly changed depend on the amount and kinds of additives. The addition of alumina up to 10% and BFQ slag up to 20% by weight on converter slag was effective to enhance the hydraulic properties of modified and quenched slag. The addition of reduced and quenched converter slag up to 20% by weight in replacement of portland cement in mixing of concrete mortar were shown higher compressive strength than 100% cement concrete mortar.

  • PDF

Superconducting magnetic separation of ground steel slag powder for recovery of resources

  • Kwon, H.W.;Kim, J.J.;Ha, D.W.;Choi, J.H.;Kim, Young-Hun
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제19권1호
    • /
    • pp.22-25
    • /
    • 2017
  • Steel slag has been considered as an industrial waste. A huge amount of slag is produced as a byproduct and the steel slag usually has been dumped in a landfill site. However the steel slag contains valuable resources such as iron, copper, manganese, and magnesium. Superconducting magnetic separation has been applied on recovery of the valuable resources from the steel slag and this process also has intended to reduce the waste to be dumped. Cryo-cooled Nb-Ti superconducting magnet with 100 mm bore and 600 mm of height was used as the magnetic separator. The separating efficiency was evaluated in the function of magnetic field. A steel slag was ground and analyzed for the composition. Iron containing minerals were successfully concentrated from less iron containing portion. The separation efficiency was highly dependent on the particle size giving higher separating efficiency with finer particle. The magnetic field also effects on the separation ratio. Current study showed that an appropriate grinding of slag and magnetic separation lead to the recovery of metal resources from steel slag waste rather than dumping all of the volume.

황산암모늄에 의한 훼로망간 슬랙으로부터 망간의 전착 (Electrodeposition of Manganese from Ferromanganese Slag with Ammonium Sulfate)

  • 김덕묵
    • 대한화학회지
    • /
    • 제29권4호
    • /
    • pp.390-396
    • /
    • 1985
  • 황산암모늄을 이용하여 훼로망간슬랙중에 망간만을 분리, 추출하고 황화암모늄으로 정제한 후 소량의 $H_2SeO_3$를 첨가제로 가하여 환원전극으로는 Stainless steel판을, 산화전극으로는 납(Pb + 1% Ag)전극을 이용하여 60mA/cm$^2$정도의 전류밀도에서 90%이상의 전류효율로 순수한 망간금속을 얻었다.

  • PDF

망간슬래그의 비소에 대한 수착특성 연구 (Characterization of Arsenic Sorption on Manganese Slag)

  • 설정우;김성희;이우춘;조현구;김순오
    • 한국광물학회지
    • /
    • 제26권4호
    • /
    • pp.229-244
    • /
    • 2013
  • 비소의 오염은 다양한 자연적 또는 인위적 원인들로 인하여 발생할 수 있다. 비소의 자연상 다양한 화학종 중 3가와 5가 형태로 대부분 존재하고, 비소의 거동은 Al, Fe, Mn 산화물 등에 의해 영향을 받는다. 이에 본 연구는 Mn, Si, Ca 등의 성분이 많이 포함된 망간슬래그를 이용한 비소 수착특성을 규명하기 위해 수행되어졌다. 망간슬래그의 수착제로서의 주요한 특성을 조사하고 평형론과 반응 속도론 실험을 통해 비소 화학종별 수착양상을 고찰하였다. 망간슬래그의 비표면적은 $4.04m^2/g$, 전위차 적정법에 의해 측정된 영전하점(point of zero salt effect, PZSE)은 7.73으로 측정되었다. pH 4, 7, 10의 조건으로 두 비소 화학종의 수착반응에 대한 평형실험 결과 3가 비소보다 5가 비소가 수착량이 더 컸으며 망간슬래그와의 친화력이 더 높은 것으로 나타났다. 3가 비소는 pH 7에서, 5가 비소는 pH 4에서 수착량이 가장 높게 나타났는데 이는 pH에 따른 두 비소 화학종의 존재형태와 망간슬래그의 표면전하 간 상호작용에 기인한 것이다. 수착반응은 3가 비소와 5가 비소 모두 2시간 이내에 최대 수착량에 도달하였고, 반응속도 실험결과를 다양한 반응속도 모델들에 모사하였을 때, 유사이차(pseudo-second-order)와 포물선(parabolic) 모델이 가장 적합한 모델로 조사되었다.

망간단괴 용융환원 제련공정의 물질 및 열수지 모델링 (A Study on the Heat and Mass Balance of Smelting Reduction Process for Manganese Nodules)

  • 조문경;박경호;민동준
    • 대한금속재료학회지
    • /
    • 제47권5호
    • /
    • pp.304-310
    • /
    • 2009
  • Recently, manganese nodule has been focused on alternative resources because of its high grade of noble metallic elements such as Co, Ni, and Cu etc. From the viewpoint of an optimization the operating variables for energy efficiency of smelting reduction process, thermodynamic model for smelting reduction process of Manganese nodule was developed by using energy and material balance concept. This model provided that specific consumption of pure oxygen and coke was strongly depended on post combustion ratio (PCR) and heat transfer efficiency (HTE). The dressing and dehydrating process of low grade manganese can be proposed an essential process to minimize the specific energy consumption with decreasing slag volume. The effect of electricity coal base smelting reduction process was also discussed from the energy optimizing point of view.

테르밋 반응을 이용한 페로망간 전기로 분진의 재활용에 관한 연구 (Recovery of manganese compounds from electric arc furnace dust by Aluminothermy Process)

  • 하태영;조영민;박영구;김윤채
    • 한국응용과학기술학회지
    • /
    • 제32권1호
    • /
    • pp.23-30
    • /
    • 2015
  • The properties of dust collected from electric arc furnace of ferro manganese production units was investigated, and also the metallic manganese was recovered from the dust by aluminothermy process. The ferromanganese dust collected from electric arc furnace contained about 15% of manganese oxide ($Mn_3O_4$) and 9% of carbon as the contaminant, and have a 5um of 50% median diameter and irregular particle shape. The carbon contaminant in the dust could be reduced until about 0.1~0.5% level by roasting in the air at a temperature of 600~900C for 60minutes. The recovery of manganese could not be carried out using only ferromanganese dust from electric arc furnace by aluminothermy process, but the ferromanganese which contained manganese of about 92% and iron of about 5% could be obtained from the mixture of ferromanganese dusts from electric arc furnace and converter. The best mixing condition of dust fixed at electric arc furnace dust / converter dust ratio of 1:9 and 2:8, and the mixing rato of 3:7 or more could not separated the metal and slag from the reactant after aluminothermy reaction.