• 제목/요약/키워드: Y-TZP

검색결과 191건 처리시간 0.025초

고에너지 분쇄 매체 지르코니아 Beads의 미세구조 및 기계적 특성에 따른 마모율 분석 (Analysis of Attrition Rate of Y2O3 Stabilized Zirconia Beads with Different Microstructure and Mechanical Properties)

  • 김정환;윤세중;한병동;안철우;윤운하;최종진
    • 한국재료학회지
    • /
    • 제28권6호
    • /
    • pp.349-354
    • /
    • 2018
  • Particle size reduction is an important step in many technological operations. The process itself is defined as the mechanical breakdown of solids into smaller particles to increase the surface area and induce defects in solids, which are needed for subsequent operations such as chemical reactions. To fabricate nano-sized particles, several tens to hundreds of micron size ceramic beads, formed through high energy milling process, are required. To minimize the contamination effects during high-energy milling, the mechanical properties of zirconia beads are very important. Generally, the mechanical properties of $Y_2O_3$ stabilized tetragonal zirconia beads are closely related to the mechanism of phase change from tetragonal to monoclinic phase via external mechanical forces. Therefore, $Y_2O_3$ distribution in the sintered zirconia beads must also be closely related with the mechanical properties of the beads. In this work, commercially available $100{\mu}m-size$ beads are analyzed from the point of view of microstructure, composition homogeneity (especially for $Y_2O_3$), mechanical properties, and attrition rate.

Evaluation of intaglio surface trueness, wear, and fracture resistance of zirconia crown under simulated mastication: a comparative analysis between subtractive and additive manufacturing

  • Kim, Yong-Kyu;Han, Jung-Suk;Yoon, Hyung-In
    • The Journal of Advanced Prosthodontics
    • /
    • 제14권2호
    • /
    • pp.122-132
    • /
    • 2022
  • PURPOSE. This in-vitro analysis aimed to compare the intaglio trueness, the antagonist's wear volume loss, and fracture load of various single-unit zirconia prostheses fabricated by different manufacturing techniques. MATERIALS AND METHODS. Zirconia crowns were prepared into four different groups (n = 14 per group) according to the manufacturing techniques and generations of the materials. The intaglio surface trueness (root-mean-square estimates, RMS) of the crown was measured at the marginal, axial, occlusal, and inner surface areas. Half of the specimens were artificially aged in the chewing simulator with 120,000 cycles, and the antagonist's volume loss after aging was calculated. The fracture load for each crown group was measured before and after hydrothermal aging. The intaglio trueness was evaluated with Welch's ANOVA and the antagonist's volume loss was assessed by the Kruskal-Wallis tests. The effects of manufacturing and aging on the fracture resistance of the tested zirconia crowns were determined by two-way ANOVA. RESULTS. The trueness analysis of the crown intaglio surfaces showed surface deviation (RMS) within 50 ㎛, regardless of the manufacturing methods (P = .053). After simulated mastication, no significant differences in the volume loss of the antagonists were observed among the zirconia groups (P = .946). The manufacturing methods and simulated chewing had statistically significant effects on the fracture resistance (P < .001). CONCLUSION. The intaglio surface trueness, fracture resistance, and antagonist's wear volume of the additively manufactured 3Y-TZP crown were clinically acceptable, as compared with those of the 4Y- or 5Y-PSZ crowns produced by subtractive milling.

비니어 세라믹과 지르코니아 세라믹의 Push-Shear 결합강도 (Push-Shear Bond Strength of Veneering Ceramics and Zirconia Ceramic)

  • 안재석;노형록;이정환
    • 한국콘텐츠학회논문지
    • /
    • 제15권9호
    • /
    • pp.384-394
    • /
    • 2015
  • 본 연구에서는 원통형 지르코니아 코어에 다섯 종류의 지르코니아 비니어 세라믹을 축성하여 push-전단결합강도를 측정하고, 비니어 세라믹의 이축굽힘강도와 지르코니아 글라스 라이너 처리에 따른 전단결합강도 차이를 알아보고자 하였다. 지르코니아 비니어 세라믹은 piston-on-three-ball test로 이축굽힘강도를 측정하였고, 지르코니아 실린더 코어와 비니어 세라믹은 push-shear test로 결합강도를 측정하였으며, 결과값은 이원분산분석을 사용하여 분석하였다. 이축굽힘강도는 Cercon ceram kiss (CE)군에서 가장 높게 측정되었고 전단결합강도는 글라스 처리군과 Triceram(TR)군이 높게 측정 되었으며 Creation ZI(CR)군에서 가장 낮은 값이 측정 되었다. 실험군에서 지르코니아 라이너 처리군이 라이너 처리하지 않는 군보다 전단결합강도가 높게 나타났으며 통계적으로 유의한 차이를 보였다(P<0.05). 따라서 지르코니아 라이너 처리는 지르코니아와 비니어 세라믹의 결합강도를 향상시킬 수 있는 것으로 사료된다.

Initial bacterial adhesion on resin, titanium and zirconia in vitro

  • Lee, Byung-Chul;Jung, Gil-Yong;Kim, Dae-Joon;Han, Jung-Suk
    • The Journal of Advanced Prosthodontics
    • /
    • 제3권2호
    • /
    • pp.81-84
    • /
    • 2011
  • PURPOSE. The aim of this in vitro study was to investigate the adhesion of initial colonizer, Streptococcus sanguis, on resin, titanium and zirconia under the same surface polishing condition. MATERIALS AND METHODS. Specimens were prepared from Z-250, cp-Ti and 3Y-TZP and polished with $1 {\mu}m$ diamond paste. After coating with saliva, each specimen was incubated with Streptococcus sanguis. Scanning electron microscope, crystal violet staining and measurement of fluorescence intensity resulting from resazurin reduction were performed for quantifying the bacterial adhesion. RESULTS. Surface of resin composite was significantly rougher than that of titanium and zirconia, although all tested specimens are classified as smooth. The resin specimens showed lower value of contact angle compared with titanium and zirconia specimens, and had hydrophilic surfaces. The result of scanning electron microscopy demonstrated that bound bacteria were more abundant on resin in comparison with titanium and zirconia. When total biofilm mass determined by crystal violet, absorbance value of resin was significantly higher than that of titanium or zirconia. The result of relative fluorescence intensities also demonstrated that the highest fluorescence intensity was found on the surface of resin. Absorbance value and fluorescence intensity on titanium was not significantly different from those on zirconia. CONCLUSION. Resin specimens showed the roughest surface and have a significantly higher susceptibility to adhere Streptococcus sanguis than titanium and zirconia when surfaces of each specimen were polished under same condition. There was no significant difference in bacteria adhesion between titanium and zirconia in vitro.

Comparison of the optical properties of pre-colored dental monolithic zirconia ceramics sintered in a conventional furnace versus a microwave oven

  • Kim, Hee-Kyung;Kim, Sung-Hun
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권5호
    • /
    • pp.394-401
    • /
    • 2017
  • PURPOSE. The purpose of this study was to compare the optical properties of pre-colored dental monolithic zirconia ceramics of various thicknesses sintered in a microwave and those in a conventional furnace. MATERIALS AND METHODS. A2-shade of pre-colored monolithic zirconia ceramic specimens ($22.0mm{\times}22.0mm$) in 3 thickness groups of 0.5, 1.0, and 1.5 mm were divided into 2 subgroups according to the sintering methods (n=9): microwave and conventional sintering. A spectrophotometer was used to obtain CIELab color coordinates, and translucency parameters and CIEDE2000 color differences (${\Delta}E_{00}$) were measured. The relative amount of monoclinic phase ($X_m$) was estimated with x-ray diffraction. The surface topography was analyzed by atomic force microscope and scanning electron microscope. Statistical analyses were conducted with two-way ANOVA (${\alpha}=.05$). RESULTS. There were small interaction effects on CIE $L^*$, $a^*$, and TP between sintering method and thickness (P<.001): $L^*$ (partial eta squared ${{\eta}_p}^2=0.115$), $a^*$ (${{\eta}_p}^2=0.136$), and TP (${{\eta}_p}^2=0.206$), although higher $b^*$ values were noted for microwave sintering regardless of thickness. Color differences between two sintering methods ranged from 0.52 to 0.96 ${\Delta}E_{00}$ units. The $X_m$ values ranged from 7.03% to 9.89% for conventional sintering, and from 7.31% to 9.17% for microwave sintering. The microwave-sintered specimen demonstrated a smoother surface and a more uniform grain structure compared to the conventionally-sintered specimen. CONCLUSION. With reduced processing time, microwave-sintered pre-colored dental monolithic zirconia ceramics can exhibit similar color perception and translucency to those by conventional sintering.

Influence of nonthermal argon plasma on the shear bond strength between zirconia and different adhesives and luting composites after artificial aging

  • Pott, Philipp-Cornelius;Syvari, Timo-Sebastian;Stiesch, Meike;Eisenburger, Michael
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권4호
    • /
    • pp.308-314
    • /
    • 2018
  • PURPOSE. Plasma activation of hydrophobic zirconia surfaces might be suitable to improve the bond strength of luting materials. The aim of this study was to analyze the influence of nonthermal argon-plasma on the shear bond strength (SBS) between zirconia and different combinations of 10-MDP adhesive systems and luting composites after artificial aging. MATERIALS AND METHODS. Two hundred forty Y-TZP specimens were ground automatically with $165{\mu}m$ grit and water cooling. Half of the specimens received surface activation with nonthermal argon-plasma. The specimens were evenly distributed into three groups according to the adhesive systems ([Futurabond U, Futurabond M, Futurabond M + DCA], VOCO GmbH, Germany, Cuxhaven) and into further two subgroups according to the luting materials ([Bifix SE, Bifix QM], VOCO GmbH). Each specimen underwent artificial aging by thermocycling and water storage. SBS was measured in a universal testing machine. Statistical analysis was performed using ANOVA and $Scheff{\grave{e}}$ procedure with the level of significance set to 0.05. RESULTS. Surface activation with nonthermal plasma did not improve the bond strength between zirconia and the tested combinations of adhesive systems and luting materials. The plasma-activation trended to reveal higher bond strength if the self-etch luting material (Bifix SE) was used, irrespective of the adhesive system. CONCLUSION. Plasma-activation seems to be suitable to improve bond strength between zirconia and self-etch resin materials. However, further research is necessary to identify the influence of varying plasma-parameters.

t-ZrO$_2$/Al$_2$O$_3$복합체 상 안정성에 대한 Eu$_2$O$_3$첨가 효과 (Effect of EuO$_3$addition on hydrothermal stability of t-ZrO$_2$/Al$_2$O$_3$composites)

  • 이득용;김대준;최성갑;이명현
    • 한국결정성장학회지
    • /
    • 제10권3호
    • /
    • pp.233-238
    • /
    • 2000
  • 생체적합성과 상 안정성이 우수한 t-$ZrO_2/Al_2O_3$복합체에 $Eu_2O_3$을 0~4 mol%첨가한 복합체를 $1600^{\circ}C$ 온도에서 1 시간 소결하여 상 안정성, 색상변화, 기계적 특성을 조사하였다. $180^{\circ}C$, 3.5MPa의 수증기 압력 하에서 20시간 열처리 후 X-선 회절법으로 관찰한 결과 $Eu_2O_3$가 첨가된 (Y,Nb,Eu)-TZP/$Al_2O_3$복합체는 우수한 상 안정성이 유지되었다. $Eu_2O_3$의 양이 증가함에 따라 백색계통의 상아색에서 미색의 핑크색으로 서서히 변화하였다 $Eu_2O_3$가 3 mol%까지 첨가된 복합체의 경우 620MPa, 7.6MPa.$m^{1/2}$ 이상의 강도와 인성값이 관찰되었다.

  • PDF

Effect of cement type on the color attributes of a zirconia ceramic

  • Tabatabaian, Farhad;Khodaei, Maliheh Habib;Namdari, Mahshid;Mahshid, Minoo
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권6호
    • /
    • pp.449-456
    • /
    • 2016
  • PURPOSE. This in vitro study evaluated the effects of four different cements on the color attributes of a zirconia ceramic. MATERIALS AND METHODS. 40 zirconia ceramic disk specimens (0.5 mm thickness, 10 mm diameter, 0.1 mm cement space) were fabricated by a computer-aided design and computer-aided manufacturing system. The specimens were divided into 4 groups of 10 specimens and cemented to composite substrates using four different cements including: Glass Ionomer, Panavia F2.0, Zinc Phosphate, and TempBond. The $L^*$, $a^*$, and $b^*$ color attributes of the specimens were measured before and after cementation by a spectrophotometer. Additionally, ${\Delta}E$ values were measured to determine color changes for the groups and then compared with the perceptional threshold of ${\Delta}E=3.3$. Repeated Measures ANOVA, Tukey Post Hoc, Bonferroni, One-way ANOVA, and One-sample t-test tests were used to analyze the data. All tests were carried out at the 0.05 level of significance. RESULTS. Statistically significant differences were detected in the ${\Delta}E$ values for Zinc Phosphate (P<.0001) and TempBond (P<.0001) groups. However, there were no statistically significant differences in this respect for Glass Ionomer (P=.99) and Panavia F2.0 (P=1) groups. The means and standard deviations of the ${\Delta}E$ values for Glass Ionomer, Panavia F2.0, Zinc Phosphate, and Tempbond groups were $2.11{\pm}0.66$, $0.94{\pm}0.39$, $5.77{\pm}0.83$, and $7.50{\pm}1.16$ Unit, respectively. CONCLUSION. Within the limitations of this study, it was concluded that Zinc Phosphate and Tempbond cements affected the color attributes of the tested zirconia ceramic beyond the perceptional threshold. However, Glass Ionomer and Panavia F2.0 cements created acceptable color changes.

지르코니아 프라이머 종류에 따른 복합레진-지르코니아의 전단결합강도 (Effec of different zirconia primers on shear bond strengths of composite resin to bonded zirconia)

  • 석홍병;김태석;안재석;이정환
    • 대한치과기공학회지
    • /
    • 제38권3호
    • /
    • pp.135-142
    • /
    • 2016
  • Purpose: The aim of this research was to evaluate the influence of different surface treatments on the shear bond strength of zirconia ceramic to composite resin. Methods: Seventy two cylinder-shape (diameter: 5 mm; height: 12 mm) blocks of experimental industrially manufactured Y-TZP ceramic were abraded with $125{\mu}m\;Al_2O_3$ particles and randomly divided into 4 groups. All the materials were categorized as group Gc(control group - composite resin veneering on zirconia surface), Gr - composite resin veneering after surface treatment of Rocatec system (3M ESPE, Seefeld, Germany) group; Gz - composite resin veneering after surface treatment of Zirconia primer (Z-primer, Bisco, U.S.A) group; Gm - composite resin veneering after surface treatment of zirconia primer (Monobond plus, ivoclar vivadent AG, Liechtenstein) group. Two different zirconia primers and Rocatec system were used to zirconia cylinders (n=16) onto the zirconia surface. Zirconia specimens, polished and roughened, were pretreated and composite bilayer cylinders bonded using conventional adhesive techniques. Results: Shear bond strengths were analyzed using single-factor ANOVA(p<0.05). Bond strength values achieved after airbone particle abrasion and zirconia surface pre-treatments(p<0.05). Conclusion: Shear bond strength tests denmonstrated that zirconia primer is a viable method to improved bond strength between zirconia ceramic core and veneering composites.

Effect of the amount of thickness reduction on color and translucency of dental monolithic zirconia ceramics

  • Kim, Hee-Kyung;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yeo, In-Sung;Ha, Seung-Ryong
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권1호
    • /
    • pp.37-42
    • /
    • 2016
  • PURPOSE. This study investigated the effect of amount of thickness reduction on color and translucency of dental monolithic zirconia ceramics. MATERIALS AND METHODS. One-hundred sixty-five monolithic zirconia specimens ($16.3mm{\times}16.3mm{\times}2.0mm$) were divided into 5 groups (Group I to V) according to the number of A2-coloring liquid applications. Each group was then divided into 11 subgroups by reducing the thickness up to 1.0 mm in 0.1-mm increments (Subgroup 0 to 10, n=3). Colors and spectral distributions were measured according to CIELAB on a reflection spectrophotometer. All measurements were performed on five different areas of each specimen. Color difference (${\Delta}E^*{^_{ab}}$) and translucency parameter (TP) were calculated. Data were analyzed using one-way ANOVA and multiple comparison $Scheff{\acute{e}}$ test (${\alpha}=.05$). RESULTS. There were significant differences in CIE $L^*$ between Subgroup 0 and other subgroups in all groups. CIE $a^*$ increased (0.52<$R^2$<0.73), while CIE $b^*$ decreased (0.00<$R^2$<0.74) in all groups with increasing thickness reduction. Perceptible color differences (${\Delta}E^*{^_{ab}}$>3.7) were obtained between Subgroup 0 and other subgroups. TP values generally increased as the thickness reduction increased in all groups ($R^2$>0.89, P<.001). CONCLUSION. Increasing thickness reduction reduces lightness and increases a reddish, bluish appearance, and translucency of monolithic zirconia ceramics.