• Title/Summary/Keyword: Zr-based alloys

Search Result 121, Processing Time 0.02 seconds

Fabrication and Hydrogen Separation Performance of Newly Created Ti-Based Alloy Membrane (신조성의 Ti-기반 합금 수소분리막의 설계 및 수소투과 성능)

  • Min Yeong Ko;Min Chang Shin;Xuelong Zhuang;Jae Yeon Hwang;Sung Woo Han;Si Eun Kim;Jung Hoon Park
    • Membrane Journal
    • /
    • v.34 no.2
    • /
    • pp.146-153
    • /
    • 2024
  • In this experiment, a Ti-based flat hydrogen separation membrane was designed and manufactured. In order to find a Ti-based hydrogen separation membrane of a new composition, the correlation between the physical-chemical properties and hydrogen permeability of various alloys was investigated. Based on this, two types of new alloy films (Ti14.2Zr66.4Ni12.6Cu6.8 (70 ㎛), Ti17.3Zr62.7Ni20 (80 ㎛)) was designed and manufactured. The manufactured flat hydrogen separation membrane was tested for hydrogen permeation using mixed gas (H2, N2) and sweep gas (Ar) at 300~500℃ and 1~4 bar. The Ti14.2Zr66.4Ni12.6Cu6.8 alloy film has a maximum flux of 16.35 mL/cm2 min at 500℃ and 4 bar, and the Ti17.3Zr62.7Ni20 alloy film has a maximum flux of 10.28 mL/cm2 min at 450℃ and 4 bar.

Effects of Surface Treatment using Oxide-Dispersion-Strengthening on the Mechanical Properties of Zr-based Fuel Cladding Tubes (산화물 분산강화 표면처리에 따른 지르코늄 피복관의 기계적 강도)

  • Jung, Yang-Il;Kim, Il-Hyun;Kim, Hyun-Gil;Jang, Hun;Lee, Seung-Jae
    • Korean Journal of Materials Research
    • /
    • v.29 no.4
    • /
    • pp.271-276
    • /
    • 2019
  • Oxide-dispersion-strengthened (ODS) alloy has been developed to increase the mechanical strength of metallic materials; such an improvement can be realized by distributing fine oxide particles within the material matrix. In this study, the ODS layer was formed in the surface region of Zr-based alloy tubes by laser beam treatment. Two kinds of Zr-based alloys with different alloying elements and microstructures were used: KNF-M (recrystallized) and HANA-6 (partial recrystallized). To form the ODS layer, $Y_2O_3$-coated tubes were scanned by a laser beam, which induced penetration of $Y_2O_3$ particles into the substrates. The thickness of the ODS layer varied from 20 to $55{\mu}m$ depending on the laser beam conditions. A heat affected zone developed below the ODS layer; its thickness was larger in the KNF-M alloy than in the HANA-6 alloy. The ring tensile strengths of the KNF-M and HANA-6 alloy samples increased more than two times and 20-50%, respectively. This procedure was effective to increase the strength while maintaining the ductility in the case of the HANA-6 alloy samples; however, an abrupt brittle facture was observed in the KNF-M alloy samples. It is considered that the initial microstructure of the materials affects the formation of ODS and the mechanical behavior.

The Effects of Heat-treatment Conditions and Alloy Compositions on Tensile Properties in Al-Mg Alloys for Automobile Body Panels (차체 판넬용 Al-Mg합금에서 열처리조건 및 조성변화가 인장특성에 미치는 영향)

  • Kang, S.B.;Lim, C.Y.;Kim, H.W.
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.2 no.2
    • /
    • pp.95-102
    • /
    • 1994
  • Aluminum sheet application to automobile body panels has now become an important objective to meet the requirements of automobile weight reduction. As the Mg content in Al-Mg based alloys increased up to 7.19%, the strength and elongation increased. For instance. Al-7.19Mg alloy had a high strength of 305MPa and a high elongation of 35%. A study was also made to investigate the interrelation between grain size and tensile properties with varying the contents of Mg, Ti and Zr elements and annealing conditions. The yield stress decreased as the grain size increased, which increased the uniform elongation. The strain hardening exponents n increased as the Mg content increased, which depended on the increasing difficulties of the cross slip of dislocation.

  • PDF

Corrosion Monitoring of PEO-Pretreated Magnesium Alloys

  • Gnedenkov, A.S.;Sinebryukhov, S.L.;Mashtalyar, D.V.;Gnedenkov, S.V.;Sergienko, V.I.
    • Corrosion Science and Technology
    • /
    • v.16 no.3
    • /
    • pp.151-159
    • /
    • 2017
  • The MA8 alloy (formula Mg-Mn-Се) has been shown to have greater corrosion stability than the VMD10 magnesium alloy (formula Mg-Zn-Zr-Y) in chloride-containing solutions by Scanning Vibrating Electrode Technique (SVET) and by optical microscopy, gravimetry, and volumetry. It has been established that the crucial factor for the corrosion activity of these samples is the occurrence of microgalvanic coupling at the sample surface. The peculiarities of the kinetics and mechanism of the corrosion in the local heterogeneous regions of the magnesium alloy surface were investigated by localized electrochemical techniques. The stages of the corrosion process in artificial defects in the coating obtained by plasma electrolytic oxidation (PEO) at the surface of the MA8 magnesium alloy were also studied. The analysis of the experimental data enabled us to determine that the corrosion process in the defect zone develops predominantly at the magnesium/coating interface. Based on the measurements of the corrosion rate of the samples with PEO and composite polymer-containing coatings, the best anticorrosion properties were displayed by the composite polymer-containing coatings.

Powder Metallurgy of Nanostructured High Strength Materials

  • Eckert, J.;Scudino, S.;Yu, P.;Duhamel, C.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.364-365
    • /
    • 2006
  • Nanostructured or partially amorphous Al-and Zr-based alloys are attractive candidates for advanced high-strength lightweight materials. Such alloys can be prepared by quenching from the melt or by powder metallurgy using mechanical attrition techniques. This work focuses on mechanically attrited powders and their consolidation into bulk specimens. Selected examples of mechanical deformation behavior are presented, revealing that the properties can be tuned within a wide range of strength and ductility as a function of size and volume fraction of the different phases.

  • PDF

Toward Improving the Dynamic Deformation Properties of Metallic Materials via Role of Microstructure Factor (미세조직 인자의 영향을 고려한 금속 소재의 동적변형 특성 향상에 관한 연구)

  • Kim, Y.G.;Hwang, B.;Lee, D.G.;Ko, Y.G.;Lee, S.
    • Transactions of Materials Processing
    • /
    • v.30 no.5
    • /
    • pp.247-254
    • /
    • 2021
  • This study reviews dynamic deformation behavior of ultra-fine-grained Al alloys, ultra-fine-grained conventional low carbon steel and dual phase steel and Zr-based amorphous alloys. Dynamic tests were conducted using a Kolsky bar then the test data was analyzed in relation to resultant microstructures, mechanical properties and propensity of adiabatic shear band. In addition, deformed microstructures and fracture surfaces were used to investigate the behavior of both the dynamic deformation and fracture, and adiabatic shear banding. As a result, increasing microstructural homogeneity, strain hardenability and forming multiple shear bands could be a better way to increase the fracture resistance under dynamic loading as the formation of adiabatic shear bands was reduced or prevented.

Formation of Anodic Films on Pure Mg and Mg alloys for Corrosion Protection

  • Moon, Sungmo;Nam, Yunkyung
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.11a
    • /
    • pp.16-16
    • /
    • 2012
  • Mg and its alloys have been of great interest because of their low density of 1.7, 30% lighter than Al, but their wide applications have been limited because of their poor resistances against corrosion and/or abrasion. Corrosion resistance of Mg alloys can be improved by formation of anodic films using anodic oxidation method in aqueous electrolytes. Plasma electrolytic oxidation (PEO) is one of anodic oxidation methods by which hard anodic films can be formed as a result of micro-arc generation under high electric field. PEO method utilize not only substrate elements but also chemical components in electrolytes to form anodic films on Mg alloys. PEO films formed on AM50 magnesium alloy in an acidic fluozirconate electrolyte were observed to consist of mainly $ZrO_2$ and $MgF_2$. Liu et al reported that PEO coating on AM30 Mg alloy consists of $MgF_2$-rich outer porous layer and an MgO-rich dense inner layer. PEO films prepared on ACM522 Mg die-casting alloy in an aqueous phosphate solution were also reported to be composed of monoclinic $Mg_3(PO_4)_2$. $CeO_2$-incorporated PEO coatings were also reported to be formed on AZ31 Mg alloys in $CeO_2$ particle-containing $Na_2SiO_3$-based electrolytes. Magnesium tin hydroxide ($MgSn(OH)_6$) was also produced on AZ91D alloy by PEO process in stannate-containing electrolyte. Effects of $OH^-$, $F^-$, $PO{_4}^{3-}$ and $SiO{_3}^{2-}$ ions and alloying elements of Al and Sn on the formation of PEO films on pure Mg and Mg alloys and their protective properties against corrosion have been investigated in this work. $PO{_4}^{3-}$, $F^-$ and $SiO{_3}^{2-}$ ions were observed to contribute to the formation of PEO films but $OH^-$ ions were found to break down the surface films under high electric field. The effect of pulse current on the formation of PEO films will be also reported.

  • PDF

The effect of substitution elements(Co, Cr, Fe) on the properties of Zr-based hydrogen storage alloy electrode for Ni-MH secondary battery (Ni-MH 2차 전지용 Zr계 수소저장합금전극의 특성에 미치는 치환원소(Co, Cr, Fe)의 영향)

  • Choi, Seung-Jun;Jung, So-Yi;Seo, Chan-Yeol;Choi, Jeon;Park, Choong-Nyeon
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.10 no.3
    • /
    • pp.185-189
    • /
    • 1999
  • Effects of alloy modification with the $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.4}$ alloy for an electrode use have been investigated. For the alloy composition, a part of Mn was substituted by Co, Cr and Fe. The experimental results showed that Co accelerated activation of alloy, and Fe and Cr improved the discharge capacity. These results agree with P-C-T curves of each alloy. But substituting Fe for Mn showed the decrease of the discharge capacity when discharged at high rate (60mA, about 1C rate). Considering both the discharge capacity and the high rate discharge property, $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.3}Cr_{0.1}$ alloy was found to be the best alloy among the alloys subjected to the test.

  • PDF

Effect of Boron Additions on Glass Formation and Magnetic Properties of Fe-Co-Ti-Zr-B Amorphous Ribbons

  • Kim, Sumin;Han, Bo Kyeong;Choi-Yim, Haein
    • Journal of Magnetics
    • /
    • v.21 no.2
    • /
    • pp.164-167
    • /
    • 2016
  • The effect of the B additions on glass formation and magnetic properties is reported for the $Fe_{(87-x-y)}Co_yTi_7Zr_6B_x$ (x = 2, 4, 6 and y = 35, 40) alloy system. The ribbon samples with the width of 2 mm for each composition were prepared by the melt spinning technique; furthermore, their phase information was obtained from X-ray diffraction. Glass formation and magnetic properties were measured using differential scanning calorimetry and vibrating sample magnetometer respectively. The $Fe_{45}Co_{40}Ti_7Zr_6B_2$ (x = 2 and y = 40) system has the nanocrystalline phase identified as ${\alpha}-Fe$, as well as the amorphous phase, whereas all other alloys are fully amorphous. It is associated with the role of B on the glass formation. The widest supercooled liquid region is obtained as 71 K at x = 4 (both y = 35 and 40). The saturation magnetization decreases with the increase of the amount of the B addition, and the highest value is 1.59 T as x = 2 and y = 35 for this alloy system.