In order to improve the flow performance of high performance concrete, use of high performance water reducing agent and low viscosity type water reducing agent is a study of suitable range of use due to side effects. in this study, we aimed at reducing viscosity and yield value using high performance water reducing agent and low viscosity type water reducing agent, and this was evaluated using a rheometer. as a result of analysis of viscosity and yield value, it was found that the high performance water reducing agent has higher reduction effect than the low viscosity type water reducing agent. however, the larger the viscosity lowering effect is, the lower the usable range is, compared to general high performance water reducing agents, and it was found that sufficient consideration for this judgment of appropriate quantity is necessary.
This paper investigates the influences of water content and viscosity agent on the bleeding of concrete. According to test results, fluidity shows decline tendency as water content decreases, and dosage of viscosity agent increases. PEO viscosity agent does not affect the air contents while, MC viscosity agent causes air loss. As for bleeding, bleeding decreases with decrease of water content. As dosage of viscosity agent increase, bleeding decreases, regardless of viscosity kinds. It is thought that viscosity agents have the favorable effect of reducing bleeding, if fluidity and air loss are improved.
High performance concrete with low water-to-cement ratio has been widely used with increased demand of high rising buildings and huge scaled structures. Additionally, for high performance concrete, various SCMs are replaced to improve its performance from fresh state to hardened state. With the drawback of increased viscosity of the concrete mixture for high performance concrete, low-viscosity typed high range water reducer is the relatively new admixture. Therefore, as a goal of the research, under using various SCMs with wide range of content, the performance of low-viscosity typed high range water reducer was evaluated. Especially, in this research, the influence of low-viscosity typed high range water reducer on rheological properties including plastic viscosity and yield stress were assessed. As a result of the research, it is expected to provide a fundamental information of low -viscosity typed high ranged water reducer on high performance concrete with various conditions of SCMs.
Experiments were carried out in humans to assess the relationship between viscosity and post-prandial glucose response of soluble fibers. Eight(3 male and 5 female) healthy individuals were tested for their glucose response after taking control meals or 3 test fiber meals of different viscosities. Meal viscosity of the test food was adjusted to be between 200 and 70, 000 cps. There was a significant increase in post-prandial glucose response(p=0.01) in control meals by solely increasing the volume of water. Fiber with the highest viscosity konjac mannan demonstrated the lowest relative glucose response(70.1$\pm$6.6), followed by medium viscosity xanthan (79.3$\pm$8.7)and low viscosity psyllium (86.3$\pm$10.5). The difference is significant at the level of p<0.05. However, no significant difference in relative glucose response of the same fiber was found when the 4 levels of water were added to make different meal viscosity of each fiber (p=0.476). This result suggested that hypoglycemic action of soluble dietary fibers is related to fiber viscosity rather than meal viscosity.
Journal of Advanced Marine Engineering and Technology
/
제7권2호
/
pp.15-21
/
1983
Preparing for treatment and management of the emulsified fuel oil which will be generalized henceforth, this paper is an attempt to examine the viscosity-temperature characteristics of emulsified heavy fuel oil which is mixed with water and emulsifier in various mixture ratio by mechanical mixer. The experimental results are summarized as follows: 1. The viscosity-temperature characteristics of the emulsified C & B grade heavy fuel oil mixed with water of same or less weight, is changed according to log.log(v+0.6)=b-3.8log T. 2. The emulsifier has to be added to the emulsified A grade heavy fuel oil mixed with water of same or less weight, because it is instable. Especially if the emulsifier is sodium stearate, it is added more than 0.3% of the weight of oil and water. 3. In the emulsified A grade heavy fuel oil mixed with water and emulsifier, the higher the ratio of water addition becomes, the higher the viscosity is and the more the viscosity-temperature slope decreases. But the higher the ratio of emulsifier addition is, the more the viscosity-temperature slope increases. In this case, the linearity of viscosity-temperature characteristic curve is poorer than that of B and C grade heavy fuel oil. 4. In the emulsified A grade heavy fuel oil mixed with emulsifier of 0.3% or less, the emulsion type is O/W type when water addition ratio is 40%, but it is W/O type when it is 10%, 20%, 30% and 50%.
In order to meet the high performance of the concrete, the viscosity increases with water binder ratio and amount of powder. because of these problems, we use high performance water reducing agent and low viscosity water reducing agent, but side effects may occur when using large amount of water reducing agent. Therefore, in this research, in order to increase the viscosity, I would like to analyze the change in viscosity and flow characteristics of paste by utilizing fly ash and lung limestone which are generally thrown away without using high performance water reducing agent.
For the application of the commercially modified starch in frozen and retort foods, apparent viscosity and water loss were measured at each stages of heating, sterilization and freezing-thawing stages. Apparent viscosity showed the exponential increase with concentration and the slopes of apparent viscosity against concentration in the Firm-Tex(hydroxypropyl distarch phosphate), Hi-Flo(acetylated distarch adipate) and Colflo 67(acetylated distarch adipate) from waxy maize starch were higher than those of Amyloacetate M20(starch acetate) and X-amylo 250(distarch phosphare) from potato starch. In the presence of 1 or 2% NaCl, X-amylo 250 among modified starches showed the increase in water loss and the decrease in apparent viscosity, whereas Colflo 67, Hi-Flo and Firm-Tex were little affected by NaCl. In the presence of 1 or 2% sucrose, water loss and apparent viscosity of the modified starches were not affected. In the range of pH 4~8, water loss and apparent viscosity of the modified starches had no change but the differences were detected to some extent between each of heating, sterilization and freezing-thawing stages. In the apparent viscosity and water loss of the modified starches after 3 week storage from heating and sterilization, Hi-Flo, Amyloacetate M20 and X-amylo 250 were not changed at the storage period, and the overall acceptability of retort food containing the modified starches such as Firm-Tex and Amyloacetate M20 were favored more than others. In the apparent viscosity and water loss of the modified starches which have been frozen and thawed three times repeatedly, Colflo 67, Hi-Flo and Firm-Tex were not changed in freezingthawing, and the overall acceptability of frozen food containing Firm-Tex was most favored.
In this paper we report fluid flow characteristics of $Al_2O_3$ nanoparicles suspended in water. Especially, the effects of volume fraction with the range of 0.01% to 0.3% and tube diameter with $310{\mu}m$ to 1.735mm on the pressure drop and the effective viscosity of $Al_2O_3$ nanoparicles suspended in water are experimentally investigated. It is shown that the effective viscosity of water-based $Al_2O_3$ nanofluids with 0.1 Vol.% through a circular tube of 1.024mm diameter is increased to about 6%. The effective viscosity from experimental results is compared with that from Einstein model. With the comparison, we show that Einstein model for determining the effective viscosity of nanofluids is not applicable to water-based $Al_2O_3$ nanofluids.
Viscosity agents were added to water to improve extinguishing performance of low pressure water mist suppression system on wood cribs fire, and a small scale wood cribs fire experiment was conducted to measure the extinguishing performance. CMC and agar were used for viscosity agent and as the amount of viscosity agent enlarges, it showed the increase of the viscosity of aqueous solution and the decrease of the fluidity. On wood cribs fire experiment, the extinguishing efficiency was improved with supplemental viscosity agent as it enhanced the adhesive time of aqueous solution on the wood, and therefore expanded the contact time of fire surface. The surface tension of aqueous solution was decreased with the addition of agar which to be assumed as an increase factor of extinguishing efficiency. By the extinguishing experimental result, the most effective extinguishing agent was CMC 0.6 wt.%, with the flame suppression time and the extinguishing time were reduced by 70s and 93s respectively at this concentration.
Bidgoli, Mahmood Rabani;Kolahchi, Reza;Karimi, Mohammad Saeed
Structural Engineering and Mechanics
/
제58권1호
/
pp.93-102
/
2016
This article presents an experimental study on the effect of temperature and solid volume fraction of nanoparticles on the dynamic viscosity for the CuO/EG-water nanofluid. Nanoparticles with diameter of 40 nm are used in the present study to prepare nanofluid by two-step method. A "Brookfield viscometer" has been used to measure the dynamic viscosity of nanofluid with solid volume fraction up to 2% at the temperature range between 20 to $60^{\circ}C$. The findings have shown that dynamic viscosity of nanofluid increases with increasing particle volume fraction and decreasing temperature. Nine different correlations are developed on experimental data point to predict the relative dynamic viscosity of nanofluid at different temperatures. To make sure of accuracy of the proposed correlations, margin of deviation is presented at the end of this study. The results show excellent agreement between experimental data and those obtained through the correlations.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.