  • Two methods that can reduce reflectance in solar cells are surface texturing and anti-reflection coating. Wet chemical etching is a typical method that surface texturing of multi-crystalline silicon. Wet chemical etching methods are the acid texturization of saw damage on the surface of multi-crystalline silicon or double-step chemical etching after KOH saw damage removal too. These methods of surface texturing are realized by chemical etching in acid solutions HF-$HNO_3$-$H_2O$. In this solutions we can reduce reflectance spectra by simple process etching of multi-crystalline silicon surface. We have obtained reflectance of 27.19% m 400~1100nm from acidic chemical etching after KOH saw damage removal. This result is about 7% less than just saw damage removal substrate. The surface morphology observed by microscope and scanning electron microscopy (SEM).

  • PDF

습식 에칭에 의한 웨이퍼의 층간 절연막 가공 특성에 관한 연구 (A Study on a Wet etching of ILD (Interlayer Dielectric) Film Wafer)

  • 김도윤;김형재;정해도;이은상
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.935-938
    • /
    • 1997
  • Recently, the minimum line width shows a tendency to decrease and the multi-level increase in semiconductor. Therefore, a planarization technique is needed and chemical mechanical polishing(CMP) is considered as one of the most suitable process. CMP accomplishes a high polishing performance and a global planarization of high quality. But there are several defects in CMP such as micro-scratches, abrasive contaminations, and non-uniformity of polished wafer edges. Wet etching include of Spin-etching can improve he defects of CMP. It uses abrasive-free chemical solution instead of slurry. On this study, ILD(INterlayer-Dielectric) was removed by CMP and wet-etching methods in order to investigate the superiority of wet etching mechanism. In the thin film wafer, the results were evaluated at a viewpoint of material removal rate(MRR) and within wafer non-uniformity(WIWNU). And pattern step height was also compared for planarization characteristics of the patterned wafer.

  • PDF

GaN계 질화합물 반도체의 습식식각 연구 (Studies on chemical wet etching of GaN)

  • 윤관기;이성대;이일형;최용석;유순재;이진구
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 1998년도 하계종합학술대회논문집
    • /
    • pp.398-400
    • /
    • 1998
  • In this paper, the etching studies for n-GaN were carried out using the wet chemical, the photo-enhanced-chemical, and the electro-chemical etching methods. The experimental results show that n-GaN is etched in diluted NaOH solution at room temperture and the etched thickness of NaOH and electron concentrations. Te etching rate of n-GaN samples with n.simeq.1*10$^{19}$ cm$^{-3}$ were used to compare the photo-enhanced-chemical etching with the electrochemical etching methods. The removed thickness was 680.angs./25min by the electrochemical etching methods. The removed thickness was 680 .angs./25min by the electrochemical etching method ad 784.angs./25min by the photoenhanced-chemical etching method. The patterns are 100.mu.m*100.mu.m rectangulars covered with SiO$_{2}$film. It is shown that the profile of etched side-wall of the pattern is vertical without dependance of the n-GaN orientations.

  • PDF

Photoelectrochemical Hydrogen Production on Textured Silicon Photocathode

  • Oh, Il-Whan
    • 전기화학회지
    • /
    • 제14권4호
    • /
    • pp.191-195
    • /
    • 2011
  • Wet chemical etching methods were utilized to conduct Si surface texturing, which could enhance photoelectrochemical hydrogen generation rate. Two different etching methods tested, which were anisotropic metal-catalyzed electroless etching and isotropic etching. The Si nano-texture that was fabricated by the anisotropic etching showed ~25% increase in photocurrent for H2 generation. The photocurrent enhancement was attributed to the reduced reflection loss at the nano-textured Si surface, which provided a layer of intermediate density between water and the Si substrate.

CoNbZr/Cu/CoNbZr 다층막의 습식 식각 거동 (A Behavior of the Wet Etching of CoNbZr/Cu/CoNbZr Multi-Layer Films)

  • 김현식;이영생;송재성;오영두;윤재홍
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권7호
    • /
    • pp.645-650
    • /
    • 1997
  • We manufactured CoNbZr/Cu/CoNbZr multi-layer films by rf magnetron sputtering methods and formed the patterns on the deposited multi-layer films. In this study, we fabricated a new etchant for forming the patterns by the wet etching with etchant and we searched for the best etching conditions and the etchant composition. Cu was etched selectively independent on the concentration of iron chloride solution, but amorphous CoNbZr thin film did not. The etchant was achieved by iron chloride solution(17.5 mol%) mixed with HF (20 mol%) during 150 sec, which etched CoNbZr/Cu/CoNbZr multi-layer films at the same time. Also, the etchant etched CoNbZr/Cu/CoNbZr multi-layer films by the three-step. It was shown that the cross-section had the isotropic structure and excellent etching characteristics with the above etchant.

  • PDF

습식 화학 식각에 의한 다결정 실리콘 웨이퍼의 표면 분석 및 효율 변화 (Surface Analysis and Conversion Efficiency of Multi-crystalline Silicon Solar Cell by Wet Chemical Etching)

  • 박석기;도겸선;송희은;강기환;안형근;한득영
    • 한국태양에너지학회:학술대회논문집
    • /
    • 한국태양에너지학회 2011년도 춘계학술발표대회 논문집
    • /
    • pp.111-115
    • /
    • 2011
  • Surface Texturing is an essential process for high efficiency in multi-crystalline silicon solar cell. In order to reduce the reflectivity, there are two major methods; proper surface texturing and anti-reflection coating. For texturization, wet chemical etching is a typical method for multi-crystalline silicon. The chemical solution for wet etching consists of HF, $NHO_3$, DI and $CH_3COOH$. We carried out texturization by the change of etching time like 15sec, 30sec, 45sec, 60sec and measured the reflectivity of textured wafers. As making the silicon solar cells, we obtained the conversion efficiency and relationship between texturing condition and solar cell characteristics. The reflectivity from 300nm to 1200nm was the lowest with 15 sec texturing time and 60 sec texturing time showed almost same reflectivity as bare one. The 45 sec texturing time showed the highest conversion efficiency.

  • PDF

HVPE로 성장된 GaN의 용융 KOH/NaOH 습식화학에칭 (The molten KOH/NaOH wet chemical etching of HVPE-grown GaN)

  • 박재화;홍윤표;박철우;김현미;오동근;최봉근;이성국;심광보
    • 한국결정성장학회지
    • /
    • 제24권4호
    • /
    • pp.135-139
    • /
    • 2014
  • 수소화기상증착에피탁시로 성장된 GaN 단결정의 표면 특성을 정밀하게 측정하기 위해, 용융 KOH/NaOH 습식화학에칭법을 적용하였다. KOH/NaOH 습식화학에칭법에 에칭속도는 기존의 황산, 인산과 같은 etchant에 비해 느린데, 이는 불용성 코팅층의 형성에 의한 것이다. 따라서 이 방법으로 etch pits density를 더 효율적으로 평가할 수 있었다. 성장된 GaN 단결정을 XRD(X-Ray Diffraction), XRC(X-ray rocking curve)로 결정성을 분석하였으며, 에칭 특성과 표면 형상은 주자전자현미경을 이용하여 관찰하였다. 에칭 실험 결과 격자결함들이 독립적으로 잘 분리되어 있고 그들의 형태가 명확하게 나타나는 최적 에칭 조건은 $410^{\circ}C$, 25분이었다. 이 조건에서 얻은 결함밀도 값은 $2.45{\times}10^6cm^{-2}$이었으며, 이는 상업적으로 이용 가능 한 정도의 재료임을 확인할 수 있었다.

GaN의 습식 화학식각 특성 (Wet chemical etching of GaN)

  • 최용석;유순재;윤관기;이일형;이진구;임종수
    • 한국결정성장학회지
    • /
    • 제8권2호
    • /
    • pp.249-254
    • /
    • 1998
  • GaN계 재료의 습식 화학식각 특성과 광 화학 및 전기 화학 및 전기 화학 습식식각 특성을 연구하였다. n형 GaN는 상온에서 NaOH 수용액에 식각되었으며 식각두께는 식각시간에 선형적으로 증가하였다. 또 광 조사 및 전기 화학을 가할 경우 식각율은 수배로 증가하였으며, 식각율은 $1{\times}10^{19};cm^{-3}$의 전자농도를 갖는 시료에서 광 조사시 최대 164${\AA}$/min을 얻었다. n-GaN의 식각율은 GaN의 전자농도에 크게 의존하는 특성을 나타내었으며 이러한 식각과정을 논의하였다. $SiO_2$ 박막으로 덮여진 100${\mu}m{\times}100{\mu}m$ 모양의 옆 식각면은 방향성을 갖지 않고 수직하였으며, 넓은 면적에서 매우 평탄하였다.

  • PDF

초정밀 나노구조물 형성을 위한 새로운 KOH 습식각 기술 (A Novel KOH Wet Etching Technique for Ultrafine Nanostructure Formation)

  • 강찬민;박정호
    • 한국전기전자재료학회논문지
    • /
    • 제24권2호
    • /
    • pp.156-161
    • /
    • 2011
  • The present study introduces a novel wet etching technique for nanostructure fabrications which usually requires low surface roughness. Using the current method, acquired profiles were smooth even in the nanoscale, which cannot be easily achieved with conventional wet or dry etching methods. As one of the most popular single crystal silicon etchant, potassium hydroxide (KOH) solution was used as a base solvent and two additives, antimony trioxide (Sb2O3) and ethyl alcohol were employed in. Four experimental parameters, concentrations of KOH, Sb2O3, and ethyl alcohol and temperature were optimized at 60 wt.%, 0.003 wt.%, 10 v/v%, and $23^{\circ}C$, respectively. Effects of additives in KOH solution were investigated on the profiles in both (110) and (111) planes of single crystal silicon wafer. The preliminary results show that additives play a critical role to decrease etch rate significantly down to ~2 nm/min resulting in smooth side wall profiles on (111) plane and enhanced surface roughness.

물중탕을 이용한 대면적 SiNx EUV 펠리클 제작 (Manufacturing Large-scale SiNx EUV Pellicle with Water Bath)

  • 김정환;홍성철;조한구;안진호
    • 반도체디스플레이기술학회지
    • /
    • 제15권1호
    • /
    • pp.17-21
    • /
    • 2016
  • EUV (Extreme Ultraviolet) pellicle which protects a mask from contamination became a critical issue for the application of EUV lithography to high-volume manufacturing. However, researches of EUV pellicle are still delayed due to no typical manufacturing methods for large-scale EUV pellicle. In this study, EUV pellicle membrane manufacturing method using not only KOH (potassium hydroxide) wet etching process but also a water bath was suggested for uniform etchant temperature distribution. KOH wet etching rates according to KOH solution concentration and solution temperature were confirmed and proper etch condition was selected. After KOH wet etching condition was set, $5cm{\times}5cm$ SiNx (silicon nitride) pellicle membrane with 80% EUV transmittance was successfully manufactured. Transmittance results showed the feasibility of wet etching method with water bath as a large-scale EUV pellicle manufacturing method.