• 제목/요약/키워드: layers

검색결과 11,783건 처리시간 0.035초

유리 기판에 Catalytic CVD 저온공정으로 제조된 나노급 니켈실리사이드와 결정질 실리콘 (Nano-thick Nickel Silicide and Polycrystalline Silicon on Glass Substrate with Low Temperature Catalytic CVD)

  • 송오성;김건일;최용윤
    • 대한금속재료학회지
    • /
    • 제48권7호
    • /
    • pp.660-666
    • /
    • 2010
  • 30 nm thick Ni layers were deposited on a glass substrate by e-beam evaporation. Subsequently, 30 nm or 60 nm ${\alpha}-Si:H$ layers were grown at low temperatures ($<220^{\circ}C$) on the 30 nm Ni/Glass substrate by catalytic CVD (chemical vapor deposition). The sheet resistance, phase, microstructure, depth profile and surface roughness of the $\alpha-Si:H$ layers were examined using a four-point probe, HRXRD (high resolution Xray diffraction), Raman Spectroscopy, FE-SEM (field emission-scanning electron microscopy), TEM (transmission electron microscope) and AES depth profiler. The Ni layers reacted with Si to form NiSi layers with a low sheet resistance of $10{\Omega}/{\Box}$. The crystallinty of the $\alpha-Si:H$ layers on NiSi was up to 60% according to Raman spectroscopy. These results show that both nano-scale NiSi layers and crystalline Si layers can be formed simultaneously on a Ni deposited glass substrate using the proposed low temperature catalytic CVD process.

Improvement of pavement foundation response with multi-layers of geocell reinforcement: Cyclic plate load test

  • Khalaj, Omid;Tafreshi, Seyed Naser Moghaddas;Mask, Bohuslav;Dawson, Andrew R.
    • Geomechanics and Engineering
    • /
    • 제9권3호
    • /
    • pp.373-395
    • /
    • 2015
  • Comprehensive results from cyclic plate loading at a diameter of 300 mm supported by layers of geocell are presented. The plate load tests were performed in a test pit measuring $2000{\times}2000mm$ in plane and 700 mm in depth. To simulate half and full traffic loadings, fifteen loading and unloading cycles were applied to the loading plate with amplitudes of 400 and 800 kPa. The optimum embedded depth of the first layer of geocell beneath the loading plate and the optimum vertical spacing of geocell layers, based on plate settlement, are both approximately 0.2 times loading plate diameter. The results show that installation of the geocell layers in the foundation bed, increase the resilient behavior in addition to reduction of accumulated plastic and total settlement of pavement system. Efficiency of geocell reinforcement was decreased by increasing the number of the geocell layers for all applied stress levels and number of cycles of applied loading. The results of the testing reveal the ability of the multiple layers of geocell reinforcement to 'shakedown' to a fully resilient behavior after a period of plastic settlement except when there is little or no reinforcement and the applied cyclic pressure are large. When shakedown response is observed, then both the accumulated plastic settlement prior to a steady-state response being obtained and the resilient settlements thereafter are reduced. The use of four layers of geocell respectively decreases the total and residual plastic settlements about 53% and 63% and increases the resilient settlement 145% compared with the unreinforced case. The inclusion of the geocell layers also reduces the vertical stress transferred down through the pavement by distributing the load over a wider area. For example, at the end of the load cycle of the applied pressure of 800 kPa, the transferred pressure at the depth of 510 mm is reduced about 21.4%, 43.9%, 56.1% for the reinforced bases with one, two, and three layers of geocell, respectively, compared to the stress in the unreinforced bed.

귀리 사일리지의 비닐겹수 및 저장기간에 따른 발효품질 (Effect of Number of Film Layers and Storage Duration and on the Fermentation Quality of Whole Crop Oat Silage)

  • 송태화;박종호;윤창;강천식;손재한;윤영미;김양길;정영근;박태일
    • 한국초지조사료학회지
    • /
    • 제38권1호
    • /
    • pp.1-6
    • /
    • 2018
  • 이 연구는 저장기간 및 비닐겹수에 따른 귀리 사일리지의 사료가치 및 사일리지 품질특성을 구명하고자 수행하였다. 귀리 사일리지의 조단백질 함량은 저장기간 모두 사일리지 제조 전에 비해 높아지는 경향을 보였고, 저장기간이 길어질수록 높은 값을 보였지만 통계적인 유의성은 없었다. 비닐겹수에 따라서는 6겹 처리한 처리구가 4겹보다 높은 경향이었다. NDF와 ADF 함량 역시 저장기간 모두 사일리지 제조 전보다 높은 경향을 보였고, 저장기간 및 비닐겹수에 따라서는 비슷하였다. TDN 함량은 저장기간 모두 사일리지 제조 전보다 낮은 경향이었고, 저장기간 및 비닐겹수에 따라서는 비슷한 값을 보였다. pH는 저장기간이 길어짐에 따라 낮아지는 경향을 보였고, 비닐겹수에 따라서는 6겹에서 낮은 값을 보였다. 유기산 함량에서는 저장기간이 길어짐에 따라 젖산함량과 초산함량은 약간 증가하는 경향을 보였고, 낙산함량은 유의적으로 증가하는 경향이었다(p<0.05). 비닐겹수에 따라서는 6겹에서 4겹보다 높은 젖산함량과 낮은 낙산함량을 보였다(p<0.05). 따라서 귀리 사일리지는 4겹으로 처리했을 경우에는 6개월 안에 사용하고, 장기저장을 고려한다면 6겹이상으로 처리하는 것이 바람직하다고 판단된다.

Characterizing buckling behavior of matrix-cracked hybrid plates containing CNTR-FG layers

  • Lei, Zuxiang;Zhang, Yang
    • Steel and Composite Structures
    • /
    • 제28권4호
    • /
    • pp.495-508
    • /
    • 2018
  • In this paper, the effect of matrix cracks on the buckling of a hybrid laminated plate is investigated. The plate is composed of carbon nanotube reinforced functionally graded (CNTR-FG) layers and conventional fiber reinforced composite (FRC) layers. Different distributions of single walled carbon nanotubes (SWCNTs) through the thickness of layers are considered. The cracks are modeled as aligned slit cracks across the ply thickness and transverse to the laminate plane, and the distribution of cracks is assumed statistically homogeneous corresponding to an average crack density. The first-order shear deformation theory (FSDT) is employed to incorporate the effects of rotary inertia and transverse shear deformation, and the meshless kp-Ritz method is used to obtain the buckling solutions. Detailed parametric studies are conducted to investigate the effects of matrix crack density, CNTs distributions, CNT volume fraction, plate aspect ratio and plate length-to-thickness ratio, boundary conditions and number of layers on buckling behaviors of hybrid laminated plates containing CNTR-FG layers.

열증착방법에 의해 제조된 Si(100)/X(500$\AA$)/Zn(1000$\AA$) 이중박막 성장에 관한 연구 (A Study on the growth of Si(001)/X(500$\AA$)/Zn(1000$\AA$) double layers deposited by thermal evaporation process.)

  • 신동원;정순종;이동윤;민복기;정원섭;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.1026-1029
    • /
    • 2001
  • Zinc films have been deposited onto various buffer layers, Al, Al-Cu, Ag and Ag-Al, by vacuum evaporation method in order to investigate the film microstructure and its consequence on the film growth. Zn films were grown onto Al buffer layers with faster rates than on Ag buffer layers, because of the presence of preferred growth orientation. Especially, in the Zn film formation on the Ag layers, intermetallic compounds AgZn was formed to cause the different growth orientation from Zn film obtained on the Al layers.

  • PDF

A STRESS ANALYSIS FOR A COATED FUEL PARTICLE OF A HTGR USING A FINITE ELEMENT METHOD

  • Kim, Young-Min;Cho, Moon-Sung
    • Nuclear Engineering and Technology
    • /
    • 제41권8호
    • /
    • pp.1087-1100
    • /
    • 2009
  • A finite element method utilizing the Galerkin form of the weighted residuals procedure was developed to estimate the mechanical behavior for a coated fuel particle (CFP) of a high temperature gas-cooled reactor (HTGR). Through a weak formulation, finite element equations for multiple layers were set up to calculate the displacements and stresses in a CFP. The finite element method was applied to the stress analyses for three coating layers of a tri-isotropic coated fuel particle (TRISO) of a HTGR. The stresses calculated by the finite element method were in good agreement with those from a previously developed computer code and depicted the typical stress behavior of the coating layers very well. The newly developed finite element method performs a stress analysis for multiple bonded layers in a CFP by changing the material properties at any position in the layers during irradiation.

경사진 원형 수층에서의 자연대류 열전달 (Natural Convection Heat Transfer in Inclined Cylindrical Water Layers)

  • 장병훈
    • 설비공학논문집
    • /
    • 제15권10호
    • /
    • pp.787-794
    • /
    • 2003
  • The effect of inclination angle on natural convection heat transfer has been studied for water layers. The range of the Raleigh number was from the subcritical value to 1.4${\times}$10$^{7}$ , and the range of the inclination angle, $\theta$, measured from the horizontal was 0$\leq$$\theta$$\leq$180$^{\circ}$. For horizontal water layers, present results agreed well with the results of previous investigators and also showed significant departures from the results of air layers in the turbulent regime. Inclined cylindrical water layers showed secondary maxima in heat transfer, whereas rectangular air layers showed continuous decline of Nusselt number.

최적화된 전자 수송층을 활용한 완전한 용액공정 기반 녹색 유기발광다이오드 (Fully Solution-Processed Green Organic Light-Emitting Diodes Using the Optimized Electron Transport Layers)

  • 한주원;김용현
    • 한국전기전자재료학회논문지
    • /
    • 제31권7호
    • /
    • pp.486-489
    • /
    • 2018
  • Solution-processed organic light-emitting diodes (OLEDs) have the advantages of low cost, fast fabrication, and large-area devices. However, most studies on solution-processed OLEDs have mainly focused on solution-processable hole transporting materials or emissive materials. Here, we report fully solution-processed green OLEDs including hole/electron transport layers and emissive layers. The electrical and optical properties of OLEDs based on solution-processed TPBi (2,2',2"-(1,3,5-Benzinetriyl)-tris(1-phenyl-1-H-benzimidazole)) as the electron transport layer were investigated with respect to the spin speed and the number of layers. The performance of OLEDs with solution-processed TPBi exhibits a power efficiency of 9.4 lm/W. We believe that the solution-processed electron transport layers can contribute to the development of efficient fully solution-processed multilayered OLEDs.

무전해 Ni-P-X(X : $Al_2O_3$, Diamond) 복합도금층의 내마모성 (A Wear Resistance of Electroless Ni-P-X(X : $Al_2O_3$, Diamond) Composite Coating Layers)

  • 김만;장도연;노병호;한성호;이규환
    • 연구논문집
    • /
    • 통권22호
    • /
    • pp.151-160
    • /
    • 1992
  • The wear resistance of electroless Ni-P-X(X A1203, Diamond) composite coating layers was studied by Taber abrasion test technique. The wear resistance of composite coating layers was particularly relied upon the codeposited content, particle size and distribution of particles, and heat treatment of coating layers, as well as the electroless nickel plating bath employed. In this study, we lay emphasis on the wear resistance of electroless composite coating layers containing A1203 particles(1.2~Im, 6.7hIm, 11.5lIm, 20l1m) or diamond particles (1.5jim, 5gm). From the result of composite coating A1203 and diamond particles, the wear resistance of composite coating layers is as follows.

  • PDF

내부의 주름설치에 따른 탄소섬유튜브 보의 성능에 대한 실험적 연구 (An Experimental Study on the Structural Capacity of Carbon Tube Beams According to the Existence of Corrugation)

  • 윤병문;박진영;이경훈;홍원기;김희철
    • 한국지진공학회:학술대회논문집
    • /
    • 한국지진공학회 2003년도 추계 학술발표회논문집
    • /
    • pp.141-146
    • /
    • 2003
  • An experimental investigation was conducted to estimate the flexural behavior of circular concrete beams confined by carbon sheet tube under the loading and unloading cycles. Six specimens were produced with different layers of carbon sheets and with or without corrugations inside of tubes. The experimental results represented that the load and displacement capacity are increased in the specimens which have increased layers of tube and have installed corrugations inside of tubes. In order to obtain enough capacity, tubes have to keep tubes at proper layers but it can not affect positively more than certain layers to increase the layers of tube. Therefore, appropriate estimation of structural member is needed to obtain enough capacity and displacement by means of proper carbon sheet direction and layers of tube.