Abstract

This study was carried out to analyze the effects on mechanical properties of deteriorated wood member by outdoor condition. The surface color, mechanical properties and structural stability of traditional wooden structures, exposed in water and UV, could be changeable. For the purpose, accelerated weathering test based on outdoor condition was carried out. The weathering time levels were composed 0, 500, 1000, 1,500 and 2,000 hours and mechanical properties were evaluated on each specimen according to weathering time level. Bending properties were decreased on weathering but recovered after 1,000 hours. Fatigue and impact strength were decreased to 1,000 hours and did not changed since then. Abrasion resistance was minimized in 1,000 hours. This results could be utilized for effectively stability management of traditional wooden structures and members.

Keywords

References

  1. 강호양, 김수원, 박상진. 2003. 무수초산 및 포름알데하이드 기상처리 산벚나무의 야외 폭로 및 촉진열화. 목재공학회 31(5): 57-64.
  2. 강호양, 박상진, 김영숙. 2002. 촉진 열화 목재의 흡습성과 초음파 전달 속도. 목재공학회 30(1): 18-24.
  3. 김광철. 2012. 소나무재의 촉진열화실험에 따른 재색변화에 대한 연구. 한국가구학회 23(2): 152-162.
  4. 김광철. 2012. 촉진열화실험에 의한 소나무의 물성 및 조직변화에 대한 연구. 한국가구학회 23(3): 324-331.
  5. 성덕룡, 박용걸, 고동춘, 이시용, 민낙기. 2010. 실물 휨 피로시험을 통한 철도 레일의 휨 피로 거동 분석. 한국철도학회 13(2): 201-207.
  6. 장동일, 재원규, 손영현. 1992. 강섬유보강 콘크리트의 휨 피로 거동에 관한 연구. 콘크리트학회 4(1): 81-87.
  7. 정호, 안병만, 이두면, 신필수, 박수연. 2002. 옥외 노출소재의 신뢰성 평가 기술 및 표준화. 한국신뢰성학회 정기학술대회. 147-155쪽.
  8. ASTM. 2008. Standard practice for collection of settled dust samples using wipe sampling methods for subsequent determination of metals. American Society of Testing and Materials, Philadelphia, USA.
  9. Kalnins, M. A., Feist, W. C. 1993. Increase in wettability of wood with weathering. Forest Prod. J. 43(2): 55-57.
  10. Pascal Nzokou, D. Pascal Kamdem, Ali Temiz. 2011. Effect of accelerated weathering on discoloration and roughness of finished ash wood surfaces in comparison with red oak and hard maple. Progress in Organic Coatings 71. 350-354. https://doi.org/10.1016/j.porgcoat.2011.03.028
  11. Wang, J., Wu, X., Jiang, M., Morris, P. 2007. Decay hazard classifications in China for exterior above-ground wood. The International Research Group on Wood Preservation IRG/WP 07-20357. Stockholm, Sweden.