• Title/Summary/Keyword: TiO2 catalyst

Search Result 443, Processing Time 0.029 seconds

Photodegradation of Gaseous Toluene Using Short-Wavelength UV/TiO2 and Treatment of Decomposition Products by Wet Scrubber (단파장자외선/TiO2 공정에 의한 가스상 톨루엔의 분해 및 습식세정장치에 의한 분해생성물의 제거)

  • Jeong, Ju-Young;Jurng, Jong-Soo
    • Journal of Environmental Science International
    • /
    • v.16 no.4
    • /
    • pp.433-440
    • /
    • 2007
  • The photodegradation and by-products of the gaseous toluene with $TiO_2$ (P25) and short-wavelength UV ($UV_{254+185nm}$) radiation were studied. The toluene was decomposed and mineralized efficiently owed to the synergistic effect of photochemical oxidation in the gas phase and photocatalytic oxidation on the $TiO_2$ surface. The toluene by the $UV_{254+185nm}$ photoirradiated $TiO_2$ were mainly mineralized $CO_2$ and CO, but some water-soluble organic intermediates were also formed under severe reaction conditions. The ozone and secondary organic aerosol were produced as undesirable by-products. It was found that wet scrubber was useful as post-treatment to remove water-soluble organic intermediates. Excess ozone could be easily removed by means of a $MnO_2$ ozone-decomposition catalyst. It was also observed that the $MnO_2$ catalyst could decompose organic compounds by using oxygen reactive species formed in process of ozone decomposition.

Crystal Structure Dependence for Reactivities of B12-TiO2 Hybrid Catalysts with Anatase and Rutile Forms

  • Shimakoshi, Hisashi;Nagami, Yoko;Hisaeda, Yoshio
    • Rapid Communication in Photoscience
    • /
    • v.4 no.1
    • /
    • pp.9-11
    • /
    • 2015
  • The debromination of phenethyl bromide by the $B_{12}-TiO_2$ hybrid catalyst under UV light irradiation was investigated. The catalytic efficiency was dependent on the type of $TiO_2$. The anatase form of $TiO_2$ was superior to the rutile form of $TiO_2$. The selectivity of the product was also dependent on the crystal structure of $TiO_2$, and the rutile form of $TiO_2$ showed a high selectivity for the formation of the coupling product, 2,3-diphenylbutane, when compared to that of the anatase form of $TiO_2$.

Anodic surface treatment for the fabrication of catalyst-doped TiO2 nanotubes (전기화학적 표면처리를 이용한 촉매가 도핑된 TiO2 나노튜브의 제조)

  • Yu, Hyeon-Seok;Seong, Mi-Jeong;Choe, Jin-Seop
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2014.11a
    • /
    • pp.266-267
    • /
    • 2014
  • $TiO_2$ 기반의 DSA 전극에 촉매제를 동시에 도핑할 수 있는 양극산화 단일 공정을 연구하였다. 에틸렌 글리콜 용매하에 $KRuO_4$$NH_4F$를 전해질로 사용하여 타이타늄을 양극산화 할 때 도핑과 나노구조 제어를 동시에 수행할 수 있었다. TEM과 XPS 분석 결과, 균일한 Ru 산화물이 $TiO_2$ 구조 내에 분포함을 확인할 수 있었다.

  • PDF

Physico-chemical effects of cerium oxide on catalytic activity of CeO2-TiO2 prepared by sol-gel method for NH3-SCR (CeO2가 졸겔법으로 합성한 CeO2-TiO2계 SCR용 촉매의 활성에 미치는 물리화학적 영향)

  • Kim, Buyoung;Shin, Byeongkil;Lee, Heesoo;Chun, Ho Hwan
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.6
    • /
    • pp.320-324
    • /
    • 2013
  • The effects of $CeO_2$ on catalytic activity of $CeO_2-TiO_2$ for the selective catalytic reduction (SCR) of $NO_x$ were investigated in terms of structural, morphological, and physico-chemical analyseis. $CeO_2-TiO_2$ catalysts were synthesized with three different additions, 10, 20, and 30 wt% of $CeO_2$, by the sol-gel method. The XRD peaks of all specimens were assigned to a $TiO_2$ phase (anatase) and the peaks became broader with the addition of $CeO_2$ because it was dispersed as an amorphous phase on the surface of $TiO_2$ particles. The specific surface area of $TiO_2$ increased with the addition of $CeO_2$ from $60.6306m^2/g$ to $116.2791m^2/g$ due to suppression of $TiO_2$ grain growth by $CeO_2$. The 30 wt% $CeO_2-TiO_2$ catalyst, having the strongest catalytic acid sites ($Br{\Phi}nsted$ and Lewis), showed the highest $NO_x$ conversion efficiency of 98 % at $300^{\circ}C$ among the specimens. It was considered that $CeO_2$ contributes to the improvement of the $NO_x$ conversion of $CeO_2-TiO_2$ catalyst by increasing specific surface area and catalytic acid sites.

Degradation and mineralization of violet-3B dye using C-N-codoped TiO2 photocatalyst

  • Putri, Reza Audina;Safni, Safni;Jamarun, Novesar;Septiani, Upita;Kim, Moon-Kyung;Zoh, Kyung-Duk
    • Environmental Engineering Research
    • /
    • v.25 no.4
    • /
    • pp.529-535
    • /
    • 2020
  • The present study investigated the photodegradation of synthetic organic dye; violet-3B, without and with the addition of C-N-codoped TiO2 catalyst using a visible halogen-lamp as a light source. The catalyst was synthesized by using a peroxo sol-gel method with free-organic solvent. The effects of initial dye concentration, catalyst dosage, and pH solution on the photodegradation of violet-3B were examined. The efficiency of the photodegradation process for violet-3B dye was higher at neutral to less acidic pH. The kinetics reaction rate of photodegradation of violet-3B dye with the addition of C-N-codoped TiO2 followed pseudo-first order kinetics represented by the Langmuir-Hinshelwood model, and increasing the initial concentration of dyes decreased rate constants of photodegradation. Photodegradation of 5 mg L-1 violet-3B dye achieved 96% color removal within 240 min of irradiation in the presence of C-N-codoped TiO2 catalyst, and approximately 44% TOC was removed as a result of the mineralization.

Morphology Control of Single Crystalline Rutile TiO2 Nanowires

  • Park, Yi-Seul;Lee, Jin-Seok
    • Bulletin of the Korean Chemical Society
    • /
    • v.32 no.10
    • /
    • pp.3571-3574
    • /
    • 2011
  • Nano-scaled metal oxides have been attractive materials for sensors, photocatalysis, and dye-sensitization for solar cells. We report the controlled synthesis and characterization of single crystalline $TiO_2$ nanowires via a catalyst-assisted vapor-liquid-solid (VLS) and vapor-solid (VS) growth mechanism during TiO powder evaporation. Scanning electron microscope (SEM) and transmission electron microscope (TEM) studies show that as grown $TiO_2$ materials are one-dimensional (1D) nano-structures with a single crystalline rutile phase. Also, energy-dispersive X-ray (EDX) spectroscopy indicates the presence of both Ti and O with a Ti/O atomic ratio of 1 to 2. Various morphologies of single crystalline $TiO_2$ nano-structures are realized by controlling the growth temperature and flow rate of carrier gas. Large amount of reactant evaporated at high temperature and high flow rate is crucial to the morphology change of $TiO_2$ nanowire.

Catalytic Effects and Characteristics of Ni-based Catalysts Supported on TiO2-SiO2 Xerogel

  • Jeong, Jong-Woo;Park, Jong-Hui;Choi, Sung-Woo;Lee, Kyung-Hee;Lee, Chang-Seop
    • Bulletin of the Korean Chemical Society
    • /
    • v.28 no.12
    • /
    • pp.2288-2292
    • /
    • 2007
  • The catalytic activities of nickel-based catalysts were estimated for oxidizing acetaldehyde of VOCs exhausted from industrial facilities. The catalysts were prepared by sol-gel methods of SiO2 and SiO2-TiO2 as a xerogel followed by impregnating Al2O3 powder with the nickel nitrate precursor. The crystalline structure and catalytic properties for the catalysts were investigated by use of BET surface area, X-ray diffraction (XRD), Xray photoelectron spectroscopy (XPS) and temperature programmed reduction (TPR) techniques. These results show that nickel oxide is transformed to NiAl2O4 spinel structure at the calcination temperature of 400 °C in response to the steps with after- and co-impregnation of Al2O3 powder in sol-gel process. The NiAl2O4 could suppress the oxidation reaction of acetaldehyde by catalysts. The NiO is better dispersed on SiO2-TiO2/Al2O3 support than SiO2/Al2O3 and SiO2-TiO2-Al2O3 supports. From the testing results of catalytic activities for oxidation of acetaldehyde, Catalysts showed a big difference in conversion efficiencies with the way of the preparation of catalysts and the loading weight of nickel. The catalyst of 8 wt.% Ni/TiO2-SiO2/Al2O3 showed the best conversion efficiency on acetaldehyde oxidation with 100% conversion efficiency at 350 °C.