• Title/Summary/Keyword: bonding glass

Search Result 429, Processing Time 0.028 seconds

Processing and Electrical Properties of COG(Chip on Glass) Bonding Using Fine-pitch Sn-In Solder Bumps (미세피치 Sn-In 솔더범프를 이용한 COG(Chip on Glass) 본딩공정 및 전기적 특성)

  • Choe Jae Hun;Jeon Seong U;Jeong Bu Yang;O Tae Seong;Kim Yeong Ho
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2003.11a
    • /
    • pp.103-105
    • /
    • 2003
  • COG (Chip on Glass) technology using solder bump reflow has been investigated to attach IC chip directly on glass substrate of LCD panel. As It chip and LCD panel have to be heated to reflow temperature of the so]der bumps for COG bonding, it is necessary to use low-temperature solders to prevent the damage of liquid crystals of LCD panel. In this study, using the Sn-52In solder bumps of $40{\mu}m$ pitch size, solder joints between Si chip and glass substrate were made at temperature below $150^{\circ}C$. The contact resistance of the solder joint was $8.58m\Omega$, which was much lower than that of the joint made using the conventional ACF bonding technique. The Sn-52In solder joints with underfill showed excellent reliability at a hot humid environment.

  • PDF

Wafer-Level Package of RF MEMS Switch using Au/Sn Eutectic Bonding and Glass Dry Etch (금/주석 공융점 접합과 유리 기판의 건식 식각을 이용한 고주파 MEMS 스위치의 기판 단위 실장)

  • Kang, Sung-Chan;Jang, Yeon-Su;Kim, Hyeon-Cheol;Chun, Kuk-Jin
    • Journal of Sensor Science and Technology
    • /
    • v.20 no.1
    • /
    • pp.58-63
    • /
    • 2011
  • A low loss radio frequency(RF) micro electro mechanical systems(MEMS) switch driven by a low actuation voltage was designed for the development of a new RF MEMS switch. The RF MEMS switch should be encapsulated. The glass cap and fabricated RF MEMS switch were assembled by the Au/Sn eutectic bonding principle for wafer-level packaging. The through-vias on the glass substrate was made by the glass dry etching and Au electroplating process. The packaged RF MEMS switch had an actuation voltage of 12.5 V, an insertion loss below 0.25 dB, a return loss above 16.6 dB, and an isolation value above 41.4 dB at 6 GHz.

ANODICALLY-BONDED INTERFACE OF GLASS TO ALUMINIUM

  • Takahashi, Makoto;Nishikawa, Satoru;Chen, Zheng;Ikeuchi, Kenji
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.65-69
    • /
    • 2002
  • An Al film deposited on the Kovar alloy substrate was anodically-bonded to the borosilicate glass, and the bond interfaces was closely investigated by transmission electron microscopy. Al oxide was found to form a layer ~l0 nm thick at the bond interface, and fibrous structure of the same oxide was found to grow epitaxially in the glass from the oxide layer. The fibrous structure grew with the bonding time. The mechanism of the formation of this fibrous structure is proposed on the basis of the migration of Al ions under the electric field. Penetration of Al into glass beyond the interfacial Al oxide was not detected. The comparison of the amount of excess oxygen ions generated in the alkali depletion layer with that incorporated in the Al oxide suggests that the growth of the alkali-ion depletion layer is controlled by the consumption of excess oxygen to form the interfacial Al oxide.

  • PDF

BONDING STRENGTH OF GLASS-IOMOMER CEMENT AND COMPOSITE RESIN COMBINATION (Glass ionomer cement의 상아질 결합력에 관한 연구)

  • Um, Chung-Moon;Oilo, Gudbrand
    • Restorative Dentistry and Endodontics
    • /
    • v.19 no.2
    • /
    • pp.633-640
    • /
    • 1994
  • The tensile bond strength to dentin was measured for three glass-ionomer cement and composite resin combinations: two light-curing glass-ionomer cements(Vitrebond and XR - Ionomer) and one traditional glass - ionomer cement(Ketac - Bond), two adhesive systems(Scotchbond, and XR - Bonding System), and a corresponding composite resin. The bond strength of this "sandwich" was also compared with that of the same cements used in bulk. Vitredbond showed a significantly higher bond strength in bulk than did the other two cements. Of the sandwiches, the XR - Iomomer and XR - Bond combination showed a bond strength significantly higher than that of the Vitrebond and Scotchbond or Ketac- bond and Scotchbond combination. The fracture of the bond was mainly adhesive for Vitrebond, cohesive for XR - Ionomer when used in bulk and adhesive - cohesive when used in a sandwich, and cohesive for Ketac-Bond.

  • PDF

A study on development of methods to rehabilitate the damaged prestressed concrete beam using glass fiber (유리섬유를 이용한 손상된 프리스트레스트 콘크리트보의 보강공법 개발연구)

  • 한만엽;이택성;강원호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10b
    • /
    • pp.815-820
    • /
    • 1998
  • Many composite girder bridges have been constructed for about thirty five years. Nowadays they are aged or deteriorated because of th increase in traffic and vehicle loads. In this study, the effect of strengthening with glass fiber sheet is investigated to estimate the possibility for appling for damaged prestressed concrete bridges. One normal and eight cracked specimens which had been preloaded were tested. The cracked specimens were strengthened with either external prestressing or bonding glass fiber sheet, or using both methods. The results showed that the maximum loads are almost same for both methods. So it seems that the strengthening with glass fiber sheet can be used for strengthening damaged prestressed concrete girders. It is important that proper devices should be selected to prevent glass fiber sheet from premature bonding failure below its maximum load, which is similar to end anchorage problem in external prestressing method. It is proved that the devices proposed in this paper have sufficient anchoring capability to increase load carrying capacity.

  • PDF

Study of Chip On Glass Bonding Method using Diode Laser (다이오드 레이저를 이용한 Chip On Glass 접합에 관한 연구)

  • Seo M.H.;Ryu K.H.;Nam G.J.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.423-426
    • /
    • 2005
  • A new chip on glass(COG) technique by making use of a high power diode laser for LCD driver IC packaging of LCD has been developed. A laser joining technology of the connection of IC chip to glass panel has several advantages over conventional method such as hot plate joining: shorter process time, high reliability of joining, and better fur fine pitch joining. The reach time to cure temperature of ACF in laser joining is within 1 second. In this study, results show that the total process time of joining is reduced by halves than that of conventional method. The adhesion strength is mainly 100-250 N/cm. It is confirmed that the COG technology using high power diode laser joining can be applied to advanced LCDs with a fine pitch.

  • PDF

Anodic bonding Characteristics of MLCA to Si-wafer Using Evaporated Pyrex #7740 Glass Thin-Films for MEMS Applications (파이렉스 #7740 유리박막을 이용한 MEMS용 MLCA와 Si기판의 양극접합 특성)

  • Chung, Gwiy-Sang;Kim, Jae-Min;Yoon, Suk-Jin
    • Journal of Sensor Science and Technology
    • /
    • v.12 no.6
    • /
    • pp.265-272
    • /
    • 2003
  • This paper describes anodic bonding characteristics of MLCA (Multi Layer Ceramic Actuator) to Si-wafer using evaporated Pyrex #7740 glass thin-films for MEMS applications. Pyrex #7740 glass thin-films with same properties were deposited on MLCA under optimum RF magneto conditions(Ar 100%, input power $1\;W/cm^2$). After annealing in $450^{\circ}C$ for 1 hr, the anodic bonding of MLCA and Si-wafer was successfully performed at 600 V, $400^{\circ}C$ in - 760 mmHg. Then, the MLCA/Si bonded interface and fabricated Si diaphragm deflection characteristics were analyzed through the actuation test. It is possible to control with accurate deflection of Si diaphragm according to its geometries and its maximum non-linearity is 0.05-0.08 %FS. Moreover, any damages or separation of MLCA/Si bonded interfaces do not occur during actuation test. Therefore, it is expected that anodic bonding technology of MLCA/Si wafers could be usefully applied for the fabrication process of high-performance piezoelectric MEMS devices.

Adhesive bonding using thick polymer film of SU-8 photoresist for wafer level package

  • Na, Kyoung-Hwan;Kim, Ill-Hwan;Lee, Eun-Sung;Kim, Hyeon-Cheol;Chun, Kuk-Jin
    • Journal of Sensor Science and Technology
    • /
    • v.16 no.5
    • /
    • pp.325-330
    • /
    • 2007
  • For the application to optic devices, wafer level package including spacer with particular thickness according to optical design could be required. In these cases, the uniformity of spacer thickness is important for bonding strength and optical performance. Packaging process has to be performed at low temperature in order to prevent damage to devices fabricated before packaging. And if photosensitive material is used as spacer layer, size and shape of pattern and thickness of spacer can be easily controlled. This paper presents polymer bonding using thick, uniform and patterned spacing layer of SU-8 2100 photoresist for wafer level package. SU-8, negative photoresist, can be coated uniformly by spin coater and it is cured at $95^{\circ}C$ and bonded well near the temperature. It can be bonded to silicon well, patterned with high aspect ratio and easy to form thick layer due to its high viscosity. It is also mechanically strong, chemically resistive and thermally stable. But adhesion of SU-8 to glass is poor, and in the case of forming thick layer, SU-8 layer leans from the perpendicular due to imbalance to gravity. To solve leaning problem, the wafer rotating system was introduced. Imbalance to gravity of thick layer was cancelled out through rotating wafer during curing time. And depositing additional layer of gold onto glass could improve adhesion strength of SU-8 to glass. Conclusively, we established the coating condition for forming patterned SU-8 layer with $400{\mu}m$ of thickness and 3.25 % of uniformity through single coating. Also we improved tensile strength from hundreds kPa to maximum 9.43 MPa through depositing gold layer onto glass substrate.

Mechanical Characteristics of MLCA Anodic Bonded on Si wafers (실리콘기판위에 양극접합된 MLCA의 기계적 특성)

  • Kim, Jae-Min;Lee, Jong-Choon;Yoon, Suk-Jin;Chung, Gwiy-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07a
    • /
    • pp.160-163
    • /
    • 2003
  • This paper describes on anodic bonding characteristics of MLCA(Multi Layer Ceramic Actuator) to Si-wafer using evaporated Pyrex #7740 glass thin-films for MEMS applications. Pyrex #7740 glass thin-films with same properties were deposited on MLCA under optimum RF magneto conditions(Ar 100 %, input power $1\;/cm^2$). After annealing in $450^{\circ}C$ for 1 hr, the anodic bonding of MLCA to Si-wafer was successfully performed at 600 V, $400^{\circ}C$ in - 760 mmHg. Then, the MLCA/Si bonded interface and fabricated Si diaphragm deflection characteristics were analyzed through the actuation test. It is possible to control with accurate deflection of Si diaphragm according to its geometries and its maximum non-linearity is 0.05-008 %FS. Moreover, any damages or separation of MICA/Si bonded interfaces do not occur during actuation test. Therefore, it is expected that anodic bonding technology of MICA/Si wafers could be usefully applied for the fabrication process of high-performance piezoelectric MEMS devices.

  • PDF

Electrostatic bonding between Si and ITO-coated #7059 glass substrates (실리콘 기판과 ITO가 코팅된 #7059 유리 기판간의 정전 열 접합)

  • Ju, Hyeong-Kwon;Chung, Hoi-Hwan;Kim, Young-Cho;Han, Jeong-In;Cho, Kyoung-Ik;Oh, Myung-Hwan
    • Journal of Sensor Science and Technology
    • /
    • v.7 no.3
    • /
    • pp.211-217
    • /
    • 1998
  • Si and ITO-coated #7059 glass wafers were electrostatically bonded by employing #7740 interlayer. It was inferred that the thermionic- electrostatic migration of $Na^{+}$ ions in the #7740 interlayer played an important role in the bonding process through SIMS analysis. The temperature and voltage required for reliable electrostatic bonding were in the range of $180{\sim}200^{\circ}C$ and $50{\sim}70V_{dc}$(10min), respectively. The low temperature Si-ITO coated glass bonding can be effectively applied to the packaging of field emission devices.

  • PDF