Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$-PbZrO$_3$-PbTiO$_3$ thick films were screen-printed on platinized alumina substrates and fired at 800-1000$^{\circ}C$. Two kinds of powders with different particle size were prepared by attrition and ball milling methods. Effects of particle size of starting material on the microstructure and electrical properties of the thick films were investigated. Average particle size of attrition milled-powder (0.44 ${\mu}$m) was much smaller than that of ball milled-powder (2.87 ${\mu}$m). Average grain size of the thick film prepared from attrition-milled powder was smaller than that of the thick film prepared from ball-milled powder at the sintering temperature of 800$^{\circ}C$. However, the difference in average particle size became smaller with increasing the sintering temperature. Thick films prepared from attrition-milled powders showed more uniform and denser microstructures at all firing temperatures. Thick films prepared from attrition-milled powders had better electrical properties at the firing temperature above 900$^{\circ}C$ than thick films prepared from ball-milled powders. Dielectric constant, remanent polarization and coercive field of the thick film prepared from attrition-milled powders and fired at 900$^{\circ}C$ were 559, 16.3 ${\mu}$C/cm$^2$, and 51.3 kV/cm, respectively.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.23
no.5
/
pp.255-264
/
2013
Cobalt aluminate ($CoAl_2O_4$) is a highly stable pigment with excellent resistance to light, weather, etc., which has resulted in widespread use as a ceramic pigment. Due to the unique optical characteristics, $CoAl_2O_4$ is generally used as a coloring agent to decorate porcelain products, glass, paints and plastics. Here, $CoAl_2O_4$ pigments were synthesized by polymerized complex method and solid state reaction. Then $CoAl_2O_4$ pigment were grinded using the attrition milling with 1 mm size zirconia ball for 3 hours. The attrition milling process was performed at the constant speed of 800 rpm and ball to powder weight ratio (BPR) was 100 : 1. The characteristics of synthesized pigment were analyzed by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM), particle size analyser (PSA) and CIE $L^*a^*b^*$. The XRD patterns of $CoAl_2O_4$ show single phase spinel structure. The particle size of $CoAl_2O_4$ measured by FE-SEM, TEM and PSA analysis was in the range of 100~200 nm. The blue color of obtained $CoAl_2O_4$ pigments could be confirmed through CIE $L^*a^*b^*$ measurement.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2008.06a
/
pp.325-325
/
2008
스크린 프린팅에 의한 압전 후막은 MEMS 공정을 이용하여 마이크로 펌프, 마이크로 벨브, 마이크로 센서, 마이크로 로봇 등 여러 초소형 기계부품에 응용되고 있으며, Sol-Gel, PLD를 이용해 증착된 막 등에 비해 수십${\mu}m$의 비교적 두꺼운 막을 형성시킬 수 있는 장점을 가지고 있다. 그러나 실리콘 기판을 사용하여 스크린 프린팅으로 형성된 압전 후막의 경우, 공정상 바인더를 연소시키는 과정을 거치게 되므로, 밀집된(Dense) 구조를 가지는 막을 만들기가 어렵다. 이로 인해 스크린 프린팅에 의한 후막은 전기적 특성 및 기계적 특성이 떨어지는 경향이 있다. 본 연구에서는 스크린 프린팅에 의한 압전 후막의 밀집된 구조 및 특성을 향상시키기 위해 0.01Pb$(Mg_{1/2}W_{1/2})$O3-0.41Pb$(Ni_{1/3}Nb_{2/3})O_3-0.35PbTiO_3-0.23PbZrO_3$의 powder와 Attrition 밀링 처리된 powder를 비율별로 혼합하여 입자의 크기를 변화시켜 막의 충진 밀도를 향상시켰으며, 열처리 효과를 극대화시키기 위해 RTA(Rapidly Thermal Annealing)를 통해 열처리 하였다. Attrition 밀링에 의한 파우더를 각각 비율별로 100%, 50%, 25%로 혼합하여 만든 압전 세라믹 페이스트는 P-type(100)Si Wafer sample 위에 $1{\mu}m$의 하부전극용($1100^{\circ}C$) Ag 전극을 screen print하여 소결했다. 그리고 다시 전극이 형성된 Si wafer 위에 스크린 프린팅하고, 건조 한 후 RTA로 300초 동안 열처리 한 결과 밀집된 구조를 가지는 압전 후막을 제작 수 있었다.
Microstructure and phase transformation of Ti-Ni-Cu alloy powders produced by using attrition milling method were studied. Mixed powders of Ti-(50-X)Ni-XCu ($X=0{\sim}20$ at%) in composition range were mechanically alloyed for maximum 20 hours by using SUS 1/4" ball in argon atmosphere. Ball to powder ratio was 50: 1 and impeller speed was 350rpm. Mechanically alloyed with attrition millimg method. powder was heat treated at the temperature up to $850^{\circ}C$ for 1 hour in the $10^{-6}$ torr vacuum. Ti-Ni-Cu alloy powders have been fabricated by attrition milling method. and then phase transformation behaviours and microstructual properties of the alloy powders were investigated to assist in improving the the high damping capacity of Ti-Ni-Cu shape memory alloy powders. The results obtained are as follows: 1. After heat treating of fully mechanically alloyed powder at $850^{\circ}C$ for 1hour. most of the B2 and B 19' phases was formed and $TiNi_3$ were coexisted. 2. The B 19' martensite were formed in Ti-Ni-Cu alloy powders whose Cu-content is less than 5a/o. where as the B19 martensite in those whose Cu-content is more than 10at%. 3. The powders of as-milled Ti-Ni-Cu alloys whose Cu-contents is less than 5at% are amorphous. whereas those of as-milled Ti-Ni-Cu alloys whose Cu-content is more than 10at% are crystalline. This means that Cu addition tends to suppress amorphization of Ti-Ni alloy powders.
This study is focused on investigating the relation between the particle size of silver flake powder and mechanical milling parameters. Mechanical milling parameters such as ball size, impeller rotation speed and milling time of the attrition ball-mill were controlled to produce silver flake powder. The particle size of the silver flake powder increased with increasing ball size and impeller rotation speed. The change of the particle size of the silver flake powder with mechanical milling parameters was analyzed based on balls motion in the mill container of the attrition ball-mill. The silver flake particles were formed at the elastic deformation area of the ball due to the collision between balls. The change of the particle size of the silver flake powder with mechanical milling parameters well consists with the change of the collision energy of ball with parameters mentioned above.
Journal of the Korean Academy of Esthetic Dentistry
/
v.25
no.2
/
pp.68-78
/
2016
Recently, digital technology has become increasingly prevalent in the dental clinic. Using a milling machine for clinic, it is possible to produce provisional restoration inside the clinic. This can promote large clinical cases such as full mouth rehabilitation with the help of a tabletop scanner, which is capable of semi-adjustable articulator equipment, and a powerful dental CAD software with excellent user convenience. In this case report, a full-mouth rehabilitation was done with digital technology to a 55 year-old female patient, who has lost vertical dimension through the attrition, and has got inclined occlusal plane with unplanned and repeated dental reconstruction. Through the design and milling of the provisional restoration in the clinic and the duplication of these provisionals by double scanning technique, a good functional and esthetic result could be achieved.
In this research, magnesium powder was prepared by gas atomizing. Refinement behaviors of magnesium powder produced under different conditions were investigated using a mechanical milling (attrition milling) process. Analyses were performed to assess the characterization and comparison of milled powder with different steel ball sizes and milling times. The powders were analyzed by field emission scanning electron microscope, apparent density and powder fluidity. The particle morphology of the Mg powders changed from spherical particles of feed metals to irregular oval particles, then plate type particles, with an increasing milling time. Because of the HCP structure, deformation occurs due to the existence of the easily breakable C-axis perpendicular to the base, which results in producing plate-type powders. An increase in ball size and the impact energy of the magnesium powder maximizes the effect of refinement. Furthermore, it is possible to improve the apparent density and fluidity according to the smoothness of the surface of the initial powder.
The effect of a CAM (Continuous Attrition Mill) treatment on the sinterability of ex-ADU $UO_2$ powder was investigated. As the cycles of a CAM increased, the apparent density, specific surface area and O/U of the milled powder increased, but there particle sizes decreased. However the sintered density of the $UO_2$ pellet decreased as the cycles of the CAM increased. It is considered that the decrease of the sintered density is due to the formation of $U_3O_8$, which was produced by a CAM mechanism.
Three mixtures of elemental powders of Al-25at.%Ti, 48at.%Ti and 70at.%Ti were offered to ball milling process for the formation of intermetallic compounds of $Al_3Ti$, AlTi and $Ti_3Al$. Ballmilling or attrition process were carried out at the condition of rotaing speed of 110 or 350 rpm at $10^{-3}$ torr vacuum or argon atmospheres. $Al_3Ti$phases were fully obtained by heat treatment for 1 hors at $600^{\circ}C$ with Al-25at.%Ti composition mixtures milled by 100 hours. The amorphous phase was completely formed at the composition of Al-48at.%Ti mixed powders by milling 100hours at the 50 to 1 weight ratio of ball to powder, and AlTi compounds were obtained by heat treament. In the case of Al-70at%Ti mixed powders milled for 100 hours, $Ti_3Al$ and $Al_3Ti$intermetallic compounds were formed by heat treatment for 1 hour at $600^{\circ}C$. By attrition milling of 350rpm for 10 hours, $Ti_3Al$ phase was formed completley after heat treatment for 1 hour at $600^{\circ}C$.
The characteristics of dry and wet milled powder prepared by 1 cycle OREOX (oxidation and reduction of oxide fuels) treatment were investigated using the simulated spent fuel pellet. Sintered pellets simulating spent nuclear fuel burned in reactor were fabricated from $UO_2$ powder using as a starting material in fabrication of nuclear fuel. The 1 cycle OREOX-treated powder was prepared by only one path of oxidation md reduction of the simulated pellet. Powder having average particle size of less than 1 $\mu\textrm{m}$ could be easily obtained by dry milling, but not be achieved by wet milling. And, specific surface area of dry milled pow-der was higher than that of wet milled powder. Dry milled powder formed loose agglomerate, while wet milled powder showed the shape of irregular and angular particles. Dry milled powder provided higher green density, resulting in higher sintered density of higher than 95% TD and average grain size of larger than 8 $\mu\textrm{m}$ satisfying the standard specification of sintered pellets.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.