• Title/Summary/Keyword: Wet-Etching

Search Result 469, Processing Time 0.022 seconds

Maskless Pattern Fabrication on Si (100) Surface by Using Nano Indenter with KOH Wet Etching (나노인덴터와 KOH 습식 식각 기술을 병용한 Si(100) 표면의 마스크리스 패턴 제작 기술)

  • 윤성원;신용래;강충길
    • Transactions of Materials Processing
    • /
    • v.12 no.7
    • /
    • pp.640-646
    • /
    • 2003
  • The nanoprobe based on lithography, mainly represented by SPM based technologies, has been recognized as potential application to fabricate the surface nanostructures because of its operational versatility and simplicity. The objective of the work is to suggest new mastless pattern fabrication technique using the combination of machining by nanoindenter and KOH wet etching. The scratch option of the nanoindenter is a very promising method for obtaining nanometer scale features on a large size specimen because it has a very wide working area and load range. Sample line patterns were machined on a silicon surface, which has a native oxide on it, by constant load scratch (CLS) of the Nanoindenter with a Berkovich diamond tip, and they were etched in KOH solutions to investigate chemical characteristics of the machined silicon surface. After the etching process, the convex structure was made because of masking effect of the affected layer generated by nano-scratch. On the basis of this fact, some line patterns with convex structures were fabricated. Achieved patterns can be used as a mold that will be used for mass production processes such as nanoimprint or PDMS molding process. All morphological data of scratch traces were scanned using atomic force microscope (AFM).

A Study on the Electrical Characteristics of Dye-Sensitized Solar Cell with Glass Substrate surface Etching (유리기판 표면 Etching을 통한 분광특성연구)

  • Kim, Haemaro;Lee, Don-Kyu
    • Journal of IKEEE
    • /
    • v.23 no.2
    • /
    • pp.534-537
    • /
    • 2019
  • The optical loss is caused by reflection on the surface of the solar cell, without being absorbed inside the solar cell. Research is actively being conducted to reduce optical loss due to such reflection of light and to improve conversion efficiency of solar cells. In this paper, the surface of the FTO glass substrate was wet etched, and the structural characteristics of the tough surface were evaluated. In addition, optical properties on the surface were analyzed, etched using spectrometer. When light was introduced to a rough surface formed by etching, it was confirmed that the multiple reflections reduced the amount of light reflection from the surface, thereby increaseing the amount of light penetrating the glass substrate.

The Wet and Dry Etching Process of Thin Film Transistor (박막트랜지스터의 습식 및 건식 식각 공정)

  • Park, Choon-Sik;Hur, Chang-Wu
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.13 no.7
    • /
    • pp.1393-1398
    • /
    • 2009
  • Conventionally, etching is first considered for microelectronics fabrication process and is specially important in process of a-Si:H thin film transistor for LCD. In this paper, we stabilize properties of device by development of wet and dry etching process. The a-Si:H TFTs of this paper is inverted staggered type. The gate electrode is lower part. The gate electrode is formed by patterning with length of 8 ${\mu}$m${\sim}$16 ${\mu}$m and width of 80${\sim}$200 ${\mu}$m after depositing with gate electrode (Cr) 1500 ${\AA}$under coming 7059 glass substrate. We have fabricated a-SiN:H, conductor, etch-stopper and photo resistor on gate electrode in sequence, respectively. The thickness of these thin films is formed with a-SiN:H (2000 ${\mu}$m), a-Si:H(2000 ${\mu}$m) and n+a-Si:H (500 ${\mu}$m), We have deposited n-a-Si:H, NPR(Negative Photo Resister) layer after forming pattern of Cr gate electrode by etch-stopper pattern. The NPR layer by inverting pattern of upper gate electrode is patterned and the n+a-Si:H layer is etched by the NPR pattern. The NPR layer is removed. After Cr layer is deposited and patterned, the source-drain electrode is formed. In the fabricated TFT, the most frequent problems are over and under etching in etching process. We were able to improve properties of device by strict criterion on wet, dry etching and cleaning process.

Alkali metal free texturing for mono-crystalline silicon solar cell (알카리 금속을 배재한 단결정 실리콘 태양전지의 텍스쳐링 공정)

  • Kim, Taeyoon;Kim, Hoechang;Kim, Bumho
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2010.11a
    • /
    • pp.48.1-48.1
    • /
    • 2010
  • Mono-crystalline silicon solar cell is fabricated by using alkali metals. These alkali metal, used in wet etching process, must be removed for the high efficiency solar cell. As wet etching process has been adapted due to its low cost. But lots of alkali metals like potassium remains on the silicon surface and acts as impurities. To remove these alkali metals many of cleaning process have to be applied when solar cell manufacturing process. In terms of alkali metal removal, modified etchant solution is required for concise cleaning process. In this paper ethylenediamine was used and proposed for the substituion of postassium hydroxide.

  • PDF

Development of sacrificial layer wet etch process of TiNi for nano-electro-mechanical device application

  • Park, Byung Kyu;Choi, Woo Young;Cho, Eou Sik;Cho, Il Hwan
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • v.13 no.4
    • /
    • pp.410-414
    • /
    • 2013
  • We report the wet etching of titanium nickel (TiNi) films for the production of nano-electro-mechanical (NEM) device. $SiO_2$ and $Si_3N_4$ have been selected as sacrificial layers of TiNi metal and etched with polyethylene glycol and hydrofluoric acid (HF) mixed solution. Volume percentage of HF are varied from 10% to 35% and the etch rate of the $SiO_2$, $Si_3N_4$ and TiNi are reported here. Within the various experiment results, 15% HF mixed polyethylene glycol solution show highest etch ratio between sacrificial layer and TiNi metal. Especially $Si_3N_4$ films shows high etch ratio with TiNi films. Wet etching results are measured with SEM inspection. Therefore, this experiment provides a novel method for TiNi in the nano-electro-mechanical device.

The Effect of Surface Roughness on SiC by Wet Chemical Etching (SiC 표면 거칠기에 미치는 습식식각의 영향)

  • Kim, Jae-Kwan;Jo, Young-Je;Han, Seung-Cheol;Lee, Hae-Yong;Lee, Ji-Myon
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.11
    • /
    • pp.748-753
    • /
    • 2009
  • The surface morphology and the surface roughness of n-type SiC induced by wet-treatment using 45% KOH and buffered oxide etchant (BOE-1HF : $6H_2O$) were investigated by atomic force microscopy (AFM). While Si-face of SiC could be etched by alkali solutions such as KOH, acidic solutions such as BOE were hardly able to etch SiC. When the rough SiC samples were used, the surface roughness of etched sample was decreased after wet-treatment regardless of etchant, due to the planarization the of surface by widening of scratches formed by mechanical polishing. It was observed that the initial etching was affected by the energetically unstable sites, such as dangling bond and steps. However, when a relatively smooth sample was used, the surface roughness was rapidly increased after treatment at $180^{\circ}C$ for 1 hr and at room temperature for 4 hr by using KOH solution, resulting from the nano-sized structures such as pores and bumps. This indicates that porous SiC surface can be achieved by using purely chemical treatment.

A Study on the Fabrication of Sub-Micro Mold for PDMS Replica Molding Process by Using Hyperfine Mechanochemical Machining Technique (기계화학적 극미세 가공기술을 이용한 PDMS 복제몰딩 공정용 서브마이크로 몰드 제작에 관한 연구)

  • 윤성원;강충길
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2004.10a
    • /
    • pp.351-354
    • /
    • 2004
  • This work presents a simple and cost-effective approach for maskless fabrication of positive-tone silicon master for the replica molding of hyperfine elastomeric channel. Positive-tone silicon masters were fabricated by a maskless fabrication technique using the combination of nanoscratch by Nanoindenter ⓡ XP and XOH wet etching. Grooves were machined on a silicon surface coated with native oxide by ductile-regime nanoscratch, and they were etched in a 20 wt% KOH solution. After the KOH etching process, positive-tone structures resulted because of the etch-mask effect of the amorphous oxide layer generated by nanoscratch. The size and shape of the positive-tone structures were controlled by varying the etching time (5, 15, 18, 20, 25, 30 min) and the normal loads (1, 5 mN) during nanoscratch. Moreover, the effects of the Berkovich tip alignment (0, 45$^{\circ}$) on the deformation behavior and etching characteristic of silicon material were investigated.

  • PDF

A Study of Mechanochemical Hyperfine-Writing Technique Using Deformation Induced Etch Hillock Phenomena (변형유기 식각 힐록 현상을 이용한 기계화학적 극미세 Writing 기법에 대한 연구)

  • Kang Chung Gil;Youn Sung Won
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.22 no.7 s.172
    • /
    • pp.71-78
    • /
    • 2005
  • The purpose of this study is to suggest a hyperfine maskless writing technique by using the nanoindentation and HF wet etching technique. Indents were made on the surface of Pyrex7740 glass by the hyperfine indentation process with a Berkovich diamond indenter, and they were etched in $50\;wr\%$ HF solution. After etching process, convex structure was obtained due to the deformation-induced hillock phenomena. In this study, effects of indentation process parameters (etching time, normal load, loading .ate, hold-time at the maximum load) on the morphologies of the indented surfaces after isotopic etching were investigated from an angle of deformation energies. Finally, sample characters were written to show the possibility of the application.