A Study on the Mechanical Properties of Joints in Laser Transmission Joining of Polymers (폴리머의 레이저 투과접합 시 접합부의 기계적 성질에 관한 연구)

  • Cha, Sang-Woo;Kim, Jin-Beom;Yoon, Suk-Hwan;Na, Suck-Joo
    • Journal of Welding and Joining
    • /
    • v.25 no.2
    • /
    • pp.43-48
    • /
    • 2007
  • Laser Transmission Joining (LTJ) of plastics is a process in which light of suitable wavelength is transmitted through a transparent substrate that is in contact with an absorbing one. In this paper, LTJ is investigated by preliminary experiments from the viewpoint of mechanical engineering. To understand transmitting characteristics of each polymer substrate, transmission rate, reflection rate and absorption coefficient of polymer are measured by using a laser power-meter. Characteristics of joining in the spot welding and seam welding are investigated by measuring the fracture load. Fracture load increases in accordance to the laser power and irradiation time. However, when the laser power is over 60W and irradiation time over 4seconds, fracture load decreases. This phenomenon is probably due to heat-softening of materials. Besides, cavities are generated at a joint by evaporation of water molecules, which can be suppressed by introduction of a gap between two substrates.

Experimental testing of cold-formed built-up members in pure compression

  • Biggs, Kenneth A.;Ramseyer, Chris;Ree, Suhyun;Kang, Thomas H.-K.
    • Steel and Composite Structures
    • /
    • v.18 no.6
    • /
    • pp.1331-1351
    • /
    • 2015
  • Cold-formed built-up members are compression members that are common in multiple areas of steel construction, which include cold-formed steel joints and stud walls. These members are vulnerable to unique buckling behaviors; however, limited experimental research has been done in this area. Give this gap, experimental testing of 71 built-up members was conducted in this study. The variations of the test specimens include multiple lengths, intermediate welds, orientations, and thicknesses. The experimental testing was devised to observe the different buckling modes of the built-up C-channels and the effects of the geometrical properties; to check for applicability of multiple intermediate welding patterns; and to evaluate both the 2001 and 2007 editions of the American Iron and Steel Institute (AISI) Specification for built-up members in pure compression. The AISI-2001 and AISI-2007 were found to give inconsistent results that at times were un-conservative or overly conservative in terms of axial strength. It was also found that orientation of the member has an important impact on the maximum failure load on the member.

The Application of 3-dimensional Surface Imaging to the Early Detection of Sacroiliitis (3차원 영상기법을 이용한 천장골염의 조기 진단)

  • Jeon, Jae-Han;Kim, Seon-Il;Lee, Du-Su
    • Journal of Biomedical Engineering Research
    • /
    • v.14 no.3
    • /
    • pp.235-242
    • /
    • 1993
  • In the early stage of sacroilitis, it is'difficult to detect sacroiliac(Sl) abnormalities by conventional plain X-ray even though there are characteristic symptoms of ankylosing spondylitis. 3 dimensional volume rendering from the CT image was performed to make an early de tection of the structural changes of Sl joint. 2 cases who had clinical impression of ankylosing spondylitis without sacroilitis in plane X-ray and 1 case of typical ankylosing spondylitis as well as 1 case of normal control were studied. The Sl Joints were separated and each joint surface of sacrum and ilium was independently reconstructed by a special 3D manipulation program. All 2 patiant who complained of inflammatory lower back pain with no abnormal findings in the plain X-ray showed structural changes in 3 dimensionally reconstructed surface Image of the Sl joint compared to the normal control. Authors tried several parameters, such as fourler analysis of each surface and the mean and variance of Sl joint gap. We couldn't tell the statistical significance because of the limited number of cases. However, the parameters showed difference according to the progression of disease.

  • PDF

Morphological and Biomechanical Study of the Pulley System of the Thumb

  • Kim, Ji-Won
    • Physical Therapy Korea
    • /
    • v.12 no.4
    • /
    • pp.33-40
    • /
    • 2005
  • The purpose of this study was to define more precisely the anatomy of the thumb flexor pulley system and to determine the relative contribution of each of the pulleys to the biomechanics of thumb motion at the metacarpophalangeal (MP) and interphalangeal (IP) joints. For this, 22 hands from 11 cadavers were used and randomly assigned to two groups. In the first group, the first annular (A1) pulley was cut first followed by the variable annular (Av) pulley and then the oblique pulley. In the second group, the oblique pulley was cut first followed by the, pulley and then the Av pulley. In 7 of 22 hands, it was a transverse structure parallel to the, pulley with a gap between the A1 and Av pulleys, referred to here as type I. In 9 hands, the A1 and Av pulleys were connected without any gap (type II). In 6 hands, the space between the A1 and Av pulleys were triangular in shape with fibers of the Av pulley converging toward the radial side (type III). In biomechanical study of both first and second experiments, there was no significant difference in MCP joint flexion between the all intact, A1 section, A1/Av section, A2 intact (A1/Av/oblique section), and no pulley configuration (p>.05). In occurring displacements less than 10 mm, there was no significant difference in IP joint flexion (p>.05). However, there was a significant decrease in IP joint flexion occurred in both 15 mm and 20 mm excursion (p<.05), when the oblique pulley was resected additionally after cutting the A1 and Av pulleys in first experiment, and when the A1 pulley was resected additionally after cutting the oblique pulley. According to the results, the injury of only the oblique pulley does not decrease thumb motion significantly. The oblique pulley injury with both the A1 and Av pulleys laceration decreased thumb motion significantly. The additional laceration of the A2 pulley does not decrease thumb motion.

  • PDF

SEISMIC ISOLATION OF LEAD-COOLED REACTORS: THE EUROPEAN PROJECT SILER

  • Forni, Massimo;Poggianti, Alessandro;Scipinotti, Riccardo;Dusi, Alberto;Manzoni, Elena
    • Nuclear Engineering and Technology
    • /
    • v.46 no.5
    • /
    • pp.595-604
    • /
    • 2014
  • SILER (Seismic-Initiated event risk mitigation in LEad-cooled Reactors) is a Collaborative Project, partially funded by the European Commission in the $7^{th}$ Framework Programme, aimed at studying the risk associated to seismic-initiated events in Generation IV Heavy Liquid Metal reactors, and developing adequate protection measures. The project started in October 2011, and will run for a duration of three years. The attention of SILER is focused on the evaluation of the effects of earthquakes, with particular regards to beyond-design seismic events, and to the identification of mitigation strategies, acting both on structures and components design. Special efforts are devoted to the development of seismic isolation devices and related interface components. Two reference designs, at the state of development available at the beginning of the project and coming from the $6^{th}$ Framework Programme, have been considered: ELSY (European Lead Fast Reactor) for the Lead Fast Reactors (LFR), and MYRRHA (Multi-purpose hYbrid Research Reactor for High-tech Applications) for the Accelerator-Driven Systems (ADS). This paper describes the main activities and results obtained so far, paying particular attention to the development of seismic isolators, and the interface components which must be installed between the isolated reactor building and the non-isolated parts of the plant, such as the pipe expansion joints and the joint-cover of the seismic gap.

An Availability Analysis on the Gap K-Joints using High Strength Circular Hollow Section Members (고강도 원형강관 갭K형 접합의 사용성 해석)

  • Ahn, Kwan-Su;Choi, Byong-Jeong;Oh, Young-Suk;Kim, Jae-Woon
    • Journal of Korean Society of Steel Construction
    • /
    • v.22 no.2
    • /
    • pp.109-119
    • /
    • 2010
  • There are many restrictions in the application of high-strength HSSs, including yield strength and yield ratio for the 600-MPa steel. The AISC and Canadian codes recommend that the yield strength and yield ratio of HSS members be 360 MPa and 80%, respectively. It is important to understand the true buckling behaviors of HSSs using high-strength steel at the limit states. There are many experimental data regarding the rectangular HSSs, and the circular ones are not enough for high-strength steel. Therefore, this study was conducted to create a better understanding of the buckling behaviors of the 600- and 400-MPa steels based on the results of the finite-element analysis that was done before the experiment. To understand the structural behaviors of the aforementioned steels, the width-to-thickness ratios, the angle of the web members, the yield strength, and the gap of the web members were selected as the main parameters in this study, and ABAQUS, a general finite-element program, was used.As a result, the compression web member reached elastic buckling in the 600-MPa steel and inelastic buckling in the 400-MPa steel. A brittle fracture occurred in the case where the yield ratio was greater than 80%. At the same time, it was found that the limit strength determined via FEM analysis had a higher value compared to the code evaluation with the variation of the width-to-thickness ratio in the main code member. The change in the connection load in high-strength steels was not identified by the other factors.

Waterproofing performance evaluation according to the number of layer for shield TBM segment hydrophilic rubber waterstop (쉴드 TBM 세그먼트 지수재의 배열수 변화에 따른 방수성능 평가)

  • Ham, Soo-Kwon;Jung, Hoon;Kim, Beom-Ju;Jeong, Kyeong-han;Lee, Seok-Won
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.22 no.1
    • /
    • pp.47-58
    • /
    • 2020
  • The interest in the use of shield TBM (Tunnel Boring Machine) on the tunnel excavation has been increased rapidly in Korea. The shield TBM tunnel is generally designed as non-drainage tunnel. Consequently, if water leakage through the segment joints happens, big problems on the usage and stability of tunnel can be occurred. In this study, the variation of waterproof capacity of hydrophilic rubber waterstop by the construction error and excessive displacement of segment was studied. In particular, the waterproof capacity of each of single and double layer arrangements of hydrophilic rubber waterstop was examined to verify the efficiency of the double layer arrangement. The test results show that the single layer and double layer hydrophilic rubber waterstop showed the same waterproof performance. hydrophilic rubber waterstop has favorable on the offset, however unfavorable on the gap.

Investigation of Electrically Small Folded Slot Spherical Helix Magnetic Dipole Antenna (전기적 소형 Folded Slot Spherical Helix 자기 다이폴 안테나에 관한 연구)

  • Shin, Geonyeong;Kong, Myeongjun;Lee, Su-Hyeon;Yoon, Ick-Jae
    • The Journal of Korean Institute of Electromagnetic Engineering and Science
    • /
    • v.28 no.4
    • /
    • pp.261-268
    • /
    • 2017
  • In this paper, we propose an FSSH(Folded Slot Spherical Helix) magnetic dipole antenna with a form factor easy to build and study its radiation properties. The number of folded arms, the gap between them and the metal thickness are tuned to achieve relatively simple structure to realize whereas maintaining high radiation efficiency at an electrically small size. The proposed design shows wide radiation efficiency bandwidth and it is confirmed by circuit simulation that the non-Foster impedance matching techniques could be utilized for its practical use. The prototype of the proposed antenna is built with the aid of an SLS(Selective Laser Sintering) 3D printing technology. The measured result shows lower Q impedance characteristic due to high resistive loss of the copper tape joints.

TENSILE STRENGTH OF LASER WELDED-TITANIUM AND GOLD ALLOYS (티타늄과 금합금의 레이저 용접부의 인장강도)

  • Song, Yun-Gwan;Ha, Il-Soo;Song, Kwang-Yeob
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.38 no.2
    • /
    • pp.200-213
    • /
    • 2000
  • Lasers have given dentistry a new rapid, economic, and accurate technique for metal joining. Although laser welding has been recommended as an accurate technique, there are some limitations with this technique. For example, the two joining surfaces must have a tight-fitting contact, which may be difficult to achieve in some situations. The tensile samples used for this study were made from a custom-made pure titanium and type III gold alloy plates. 27 of 33 specimens were sectioned perpendicular to their long axis with a carborundum disk and water coolant. Six specimens remained and served as the control group. A group of 6 specimens was posed as butt joints in custom parallel positioning device with a feeler gauge at each of three gaps : 0.00, 0.25. and 0.50mm. All specimens were then machined to produce a uniform cross-sectional dimension, none of the specimens was subjected to any subsequent form of heat treatment. Scanning electron microscopy was performed on representative tested specimens at fractured surfaces in both the parent metal and the weld. Vickers hardness was measured at the center of the welds with a micropenetrometer using a force of 300gm for 15 seconds. Measurement was made at approximately $200{\mu}m\;and\;500{\mu}m$ deep from each surface. One-way analysis of variance (ANOVA) and Scheffe's test was calculated to detect differences between groups. The purpose of this study is to compare the strength and properties of the joint achieved at various butt Joint gaps by the laser welding of type III gold alloy and pure titanium tensile specimens in an argon atmosphere. The results of this study were as follows : 1. When indexing and welding pure titanium, there was no decrease in ultimate tensile strength as compared with the unsectioned alloys for indexing gaps of 0.00 to 0.50mm, although with increasing gap size may come increased distortion (p>0.05). 2. When indexing and welding type III gold alloy, there were significant differences in ultimate tensile strength among groups with weld gaps of 0.00mm, 0.25 and 0.50mm, and the control group. Group with butt contact without weld gap demonstrated a significant higher ultimate tensile strength than groups with weld gaps of 0.25 and 0.50mm (p<0.05). 3. When indexing and welding the different metal combination of type III gold alloy and pure titanium, there were significant differences in ultimate tensile strength between groups with weld gaps of 0.00, 0.25, and 0.50mm. However, the mechanical properties of the welded joint would become too brittle to be acceptable clinically (p<0.05). 4. The presence of large pores in the laser welded joint appears to be the most important factor in controlling the tensile strength of the weld in both pure titanium and type III gold alloy.

  • PDF

Flip Chip Process for RF Packages Using Joint Structures of Cu and Sn Bumps (Cu 범프와 Sn 범프의 접속구조를 이용한 RF 패키지용 플립칩 공정)

  • Choi, J.Y.;Kim, M.Y.;Lim, S.K.;Oh, T.S.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.16 no.3
    • /
    • pp.67-73
    • /
    • 2009
  • Compared to the chip-bonding process utilizing solder bumps, flip chip process using Cu pillar bumps can accomplish fine-pitch interconnection without compromising stand-off height. Cu pillar bump technology is one of the most promising chip-mounting process for RF packages where large gap between a chip and a substrate is required in order to suppress the parasitic capacitance. In this study, Cu pillar bumps and Sn bumps were electroplated on a chip and a substrate, respectively, and were flip-chip bonded together. Contact resistance and chip shear force of the Cu pillar bump joints were measured with variation of the electroplated Sn-bump height. With increasing the Sn-bump height from 5 ${\mu}m$ to 30 ${\mu}m$, the contact resistance was improved from 31.7 $m{\Omega}$ to 13.8 $m{\Omega}$ and the chip shear force increased from 3.8 N to 6.8 N. On the contrary, the aspect ratio of the Cu pillar bump joint decreased from 1.3 to 0.9. Based on the variation behaviors of the contact resistance, the chip shear force, and the aspect ratio, the optimum height of the electroplated Sn bump could be thought as 20 ${\mu}m$.

  • PDF