무도장 내후성 강교량의 Box Girder 내부볼트 연결부에 대한 외부전원식 정기방식효과에 관한 연구 (A study on the effect of the external electric type corrosion resistance for the bolt connection in weathering steel box girders.)

  • 박용걸;김헌태;백찬호;최정열
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2004년도 추계학술대회 논문집
    • /
    • pp.988-993
    • /
    • 2004
  • This paper considers corrosion problems in the bolt connection of weathering steel box girder bridge using the external electric type corrosion resistance method which resisted to local corrosion in coated steel surface with contacted air. The weathering steel was created a rust itself in the passive state. but a coated box girder type was easily dew form could be made galvanic cell that accelerated corrosion. so that it was ruled by protection coat with some paint. Therefore, it needed that can be applied the external electric type corrosion resistance method in coated surface. As a result of the test of polarization amount had measured that the weathering steel was higher currents than the general steel by about $5\~10\%$. Therefore. an external electric type corrosion resistance method can be used to protect local corrosion in the coated bolt connection of weathering steel box girders effectively.

  • PDF

에폭시와 아크릴 전착도료의 혼용성에 따른 물성 변화 연구 (Study on the Physical Properties by Combining Epoxy and Acryl Electrodeposition Paints)

  • 정성수;이동욱;김동원;김명환;곽삼탁;문명준
    • 한국표면공학회지
    • /
    • 제47권3호
    • /
    • pp.137-146
    • /
    • 2014
  • The important drawback of epoxy electrodeposition(ED) coatings is the lack of the weathering resistance caused by the structure of bisphenol A. To improve this yellowing phenomena, acryl ED coatings have been developed. Compared with the epoxy ED coatings, however, acryl ED coatings are relatively weak in the corrosion resistance and mechanical properties. The purpose of this study is complemented their drawbacks by mixing epoxy and acryl ED paints. The salt spray, accelerated weathering test(QUV) and cupping, bending, impact test were employed to investigate the corrosion resistance, weathering resistance, and mechanical properties of ED coatings. When the ratio of acryl to epoxy resin of ED coating is 0.33, the weathering resistances are appropriately improved in condition maintaining the corrosion resistance. It was shown that the weathering resistance for epoxy ED coating was adjusted by optimally mixing acryl ED paint.

촉진 열화 느티나무 부재의 역학적 특성 (Mechanical Properties of Zelkova Serrata Makino in Accelerated Weathering Test)

  • 김광철;박천영
    • 한국가구학회지
    • /
    • 제26권4호
    • /
    • pp.392-397
    • /
    • 2015
  • This study was carried out to analyze the effects on mechanical properties of deteriorated wood member by outdoor condition. The surface color, mechanical properties and structural stability of traditional wooden structures, exposed in water and UV, could be changeable. For the purpose, accelerated weathering test based on outdoor condition was carried out. The weathering time levels were composed 0, 500, 1000, 1,500 and 2,000 hours and mechanical properties were evaluated on each specimen according to weathering time level. Bending properties were decreased on weathering but recovered after 1,000 hours. Fatigue and impact strength were decreased to 1,000 hours and did not changed since then. Abrasion resistance was minimized in 1,000 hours. This results could be utilized for effectively stability management of traditional wooden structures and members.

상주지역 화강암의 풍화 특성에 대한 평가 (Evaluation about Weathering Characteristics of Granite at Sangju Area)

  • 강창우;김봉수;손광록;배우석
    • 한국지반환경공학회 논문집
    • /
    • 제17권5호
    • /
    • pp.17-25
    • /
    • 2016
  • 지표에 노출되는 암석은 기상작용 등의 영향으로 풍화가 가속되며, 풍화작용은 광물의 성질을 변화시켜 암석의 안정성을 저하시키게 되므로 암석의 풍화에 대한 저항은 광물의 조성을 파악하는 것이 중요하며 이는 풍화 민감도 분석을 통해 이루어진다. 따라서 본 연구에서는 시추된 시료에 대한 현미경 박편 시험을 실시하고 모드분석을 통해 풍화 취약광물의 구성비를 측정하였으며, 이를 통해 대상사면의 암석학적 광물학적 풍화요인을 평가하였다. 또한, X-Ray 회절분석을 이용하여 암석을 구성하는 실제적인 광물조성을 정량적으로 측정하고 주사현미경관찰을 통해 이차광물을 동정하여 풍화의 진행 정도를 파악하였다. 이러한 풍화 민감도 기법을 통하여 풍화 저항도를 판단할 수 있는 적절한 지시자를 결정할 수 있으며 화학적 풍화속도를 이용한 풍화등급의 예측이 가능할 것으로 분석되었다.

Decay Efficacies of Plywoods Manufactured by ACQ-treated Veneers of Domestic Softwood and Hardwood Species

  • Suh, Jin Suk;Lee, Hyun Mi;Hwang, Won Jung;Hwang, Sung Wook;Lee, Dong Heub;Park, Sang Bum
    • 한국가구학회지
    • /
    • 제25권3호
    • /
    • pp.233-237
    • /
    • 2014
  • The eco-friendly preservatives such as ACQ or CUAZ have been used in landscape architectural facilities these days. In this study, the decay efficacies of ACQ treatments were evaluated according to domestic veneer species, concentration of ACQ, weathering test, adhesive type, and fungus type. In case of veneer species, hinoki cypress and yellow poplar showed the highest and lowest decay resistance, respectively. And the decay resistance appeared to be greater in plywoods bonded by resorcinol resin-bonded plywood and non-weathering treated plywood than polyurethane resin-bonded plywood and weathering treated plywood.

  • PDF

Design of Advanced Weathering Steel with High Corrosion Resistance for Structural Applications

  • Choi, B.K.;Jung, H.G.;Yoo, J.Y.;Kim, K.Y.
    • Corrosion Science and Technology
    • /
    • 제4권4호
    • /
    • pp.121-129
    • /
    • 2005
  • Basic design concept of the future steel structure requires environmental compatibility and maintenance free capability to minimize economic burdens. Recent trends in alloy design for advanced weathering steel include addition of various alloying elements which can enhance formation of stable and protective rust layer even in polluted urban and/or high $Cl^{-}$ environment. The effects of Ca, Ni, W, and Mo addition on the corrosion property of Ca-modified weathering steel were evaluated through a series of electrochemical tests (pH measurement and electrochemical impedance spectroscopy: EIS) and structural analysis on rust layer formed on the steel surface. Ca-containing inclusions of Ca-Al-Mn-O-S compound are formed if the amount of Ca addition is over 25 ppm. Steels with higher Ca content results in higher pH value for condensed water film formed on the steel surface, however, addition of Ni, W, and Mo does not affect pH value of the thin water film. The steels containing a high amount of Ca, Ni, W and Mo showed a dense and compact rust layer with enhanced amount of ${\alpha}-FeOOH$. Addition of Ni, W and Mo in Ca-modified weathering steel shows anion-selectivity and contributes to lower the permeability of $Cl^{-}$ ions. Effect of each alloying element on the formation of protective rust layer will be discussed in detail with respect to corrosion resistance.

풍화에 따른 퇴적암의 강도 변화 (The Variation of Sedimentary Rock Strength due to Weathering)

  • 배우석;이봉직;오세욱;이종규
    • 한국안전학회지
    • /
    • 제18권1호
    • /
    • pp.89-93
    • /
    • 2003
  • The failure of rock slopes were influenced by weathering, which causes change in the shear strength. The weathering is also directly related to slaking and swelling characteristics. In the paper, the core of diameter loom was obtained by digging on rock slope of Kong-ju in Korea and then EDX(Energy Dispersive X-ray spectrometer) analysis was carried out to verified element of chief rock-forming minerals. Uniaxial compression tests, slaking tests, and point load test are performed to study engineering characteristics of conglomerate and red shale. As a results of slaking test, slaking index of conglomerate indicate range of 85.11-99.58 and shale indicate 58.37-99.23. Therefore, it is recognized that the resistance of shale to weathering decreases in shallow depth and it greatly influences the strength of rock. The result of uniaxial compression test and Point load test show that the strength of sedimentary such as conglomerate and red shale has an influence on both weathering and saturation.

싸이클로알리파틱 에폭시 절연재료의 옥외 성능에 미치는 층전재 및 첨가물의 영향 (Effect of Filler and Additive on Performance of Cycloaliphatic Epoxy used for Outdoor Insulators)

  • 허창수;연복희;서유진;이기택;김남렬;황명근;김완태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.431-434
    • /
    • 2002
  • This paper reports on the evaluation of weathering resistance, tracking test and salt-fog of various kinds of cycloaliphatic epoxy systems. It was found that UV irradiation induced the loss of hydrophobic level due to the chain scission attack at the surface. It could be seen that samples containing an UV absorbent/antioxidant and a silicone oil additive knave a good performance in weathering ageing, whereas ATH filled ones have high resistance against tracking failure than others. Under salt-fog test, specimens mixed with silicone oil could suppress leakage current development. It was thought that silicone oil mixed into cycloaliphatic epoxy system could lead to lower the surface energy and to retain hydrophobic properties for a long time, which are desirable for outdoor performances.

  • PDF

Atmospheric Corrosion Process for Weathering Steel

  • Nagano, Hiroo;Yamashita, Masato
    • Corrosion Science and Technology
    • /
    • 제7권2호
    • /
    • pp.119-124
    • /
    • 2008
  • Steel is generally not corrosion resistant to water with formation of non protective rusts on its surface. Rusts are composed of iron oxides such as $Fe_3O_4$, $\alpha-$, $\beta-$, $\gamma-$and ${\delta}-FeOOH$. However, steel, particularly weathering steel containing small amounts of Cu, Ni and Cr etc., shows good corrosion resistance against rural, industrial or marine environment. Its corrosion rate is exceedingly small as compared with that of carbon steel. According to the exposure test results undertaken in outdoor environments, the atmospheric corrosion rate for weathering steel is only 1 mm for a century. Atmospheric corrosion for steels proceeds under alternate dry and wet conditions. Dry condition is encountered on steel surface on fine or cloudy days, and wet condition is on rainy or snowy days. The reason why weathering steel shows superior atmospheric corrosion resistance is due to formation of corrosion protective rusts on its surface under very thin water layer. The protective rusts are usually composed of two layer rusts; the upper layer is ${\gamma}-FeOOH$ termed as lepidocrocite, and inner layer is nano-particle ${\alpha}-FeOOH$ termed as goethite. This paper is aimed at elucidating the atmospheric corrosion mechanism for steel in comparison with corrosion in bulky water environment by use of empirical data.The summary is as follows: 1. No corrosion protective rusts are formed on steel in bulky water. 2. Atmospheric corrosion for steel is the corrosion under wetting and drying conditions. Corrosion and passivation occur alternately on steel surface. Steel, particularly weathering steel with small amounts of alloying elements such as Cu, Ni and Cr etc. enhances forming corrosion protective rusts by passivation.

무도장 내후성강의 장기 내식성 및 그 현장즉시측정법 (Long-term corrosion-resistance of an uncoated weathering steel and its on-line and in-situ measurements)

  • 박정렬;김규영
    • 한국강구조학회 논문집
    • /
    • 제16권4호통권71호
    • /
    • pp.415-423
    • /
    • 2004
  • 옥외 강구조물의 중요 소재인 무도장 내후성강의 장기 내식성을 평가하기 위해 우선 9년 이상 산업대기와 전원대기에 폭로된 본 강판 및 비교재 일반강판 시편의 천향면에 대해 중성의 인공우수에 침적시켜 전기화학적 부식전위, 임피던스 및 동전위 양분극 곡선으로 측정 및 그 결과를 고찰하였다. 산업대기 및 전원대기에 천향면으로 폭로된 내후성강 표면에는 부동태적인 안정화 녹층이 발달하였으며, 산업대기 폭로 표면의 인공우수에서의 부식속도는 $3{{\mu}m}/y$로 측정되어 우수한 내후내식 녹층으로 덮혀 있었다. 지속적으로 인공우수에 침적시키면 모든 시편 녹층은 점진적으로 열화되어 모재 철분의 양극산화용해 율속의 부식으로 진전됨을 나타내었다. 내후성 합금성분은 이런 부식의 진전을 지연시키고 있었다. 장기 내식성을 잘 평가하기 위해서는 9년보다 훨씬 장기간 대기폭로된 강재표면과 해당 대기 응축수 모사 수용액을 이용한 전기화학적 측정이 필요하다. 특히 본 측정방법들은 강재 표면의 원하는 부위와 폭로시간대에 거의 비파괴적으로 부식상황과 녹층의 상태와 정량적인 부식속도를 직접 바로 측정할 수 있게 하므로 강재를 사용한 교량, 탑, 건축물 등의 강구조물의 표면에 전기화학적 cell을 구성하고 이동측정기를 사용하면 강구조물의 내후 내식성을 현장즉시 측정 및 평가를 효과적으로 가능하게 할 수 있다.