Flame Retardancy of Polypropylene/Montmorillonite Nanocomposites with Halogenated Flame Retardants (할로젠 계열의 난연제가 첨가된 폴리프로필렌/몬모릴로나이트 나노복합재료의 난연특성)

  • 이종훈;나중현;이대회;김명덕;공정호;이영관;남재도
    • Polymer(Korea)
    • /
    • v.27 no.6
    • /
    • pp.569-575
    • /
    • 2003
  • The flame retardancy was investigated when the halogenated flame retardant, decabromodiphenyl oxide (DBDPO) and chlorinated paraffin wax (CPW), was added to the polypropylene (PP) / montmorillonite (MMT) nanocomposites. The flame retardancy of polymer resin could be improved not only by addition of flame retardant but also with nanoparticles compositions. The effect of the contents of flame retardant and nanoparticles on the flame retardancy of polypropylene/ montmorillonite nanocomposite systems was thoroughly examined in terms of limited oxygen index (LOI) and cone calorimetry. As a results of cone calorimetry, the heat release rate (HRR) was reduced by the flame retardant DBDPO and CPW, and CPW was a little better than DBDPO. The LOI increased from flammable region (LOI<19) to nonflammable region (LOI>20) for all the flame retardants used in this study. Especially, the improvement in flame retardancy by compounding with PP and MMT was better than that by adding flame retardant to polypropylene. So, the addition of flame retardant after compounding with montmorillonite was more efficient than simple addition of flame retardant.

Fire Resistance and Thermal Stability Study of Fire-Retarded Polypropylene Systems by Using Cone Calorimeter and Thermogravimetry (콘 칼로리미터와 TGA를 이용한 할로겐 계통의 난연제를 첨가한 폴리프로필렌 수지의 난연성 및 열 안정성에 관한 연구)

  • 곽성복;정찬화;남재도;김준형;최미애
    • Polymer(Korea)
    • /
    • v.24 no.6
    • /
    • pp.777-786
    • /
    • 2000
  • Fire resistance and thermal stability of polypropylene composite systems were investigated by using several halogenated fire-retardants such as decabromodiphenyl oxide (DBDPO) and chlorinated paraffin wax (CPW). The fire resistance of composite systems was thoroughly examined by measuring limited oxygen index (LOI, ASTM D2863, ISO 4589) and characteristic properties of cone calorimetry(ASTM E1354, ISO 5660) heat release rates (HRR), time to ignition (TTI), total heat release (THR), effective heat of combustion (EHC), mass loss rates, etc. Comparing the cone calorimetry experimental results of the halogen flame retardants, DBDPO exhibited twice higher efficiency than CPW in polypropylene systems, and the LOI also showed similar trends to cone calorimetry. The thermo-oxidative stability of the composite systems was increased about 30-5$0^{\circ}C$ in thermogravimetry analysis.Collectively, the combustion, extinction and thermally-stable characteristics of flame retardants were identified in this study.

  • PDF

Study on Flame Retardancy and Thermal Resistance Properties of Phenolic Foam and Polyurethane Foam (페놀 폼과 폴리우레탄 폼의 난연 및 내열성 연구)

  • Lee, Ju-Chan;Seo, Jung-Seok;Kim, Sang Bum
    • Journal of the Korean Institute of Gas
    • /
    • v.17 no.1
    • /
    • pp.35-41
    • /
    • 2013
  • In this study, flame retardancy of polyurethane foam and phenolic foam were investigated by addition of phosphorous flame retardants. The thermal degradation behavior of polyurethane foam and phenolic foam in the presence of flame retardants has been studied by thermogravimetric analysis(TGA). Heat release rate(HRR), mean HRR, mass loss rate(MLR), total smoke released(TSR) and limited oxygen index(LOI) were tested by cone calorimeter. From the test results, Phenolic foam showed low HRR, MLR and TSR than polyurethane foam.

Study on the Oil Resistance, Morphological and Dynamic Mechanical Properties, Flame Retardance of Ethylene Vinyl Acetate Copolymer and Ethylene Propylene Rubber Compounds

  • Sung, Il Kyung;Lee, Won Ki;Park, Chan Young
    • Elastomers and Composites
    • /
    • v.52 no.1
    • /
    • pp.27-34
    • /
    • 2017
  • In this experiment, blends of ethylene vinyl acetate rubber (EVM) with a vinyl acetate (VA) content greater than 40 wt% and ethylene propylene rubber (EPM) were prepared by mechanical mixing; a number of parameters of the blends, including oil resistance, morphological and dynamic mechanical properties and flame retardancy, were subsequently measured. In the $100^{\circ}C$ oil resistance test, both the ammonium polyphosphate/dipentaerythritol/expandable graphite (APP/DPER/EG) and aluminum hydroxide (ATH) flame retardant systems showed an increase in volume change with increasing EPM content. For the ATH system, the dispersion shape was coarse and aggregation was observed. The results of a dynamic mechanical test showed slightly higher E' and E'' for the APP/DPER/EG flame retardant system when compared to the single ATH system. For both the APP/DPER/EG and ATH systems, the limited oxygen index (LOI) tests performed at increasing content of EPM showed a LOI value higher than 30, indicating excellent flame resistance.

Flame-retardant Finish of Cotton Fabrics Using UV-curable Phosphorous-containing Monomers (자외선 경화형 인계 단량체를 이용한 면직물의 방염가공)

  • Jang, Jin-Ho;Jeong, Yong-Kyun
    • Textile Coloration and Finishing
    • /
    • v.20 no.4
    • /
    • pp.8-14
    • /
    • 2008
  • Flame-retardant cotton fabrics were prepared by UV curing of photocurable aqueous formulations of phosphorous-containing methacrylate monomers and 2-hydroxy-2-methyl-1-phenyl-1-propanone as flame retardants and a photoinitiator respectively, which is an environmentally friendly and energy-saving process. The characterization of the UV-coated cotton fabric was made by ATR, TGA and limited oxygen index measurement. UV cured coating onto cotton fabrics reduced the first thermal decomposition temperature and mass loss as well as increase in the amount of char residue compared with the untreated cotton fabric presumably due to modified thermal decomposition process. The LOI values up to 28.5 and 27.2 were obtained by the UV curing of MMEP and TMEP respectively. The treatment was durable to five laundering cycles, which was more prominent in the case of trifunctional TMEP treatment.

Influence of Fluoro-illite on Flame Retardant Property of Epoxy Complex (에폭시 복합체의 난연 특성에 미치는 불소화 일라이트의 영향)

  • Yu, Hye-Ryeon;Jeong, Eui-Gyung;Kim, Jin-Hoon;Lee, Young-Seak
    • Polymer(Korea)
    • /
    • v.35 no.1
    • /
    • pp.47-51
    • /
    • 2011
  • In this study, illite, an environmental friendly, low cost, and high aspect ratio additive, was used to improve flame retardant property of epoxy and it was fluorinated to enhance dispersion of hydrophilic illite in hydrophobic epoxy by introducing hydrophobic functional groups. Fluorination of illite enhanced illite dispersion ill epoxy solution before curing and that in the complex after curing. These enhanced dispersions were attributed to the increased affinity of illite to hydrophobic epoxy solution induced by fluorination of illite and the increased intercalation of epoxy polymer or exfoliation of illite by epoxy curing. Hence, limited oxygen index(LOI) of fluorinated illite/epoxy complex increased by 24%, compared to that of epoxy, suggesting that the preparation of fluorinated illite/epoxy complex increased their flame retardant properties.

A Study on Combustion Characteristics in each Coating Thickness of Fire Retardant Paints (난연도료의 도포 두께별 연소특성에 관한 연구)

  • Kim, Hong;Park, Hyung-Ju
    • Fire Science and Engineering
    • /
    • v.17 no.4
    • /
    • pp.36-41
    • /
    • 2003
  • This experimental study shows the combustion characteristics for each coating thickness of water and oil paint which are used as fire retardant paints that prevent fire propagation through cables in underground culverts and trays. To evaluate combustion characteristics, smoke density(ASTM E 662) and Limited Oxygen Index(ASTM D 2863) experiment method was used. As the results of this study, the combustion characteristics of fire retardant paints produced the following : (a) The molt suitable coating thickness of fire retardant paint was 1.5∼2.0 mm in water paint and 0.2 mm in oil paint. (b) Flaming method in experiments of smoke density were found to be higher than Non-flaming method. (c) Water paint has the fire retardant effect and characteristics better than oil paint in measurement results of smoke density and oxygen index. (d) The oxygen index of water and oil fire retardant was able to know that it was satisfied a standard (30 or above).

Effects of NaCl/H3PO4 Flame Retardant Treatment on Lyocell Fiber for Thermal Stability and Anti-oxidation Properties (NaCl/H3PO4 내염화 처리가 라이오셀 섬유의 열 안정 및 내산화 특성에 미치는 영향)

  • Kim, Eun Ae;Bai, Byong Chol;Jeon, Young-Pyo;Lee, Chul Wee;Lee, Young-Seak;In, Se Jin;Im, Ji Sun
    • Applied Chemistry for Engineering
    • /
    • v.25 no.4
    • /
    • pp.418-424
    • /
    • 2014
  • The improved thermal stability and anti-oxidation properties of Lyocell fiber were studied based on flame retardant treatment by using NaCl/$H_3PO_4$ solution. The optimized conditions of flame retardant treatment were studied on various maxing ratio of NaCl and $H_3PO_4$ and the mechanism was proposed through experimental results of thermal stability anti-oxidation. The IPDT (integral procedural decomposition temperature), LOI (limited oxygen index) and $E_a$ (activation energy) increased 23, 30 and 24% respectively via flame retardant treatment. It is noted that thermal stability and anti-oxidation improved based on char and carbon layer formation by dehydrogenation and dissociation of C-C bond resulting the hindrance of oxygen and heat energy into polymer resin. The optimized conditions for efficient flame retardant property of Lyocell fiber were provided using NaCl/$H_3PO_4$ solution and the mechanism was also studied based on experimental results such as IDT (initial decomposition temperature), IPDT, LOI and $E_a$.

Flame Retardant Properties of Basalt Fiber Reinforced Epoxy Composite with Inorganic Fillers (무기 필러가 첨가된 현무암섬유 강화 에폭시 복합재료의 난연 특성)

  • Mun, So Youn;Lee, Su Yeon;Lim, Hyung Mi
    • Composites Research
    • /
    • v.32 no.6
    • /
    • pp.368-374
    • /
    • 2019
  • Basalt fiber reinforced epoxy composites with inorganic filler (BFRP-F) such as Mg(OH)2 (magnesium hydroxide), Al(OH)3 (aluminum hydroxide), Al2O3 (aluminum oxide) and AlOOH (boehmite) were prepared by hand lay-up and hot pressing. The combustive properties of BFRP-F were improved comparing with basalt fiber reinforced epoxy composite (BFRP) without inorganic filler. At a 30 wt% resin content, the limited oxygen index (LOI) of BFRP is 28.9, which is higher than that of epoxy (21.4), and the LOI of BFRP-F is higher than that of BFRP. The BFRP-F showed the lower peak heat release rate (PHRR), total heat release (THR) and total smoke release rate (TSR) than those of BFRP. We confirmed that the flame retardant properties of the composite were improved by the addition of inorganic filler through the dehydration reaction and oxide film formation.

Preparation of Flammability Artificial Hair based on Super Engineering Plastic (슈퍼엔지니어링 플라스틱 기반 난연성 가발사 제조)

  • Choi, Hyun-Jung;Gong, Da Jeong;Youn, Chulmin;Yeo, Sang Young
    • Textile Coloration and Finishing
    • /
    • v.32 no.2
    • /
    • pp.103-110
    • /
    • 2020
  • Super engineering plastic(SEP) are applied to high performance and high value industries due to their excellent mechanical properties and high continuous operating temperature. Among them, PES and PEI are amorphous SEPs, and have the advantages of high flexibility, mechanical properties, transparency, and thermal stability. In this study, polyethersulfone(PES) and polyetherimide(PEI) fibers were manufactured to produce flame retardant artificial hair. PES and PEI fibers prepared through a melt-spinning process at a high temperature of 360 to 420℃. They are compared with commercial artificial hair by thermal gravimetric analysis(TGA), linear density, tenacity, and limited oxygen index(LOI) analysis. PES and PEI fibers have similar linear density and tenacity to commercial artificial hair, while their thermal stability and flame retardant are excellent. In particular, flame retardant was analyzed through LOI value and PES was 35.1%, which is superior to commercial artificial hair PET/Br(28.2%) and PET/P(20.2%). Therefore, PES and PEI are suitable as artificial hair for flame retardant.