• Title/Summary/Keyword: Teeth wear

Search Result 172, Processing Time 0.021 seconds

COMPARISON OF WEAR RESISTANCE AMONG RESIN DENTURE TEETH OPPOSING VAR10US RESTORATIVE MATERIALS (수복재료에 대합되는 의치용 레진치의 마모저항성 비교)

  • Lee, Chul-Young;Chung, Moon-Kyu
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.3
    • /
    • pp.313-327
    • /
    • 1999
  • The aim of this study was to compare wear resistance of resin denture teeth opposing various restorative materials. The wear resistance of conventional acrylic resin teeth(Trubyte Biotone) and three high-strength resin teeth(Bioform IPN, Endura, SR-Orthosit-PE) opposing different restorative materials(gold alloys, dental porcelain, composite resin) was compared. Wear tests were conducted with a sliding-induced wear testing apparatus which applied 100,000 strokes to the specimen in a mesio-distal direction under conditions of 100 stroke/min and constant loading of 1Kgf/tooth. Wear resistance of the resin denture teeth was evaluated by the following criteria : 1) wear depth, 2) weight loss, and 3) SEM observation. Results were as follows. 1. When opposed to gold alloys and composite resin, high-strength resin teeth showed superior wear resistance compared to acrylic resin teeth. But, in cases opposing dental porcelain, differences between the wear of the high-strength and acrylic resin teeth were not statistically significant (p<0.05). 2. When comparing wear resistance among high-strength resin teeth, opposing gold alloys, Endura was slightly more resistant and while in cases opposing dental porcelain, SR-Orthosit-PE was showed to be slightly resistant(p<0.05). 3. The wear of high-strength resin teeth was greater by 5 to 7 times when opposing porcelain and 2 to 3 times when opposing composite resin compared to gold alloys(p<0.05). 4. SEM observations of the wear surface showed that wear of resin teeth opposing gold alloys is a fatigue type of wear and wear of resin teeth opposing dental porcelain is fatigue and abrasion type of wear. Trubyte Biotone showed more severe fatigue type of wear than high-strength resin teeth. In conclusion, the use of dental porcelain should seriously be considered as restorative material in cases opposing resin denture teeth and improvement seems to be needed on resin teeth in the areas of wear resistance.

  • PDF

Comparison Study of Wear Resistance Among Several Denture Teeth Opposing Various Restorative Materials (대합되는 재료에 따른 합성수지 인공치의 마모저항성에 관한 비교 연구)

  • Park, Young-Bae
    • Journal of Technologic Dentistry
    • /
    • v.31 no.1
    • /
    • pp.63-74
    • /
    • 2009
  • Partial or complete prosthesis is needed when teeth are lost due to various kinds of reason. Artificial teeth recover occlusion instead of natural teeth. Artificial teeth are required of esthetics, fragile resistance and abrasive resistance. Artificial tooth is made of acrylic resin or porcelain. Nowadays, acrylic resin artificial teeth are mainly used. Acrylic resin teeth are occluded with natural teeth, gold alloy, Ni-Cr alloy or porcelain etc. Acrylic resin teeth have similar translucency, gloss of natural teeth. And it has good chemical bond with denture base material, but it has low wear resistance. The aim of this study is to compare wear resistance among several denture teeth(Endura, SR-orthosit-PE, Planustar) and between artificial resin denture teeth and opposing 3 restorative materials(gold, Ni-Cr alloy, porcelain). Wear tests were conducted with a rotating wear testing apparatus(pin-on-disk type wear tester) under conditions of rpm 180, 75 minutes and constant loading of 50N. The upper part was the cusp of maxillary first molar and the lower part was a disk type restorative materials. To make similar oral environment, water was supplied continually. The acrylic resin teeth wear was determined by weighing the cusp each 5 minutes during 75 minutes test. Vicker's hardness tester was used to evaluate the surface hardness of test specimens. The SEM was used to evaluate the wear surfaces. The results were as follows: 1. Wear rates of acrylic resin teeth opposing to the restorative materials were high in order of Porcelain, Gold, Ni-Cr alloy (p<.05). 2. Wear resistance rate opposing to the Porcelain disk, was shown in order of Endura, SR-orthosit-PE, Planustar. The wear rate of opposing to porcelain disk was above two times more than that of other groups (p<.05). 3. Wear resistance rates opposing to the Gold, Ni-Cr alloy disk, was shown in order of Endura, SR-orthosit-PE, Planustar (p<.05). 4. A degree of the surface hardness is directly proportional to the degree of wear resistance. There are statistically significant differences between each groups (p<.05).

  • PDF

Influence of zirconia and lithium disilicate tooth- or implant-supported crowns on wear of antagonistic and adjacent teeth

  • Rosentritt, Martin;Schumann, Frederik;Krifka, Stephanie;Preis, Verena
    • The Journal of Advanced Prosthodontics
    • /
    • v.12 no.1
    • /
    • pp.1-8
    • /
    • 2020
  • PURPOSE. To investigate the influence of crown material (lithium-disilicate, 3Y-TZP zirconia) and abutment type (rigid implant, resin tooth with artificial periodontium) on wear performance of their antagonist teeth and adjacent teeth. MATERIALS AND METHODS. A mandibular left first molar (#36) with adjacent human teeth (mandibular left second premolar: #35, mandibular left second molar: #37) and antagonistic human teeth (maxillary left second premolar: #25, maxillary left first molar: #26, maxillary left second molar: #27) was prepared simulating a section of the jaw. Samples were made with extracted human molars (Reference), crowned implants (Implant), or crowned resin tooth analogues (Tooth). Crowns (tooth #36; n = 16/material) were milled from lithium-disilicate (Li, IPS e.max CAD) or 3Y-TZP zirconia (Zr, IPS e.max ZirCAD, both Ivoclar Vivadent). Thermal cycling and mechanical loading (TCML) in the chewing simulator were applied simulating 15 years of clinical service. Wear traces were analyzed (frequency [n], depth [㎛]) and evaluated using scanning electron pictures. Wear results were compared by one-way-ANOVA and post-hoc-Bonferroni (α = 0.05). RESULTS. After TCML, no visible wear traces were found on Zr. Li showed more wear traces (n = 30-31) than the reference (n = 21). Antagonistic teeth #26 showed more wear traces in contact to both ceramics (n = 27-29) than to the reference (n = 21). Strong wear traces (> 350 ㎛) on antagonists and their adjacent teeth were found only in crowned groups. Abutment type influenced number and depth of wear facets on the antagonistic and adjacent teeth. CONCLUSION. The clinically relevant model with human antagonistic and adjacent teeth allowed for a limited comparison of the wear situation. The total number of wear traces and strong wear on crowns, antagonistic and adjacent teeth were influenced by crown material.

A Study on the Wear of Artificial Resin Teeth (수종 레진 인공치의 마모도에 관한 연구)

  • Lee, Jung-Oh
    • Journal of Technologic Dentistry
    • /
    • v.20 no.1
    • /
    • pp.51-60
    • /
    • 1998
  • The artificial resin teeth used for removable prosthesis have good physical properties, but they have great wear rate. The purpose of this study is to compare the wear characteristics of several artificial resin teeth, such as Myerson teeth(Myerson Crop), Trubite IPN(Dentsply), Endura Posterio(Shofu), SROrthosit(Ivoclar), Trubite Biotone(Dentsply), Five samples of each resin tooth were abraded against natural teeth, type III gold for 150,000 cycles on the wear machine. The results obtained were as follow 1. The wear rate of artificial resin teeth when opposing enamel was the lowest in Myerson teeth($8.60{\mu}m$), followed by Trubite IPN($41.30{\mu}m$), Endure poster($63.00{\mu}m$), SR-Orthosit($68.40{\mu}m$), Trubite Biotone($209.90{\mu}m$) 2. The wear rate of artificial teeth when opposting type III gold specimens was the lowest in Myerson teeth($13.50{\mu}m$) followed by Endura Posterio($14.75{\mu}m$), Trubite IPN($53.40{\mu}m$), SROrthosit($54.20{\mu}m$), Trubite Boitone($341.50{\mu}m$)

  • PDF

COMPARISON OF THE PHYSICAL PROPERTIES OF FOUR KINDS OF ACRYLIC RESIN DENTURE TEETH (4종 아크릴릭 레진 인공치의 물리적 성질에 관한 비교)

  • Hwang, Jong-Woo;Chung, Chae-Heon;Ko, Yeong-Mu
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.33 no.2
    • /
    • pp.210-230
    • /
    • 1995
  • To compare the wear resistance of four kinds of commercial acrylic resin teeth [SR-Orthosit PosterioresR(Ivoclar Co., Liechtenstein), Endura PosteriorR(Shofu Inc. Japan), trubyte IPN teethR(Dentsply International Inc., York,), Trubyte BiotoneR(dentsply Inermational Inc. Brazil) by means of the toothbrush abrasion method, the artificial resin teeth were embedded in epoxy resin with the occlusal surfaces aligned in one plane for a total of 40 blocks. There after, each lock was mounted in the arm of the toothbrush abrasion machine(K 236, Japan). Wear measurements were made on the three preconditioned states. Those were as follows : no treatment specimens, thermocycled specimens, and thermocycled specimens which were immeresed applied load of 400g during the buring the brushing cycle. At the end of the 30,000-stroke cycle, each specimen was removed, and weighed. The microhardness of four kinds of commercial resin teeth were determined by means of microhardness tester. Microhardness tests were performed on te no treatment specimens, thermocycled specimens, and thermocycled specimens with immersion in the denture cleansing solution. Finally, the comparison of thermal properties were perfomed using differential scanning calorimeter(DSC-1500). The following results were obtained : 1. In the case of no treatment teeth, the wear amount of endura Posterior(EN) was the greatest among the others(p<0.01), and the wear amount of three kinds of artificial resin teeth was increased in the order of Trubyte IPN teeth(IN), Trubyte Biotone(BN), SR-Orthosit Posteriores(SN) but there was no statistic significance(p>0.01). 2. The wear amount of Trubyte IPN teeth(IT) and Trubyte Biotone(BT), was increased due to thermocycling effect, but that of Endura Posteriores(ET) was decreased conversely(p<0.01). 3. Except for the SR-Orthosit Posteriores(STC), the wear amount of three kinds of artificial resing teeth(that is, ETC, ITC, BTC) was increased due to denture cleansing solution$(Cledent^R)$, but there was no statistic significance(p>0.01). But the wear amount of the SR-Orthosit Posteriores(STC) was the greatest among the others(p<0.01). 4. The wear amount of toothbrush was the greatest in case of contact with occlusal surface of SROrthosit Posteriores resin teeth(p<0.01). 5. the microhardness values(KHN) of the SR-Orthosit Posteriores was the highest among the experimental artificial resin teeth(p<0.01). 6. There was no relationship between microhardness valuse(KHN) and wear amount of four kinds of experimental artificial resin teeth(p<0.01). 7. The differential canning calorimetric property of four kinds of artificial resin teeth did not show endothermal or exothermal peak in the range of $100^{\circ}C$

  • PDF

Wear Characteristics of Plastic Pinion Against Steel Gear (플라스틱기어의 마멸특성에 관한 고찰)

  • 김충현;김영민;안효석;정태형
    • Tribology and Lubricants
    • /
    • v.16 no.5
    • /
    • pp.324-331
    • /
    • 2000
  • Wear characteristics of Plastic and Nylon pinions against steel gear were studied to gain a better understanding of their tribological behaviors. Wear tests were conducted with power circulating gear test rig under dry contact conditions. Specific wear rates were measured as a function of applied load and the number of revolution. The worn teeth surfaces were examined with a profile projector and a camera. Nylon pinion showed lower specific wear rates than acetal pinion, but suffered teeth breakage under high load per unit tooth width. The dominant wear mechanisms found were adhesion and abrasion.

Development of Polycrystalline Diamond Tungsten Carbide Combination Circular Saw and Comparison of Tool Wear (PCD 초경 복합 원형 톱 개발과 공구마모 비교)

  • Joo, Chang-Min;Park, Yoon-Ok;Kim, Su-Jin
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.9
    • /
    • pp.48-56
    • /
    • 2021
  • Tungsten carbide (WC) circular saws have been widely used to cut plywood. Recently, expensive polycrystalline diamond (PCD) were adopted to extend the tool life of circular saws. This study developed a PCD-WC combination circular saw and compared its performance with that of existing WC and PCD saws. Flank wear of WC saw blades and edge chipping of rectangular PCD was observed during the experiments. The PCD-WC saw replaced half of the chamfered teeth with PCD and applied tough WC for all rectangular teeth. In the experiments, edge chipping was not observed in rectangular WC teeth and the flank wear of chamfered teeth was decreased compared with that of conventional circular saws.

Preliminary Study on the Age Estimation through a New Scoring System of Tooth Wear

  • Young-Ku Kim;Hyung-Soon Lim;Seung-Ryeul Lee
    • Journal of Oral Medicine and Pain
    • /
    • v.17 no.1
    • /
    • pp.31-39
    • /
    • 1992
  • The authors evaluated the degree of permanent tooth wear in order to make the basic date that are necessary to estimate the age. 10443 teeth of 389 individuals with known age were selected to estimate the degree of tooth wear. The obtained results were as follows : 1. The degree of tooth wear was decreased in males and females with aging. (P<0.001) 2. The degree of tooth wear in males in higher than that of females.(P<0.05) 3. The decision coefficient increased gradually from anterior teeth to posterior teeth.

  • PDF

A study on the in-vitro wear of the natural tooth structure by opposing zirconia or dental porcelain

  • Jung, Yu-Seok;Lee, Jae-Whang;Choi, Yeon-Jo;Ahn, Jin-Soo;Shin, Sang-Wan;Huh, Jung-Bo
    • The Journal of Advanced Prosthodontics
    • /
    • v.2 no.3
    • /
    • pp.111-115
    • /
    • 2010
  • PURPOSE. This study was conducted to evaluate clinical validity of a zirconia full-coverage crown by comparing zirconia's wear capacity over antagonistic teeth with that of feldspathic dental porcelain. MATERIALS AND METHODS. The subject groups were divided into three groups: the polished feldspathic dental porcelain group (Group 1), the polished zirconia group (Group 2), and the polished zirconia with glazing group (Group 3). Twenty specimens were prepared from each group. Each procedure such as plasticity, condensation, and glazing was conducted according to the manufacturer's manual. A wear test was conducted with 240,000 chewing cycles using a dual-axis chewing simulator. The degree of wear of the antagonistic teeth was calculated by measuring the volume loss using a three-dimensional profiling system and ANSUR 3D software. The statistical significance of the measured degree of wear was tested with a significant level of 5% using one-way ANOVA and the Tukey test. RESULTS. The degrees of wear of the antagonistic teeth were $0.119{\pm}0.059\;mm^3$ in Group 1, $0.078{\pm}0.063\;mm^3$ in Group 3, and $0.031{\pm}0.033\;mm^3$ in Group 2. Statistical significance was found between Group 1 and Groups 2 and between Group 2 and 3, whereas no statistical significance was found between Group 1 and Group 3. CONCLUSION. Despite the limitations of this study on the evaluation of antagonistic teeth wear, the degree of antagonistic tooth wear was less in zirconia than feldspathic dental porcelain, representing that the zirconia may be more beneficial in terms of antagonistic tooth wear.

Full mouth rehabilitation of the patient with severely worn dentition: a case report

  • Song, Mi-Young;Park, Ji-Man;Park, Eun-Jin
    • The Journal of Advanced Prosthodontics
    • /
    • v.2 no.3
    • /
    • pp.106-110
    • /
    • 2010
  • The severe wear of anterior teeth facilitates the loss of anterior guidance, which protects the posterior teeth from wear during excursive movement. The collapse of posterior teeth also results in the loss of normal occlusal plane and the reduction of the vertical dimension. This case report describes 77-year-old female, who had the loss of anterior guidance, the severe wear of dentition, and the reduction of the vertical dimension. Occlusal overlay splint was used after the decision of increasing vertical dimension by anatomical landmark, facial and physiologic measurement. Once the compatibility of the new vertical dimension had been confirmed, interim fixed restoration and the permanent reconstruction was initiated. This case reports that a satisfactory clinical result was achieved by restoring the vertical dimension with an improvement in esthetics and function.